IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3213 documents. Displaying 25 entries per page.


Studies on the resistance of DMDHEU treated wood against white-rot and brown-rot fungi
2005 - IRG/WP 05-10566
Beech wood (Fagus sylvatica) modified with the textile finishing agent 1,3 dimethylol-4,5-dihydroxyethylen urea (DMDHEU) has shown to improve durability against the white-rot fungus Trametes versicolor. In a mini-block test, the weight loss over eight weeks of incubation decreased with increasing weight percent gain (WPG) of DMDHEU. At 25% WPG, no significant weight loss was observed, while untrea...
P Verma, C Mai, A Krause, H Militz


X-ray photoelectron spectroscopic analysis of CCA treated wood
1992 - IRG/WP 92-3700
Ponderosa pine and Douglas-fir wood sections were treated with CCA preservative. To elucidate the mechanism of fixation of the CCA, the wood surface was analyzed by X-ray photoelectron spectroscopy (XPS). CCA treatment increased C1 (carbon bonded to carbon and/or hydrogen) and decreased C2 (carbon bonded to one oxygen) in XPS C1s spectra, both in unextracted and pre-extracted sections. This sugges...
J N R Ruddick, K Yamamoto, P C Wong, K A R Mitchell


Destaining wood sapstains caused by Ceratocystis coerulescens
1996 - IRG/WP 96-10159
Fungal sapstain does not reduce the strength of wood, but it does discolor the wood, detracting from its appearance and decreasing the value of wood and wood products. The purpose of this investigation was to assess whether wood sapstain caused by Ceratocystis coerulescens could be destained and existing growth eradicated. The hydroxyl radicals generation under optimized conditions destained the s...
S C Croan


Environmental risk assessment of treated wood - A mesocosm study
2005 - IRG/WP 05-50224-8
In order to evaluate the environmental impact of treated poles, we have developed physical models (mesocosms) containing around 250 kg of natural soil and a treated pole. On the top of each mesocosm, a spraying mechanism, which can distribute ultrapure water through several nozzles, was built. On the lower part of each mesocosm, a small tank, which can contain some litres of leachate, was placed...
P Marchal, F Poly


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 6: Report of third inspection (24 months) in Australia
1980 - IRG/WP 456
This report presents the results of the third inspection of the IRG/COIPM International Marine Test specimens installed at the Goat Island Marine Biological Station of the Maritime Services Board of New South Wales, in Sydney Harbour. The inspection was completed on 5th December, 1979, after 24 months exposure. As on previous occasions, this inspection was carried out in conformity with the provis...
J Beesley


Tendency of the preservative use for impregnation industries in Japan
1998 - IRG/WP 98-50101-05
In Japan, since 1997, the acceptable limit of the arsenic in the waste water become to 0,1 mg/l and the additional regional severer restriction can be established. In this reason, Japanese wood preservation industries intend to use other than CCA, like DDAC, ACQ, Tanalith CuAz, copper-naphthate and zinc-naphthenate, as replacing from CCA. In Jan-June 1997, the share of CCA preservatives was less t...
K Suzuki


A field method for determining the above-ground resistance of wood and wood products to attack by subterranean termite
1994 - IRG/WP 94-20035
A method for determining the above-ground resistance of wood and wood products to subterranean termites in the field is described. Termites are aggregated in 20-litre steel drums, each containing a highly susceptible timber substrate. At the centre of each drum, specimens of the test material under evaluation are sandwiched, using circular sections of wire mesh, between two layers of the substrate...
J W Creffield


Evaluation of bacteria for biological control of wood decay
1990 - IRG/WP 1426
Laboratory soil-block and agar-block tests were carried out to evaluate the efficacy of bacteria as biological control agents against 5 brown-rot and 3 white-rot fungi. Pretreatment of Southern pine and sweetgum with a bacterial solution prevented decay in agar-block tests. However, the bacteria were generally ineffective in preventing decay in Southern pine, Douglas-fir, sweetgum and yellow popla...
R Benko, T L Highley


Evaluation of chlorpyrifos and fungicides alone and in combination for control of insects and fungi in wood and wood composites
1998 - IRG/WP 98-30187
Wood composites are rapidly being adapted for use in exterior applications. The incorporation of a preservative system to prevent fungus and insect attack is necessary with most exterior composites. Research studies were reviewed pertaining to organic preservative systems based on Lentrek* insecticide wood treatment which contains the active ingredient chlorpyrifos alone and in combination with te...
M P Tolley, P E Laks, R Fears


Evaluation of wood durability by laboratory test - A new equation to predict wood durability
2001 - IRG/WP 01-20230
To estimate the wood durability in a short term, periodical weight determination was carried out in a laboratory test. This test provided the results comparable to those of the field test and the fungus cellar test, but it required much more jobs in comparison to the usual accelerated laboratory test. To save the time and jobbing for this method, a new equation was devised from simple two assumpti...
I Momohara, K Yamamoto


Why did Japan replace CCA by alternatives?
2004 - IRG/WP 04-50215
Since chromated copper arsenate (CCA) was technically introduced into Japan in 1963, CCA was used for extending service life of various wood commodities, especially sill plates (dodai) in Japanese houses. However, the problem on the disposal of CCA-treated wood waste became public and related industry concern, and questionnaire survey conducted by Japan Wood Preservers’ Industry Association ind...
H Ishida, T Ito, M Yamai, H Matsusaka, K Tsunoda


Degradation features of waterlogged archaeological compression wood
1998 - IRG/WP 98-10258
The degradation characteristics of waterlogged archaeological compression wood excavated in South Korea were examined by transmission electron microscopy (TEM) and confocal laser scanning microscopy (CLSM). Degradation of Pinus compression wood occurred mainly in the inner part of S2 layer. In contrast, the outer part of S2 layer remained relatively intact. CLSM and TEM showed the erosion type of ...
Yoon Soo Kim, A P Singh


A study on the pressure impregnation of Eucalyptus globulus fence-posts with CCA preservatives. Part 2
1989 - IRG/WP 3514
This paper describes the second part of a study on pressure impregnation of Eucalyptus globulus fence-posts with CCA preservatives presented at the IRG 19th Meeting. Fence-posts of three diameter classes, were treated, considering only one treatment schedule. The results show possibility of vacuum-pressure impregnation of blue gum fence-posts, with diameter less than 9 cm, though mainly by longitu...
L Nunes, D De Sousa Castro Reimão


Protection of southern pine using N,N-Napthaloylhydroxylamine: Field tests, soft-rot cellars and aquatic bioassay leach testing
1999 - IRG/WP 99-30204
Recent environmental restrictions are limiting the use of broad-spectrum biocides for wood preservation. There is an urgent need for new, sharply targeted, environmentally benign wood preservatives. N'N-Napthaloylhydroxylamine (NHA), a water-soluble calcium-precipitating agent, has been shown to inhibit decay by brown-rot and white-rot fungi in soil-block tests and prevent damage by Easte...
D M Crawford, F Green III


Effectiveness of the new chemical wood preservative Borosol 9? against a house longhorn beetle Hylotrupes bajulus
2004 - IRG/WP 04-30355
Chemical wood preservative Borosol 9, consisting of boric acid - alkanolamine complex, is a new wood preservative with proven efficacy against wood decay fungi. However, we were interested in its efficacy against larvae of house longhorn beetle (Hylotrupes bajulus). Thus, experiment according to the EN 46 procedure was performed. Specimens made of Norway spruce wood (Picea abies) were ...
G Babuder, M Petric, F Cadež, M Humar, F Pohleven


Suitability of cyfluthrin in wood protection
1992 - IRG/WP 92-3735
Cyfluthrin, a well-known and in agriculture and household widely used insecticide based on synthetic pyrethroides, is evaluated now concerning its suitability as insecticide in wood protection. An overview about the physical and chemical properties is given. Test results in accordance with European standards show the high efficacy and broad-spectrum activity of Cyfluthrin against wood rotting inse...
H-U Buschhaus


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 14: Report of fifth inspection (48 months) in Australia
1982 - IRG/WP 484
This report presents the results of the fifth inspection of the IRG/ COIPM Internatlonal Marine Test specimens installed in Sydney Harbour in December, 1977. This inspection took place on 9th December, 1981, just 48 months after the specimens were installed. Earlier reports have contained full details of the treatment and installation of the specimens as well as results of all previous inspections...
J Beesley


Fungitoxic effect of the quaternary ammonium compounds preservatives against Basidiomycetes by using agar-plate and agar-block methods
1996 - IRG/WP 96-30118
Results of investigations on the fungitoxic value of three versions of wood preservatives based on the quaternary ammonium compounds (lauryldimethylbenzylammonium chloride, lauryldimethyl-benzylammonium bromide and alkylbenzyldimethylammonium chloride) and borates in relation to the wood destroying fungi have been presented. The agar-plate (screening) and agar-block method were applied. A wide ran...
J Wazny, P Rudniewski


Quantification of wood decay effects by HPLC analysis
1992 - IRG/WP 92-1576
The present work quantified the effects of the white rot basidiomycetes Coriolus versicolor and Phanaerochaete chrysosporium, and also those of the brown rot fungi Coniophora puteana and Lentinus lepideus, on Pinus patula and Eucalyptus grandis. Wood colonisation was quantified by Kjeldahl nitrogen determinations converted to biomass assays, and degradation was quantified by weight losses produced...
V Singh, M Tarin, G D Shelver, A A W Baecker


Analysis of contaminants in waste wood
2001 - IRG/WP 01-50179
Waste wood is increasingly used as fuel in Sweden. It is of Swedish origin as well as imported, Mainly from Germany and the Netherlands. The major chemical contaminants are surface treatments (paints etc) and wood preservatives. The surface treatments contribute in particular to contaminants of zinc and lead. In some cases zinc has been found to cause severe deposits in the furnaces. Surface treat...
J Jermer, A Ekvall, C Tullin


Combustion properties of Alder wood treated with some new environment friendly natural extractives. Part 1. Effect of Natural Tannins on the Combustion Properties
2002 - IRG/WP 02-40234
Powders of the brutia pine bark, sumach leaves, acorn, gall-nut and boric acid and borax which are known as potential environment friendly wood preservatives were impregnated according to ASTM D 1413-88 in order to determine their combustion properties. A commercial treatment compound, Tanalith-CBC, was also used for comparison. The results indicated that the natural extractives did not have an...
Ü C Yildiz, A Temiz, E D Gezer, S Yildiz


Treatability and natural durability of some lesser used or unused wood species of Bangladesh
2000 - IRG/WP 00-40170
A research study was conducted to determine the natural durability and treatability of heartwood of some lesser used or unused wood species. The treatability of species has been studied along with certain anatomical concepts association with preservative penetrability of the wood. It was observed that grain structure and presence of tyloses appeared to be correlated with penetrability of the wood....
K Akhter, M Younusuzzaman, M H Chowdhury


The influence of the location of a wood defect on the modulus of elasticity determination in wood durability testing
2004 - IRG/WP 04-20287
This study investigates the influence of the location of a wood failure in stakes upon elastic changes observed in beech specimens with the resonance vibration technique. Natural failures were simulated by artificially created defects at different locations of the test stake. The results indicate that the location of an attack in a stake is important for the measurement outcome. When the attack is...
L Machek, H Militz


Fungi causing sap stain in wood
1980 - IRG/WP 199
The present paper is a revised edition of former Document No: IRG/WP/125. It contains some additions and an explanation of terminology, as was suggested at a previous meeting of the Group. The paper is a compilation based mainly on available literature. Some of my own unpublished results have been added together with other unpublished data which have been received from the Bundesanstalt für Mater...
A Käärik


Influence of CCA and TnBTO on wood decay, under different oxygen levels and various initial moisture content
2001 - IRG/WP 01-10415
Fagus sylvatica (beech) and Pinus sylvestris (Scots pine) were impregnated by TnBTO (tributyl-tin oxide) and CCA (chromated copper arsenate). In wood blocks two levels of moisture content (50% and 100% of saturation point) were used. Three levels of oxygen concentrations (10, 21, and 50%) were chosen. Treated and untreated wood were exposed to three fungi (C. versicolor a white rot, C. puteana, a ...
S M Kazemi, R J Murphy, D J Dickinson