UV-microspectrophotometry of lignin and accessory compounds in wood cell walls of conifers
1999 - IRG/WP 99-20171
The distribution of lignin in the cell wall of conifer tracheids was determined by UV-VIS microspectro-photometer. Wood sections of one micron thickness were measured between the wavelength 240 and 700 nm. Spectral analyses revealed that the conifer lignin associated with the tracheid secondary wall and middle lamella is composed of guiacylpropane units which exhibit a characteristic UV absorption...
G Kleist, G Koch, J Bauch


Remediation of pentachlorophenol- and creosote-contaminated soils using wood-degrading fungi
1994 - IRG/WP 94-50021
Microbiological treatment of hazardous wastes has generally been associated with the use of bacteria. During the past decade a significant body of evidence has accumulated that demonstrates that fungi, in particular white-rot fungi, have the ability to degrade a wide range of hazardous organic compounds (xenobiotics) and thus might also be useful for treatment of materials contaminated with these ...
R T Lamar, T K Kirk


Fungi used in standard tests on the toxicity value of wood preservatives in various European countries
1975 - IRG/WP 255
The aim of the present paper is to make the comparative analysis of test fungi used in various European countries in order to define the toxicity value of wood preservatives against fungi of the Basidiomycetes class. Only the methods with national standard rank, present on the currently binding standards list are taken for consideration. The analysis of similarities and differences in the choice o...
J Wazny


Fungal Stain Development in Canadian Hardwood Logs
2004 - IRG/WP 04-10505
In most sawmills around the world, trees are harvested into logs and stored in the forest or in a log yard for a period of time before being sawn into lumber. These logs may be attacked by various pigmented fungi, which results in staining of the wood. Since hardwood species are used to a great extent in furniture manufacturing and in the making of other valuable wood products, the reduction of wo...
Dian-Qing Yang, M-C Bisson


Standardisation of sapstain tests - A challenge
1992 - IRG/WP 92-2403
In the last decade many new anti-sapstain products have been tested world-wide under laboratory and field conditions. Several extensive test programmes have been executed with different non-standardized test methods and procedures, with the result that the biological findings cannot be compared with each other. In this paper, gathered recommendations will be given in order to standardize test meth...
G Rustenburg, C J Klaver


Attempt for developing a new method for above ground field testing of wood durability
2000 - IRG/WP 00-20199
Field testing remains the most appropriate way for evaluation of wood preservatives or natural durability of wood species. Above ground tests are designed to answer specific questions concerning the outdoor utilisation of wood. Such methods supply additional information and confirm or reject preliminary laboratory results. The European standard (ENV 12037, "lap-joint") for assessment of the durabi...
N Terziev, M-L Edlund


Susceptibility of CCB treated wood to fungal colonization
2003 - IRG/WP 03-10492
CCB treated wood is generally resistant to all wood decay fungi. However, like CCA impregnated wood, susceptibility of CCB treated wood to copper tolerant fungi have been observed. The ability of various brown rot fungal hyphae to penetrate and overgrow the wood samples was investigated. Samples made of Norway spruce (Picea abies) were impregnated with 5 % CCB solution according to the EN 113 proc...
F Pohleven, U Andoljsek, P Karabegovic, C Tavzes, S A Amartey, M Humar


Variation in infection rates of blue-stain, mould and white rot tropical fungi on mixed light Malaysian woods
2000 - IRG/WP 00-10334
The modified 3-week FRIM laboratory method for screening of anti-sapstain formulations against three representative tropical fungi causing blue-stain (Botryodiplodia theobromae), mould (Paecilomyces variotii) and white rot (Schizophyllum commune) infection of sapwood species was used to examine the relative resistance of the sapwood of eight mixed light Malaysian woods, Scots pine (Pinus sylvestri...
A H H Wong, S Ahmad


Preventive effectiveness of petroleum derivatives against blue-stain fungi. Part 2
1993 - IRG/WP 93-30001
Solvex-Tar, a product derived from the distillation of petroleum could be suitable for the treatment against blue-stain fungi in wood used in exterior carpentry, due to its effectiveness as a fungicide. The aim of this work has been to optimize the application of this product, modifying it as necessary, so as to improve its physical characteristics without interfering with its preventive effective...
E Sanchez, M T De Troya, A M Navarrete, A Guijarro


Evaluation of fungal remediation of creosote treated wood
1998 - IRG/WP 98-50101-25
Biotechnological remediation of creosote treated wood may be of interest in connection with novel recycling processes. White rot fungi and/or their ligninolytic enzyme systems are supposed to be valuable tools for such processes. This paper reports about results achieved when creosoted wood was treated in solid substrate fermentation with selected white rot fungi after different extraction procedu...
K Messner, S Böhmer


Evidence for wood cell wall degradation by the blue stain fungus Botryodiplodia theobromae Pat
1994 - IRG/WP 94-10077
Botryodiplodia theobromae Pat., a world wide ubiquitous polyfagus sapstain fungus, was found able to destroy the cell walls of birch fibres (Betula verrucosa Ehrh.) but not Caribbean (Pinus caribaea var. hondurensis Barr. and Golf.) and Scots pine (Pinus sylvestris L.) tracheids. The fungus caused characteristic erosion of fibre cell walls similar to soft rot type 2; destruction of the S1 - S2 int...
O Encinas, G F Daniel


Using DNA probes to characterize the metabolic pathway of pigment production in several wood-staining fungi
1996 - IRG/WP 96-10146
During shipment and storage, lumber is susceptible to sapstain, a wood discoloration caused by fungi. Currently kiln drying and chemical applications are used to control sapstain. However, the chemicals used to protect wood have a broad range of action, and so can affect other organisms. In addition, in Canada most of these chemicals are under temporary registration. Thus there is a need to develo...
R Eagen, S Riecken, J Kronstad, C Breuil


In vitro sporulation of selected wood decay fungi
1978 - IRG/WP 190
Basidiospores produced axenically without laborious attention in the laboratory are useful in studies of wood decay initiation. Such spores presumably approach those collected from natural sporophores in size and germinability (Morton, 1964). Production of spores in vitro by inversion of cultures grown on 2% malt extract agar in deep glass dishes (100x80 mm²) has been the preferred method (Morton...
E L Schmidt, D W French


Wood extractives as carbon sources for staining fungi in the sapwood of lodgepole pine and trembling aspen
1995 - IRG/WP 95-10098
Wood discoloration by sapstaining fungi reduces lumber value. In Canada, the most commonly recorded sapstaining fungi belong to the genera Ophiostoma. This work evaluated the effect that Ophiostoma piceae, Ophiostoma ainoae, and Ophiostoma piliferum used the lipids present in the sapwood of lodgepole pine (Pinus contorta Dougl.) and trembling aspen (Populus tremuloides Michx.). Wood lipids, common...
Yong Gao, C Breuil


Moisture requirements and wood degradation of pine and spruce wood by some Basidiomycetes-fungi
1989 - IRG/WP 1406
The minimum moisture requirements for the growth of the brown rot fungi, Coniophora puteana, Gloeophyllum trabeum and Serpula lacrymans were near or above the fibre saturation point of pine and spruce, sap and heartwood, during 160 days incubation according to the standard method EN 113. The moisture of wood for the optimum growth of Coniophora puteana and Serpula lacrymans was about 35-80% and fo...
H Viitanen, A-C Ritschkoff


Durability of Wood Plastic Composites Relative to Natural Weathering and Preservative Treatment With Zinc Borate
2005 - IRG/WP 05-40316
Wood-Plastic Composites (WPCs) used for decking have experienced dramatic increases in North America, averaging 25% growth per annum since 1998. A key factor contributing to this growth has been the successfully communicated message that they are "virtually maintenance free". The common perception being that the wood fiber is completely encapsulated by the thermoplastic resin, minimizing the pot...
M E Mankowski, F M Ascherl, M J Manning


Using image analysis to rate wood stain trials
1993 - IRG/WP 93-10034
Assessing the extent of fungal discoloration on wood during laboratory trials is a subjective process which provides an opportunity for considerable variation between individual evaluators of specimens. The development of reliable systems for automatically assessing discoloration would minimize evaluator bias and permit comparisons between results from different laboratories. The use of image anal...
C M Sexton, A G Maristany,C C Brunner, J J Morrell


Decrease in the mechanical resistance of blue stained and "orange stained" Pinus radiata wood
1999 - IRG/WP 99-10313
It is recognised that sapwood attacked by Ceratocystis pilifera increases its permeability to pressure preservative treatments. Since hiphae not only utilise pits, but also the cell wall for crossing from one cell to another, the mechanical resistance of the stained wood might be affected. The orange colour very commonly present in Pinus radiata logs heartwood under water sprinklers, has not recei...
M C Rose, L Reyes, J Alvarez, A Andaur, C Beltran, D Rivera


Changes in pore structure and cell wall volume in wood decayed by brown- and white-rot fungi
1991 - IRG/WP 1501
Sweetgum (Liquidambar styraciflua L.) wood blocks were decayed by Postia (=Poria) placenta or Phanerochaete chrysosporium in soil-block cultures. Decay was terminated at various weight losses, and the pore volumes available to probes of various molecular weight and diameter were determined by the solute exclusion technique (Stone, J.E. and A.M. Scallan. 1968. Cellulose Chem. Technol. 2, 343-358.)....
D S Flournoy


The fungal degradation of quaternary ammonium compounds in wood
1998 - IRG/WP 98-10263
This work focuses on the biodegradation of didecyldimethylammonium chloride (DDAC) by the mould fungus Gliocladium roseum within a woody matrix. Three sawdust types, distinguished by their treatment and amount of DDAC retained, were inoculated with the fungus and their DDAC loss was measured over 11 weeks. The rates of degradation varied depending on the sawdust; however, a significant loss of DDA...
J W Dubois, J N R Ruddick


Preventive effectiveness of petrol derivatives against blue-stain fungi
1992 - IRG/WP 92-3716
A possible application of fractions obtained on petrol pyrolysis is their use as a wood preservative against wood-decay and sap-stain fungi. From two of these fractions were prepared three different products (ST, STL and SST). The aim of this work has been the possibility of utilizing these products in the treatment of wood used for external joinery, determining their effectiveness against blue-st...
A M Navarrete, M T De Troya, E Sanchez, A Guijarro


An attempt to develop a direct and reliable method for testing the preventive action of preservation treatments of wood against fungal decay
1980 - IRG/WP 2139
In wood preservation there are two classical ways for assessing the reliability of preventive treatments against wood decay: the laboratory tests in which the various parameters are evaluated independently and the field tests or service tests in which those parameters are acting together in the natural environment. One has always tried to build bridges between the two types of experiments and to e...
M Fougerousse


Soft rot decay of Belian (Eusideroxylon zwageri) wood
1995 - IRG/WP 95-10119
The heartwood of Belian (Eusideroxylon zwageri), an East Malaysian timber species, is naturally durable due to its certain unique anatomical features and high content of extractives. The timber can tolerate years of exposure to hazardous conditions in ground contact and other situations without any significant loss in its strength. A few Belian transmission poles sampled from one locality in Saraw...
A H H Wong, A P Singh


Environmentally benign biological wood preservatives by Streptomyces rimosus, SC-36
1997 - IRG/WP 97-10196
Microbiocides obtained from mutant culture Streptomyces rimosus SC-36 were evaluated for their abilities to inhibit the growth of brown-rot, soft-rot, white-rot, and sapstain fungi on wood. The test fungi were the brown-rot fungi Antrodia carbonica, Gloeophyllum trabeum, Neolentinus lepideus, and Postia placenta; soft-rot fungi Chaetomium globosum, Paecilomyces variotti, Phialocephala dimorphospor...
S C Croan


Effect of fumigant residue in aerated wood blocks on the spore germination of decay fungi
1991 - IRG/WP 2382
Fumigants are increasingly used in several countries for remedial treatments of transmission poles to increase the service life. The present study was initiated primarily to test the remaining toxic effects of spruce (Picea rubra) wood, fumigated with chloropicrin (trichloronitro methane) or MIT (Methyl isothiocyanate) after long period of aeration, on the spore germination of decay fungi. This st...