Minutes of WG I, Sub-group 5 Insects in dry wood
1983 - IRG/WP 1220
IRG Secretariat


Soil chemistry and wood decay
1978 - IRG/WP 2109
Soil is a most complex biological, chemical and physical material; its study is effectively a separate branch of science but almost entirely in relation to ist ability to grow plants - this paper is intendet just to note some known facets that might have relevance to the decay of wood and the performance of wood preservatives....
E A Hilditch


The use of zirconium as an inert fixative for borates in preservation
2001 - IRG/WP 01-30256
Stand-alone borates have been used in internal protected situations as wood preservatives for about 60 years. They have not been deemed acceptable for external situations because of their leaching characteristics. Work carried out to reduce the leachability of borates has been reviewed briefly here, and a specific fixation agent based on zirconium has been tested in standard leaching and decay tes...
J D Lloyd, J L Fogel, A Vizel


Risk assessment and the approval of wood preservatives in the United Kingdom
1995 - IRG/WP 95-50040-23
An approval system operates in the United Kingdom (UK) for the regulation of wood preservatives. The regulatory authority uses a risk assessment approach to evaluate how far the potential for harm to people and the environment from wood preservatives is likely to be realised in practise, and hence the controls required for products to be, used safely. The evaluation for approval purposes also take...
R M Turner


Wood preservation research at the Technical University in Zvolen - Slovakia
2004 - IRG/WP 04-10538
Presented paper gives basic information about wood protection in Slovakia and research in the field of wood preservation at the Technical University in Zvolen – the Faculty of Wood Sciences and Technology. The degradation processes in wood and wooden composites caused by fungi, environmental factors and fire, the identification of these processes, the protection of wood with fungicides and ot...
L Reinprecht


Evaluation of a solid remedial wood preservative containing boron and fluorine
1993 - IRG/WP 93-30022
The fungicidal and termiticidal effectiveness of a new rod form of diffusible remedial wood preservative, containing disodium octaborate tetrahydrate/sodium fluoride and marketed as Polesaver Rod, was evaluated in laboratory tests against three species of basidiomycete fungi (Coniophora olivacea, Pycnoporus coccineus, Perenniporia tephropora) and two species of subterranean termites (Coptotermes a...
K J McCarthy, J W Creffield, L J Cookson, H Greaves


Co-operative research at the Naval Research Laboratory on wood extractives and related compounds as antiborer agents
1977 - IRG/WP 429
J D Bultman, K K Parrish


Information from the Wood Group of COIPM
1982 - IRG/WP 494
A Gambetta


Contribution of wood components on the absorption of copper amine
2000 - IRG/WP 00-30216
The contribution of wood components on the absorption of copper amine was investigated. Holocellulose, lignin and xylan absorbed significant amount of copper. The amount of copper absorbed by cellulose was almost negligible. The removal of extractive also decreased the amount of copper absorption. This study clearly indicates the importance of lignin, hemicellulose in the absorption of copper amin...
D P Kamdem, Jun Zhang


Effect of soft-rot decay on the static bending strength of wood
1991 - IRG/WP 2361
In this study, a modified static bending test has been developed as a method for measuring soft-rot decay in soil bed studies. A good correlation was found between the strength loss of the southern pine test specimens and extent of decay. This data suggests that it may be possible to develop a dynamic test based on stress relaxation that is more sensitive than static bending....
D D Nicholas, J A Wilson, R C Vasishth


Assessment of wood preservation facilities in Canada
1989 - IRG/WP 3557
This document sets out an assessment procedure for the current status of the wood preservation industry in Canada in relation to the Technical Recommendations (TR) documents for the Design and Operation of Wood Preservation Facilities published by the Government of Canada in April 1988. A questionnaire has been prepared in consultation with industry and the Canadian Institute of Treated Wood. An a...
G Das, V N P Mathur


Literature survey on the permanence and distribution of salt-type wood preservatives
1969 - IRG/WP III 1B
The objective of this survey is generally to review some of the more important published work dealing with the distribution and permanence of salt-type waterborne wood preservatives in treated timber. The survey is limited to the major chrome-containing formulations and the classification system proposed by Becker (1964) has been adopted throughout. CK - chromium, copper (copper, chrome); CKA - c...
Anonymous


Biological degradation resistance of pine wood treated with dimethylol compounds
1989 - IRG/WP 3528
The study reports the increase of dimensional stability and biological degradation resistance of pine wood (Pinus sylvestris L) after impregnation with dimethyloldibydroxyethyleneurea. Decay resistance was determined according to BS 838:961. Nearly complete protection against Coniophora puteana, (Schum.ex Fr. Karst) weight loss of 2-3% was shown when modification, expressed as weight gain, exceede...
C L Videlov


Methods of treatment of wood preservatives. The selection of appropriate preservation process with particular reference to mixed tropical forest resources. A key address
1982 - IRG/WP 3177
All wood is biodegradable. Many timber species have, however, sufficient natural durability to permit their use, particularly in protected situations, without any special precautions. Many others, of course, are readily attacked by insects and where there is sufficient moisture and air, by wood-decaying fungi. It is these timber species which benefit most from treatment with wood preservatives. Ev...
C R Levy


Investigation of the fixation in wood of chromated zinc chloride and copperised chromated zinc chloride preservatives
1976 - IRG/WP 372
A biological method of evaluating the extent to which CZC and CCZC preparations are retained in wood in terms of the potential protection which they afford against destruction by Merulius lacrymans (dry rot) is given. CCZC is recommended for protection of wood under moderate leaching conditions, while the use of CZC under such conditions is not recommended....
V N Sozonova, D A Belenkov


Documentation on Merulius (Serpula) lacrimans (Wulf.) Fr. according to the "Model Questionnaire for preparation of monographic cards for wood-destroying fungi"
1972 - IRG/WP 108
J Segmüller, O Wälchli


Development of a method for testing wood preservatives with soft rot fungi
1975 - IRG/WP 250
Although the first publications on experimental soft rot attack date back 20 years ago, so far no test method for evaluating the efficacy of wood preservatives against soft rot attack (Ascomycetes and Fungi Imperfecti) has been generally accepted. The reasons are diverse and the shortcomings and the disadvantages of the methods described are well known and have repeatedly been discussed. The soil ...
M Gersonde, W Kerner-Gang


Involvement of hydrogen peroxide in wood decay by brown-rot and white-rot fungi
1985 - IRG/WP 1256
To gain further understanding of the role of H2O2 in wood degradation by brown- and white-rot fungi, we studied the following: (a) extracellular H2O2 production, (b) effect of various hydroxyl radical (·OH) and singlet O2 (1O2) quenching agents on wood and cellulose degradation, (c) intracellular H2O2 production and catalase activity, and (d) cytochemical localization of H2O2 with diaminobenzidin...
T L Highley, L L Murmanis


Pyrolytic treatment of CCB treated wood
2005 - IRG/WP 05-50224-23
Environmental problems caused by the toxicity of metallic elements of the preservative occur when treated wood comes to end of use. In the experiment, CCB treated wood chips were pyrolysed at various temperatures and residence times and the behaviour of boron, chromium and copper was observed. The three elements are almost entirely retained in the charcoal. There is no influence of final tempera...
J F Collin, C G Jung, J M Romnée, J Delcarte


Decay, decayed wood and the Shigometer
1980 - IRG/WP 281
A L Shigo


Questionnaire on the most important wood-destroying insects in your country and/or state
1980 - IRG/WP 1125
S Cymorek


New conception for shortering the duration of fungitoxic test of wood preservatives. Part 3: Proposal for interlaboratory test on miniaturisation of wood specimens
1994 - IRG/WP 94-20053
In connection with documents IRG/WP 94-20044 and IRG/WP 94-20052 the proposal for interlaboratory test on miniaturization of wood specimens is given....
J Wazny, J J Krajewski


Production of preservative-treated wood in some countries
1990 - IRG/WP 3598
This report presents figures of the production of preservative-treated wood and wood treated with anti-stain chemicals in 26 and 20 countries respectively from all over the world....
J Jermer


Identification card for Coriolopsis polyzona (Pers.) Ryv
1977 - IRG/WP 161
A Ofosu-Asiedu


Fungicidal properties of boron containing preservative Borosol 9
2004 - IRG/WP 04-30348
The fungicidal properties of new boron containing wood preservative Borosol 9 is described in this paper. These properties were of particular interest as this new boron containing preservative, exhibit very good performance against wood damaging insects. But because the tested boron formulation contain also nitrogen compounds, we wanted to verify if nitrogen as a nutrient could promote...
G Babuder, M Petric, F Cadež, M Humar, F Pohleven