Wood decay fungi from New Zealand ‘leaky’ buildings: PCR identification and laboratory decay tests of wood preservative-treated Pinus radiata (Part 1)
2007 - IRG/WP 07-10620
Fungi colonising Pinus radiata D. Don framing timber of ‘leaky’ New Zealand buildings were isolated to produce pure cultures. Mycelia from these cultures on agar media were collected to extract DNA. To identify the fungi to the species level, polymerase chain reaction (PCR) with primer pairs ITS1-F and ITS4 were performed followed by sequencing of the internal transcribed spacer (ITS) region. ...
D Stahlhut, R L Farrell, R Wakeling, M Hedley


Corrosion of metal fasteners in contact with copper preservative treated wood
2007 - IRG/WP 07-20370
The corrosion rates of metal fasteners in contact with alkaline copper quat (ACQ) treated wood with or without commercially available water repellent was compared to that of cedar. In this experiment, fasteners were sandwiched between two pieces of treated wood and exposed to a humid environment at a slightly elevated temperature. The use of a “sandwich” design allowed periodic examination of ...
BaekYong Choi, J N R Ruddick


Permethrin: A Critical Review of an Effective Wood Preservative Insecticide
2007 - IRG/WP 07-30413
Permethrin is a synthetic pyrethroid used in the wood preservation industry. The generally favorable environmental profile of pyrethroids coupled with their high efficacy led to their wide substitution of the chemically resistant organochlorines dieldrin, lindane, and chlordane formerly used for protection of buildings against wood destroying organisms. Much of the research on performance of perm...
M H Freeman, D N Obanda, T F Shupe


Efficacy of chitosan in combination with GRAS (Generally Recognised As Safe) compounds as a potential wood preservative
2007 - IRG/WP 07-30414
In vitro studies were undertaken to evaluate the synergy between chitosan and selected GRAS (Generally Recognised As Safe) compounds against two sapstain fungi Sphaeropsis sapinea and Leptographium procerum. Bioassays performed on nutrient medium suggested that some of the GRAS compounds tested including sodium benzoate, potassium sorbate and ascorbic acid had a synergistic effect when combined w...
C Chittenden, K Thämelt, T Singh


Silver – The Next Generation Wood Preservative
2007 - IRG/WP 07-30419
The successful introduction and commercial use of products designed to have controlled release of silver ion over long time periods prompted the Silver Research Consortium and the US Forest Products Laboratory to undertake research to see if silver could also be an effective wood preservative to be used in place of chromated copper arsenate (CCA) now prohibited for use in the United States and els...
J R Ellis, K Jayachandran, D Nicholas


Silver as a Wood Preservative Environmental Requirements and Concerns
2007 - IRG/WP 07-30420
The pesticide uses of silver and its compounds fall under the jurisdiction of the United States Environmental Protection Agency (USEPA) under the US Federal Insecticide Fungicide and Rodenticide Act. In addition, many other national and international organizations maintain close observance of the effects of silver in different environments. The US EPA has also issued a specific announcement that t...
J R Ellis


Use of Moisture Meters with Treated Wood
2007 - IRG/WP 07-40382
Drying wood treated with waterborne preservatives after treatment to near outdoor EMC conditions improves its physical performance characteristics. This is primarily due to the reduced checking, splitting and warping which can occur when wet wood, particularly if restrained from shrinking by being nailed or otherwise fastened, shrinks in use. Monitoring of the drying process, rate, and end point...
W B Smith, Hwan Myeong Yeo, C Stark, B Morey, C Tascioglu, P Schneider, D Herdman, M Freeman


Tropical In-Ground Durability of CCB-treated Keruing and other Structural Sarawak Timbers after 8 – 10 Years Exposure
2007 - IRG/WP 07-30439
The heartwood of 12 mainly low-durability native timber species of Sarawak [4 Dipterocarpus (Keruing) species, Anisoptera grossivenia (Mersawa kunyit), Canarium apertum (Seladah), Dacryodes incurvata (Seladah laut), Dryobalanops oblongifolia (Kapur kelansau), Mesua macrantha (Mergasing), Podocarpus micropedunculatus (Kayu cina), Shorea compressa (Engkabang langgai), and Pterospermum javanicum (Ba...
A H H Wong, Ling Wang Choon


Micro-Distribution of Metals in Wood Treated with a Nano-Copper Wood Preservative
2007 - IRG/WP 07-40360
The microdistribution of copper in southern pine treated with a newly-developed nano-copper wood preservative was examined to determine if it differed from that reported for wood treated with conventional copper-based wood preservatives. Field Emission Scanning Electron Microscopy (FE-SEM) in combination with x-ray microanalysis (EDX) revealed the presence of nano-sized copper and iron particles i...
H Matsunaga, M Kiguchi, P Evans


Durability of some alternatives to preservative-treated wood. Progress report 2: Results from field tests after 5 years’exposure
2007 - IRG/WP 07-30442
A number of alternatives to preservative-treated wood have been tested according to EN 252 (stake test) and a specially designed ground-proximity field test, the latter in Sweden as well as in Hawaii, USA. Seven untreated wood species and four alternative wood treatments labelled as environmentally friendly (acetylation, linseed oil, heat treatment, vinyl polymer) were included in the study. Four ...
M-L Edlund, J Jermer


Primary Study on Compressed Preservative-treated Wood (CPW) for Outdoor Applications
2008 - IRG/WP 08-40412
In this study, the compressed wood samples pre-treated with hot water bath or water spraying were immersed in the ammoniacal copper quat –type D (ACQ-D) preservative solution to get compressed preservative-treated wood (CPW). The liquid absorption and the recovery rate of compression deformation of the compressed wood was determined, as well as the surface hardness, the distribution of density a...
Jinzhen Cao, Jia Mao


The role of chromium in wood preservatives under BPD - a review and the current situation in Europe
2008 - IRG/WP 08-30468
Already during the IRG-meeting in Trømso a paper was presented to give an overview regarding the situation on chromium (JÜNGEL et al. 2006). Already in that year there was an increased attempt to achieve a science-based correct and harmonised solution in Europe regarding the chromium-question by the European Commission. Nevertheless the competent authorities (CAs) and the industry were similarly...
P Jüngel, S Hellkamp


Formation and Structure of Metal Azole Complexes
2008 - IRG/WP 08-30469
Divalent copper and zinc complexes with metal:azole ratio 1:2 were readily formed at room temperature with the fungicides tebuconazole and propiconazole. The structure of copper and zinc tebuconazole acetate and zinc cis-propiconazole chloride were examined by X-ray crystallography. In copper tebuconazole acetate, the copper atom lies on a crystallographic inversion centre and is coordinated to tw...
P D Evans, K J Schmalzl, C M Forsyth, G D Fallon, S Schmid, B Bendixen, S Heimdal


Effect of steam on fixation of Cu-amine preservative treated wood
2008 - IRG/WP 08-50251
The rates of copper fixation in copper amine preservative treated wood were investigated with different fixation conditions (20° with drying and 50° without drying) and post-steaming. We also measured the degree of leaching for other biocide components (azoles, quatz, and Cu-HDO). Treatments conditioned at 20° with drying required 50 days or more to fix in woods. While copper was stabilized i...
Sung-Mo Kang, In-Yong Hwang, Suk-Kuwon Kim


Thermochemical Remediation of Preservative-Treated Wood
2008 - IRG/WP 08-50254
Remediation methods continue to be developed and refined for CCA-treated wood in order to divert this material from landfills and create secondary products from the wood fiber. A two-step thermochemical remediation method was developed to assess the efficiency of metal removal from CCA-treated spruce flakes. Nearly all the metals (As, Cr, and Cu) were thermochemically extracted from chromated copp...
R Sabo, C A Clausen, J E Winandy


Measurement of wood decay by dynamic MOE in an accelerated soil contact test
2008 - IRG/WP 08-20390
Current laboratory and field testing of preservatives involves various techniques to determine the extent of fungal attack, including visual inspection, mass loss, and static bending and compression strength measurements. The objective of this study was to compare decay measurement by conventional compression strength versus dynamic MOE, employing small wood stakes in an accelerated laboratory so...
Gan Li, D D Nicholas, T P Schultz


Effectiveness of MOQ® OX 50 (CCB-Oxide) wood preservative – Part 2: Field tests
2008 - IRG/WP 08-30483
MOQ® OX 50 is a chromated copper borate preservative known around the world as CCB. In Brazil, this product is the only CCB-oxide type preservative with fungicide and insecticide properties registered at the Brazilian Institute for the Environment and Renewable Resources (IBAMA) that complies with the requirements of the Brazilian and European markets for preserved wood. For over five decades, s...
A Gandolfi Jr, C Salvela, D R Macedo, J M Vidal


Polymeric Betaine as a Wood Preservative
2008 - IRG/WP 08-30487
Didecyl polyoxyethyl ammonium borate (DPAB), also known as Polymeric Betaine, was developed as a co-biocide for chromium-free copper based wood preservatives in Europe in the 1980’s. This paper summarizes the properties of DPAB as a wood preservative. Unique properties related to the betaine nature of DPAB are discussed in terms of the structure-property relationship. Physical properties of D...
H Härtner, S Schmitt, Futong Cui, H M Barnes


Biological Performance of micronized copper wood preservative formulations in field and laboratory tests
2008 - IRG/WP 08-30488
Micronized Copper wood preservative formulations with different co-biocides were exposed to brown rot fungi in an 8-week AWPA E10 soil block decay test and two AWPA E7 ground-contact decay tests in Hawaii. The micronized copper formulations performed well against decay at or above the AWPA UC3 and UC4 retentions stipulated by the ICC-ES. Micronized copper preservatives performed comparably to a ...
G M Larkin, J Zhang, D L Richter, R J Ziobro, P E Laks


Wood preservative obtained by recycling – preliminary selection of leaching inhibitor
2008 - IRG/WP 08-50252
Based on recycling of used household batteries, a process was developed to enable the recovery of major manufacturing components, leading to a solution of zinc (32 g.l-1) and manganese (15 g.l-1) salts, free of heavy metals. The potential use of the above solution as wood preservative was demonstrated by means of assays both of fungicidal activity -using white and brown rot fungi- and of insectici...
C Ibáñez, C Mantero, G Cecchetto, M Rabinovich, M Cerdeiras


Durability and fungal colonisation patterns in wood samples after six years in soil contact evaluated with qPCR, microscopy, TGA, chitin- and ergosterol assays
2009 - IRG/WP 09-20402
There is a need to establish new objective and sensitive methods for early detection and quantification of decay fungi in wood materials. Molecular methods have proven to be a useful tool within wood protection issues, however, this field is still poorly explored and so far relatively few have used these methods within the field of wood deterioration. Among the techniques used in the indirect quan...
A Pilgård, G Alfredsen, I Børja, C Björdal


Copper to quat ratio in alkaline copper quat (ACQ) wood preservative - Effects on fixation and leaching of preservative components in red pine
2009 - IRG/WP 09-30496
This study investigates the effect of the relative proportion of copper oxide (CuO) to didecy dimethyl ammonium carbonate (DDACb) in an alkaline copper quat (ACQ) formulation on the rate of copper fixation or stabilization and the resistance of treated wood to leaching of copper and quat (DDACb). Red pine samples were treated with ACQ, having CuO to DDACb ratios of 2:1 (the normal ratio for ACQ-D...
S Pankras, P A Cooper, T Ung, L Awoyemi


Micronized Copper Preservative Systems: Observations on the Release of Cupric ion (Cu2+) from Treated Wood and Performance against Wood Decay Fungi
2009 - IRG/WP 09-30519
In an attempt to address the mechanism of action of micronized copper preservatives, a 20-week continuous water leaching study was conducted. The leaching results indicated that, once impregnated in wood, micronized copper preservatives continuously release cupric ion, and the levels of cupric ion released from micronized copper treated wood are higher than those released from CCA treated wood, a...
J Zhang, R Ziobro


Factors affecting sodium hypochlorite extraction of CCA preservative components from out of service treated wood for recycling
2009 - IRG/WP 09-50263
Significant amounts of chromated copper arsenate (CCA) treated wood products such as utility poles and residential constructions remain in service. There is an increasing public concern about environmental contamination from CCA treated wood when it is removed from service for reuse or recycling, placed in landfills or burned in commercial incinerators. In this paper, we investigate the effects of...
E D Gezer, P A Cooper


Microwave Surface Modification of Radiata Pine Peeler Cores for Preservative Treatment
2009 - IRG/WP 09-40453
Radiata pine peeler cores are classified as a by-product derived from the cores of logs left over after the veneer peeling process. The core can be potentially developed for value added solid wood products as it is abundantly available and has a constant diameter. However, the core needs to be preservative treated because of low durability in ground contact. An additional problem is that the wood ...
K Sugiyanto, G Torgovnikov, P Vinden