Germination of basidiospores on preservative treated wood after leaching or natural weathering
1981 - IRG/WP 2150
In tests of residual toxic efficacy after leaching or natural weathering, spore germination with Gloeophyllum trabeum has proved to be a less reliable criterion of attack than when used with unaged preservative treatments. Since spores sometimes prove more tolerant than their parent mycelium, their use should be continued....
J K Carey


Autoxidation of beech condensate
2003 - IRG/WP 03-40261
Liquid effluent from steaming beech wood was studied. The effluent contains many phenolic compounds which can present a significant toxicity. The effluent was treated by oxidation was carried out at 250 rpm for 30 min with NaOH. This was followed flocculation with CaCl2 for 30 min. The influence of parameters such as pH, time of autoxidation were studied. Experimental results reveal the electrosta...
M Irmouli, J P Haluk


Incorporating insect behaviour in standard tests of wood preservatives - A possible way to reduce pesticide loadings
2000 - IRG/WP 00-20190
The application of wood preservatives to protect timber against insect infestation is common practice world wide. The effectiveness of wood protecting insecticides is usually determined in various standard tests. Depending on the target pest species and the test method, larvae of different developmental stages and sizes or adult insects are exposed artificially to the insecticide-treated commodity...
H Hertel, R Plarre


Experience with an industrial scale-up for the biological purification of CCA-treated wood waste
1997 - IRG/WP 97-50095
The biological purification of CCA-treated wood waste was tested in co-operation of the BFH and the Italian impregnation plant SoFoMe. Chipped poles were infested with the chromium and arsenic tolerant brown-rot fungus Antrodia vaillantii which can transform in the laboratory ca. 90% of the chromium and arsenic into watersoluble salts. These can be leached to 100-200 ppm residual metal content. Th...
H Leithoff, R-D Peek


Report of activity of CEN/TC 38: Test Methods for Wood Preservatives
1987 - IRG/WP 2287
G Castan


The proposal for optimalization of the agar-block method for wood preservatives fungitoxic evaluation
1995 - IRG/WP 95-20065
On the base of own research and other scientists results the proposal for optimalization of agar-block method was presented by: - selection of test fungal species and strains and central distribution of their pure cultures, - change of the treatment and control samples exposure procedure, - application of mathematical estimation of toxic value results, - shortening the duration of fungitoxic t...
J Wazny


Questionnaire: The use of computers in wood preservation research
1985 - IRG/WP 2240
E F Baines


Towards a colour assay of wood degradation
1982 - IRG/WP 2180
A colour assay for the enzyme catalase is described. Since the activity of this enzyme has previously been shown to be correlated with degree of wood degradation as determined by other methods, this assay may provide a rapid quantitative indicator of superficial and internal wood decay....
M A Line


Influence of variable lignin content on brown rot decay of wood
1987 - IRG/WP 1320
Compilation of published data and new experiments with brown-rotting fungi on different timber species suggest that their decay activity, in contrast to soft rot and white rot fungi, is not greatly influenced by the type or amount of lignin present....
T Nilsson, G F Daniel


Wood preservation in Spain
1983 - IRG/WP 3266
This report includes some statistical data on the potential of Spanish forests and the country's timber consumption as well as detailing the extent of development of the wood products industries, and will help to give a better understanding of the use of this raw material in Spain. The main biological deteriorating organisms which damage wood are given and the capacity of the industrial t...
A Lopez de Roma, R Cockcroft


A collaborative test to determine the efficacy of poyurethane coatings on wood samples exposed in the marine environment. 1st Interim Report
1988 - IRG/WP 4145
Wood samples coated with elastomeric polyurethane (ca. 50 mils thick) were exposed for up to 2 years in 12 tropical and temperate marine test sites with known teredinid, pholad and/or crustacean infestations. All uncoated control samples were destroyed or partially destroyed. Polyurethane-coated samples were not attacked, the surfaces of the coating were sound and the polyurethane adhered well to ...
R A Eaton


Antifungal properties of new quaternary ammonium and imidazolium salts against wood decay, staining and mould fungi
2004 - IRG/WP 04-30347
The biological activity of twenty-four potential wood preservatives – imidazolium and quaternary ammonium salts with a modified anion structure was determined employing screening agar-plate and agar-block methods. Experiments were carried out on Scots pine (Pinus sylvestris L.) wood. The aim of the performed studies was to investigate the effect of structure modification of IC and QAC with organ...
J Zabielska-Matejuk, W Wieczorek


Environmental behaviour of treated wood in (semi-)permanent contact with fresh or seawater
1998 - IRG/WP 98-50101-20
This study presents a strategy for the environmental toxicity evaluation of treated wood towards the aquatic compartment, using non target water organisms toxicity tests. A lixiviation process is applied on wood (Pinus sylvestris) treated with several wood preservatives formulations. The lixiviation process is carried out in the laboratory with ultrapure water or synthetic seawater. After chemica...
P Marchal, C Martin


Reference numbers of papers of the International Research Group on Wood Preservation issued to date
1970 - IRG/WP A 4
IRG Secretariat


A bibliography of organic solvent-based wood preservatives
1973 - IRG/WP 313 E
H Alliot


Questionnaire on the state of pollution control in the field of wood preservation
1974 - IRG/WP 52
H Willeitner


Tebuconazole - a new triazole fungicide for wood preservation
1991 - IRG/WP 3680
The great potential of Tebuconazole for wood preservation is demonstrated. Test carried out by official institutes shown that Tebuconazole is particularly effective against wood-rotting basidiomycetes strains. The efficacy of Tebuconazole against the brown rot Gloeophyllum trabeum is outstanding: the toxic value measured in accordane with EN 113, without·ageing, after leaching (EN 84) and after e...
O Exner


An experimental method to simulate incipient decay of wood by basidiomycete fungi
2000 - IRG/WP 00-20200
At very early stages of decay of wood by basidiomycete fungi, strength loss can be measured from wood before any measurable weight loss. Therefore, strength loss is a more efficient measure of incipient decay than weight loss. However, common standard decay tests (e.g. EN 113 or ASTM D2017) use weight loss as the measure of decay. A method was developed that allowed progressive removal of samples ...
S F Curling, J E Winandy, C A Clausen


Leaching of inorganic wood preservatives – Investigating the relationship between leachability, dissociation characteristics and long-term leaching potential
2003 - IRG/WP 03-50199
Estimation of the leaching properties of preservative components is greatly affected by the leaching test method applied since not all methods equally consider the physical components responsible for leaching. These include: wetting of the wood and penetration of water (affected by dimensions, amount of end grain, permeability, duration and nature of water exposure); solution of preservative comp...
L Waldron, Y T Ung, P A Cooper


Decay patterns observed in butylene oxide modified ponderosa pine after exposure in unsterile soil
1982 - IRG/WP 3211
Small blocks of ponderosa pine (Pinus ponderosa Laws) chemically modified with butylene oxide to three different weight gains were exposed for 6 weeks in unsterile soil. Severe surface decay caused by soft rot fungi and tunnelling bacteria was observed in blocks with 8 weight percent gain. The soft rot attack was restricted to the outer parts of the radial walls in the latewood tracheids. Bacteria...
T Nilsson, R M Rowell


Laboratory experiments on aerial emissions from wood treated with wood stains
1993 - IRG/WP 93-50001-06
Due to the actual environmental interest in wood preservation, a series of experiments was carried out on the emission of biocides from treated wood. The research focussed on the volatilization of 5 biocides from boards treated with wood preservative finishes containing dichlofluanide (DCF) azaconazole (AZA), pentachlorphenol (PCP), iodopropynylbuthylcarbamate (IPCB) and tributhyltinoxide (TBTO). ...
G M F Van Eetvelde, M Stevens


Agenda Special Seminar: Screening techniques for potential wood preservative chemicals
1978 - IRG/WP 2115
IRG Secretariat


Developments in wood preservation processing techniques in New Zealand
1980 - IRG/WP 3143
P Vinden, A J McQuire


Disposal of Pressure Treated Wood in Construction and Demolition Debris Landfill
2005 - IRG/WP 05-50235
Pressure treated wood is often disposed in landfills in the US, very frequently in construction and demolition (C&D) debris landfills. C&D debris disposal facilities in many states are not equipped with liner systems to protect underlying groundwater. In this paper, issues associated with the disposal of metal-containing treated wood in C&D debris landfills are discussed. C&D de...
T G Townsend, B Dubey, J Jambeck, H M Solo-Gabriele


Disposal of CCA treated waste wood by combustion - An industrial scale trial
1996 - IRG/WP 96-50068
Totally 272 m³ (62.7 t) of CCA treated utility poles were chipped and incinerated at Jalasjärvi Gasification Plant. In average the whole batch of chips contained 57 kg of elementary copper, 95 kg chromium and 76 kg arsenic. During the 56 h combustion trial the measured arsenic emission to the air was 76 g in total. Copper and chromium emission was less than 1 g. The condensing water from the coo...