IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3077 documents. Displaying 25 entries per page.


Analysis of hindgut bacterial phyla frequency and diversity in subterranean termites exposed to chitosan-treated wood
2017 - IRG/WP 17-10882
The termite hindgut contains a microbial community that symbiotically aids in digestion of lignocellulosic materials. For better understanding of the dynamics of the bacteria-termite relationship, a species survey of bacterial hindgut microbes in subterranean termites (Reticulitermes flavipes: Kollar) collected from Louisville, Mississippi was performed after exposure to chitosan-treated and contr...
O Raji, J D Tang, T Telmadarrehei, D Jeremic


The First Description of Soft-rot Cavity in Waterlogged Archaeological Woods by a Japanese Wood Anatomist Prof. F. Onaka in 1935
2017 - IRG/WP 17-10885
The term soft rot, which was caused by Ascomycetes and Deuteromycetes, was first used by J G Savory in 1954. Soft rot decay can be characterized by cavities within secondary cell walls align along the cellulose microfibrils. Our recent literature search revealed, however, that Prof. F. Onaka in Kyoto University described the soft rot cavities in the waterlogged archaeological woods in detail from ...
Yoon Soo Kim, K Yamamoto


Untreated and copper-treated wood soaked in sodium oxalate: Effects of decay by copper-tolerant and copper-sensitive fungi
2017 - IRG/WP 17-10888
Copper is widely used as the primary component in wood protectants because it demonstrates a broad range of biocidal properties. However, a key concern with using copper in wood preservative formulations is the possibility for brown-rot basidiomycetes to resist the toxic effect. Many brown-rot basidiomycetes have evolved mechanisms, like the production and accumulation of oxalate, which helps thes...
K M Ohno, G T Kirker, A B Bishell, C A Clausen


Influence of organosilicon compounds and nanocellulose treatment on dimensional stability of waterlogged elm wood
2017 - IRG/WP 17-10891
Commonly used agents for waterlogged wood consolidation (including the most popular polyethylene glycol) have proved ineffective and even dangerous to the preserved objects, jeopardising their integrity. Finding new, effective alternatives for safe preservation of wooden cultural heritage is therefore of key importance. The future conservation agents should, first and foremost, provide the integri...
M Broda, B Mazela, I Dąbek, A Dutkiewicz, H Maciejewski, R Markiewicz, M Grzeszkowiak, S Jurga


A review on prediction methods of wood natural durability
2017 - IRG/WP 17-10892
Natural durability of timber may be defined as “inherent ability of timber to attack by wood destroying organisms (bacteria, fungi, insects, marine borers) without preservative treatment. On the base of biological tests, EN-350-2 standard (Afnor, 1994), describe the classification of wood species according to their natural durability. But these specifications are not adapted in the case of wood ...
N Amusant, C Flora, J Beauchène, E Houël, C Duplais


Chemical compositions and anti-termite activities of essential oils from Gabonese Canarium schweinfurthii Engl, Dacryodes buettneri Engl and Aucoumea klaineana Pierre wood resins.
2017 - IRG/WP 17-10895
Essential oil extract from resins of Canarium schweinfurthii, Dacryodes buettneri and Aucoumea klaineana woods from Cap Esterias and Oyem areas, Gabon, were prepared by Clevenger - steam distillation. The chemical compositions of these respective essential oils were analyzed by a Gas Chromatography coupled with Mass Spectrometry (GC-MS). Although monoterpenes were the main constituents of the thre...
Chemical compositions and anti-termite activities of essential oils from Gabonese Canarium schweinfurthii Engl, Dacryodes buettneri Engl and Aucoumea klaineana Pierre wood resins.


Fungal growth on coated wood exposed outdoors: influence of coating pigmentation, cardinal direction and inclination of wood surfaces
2017 - IRG/WP 17-10896
The objective of the SERVOWOOD project was to develop and establish European Standards that will facilitate the prediction of service life for exterior wood coatings. One of the objective of this project was to study fungal growth of the field exposed panels. Two coatings applied in 2 and 3 coats were exposed for one year outdoors at 45° south: one solventborne (alkyd based) and one waterborne (a...
L Podgorski, C Reynaud, M Montibus


Underground timber constructions from the First World War are well preserved after 100 years
2017 - IRG/WP 17-10897
During the Great War or World War I many underground constructions have been built for protection from shelling. They were an important part of the trench warfare as they were used as an area to rest and carry out other activities such as eating. They would usually range in size from smaller constructions that could hold several men to larger entities that could hold thousands of soldiers. In the ...
J Van Acker, I De Windt, K Haneca, H Beeckman, F Claeys, S Vandenbussche, J Vandewalle, N Robeyst, A Willems


Novel wood treatments improve resistance to the wood-boring marine isopod Limnoria quadripunctata
2017 - IRG/WP 17-10899
The marine isopod Limnoria quadripunctata degrades wooden structures in the sea and causes significant economic damage. Broad-spectrum biocides and naturally resistant tropical hardwoods have failed to prevent feeding by Limnoria and have caused ecological damage. Wood modification is now the favoured method, and resin-based modifications have been effective, while the efficacy of silica-based mod...
H Bowen, M Montibus, M Kutnik, S M Cragg


Case study: “Riesenbühlturm”
2017 - IRG/WP 17-20599
In this case study four 7 m long Douglas fir crossbeams were investigated regarding the remaining metal and moisture content. The crossbeams were replaced from a timber tower after 10 years of service in the Black Forest region (South Germany) due to fungal decay. From each of the crossbeams five stem discs were taken and relevant parameters (density, moisture and remaining metal content) were de...
E Melcher, J Müller


Use of small volume cups in XRF analysis of treated wood retention
2017 - IRG/WP 17-20602
Efforts are underway in the United States to improve the conformance of commercially-treated wood with the applicable retention standards. As part of an effort to devise a practical method for on-site assessment of within-charge retention variation, we investigated whether small-volume x-ray florescence (XRF) sample cups could be used with treated wood. A range of cup sizes, preservative types, re...
R Stelzer, A Taylor, P Lebow


The sorption behaviour of wood
2017 - IRG/WP 17-20605
The use of dynamic vapour sorption to determine the sorption properties of wood has become an increasingly popular technique. The method has many advantages when compared with many other gravimetric methods. However, it is necessary to set an equilibrium condition in order to obtain data for an isotherm in a reasonable amount of time. An important recent finding has been that multiple sorption cyc...
C Hill


Quality of the impregnated wood in the Slovenian hardware stores
2017 - IRG/WP 17-20606
Ten different samples from Slovenian hardware stores were analysed. Samples were treated with copper based wood preservatives and designed and advertised to be used in heavy duty applications in use classes 3.2 or 4. In order to determine the quality of the treatment penetration, retention and fungicidal properties were determined. Retention was determined with XRF analysis, while modified EN 113 ...
M Humar, B Lesar, N Thaler, D Kržišnik, N Kregar, S Drnovšek


Monitoring of wood biodeterioration by infrared spectroscopy
2017 - IRG/WP 17-20607
The susceptibility of wood to deterioration by rotting fungi is intrinsically related to its chemical composition and the environmental conditions at its place of use, and if not detected in time, can cause enormous financial losses. The process of wood biodeterioration by decay fungi can be evaluated through laboratory accelerated test, in specific field tests, or through non-destructive techniqu...
E Meneses Oliveira, A Florian da Costa, J W Batista Braga


Consistency of performance of acetylated wood
2017 - IRG/WP 17-20608
It is well known that acetylation of wood improves the resistance against wood decaying fungi and insects, as well as its dimensional stability under varying moisture conditions. Accsys Group continues to support a variety of laboratory and field studies around the world to assess and monitor the durability, dimensional stability and uniformity of its products. To gain and maintain market acceptan...
F Bongers, J van Zetten


Three-Dimensional Digital Image Correlation of Strains in Profiled Wood Decking Exposed to Wetting & Drying
2017 - IRG/WP 17-20611
We use three dimensional digital image correlation to measure the strains that develop at the surface of profiled radiata pine (Pinus radiata D. Don) deck boards subjected to a wetting and drying cycle. We hypothesise that surface profiling will change the pattern of strain distribution at the surface of deck boards by concentrating stresses at the base of profile grooves. Five groups of three deck board samples were produced from five different pieces of machine stress-graded radiata pine wood. Two wavy profiles, ribble or ripple, were tested. Flat unprofiled boards acted a control. Each board was fixed to a rigid frame and subjected to a wetting and drying cycle. Full field surface strain data was collected using 3D digital image correlation. Strains varied across the surface of both flat and profiled boards. Profiling changed surface strain patterns; strain maxima and minima developed in the profile ridges and grooves during wetting, respectively, but this pattern of strains reversed during drying. Such a pronounced reversal of strains was not observed when flat boards were exposed to wetting and drying, although there was a shift towards negative strains when flat boards were dried. We conclude that profiling changes surface strain distribution in deck boards exposed to wetting and drying, and causes high strains to develop in the grooves of profiled boards. These findings help explain why checks in profiled deck boards are mainly confined to profile grooves where they are difficult to see, and the success of profiling at reducing the negative effects of checking on the appearance of wood decking.
J Mallet, S Kalyanasundaram, P D Evansa


Rapid detection of the Alaska yellow cedar, Callitropsis nootkatensis (Cupressaceae) extractives using Fourier transform infrared (FT-IR) spectroscopy
2017 - IRG/WP 17-20612
Global changes in wood harvesting towards plantation species grown on much shorter rotations has the potential to markedly alter wood quality perceptions. Nowhere is this more risky than with naturally durable species where there is compelling evidence that faster grown woods tend to be less durable. The ability to non-destructively assess durability may allow growers to identify materials that re...
S Lipeh, J J Morrell


Monitoring Diversity and Colonization Patterns of Wood-Inhabiting Fungi Using Field Stake Tests
2017 - IRG/WP 17-20614
Advances in molecular identification of microbial communities enabling rapid microorganism determination have allowed ecological data to be increasingly incorporated into standardized wood performance tests. Combining standard field tests with molecular methods to study wood-associated microflora can help to better understand fungal colonization and decay processes of wood in service. The potentia...
P Torres-Andrade, J Cappellazzi, J J Morrell


Overview of the treated wood quality control program in the United States with the recent challenges and advances
2017 - IRG/WP 17-20616
In the past two decades, there have been significant and rapid changes in wood protection technologies for residential applications which have moved away from long established heavy duty metal oxide based products such as chromated copper arsenate (CCA). The successor generation of wood protection systems usually contain copper as the primary biocide, in combination with carbon-based co-biocides s...
L Jin


Evaluation of surface cracks on wood – physical assessment versus subjective sensation
2017 - IRG/WP 17-20617
In the presented studies from the University of Goettingen (Study I) and the University of Hannover (Study II), the assessment of cracks with different methods and their acceptance in general as well as depending on different target groups are investigated. The aim was to determine which factors are relevant for a crack evaluation and which visual impression of a wooden surface is tolerable for co...
A Gellerich, C Brischke, L Emmerich, L Meyer-Veltrup, P Kaudewitz


Influence of Weathering on Moisture Performance of Wood
2017 - IRG/WP 17-20619
Water performance of wood is besides the inherent durability the most important factor that influences on the performance of wood in outdoor, above ground applications. Therefore it is of significant importance to optimize the methods that are able to predict the moisture behaviour of wood in outdoor applications. In order to elucidate this questions, samples were prepared of oak (Quercus), sweet ...
M Žlahtič-Zupanc, B Lesar, N Thaler, M Humar


COST FP 1303 Cooperative Performance Test – Results after two years outdoor exposure
2017 - IRG/WP 17-20620
COST Action FP 1303 ‘Performance of Bio-Based Building Materials’ started in October 2013 and an ambitious program was set up for four years. Among this a collaborative field test was planned. The idea of the cooperative performance test was to distribute a fairly simple test set up to as many places in Europe as possible in order to collect performance data reflecting the full range of climat...
B Lesar, M Humar, C Brischke, L Meyer-Veltrup, D Jones, N Thaler, J M Abascal, G Alfredsen, B Brunnhuber, E Grodås, M Irle, J Kers, M Klamer, K-C Mahnert, E Melcher, S Palanti, M Noël, E Suttie, N Pfabigan, M Touza


Moisture performance of wood determined in laboratory and field trials
2017 - IRG/WP 17-20621
It is widely accepted that wood moisture content (MC) is the key factor when it comes to durability of wooden structures exposed to weathering. The moisture performance of wood and wood-based products has been recognized as key element in wood durability and wood protection. Actually, it should be considered as major component of the material-intrinsic resistance of wood, but never found its way i...
D Kržišnik, N Thaler, B Lesar, M Humar


An experimental study of mould growth and wood decay in timber frame walls
2017 - IRG/WP 17-20623
This paper deals with parameters related to the occurrence of mould growth and wood decay in timber frame walls. In a first part, the hygrothermal conditions inside a timber frame wall finished with brick veneer cladding are analysed to get an idea of possible moisture related problems. It is shown that, based on the VTT mould prediction model, there is a mould risk on the interface between the in...
M Vanpachtenbeke, J Van den Bulcke, I De Windt, J Langmans, S Roels, J Van Acker


New Standards for Approval of Modified Wood within the Nordic Wood Preservation Council (NWPC)
2017 - IRG/WP 17-20624
In the Nordic countries, there is a long tradition for quality labelling of preservative treated wood. Until now the labelling has been restricted to pine and other easy to treat wood species, but with the introduction of a new set of standards it is now possible to obtain the Nordic Wood Preservation Council’s (NWPC) quality labelling also for modified wood. In this paper, we will introduce th...
N Morsing, E Engelund Thybring, M Klamer


Previous Page | Next Page