IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3213 documents. Displaying 25 entries per page.


Strength properties of preservative treated pine and spruce wood after super-heated steaming
1984 - IRG/WP 3313
Possible changes of strength properties of CCF pressure impregnated pine and spruce with subsequent steaming at 110°C respective 120°C for 30 min were examined. For spruce analysis of variance indicated that none of the processes had a significant effect on bending strength, compression strength and the corresponding modulus of elasticity as well as on impact bending strength and shear strength ...
R-D Peek


Soft rot decay in acetylated wood. Chemical and anatomical changes in decayed wood
2002 - IRG/WP 02-40231
Acetylated Beech (Fagus sylvatica) and Scots Pine (Pinus sylvestris) wood were studied in soil beds under laboratory conditions for longer periods. High mass losses and dynamic MOE losses were measured in non-acetylated wood and at lower weight percent gains (WPG). Rapid losses of lignin, holocellulose and ?-cellulose occurred in non-acetylated beech wood and no losses were detected at the highest...
B Mohebby, H Militz


Efficiency of wood impregnation processes
1980 - IRG/WP 3151
Many wood impregnation processes have been in use for a very long time, up to 150 years, but they have not been progressively modified. This paper considers impregnation processes in relation to current requirements, particularly impregnation efficiency and energy consumption. The term 'pore' is used throughout in its physical sense and is not confined to botanical 'pore...
B A Richardson


Microscopic characteristics of microbial attacks of CCA-treated radiata pine wood
1993 - IRG/WP 93-10011
Light and electron microscopic observations were made of CCA-treated radiata timbers, which had been placed in service in a vineyard soil as supporting poles and as part of a house pile, to determine the cause of their deterioration. The house pile had failed in service after between 9 and 13 years and was of particular interest because decay was more severe in deeper regions than at the surface a...
A P Singh, R N Wakeling


Blue Stain Testing of Alkyd and Acrylic Stains
2003 - IRG/WP 03-20273
Resistance against blue stain of semi-transparent alkyd and acrylic stains was tested by both EN 152 and the so-called reverse exposure test methods. Comparison of the results, obtained by both methods was the most important aim of this study. As expected, performance of the water-borne acrylic paint was lower compared to protective effectiveness of the alkyd stain. This difference was even more p...
M Petric, M Pavlic, B Kricej, M Humar, F Pohleven


Rapid analysis - chances and limitations
1999 - IRG/WP 99-50130
The reuse of wood out of service in the particle board industry demands a proper handling and separation of assortments with differing content and nature of preservative. A pre-selection based on visual and olfactorial characteristics can be carried out for certain assortments like sleepers, poles, etc. Problems arise from diffuse and less intensive treated wood which is regularly dip-treated or b...
A Peylo, R-D Peek


Use of wood-decay fungi for disposal of PCP-treated wood
1995 - IRG/WP 95-50040-33
Although PCP has been classified as a priority pollutant, PCP-treated wood products are currently allowed to be disposed of as ordinary solid (non-hazardous) wastes in the US. Non-regulated disposal of these materials is allowed because PCP concentrations in extracts from PCP-treated products such as utility poles and crossarms, determined by the Toxicity Characteristic Leaching Procedure (TCLP) h...
R T Lamar


Effect of wood species on decomposition efficiency of metham sodium
1992 - IRG/WP 92-3699
The effect of wood species and temperature on efficiency of metham sodium (32.1% sodium N-methyldithiocarbamate) decomposition to methylisothiocyanate (MITC) was investigated on 10 hardwoods and 9 conifers over a 144 hour period. Gas chromatographic analyses of headspace samples and ethyl acetate extracts of the wood revealed that decomposition never approached the theoretical decomposition effici...
J J Morrell


The full guideline for the “double layer test method” - A field test method for determining the durability of wood out of ground
2004 - IRG/WP 04-20290
This guideline describes a test method for wood to be exposed to the weather out of ground contact. The main objective of the method is to evaluate the durability of wood in above ground exposure as shifted overlaid stakes, which form the so called double layer. The method is applicable to the testing of untreated, treated and modified wood. Initially it was developed and found to be most useful ...
A O Rapp, U Augusta


A comparison of the leaching resistance of diammine-copper complexes and copper carbonate precipitated in wood
1997 - IRG/WP 97-30158
Previous studies have shown that during treatment of wood with ammoniacal copper solutions, both simple copper precipitates and diammine-copper complexes are formed. The objective of the present study is to determine the relative importance of both forms of copper, on such aspects as preservative leachability and biological performance. In the current experiment, the leachability of copper carbona...
Xiao Jiang, J N R Ruddick


Vertical distribution of fouling and wood-boring organisms in the Trondheimsfjord (Western Norway)
1981 - IRG/WP 476
Results of a detailed study on the vertical distribution of fouling and wood-boring organisme of Trondheimefjord at an interval of 3 m from intertidal level to a depth of 30 m, has been presented, based on data collected from two series of panels, exposed from 15-3-1977 to 15-7-1977 (Series I) and from 22-7-1977 to 13-3-1978 (Series II). The intensity of fouling generally decreased with increasing...
L N Santhakumaran


Risk of pulmonary damage as a result of an evaporation of ca. 50 ppb = 42 mg HF, evaporated from wood treated by difluorides
1987 - IRG/WP 3401
In this review of the literature the effects of fluorides and fluorine on man are described, especially the low level effects of inhaled HF on human beings. The term "fluoride" is used as a general term everywhere, where exact differentiation between ionic and moluecular forms or between gaseous and particulate forms is uncertain or unnecessary. The term covers all combined forms of the element, r...
H F M Nijman


On the effectiveness of fumigants against wood-destroying insects and fungi in wooden cultural property
1993 - IRG/WP 93-10030
Based on a survey of the history of the use of fumigants the actual agents are mentioned in relation to their biogenic effect on wood-destroying insects and fungi as well as their corrosive behavior on cultural property. Furthermore the conditions for the use of reactive fumigants in buildings are discussed. Trials to control wood-destroying insects and fungi by nitrogen and bromomethane are the m...
W Unger, A Unger


On-site test for indicative determination of leaching of components of preservatives from treated timber
1993 - IRG/WP 93-50001-12
In the late eighties the environmental concern about treated timber increased and it is still a hot issue in the Netherlands. From the environmental point of view three phases in the timbers life cycle can be distinguished: - the production phase - the service life - the waste phase. In the Netherlands at this moment much emphasis is laid on the production phase. In 1992 this has led to a new legi...
W J Homan, H Militz


Biochemical relationships between biodegradation of cellulose and formation of oxalic acid in brown-rot wood decay
1991 - IRG/WP 1472
Non-enzymic hydrolysis of cellulose with low concentrations of oxalic acid was examined. The incubation of pine wood pulp with 1% oxalic acid (pH 1.3) at 35°C for 4 weeks reduced the original viscosity to 60%. Reducing sugars were liberated from various cellulosic samples by the oxalic acid treatment. However, crystallinities of cellulose in those samples did not change before and after the treat...
M Shimada, Y Akamatsu, A Ohta, M Takahashi


Poplar wood and its damages in Iran
1987 - IRG/WP 1332
In Iran poplar planting has been used for many centuries ago specially in regions without forests. It had rural uses in ancient time, but recently many fast growing poplar species have been planted and many hybrids also have been planted; the following species had been cultivated widely in Iran: Populus nigra L. var. italica, Populus alba L., Populus caspica Bornm, Populus deltoides L., Populus X....
D Parsapajouh, P Niloufari


Biocidal screening method of wood extractives by a direct use of cellulose TLC plate
2001 - IRG/WP 01-20226
Most of the methods to evaluate the biological durability of woods have focused on decay fungi and termite as deteriorating organisms and it is well known that one of the most important factors affecting the biological characteristics of wood is extractives. Bioassays for evaluating the biological activities of wood extractives have been mainly conducted with treated filter papers for termites or ...
R Yusiasih, T Yoshimura, T Umezawa, Y Imamura


A rapid method for collecting large numbers of subterranean termites from wood
1982 - IRG/WP 1165
A corrugated fiberboard trap is described which attracts large numbers of subterranean termites from infested logs. Single-trap collections in excess of 63 grams (wet wt.) for Reticulitermes virginicus (Banks) and 43 grams for Coptotermes formosanus Shiraki were taken one to three days following discovery by termites. If traps are removed from the source logs shortly after beeing attacked, termite...
J P La Fage, N-Y Su, M Jones, T Lawrence


Establishing standard principles for laboratory bioassays of termiticides with subterranean termites - progress, problems and prospects
1993 - IRG/WP 93-10013
Laboratory bioassays of termiticides, including wood preservatives, aim to give an indication of the likely concentrations effective in preventing damage to timber products and other materials in the field. In laboratory bioassays field conditions should be simulated as closely as possible. With a wide range of procedures in use around the world it may often be difficult to compare results between...
M Lenz, J W Creffield, Zhong Yun-hong, L R Miller


Decay and termite durabilities of heat-treated wood
2004 - IRG/WP 04-40272
Decay and termite resistances of Plato-treated timbers were evaluated using a modified JIS decay test method, feeding test in a laboratory scale and a field exposure against Reticulitermes speratus (Kolbe) or Coptotermes formosanus Shiraki. The results showed that no significant decay durability of the treated timbers although mass loss from decay slightly decreased in case of treated timbers. ...
S Doi, K Hanataa, E Kamonji, Yuuji Miyazaki


A marine borer test with water-borne preservatives
1980 - IRG/WP 452
The use of preservative treated timber in sea-water where marine borers are active is of great economic importance, since untreated wood immediately will be damaged. Vacuum/pressure treated timber has been tested in several marine exposure trials on the Swedish west coast since the 1930s (Hager 1941, Hultman 1949, Sandstrom 1951, Nylinder-Norman et al. 1974). Since new interesting materials or pre...
B Henningsson, E Norman


Lethal temperature for some wood-destroying fungi with respect to eradication by heat treatment
1984 - IRG/WP 1229
The lethal heat dosis as a function of temperature and time of exposure has been tested for mycelium and for wood infested by three strains of Serpula lacrymans and by Coniophora puteana, Poria monticola, Paxillus panuoides, Gloeophyllum trabeum and Gloeophyllum sepiarium. Even for Serpula lacrymans, which is well known for its sensivity to heat treatment, 30 min at 55°C were necessary to kill th...
M Miric, H Willeitner


Analysis of D-glucose metabolism of wood decay fungi using 13C-NMR and 13C-labeled substrates
2003 - IRG/WP 03-10475
D-Glucose metabolism is thought to be important during wood decay by fungi, not only for anabolic and catabolic purposes of central metabolism, but also as a potential source of peroxide required by extracellular peroxidases. There has been some confusion in the literature as to whether this peroxide-generating activity is of the glucose 1-oxidase or pyranose 2-oxidase (glucose 2-oxidase) type wi...
T H de Koker, M D Mozuch, P J Kersten


Equilibrium distribution of toxic elements in the burning of impregnated wood
2001 - IRG/WP 01-50172
The current work focuses on predicting the behavior of arsenic, chromium, and copper in the burning of impregnated wood. A theoretical method is used to study the chemistry of the system, with special interest directed towards the vaporization tendency of the potentially toxic elements. The core of the study is the global equilibrium analysis that simultaneously takes into consideration all chemic...
K Sandelin, R Backman


Gas chromatographic determination of 1,8-naphthalimide, N-Hydroxy-1,8-naphthalimide (N,N-naphthaloylhydroxylamine) and the sodium salt of N-Hydroxy-1,8-naphthalimide
2003 - IRG/WP 03-20259
A number of naphthalimide (NI) derivatives are used as efficient laser dyes, in medicine or in scanning electron microscopy. Only N,N-naphthaloylhydroxylamine (NHA) has been shown to be an effective wood preservative against wood decay fungi and termite damage. However, limited information is available concerning the analytical detection of NI-derivatives in treated timber. There is a clear need ...
E Melcher, F Green III