Durability of exterior natural wood finishes in Brazil
1985 - IRG/WP 3343
Wood finishes systems were evaluated in natural weathering conditions during 5 (five) years, over "Parana-pine" (Araucaria angustifolia). Test samples results show that: - Semitransparent wood preservative stains, based on polimerized linseed oil, provided very good protection to the wood, compared with the one based on alkyd varnish; - Solid color wood preservative stains provided good durability...
D R Macedo


A novel solvent penetration assessment technique for wood preservativation treatments using waterborne systems
1990 - IRG/WP 2346
Solvent and hence solute (a.i.) penetration during any wood preservation treatment cycle and the flow pathways taken by the solvent in the wood are crucial elements in determining the adequacy of any treatment. Inadequate solvent penetration into specimens or an inappropriate tissue throughflow pattern during impregnation will markedly affect the distribution pattern achieved by many non-diffusibl...
A J Pendlebury, J Coetzee, E Sorfa, A Botha


Recycling CCA-treated poles with Charterm
2005 - IRG/WP 05-50224-17
After 10 years of Research and Development, the first “Chartherm” industrial unit is now operating since nearly half a year, thanks to Thermya SA, engineering company, current owner of all the “Chartherm” process Patents and Rights. In accord with the recycling contracts signed with several French major companies, the “Chartherm” plant, located near Bordeaux, recycles every day severa...
J-S Hery


Natural durability of fifty species of Indian timber in Goa waters against marine wood-borers
1989 - IRG/WP 4150
Results of the investigations on the natural durabilitv of fifty species of Indian timber, based on data collected bv exposing test panels at Betim near Panaji (Goa) continuously for a period of 11 months are presented. The study revealed that none of the timber species tested has any natural resistance at this locality and all the panels were completely destroyed within 11 months. Details on the ...
L N Santhakumaran, S Udaya Bhaskar, J C Jain


A comparison between different accelerated test methods for the determination of the natural durability of wood
1996 - IRG/WP 96-20099
According to the European standard EN 350-1 the natural durability of wood is defined as: "the inherent resistance of wood to attack by wood destroying organisms". This standard also describes how, for certain hazard classes, the durability is determined. The two methods described in this standard are the kolleflask method (EN 113) and the field-stake-test method (EN 252). The EN 113 test gives re...
H Militz, S G L Michon, J E Polman, M Stevens


An example of media response to perceived environmental problems with CCA-treated wood
1990 - IRG/WP 3564
A recent study suggested that CCA-treated wood exposed to acidic precipitation could lose significant amounts of copper chromium and arsenic resulting in loss of efficacy and possible environmental contamination. The study received wide newspaper and radio coverage in Canada, thereby heightening public concern about CCA use. Subsequent studies in our laboratory confirmed that the high losses were ...
P A Cooper


Borate diffusion in wood from rods and liquid product. Application to laminated beams
1988 - IRG/WP 3482
In the aim to use borate preservatives (fused rods and boracol) in fields of building construction other than external joineries, tests of diffusion of borate rods and secondary boracol, were carried out on different species of woods exposed to different moisture conditions. Tests were also applied on laminated beams very often subjected to high moisture contents and thus decay of rot fungi. Diffu...
D Dirol


Non-destructive stress wave measurement of decay and termite attack in experimental wood units
1986 - IRG/WP 2256
The purpose of this study was to determine if stress wave analysis could be used to monitor the degradation of wood specimens exposed to the brown-rot decay fungi (Gloeophyllum trabeum) and of wood specimens subjected to attack by subterranean termites. One hundred fifty 3/4 by 3/4 by 12 in. Southern pine specimens were used for exposure to brown-rot decay fungi and two hundred twenty-five 3/4 by ...
R F Pellerin, R C De Groot, G R Esenther


Remediation of CCA-treated wood by chitin and chitosan
2005 - IRG/WP 05-50229
Chitin and chitosan are naturally abundant biopolymers which are interest of to research concerning the sorption of metal ions since the amine and hydroxyl groups on their chemical structures act as chelation sites for metal ions. This study evaluated the removal of copper, chromium, and arsenic elements from chromated copper arsenate (CCA)-treated wood via biosorption by chitin and chitosan. Expo...
S N Kartal, Y Imamura


Bacteria are important degraders of cooling tower timbers: New Zealand experience
1995 - IRG/WP 95-10128
Microscopic examinations of CCA-treated Pinus radiata timbers in industrial cooling towers in New Zealand showed bacteria and soft rot fungi to be primarily responsible for the decay of these timbers. Of these micro-organisms, erosion bacteria appeared to be most widespread, attacking wood cell walls independently as well as together with tunnelling bacteria and soft rot fungi. Tunnelling bacteria...
A P Singh, R N Wakeling


Severe decay damages of bridges made of ekki (Lophira alata) wood known as a durable species
2000 - IRG/WP 00-10383
Bridges made of ekki (azobe, bongossi, Lophira alata Banks et Gaertn.) timbers were severely decayed only 10 years after the construction possibly caused from no maintenance for the periods. The reason of no maintenance is due to the misunderstandings on wood durability against wood-decaying fungi. Some civil-engineers and architectures understand "durable species" means "absolutely decay-durable ...
S Doi, T Sasaki, Y Iijima


An evaluation of the efficacy of a chlorothalonil formulation and a chlorothalonil plus chlorpyrifos formulation in the field
1993 - IRG/WP 93-30005
Details on the treatment of Pinus radiata D. Don and Eucalyptus regnans F. Muell. sapwood specimens to three retentions of each of two preservative formulations (chlorothalonil in oil; chlorothalonil plus chlorpyrifos in oil) and their installation below ground at three field test sites in Australia are given. Specimens were treated with each formulation to achieve 3.2, 6.4 and 12.8 kg/m³ of chlo...
J W Creffield, N Chew


NIR spectroscopy for rapid estimation of decay resistance
2004 - IRG/WP 04-20294
In Scandinavia Scots pine (Pinus sylvestris L.) is an important commercial tree species. Its heartwood has traditionally been used in constructions exposed to risk of decay. In a laboratory experiment Scots pine wood specimens sampled from inner heartwood, outer heartwood and sapwood were exposed to the brown rot fungus Poria placenta. In general outer heartwood was more resistant than inner heart...
P O Flæte, E Ystrøm Haartveit


The influence of fungi causing blue – stain on absorptiveness of Scotch pine wood
2005 - IRG/WP 05-10565
The blue-stain fungi cause discoloration of the wood. In the course of their development in wood may have an effect on wood structures and properties influenced on its use value. Investigation has been undertaken to clear the influence of blue-stain fungi on wood absorptiveness as indicators for the wood ability to impregnation with water diluted wood preservatives. The wet sapwood samples of fres...
A Fojutowski


Cellular and fractural failure after supercritical fluid impregnation of four wood species
2004 - IRG/WP 04-10503
Supercritical fluids (SCFs) have been investigated for delivering biocides into sawn wood. Pressure differentials during treatment may exceed the compressive or tensile strength perpendicular to grain, creating a potential for transverse deformations that exceed elastic strain limits. Wood treated by SCF processing with CO2, a potential biocide carrier, was inspected macroscopically and microscopi...
M E Anderson, R J Leichti, J J Morrell


Advances in understanding the mode of action of methylene bisthiocyanate against Sphaeropsis sapinea
2002 - IRG/WP 02-30284
The importance of arresting sapstain pre-infection in radiata pine in New Zealand, to prevent downstream sapstain in both logs and sawn timbers has been clearly demonstrated. Efforts are being made to improve the efficacy of diffusible antisapstain agents through improved understanding wood/fungicide/fungus interactions. The mechanism of action of methylene bisthiocyanate (MBT) was investigated u...
T Singh, R N Wakeling, B Kreber, A Stewart


Biological resistance of wood treated with waterbased resins and drying oils in a mini-block test
1998 - IRG/WP 98-40107
In recent years it was found that the resistance of wood against fungal degradation could be increased by impregnation with an etherificated melamine formaldehyde resin. Using this resin as a reference, a waterbased fatty acid modificated alkyd-resin and two drying-oils were assessed for their biological performance in a mini-block laboratory test. Although drying-oils, like linseed-oil, are often...
M Sailer, A O Rapp, R-D Peek


Laboratory and Pilot Evaluation of Chlorothalonil Formulations for Mold and Stain Control on some Wood Species
2003 - IRG/WP 03-30317
Laboratory and pilot test of the efficacy of several fungicides such as chlorothalonil and carbendazim for control of mold and sap- stain on bamboo and slash pine and rubberwood were conducted in this paper. The result indicates that: -- Clorothalonil/carbendazim are more effective for controlling mold and stain than that of carbendazim alone in laboratory test. --Higher concentration at 0.1-0.2...
Mingliang Jiang, Zhaobang Li


Treatment of poplar plywood with solvent and water-borne preservatives
1989 - IRG/WP 3538
Poplar as a light hardwood is appropriate for plywood production. Owing to its low natural durability it is generally recommended to preserve it in all conditions where risks of fungal attack may be present. A research project has been carried out on preservative treatments of plywood commodities. Parameters studied were various treatment cycles, three types of plywood, and a number of solvent and...
J Van Acker, M Stevens


Temperature tolerance of Botryodiplodia theobromae causing sapstain on rubber wood
1998 - IRG/WP 98-10259
Botryodiplodia theobromae Pat. is the dominant fungus causing sapstain on tropical timbers. Rubber wood (Hevea brasiliensis) is highly susceptible to sapstain infection. The tropical warm-humid climate also influences the growth of B. theobromae on rubber wood. Additionally, the moisture content of timber provides conducive conditions for the entry and establishment of the fungus. Temperature tole...
E J M Florence, J K Sharma, R Gnanaharan


Laboratory testing of wood natural durability - In soil-bed assays
1998 - IRG/WP 98-20141
Laboratory methods for assessing wood decay resistance are being investigated in the framework of an ongoing European research project. This paper summarizes the main results obtained for soil-bed tests based on the European prestandard ENV 807-Test 2. The data suggest that this testing methodology is suitable for evaluating the natural durability of timber species in soil-contact under conditions...
R Sierra-Alvarez, I Le Bayon, J K Carey, I Stephan, J Van Acker, M Grinda, G Kleist, H Militz, R-D Peek


Effect of humic acid on leaching of CCA from treated wood
2000 - IRG/WP 00-50151
Laboratory studies indicate that relatively high concentrations (1.000 - 10.000 ppm) of humic acids can increase the leaching of chromium and copper from CCA-C treated wood, and that copper is most affected. They also show that leaching with natural water samples can result in higher leaching of all components than leaching with distilled water. Evaluation of CCA component retentions and mass bala...
P A Cooper, D Jeremic, J L Taylor, Y T Ung


Decay resistance of Platanus acerifolia wood against White Rot Fungi (Coriolus versicolor)
2002 - IRG/WP 02-10431
Degradation of the lignocellulose complex in wood varies on the microorganism causing decay and chemical composition of wood. The weight loss of Platanus acerifolia wood after decay by white rot fungus (Coriolus versicolor) for period 16 weeks were evaluated according to European standard EN 113 and beech wood as a control. The samples were collected in October 2000 from Nantes, France. The aim of...
M Irmouli, O Duchelier, N Ayadi, B Charrier


Water-storage for improving the permeability of sugi (Cryptomeria japonica D. Don)wood
1999 - IRG/WP 99-40129
The viable bacterial counts in sapwood and intermediate wood of sugi bolts increased immediately after floated in a fresh water pond. Bacterial invasion into the heartwood was not detected apparently during water-storage for 36 weeks, although a few bacterial species have inhabited in freshly-cut heartwood samples. The bacterial species isolated from the water-stored bolts were almost Gramnegative...
S Ohta, S Doi


Effect of vapour boron treatment on mechanical properties of wood based board materials
1992 - IRG/WP 92-3727
The mechanical properties of Medium density fibre board, Chipboard and Oriented strand board were investigated after treatment to two retention levels of boric acid applied as a vapour phase system. A range of mechanical properties were investigated. The vapour boron treatment does not have any significant effect on most of the mechanical properties of the boards. The exception is a reduction in i...
R Hashim, D J Dickinson, R J Murphy, J Dinwoodie