Inspection of tropical hardwood window frames in Nigeria for decay presence
1987 - IRG/WP 2294
A method of in situ inspection of hardwood window frames for expression of decay is discussed in this paper. The results show that about 6% of the frames inspected or 23% of the volume of wood in all the frames sampled in buildings erected between 1920 and 1984, exhibited evidence of advanced decay. Protection by the length of the eaves, species of the framing timber used, length of exposure to se...
M A Odeyinde, M A Amakiri, E B Lucas, J O Eyenike, S Akanni


On the natural durability of RED MERANTI for window frames as a function of gross density wood
2018 - IRG/WP 18-10927
MERANTI is a wood species belonging to the family Dipterocarpaceae, in the genus SHOREA (Shorea spp.). The genus has approximately 196 species with four subgenera. The subgenus RUBROSHOREA is commonly named RED MERANTI (RM) and is found on the Malayan Island of Sarawak, Indonesia, with approximately 65 varieties (Symington 1943). According to Brazier (1956), the distribution of gross densities wi...
K Hasse, W Unger, T L Woods


Wood preservatives: Field tests out of ground contact. Brief survey of principles and methodology
1976 - IRG/WP 269
This paper contains the following spots: 1.: The general need for field tests. 2.: Interests and limits of field tests in ground contact. 3.: Various methods in use for out-of-ground contact field tests. 4.: Fungal cellar tests are they an alternative to above-ground decay exposure tests? 5.: Conclusions....
M Fougerousse


Water sprinkled pine wood: A microscope study on boards showing streaking
1993 - IRG/WP 93-10033
Boards sawn from the outer sapwood of pine lumber previously water sprinkled for periods of 10-18 weeks and kiln dried, showed streaking after staining. Two types of enhanced stain uptake were noted: 1) a more concentrated and localized form after 10 weeks and 2) a more diffuse type which developed in later stages of water sprinkling. Areas showing enhanced stain uptake were examined using light a...
G F Daniel, T Elowson, T Nilsson, A P Singh, K Liukko


Novel wood modification processes for window and cladding products
2004 - IRG/WP 04-40285
Because of the low natural durability and low dimensional stability of European wood species, the usage of wood for window frames has decreased dramatically during the last decade. In a joint project of several German research institutes and the window industry, following wood modification systems were compared. heat treatment (3 different materials from 2 companies) acetylation (pine sapwood an...
A Krause, C Hof, H Militz


The window joinery test hut
1975 - IRG/WP 257
D F Purslow


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 4: Report of second inspection (12 months) in Australia
1979 - IRG/WP 448
Previous reports have presented full details of the treatment and installation of the test specimens in Sydney Harbour during December, 1977, and of the results of the first (6 months) inspection made during June, 1978. At the June inspection it was apparent that the plastic tubing used to make up the frames from which to suspend the specimens was inadequate for the job and not strong enough to su...
J Beesley


The efficacy of remedial treatments for controlling fungal decay in window millwork used in the United States
1987 - IRG/WP 3432
Conventional window millwork was subjected to basidiomycete decay by inoculation and sampled for active growth of the decay fungus before and eight months after remedial preservative treatment with fused disodium octaborate rods (IMPEL) at boric acid levels of 1.5 and 4.0 kg/m³ or liquid bifluoride injections (IMPROSOL) at 1 kg/m³. The elimination of decay fungus after remedial treatment was nea...
M G Dietz, E L Schmidt


Preservative treatments of window components with a water-based borate formulation
2000 - IRG/WP 00-40171
Factory finished window joinery components were treated with an aqueous borate preservative in order to investigate penetration and retention levels, associated drying times; and the potential impact of using a water-based treatment on finished items. It was found that by using borates applied by light double vacuum schedules, it was possible to meet standards for penetration and retention, to air...
J Jermer, J D Lloyd


Tanalith T - a new preservative system for protecting house frames in Australia from termite attack.
2003 - IRG/WP 03-30306
The sawn timber industry in Australia has expressed a desire for a new low cost termite treatment. The treatment needs to be on-line in the dry mill, minimising material handling costs and with a very fast processing time to meet timber flow through the dry mill. The preservative, Tanalith® T, forms an envelope on both Pinus radiata and Pinus elliotti sawn timber. Field trials conducted in Aus...
P R S Cobham, J Snow


An attempt to develop a direct and reliable method for testing the preventive action of preservation treatments of wood against fungal decay
1980 - IRG/WP 2139
In wood preservation there are two classical ways for assessing the reliability of preventive treatments against wood decay: the laboratory tests in which the various parameters are evaluated independently and the field tests or service tests in which those parameters are acting together in the natural environment. One has always tried to build bridges between the two types of experiments and to e...
M Fougerousse


BRE Experience in monitoring decay in out-of-ground exposure trials
1995 - IRG/WP 95-20077
The outdoor field trial has always been regarded as the ultimate test of performance for assessing the effectiveness of a wood preservative. For this reason, the Building Research Establishment (BRE) has invested much effort in such trials over many years. Emphasis in early trials was on ground contact tests which were the basis both for assessing the likely performance of a preservative in protec...
J K Carey, R J Orsler


A chemical and mycological evaluation of fused borate rods and a borate/glycol solution for remedial treatment of window joinery
1983 - IRG/WP 3225
The possibility of using fused borate rods (Impel Borpatron) and a borate/glycol solution (Boracol-40) for depot impregnation of window joinery has been examined in a co-operative project between The Swedish Forest Products Research Laboratory, The Swedish University of Agricultural Sciences and Prolignum AB. The fused Impel rod is a glassy rod composed of disodium octaborate which readily dissolv...
M-L Edlund, B Henningsson, A Käärik, P-E Dickèr


Distinguishing isolates of Aureobasidium on the basis of their ability to utilise lignin breakdown products as a sole carbon source
1996 - IRG/WP 96-10151
Wild isolates of Aureobasidium were obtained by dilution plating from a ca 20 year old painted pine window frame. Four isolates were obtained from the paint/wood interface region and four isolated from regions deep in the wood. The isolates were then used to inoculate liquid cultures containing ferulic acid, a lignin breakdown product, present as the sole carbon source. Ability of the isolates to ...
M W Schoeman, D J Dickinson


Field and greenhouse testing of window joinery of pine and spruce treated with LOSP
1991 - IRG/WP 3658
Norwegian window frame components of full size were double vacuum-treated with TBTN and TBTO, and connected as 'L-joints' and subsequently coated with stains. The corner sections were exposed (out of ground contact) both in field (temperated coastal climate, Taastrup, Denmark) and in a greenhouse (Uppsala, Sweden). The window frame L-joints of spruce (Picea abies Karst.) - treate...
F G Evans, B Henningsson, E Borsholt


Decay in window joinery in Sweden
1977 - IRG/WP 390
Systematic investigations of decay in window joinery in Sweden have not been undertaken until very recently. One might guess that one of the reasons for the minor interest is that this type of joinery did not rot strikingly faster than people expected. In the last 10-15 years, however, house owners, tenantowners, building societies and others have repeatedly argued that windows do rot more than in...
B Henningsson


Window test. Direct testing of wood resistance to decay: A study of its fitness, its reliability and its accelerating factor
1984 - IRG/WP 2219
This is the results of an experiment using the window-test specimens, exposing the specimens to three different types of testing procedure: 1. Natural infestation in the open air; 2. Artificial infestation and exposure in the open air; 3. Artificial infestation in a green-house. The results show good similiraties of the three parallel tests in term of decay, and assess the reliability of the windo...
G R Y Déon, L N Trong


Influence of preservative treatment on the glueing of the members of glued laminated frames and effectiveness with respect to newly hatched larvae of the house longhorn beetl
1971 - IRG/WP 203 E
The object of the work is to check the general properties of a glued laminated beam after treatment of the members composing it by means of commercial insecticidal and fungicidal formulations in clear solvent under the most common conditions of manufacture. The species used have been spruce, redwood and Douglas fir in planed boards of 80 cm long, 14 cm wide and 20 mm thickness at about 12% moistur...
J Guillemain-Thévenot


Decay evaluation of the effectiveness of a LOSP envelope treatment in eucalypt and meranti heartwoods for window joinery
1996 - IRG/WP 96-30099
The effectiveness and penetration in heartwood boards of an LOSP formulation containing TBTN was examined by determining decay resistance to the white-rot fungus Perenniporia tephropora. Boards, one metre long, of Eucalyptus regnans, Eucalyptus delegatensis, Eucalyptus obliqua and Eucalyptus sieberi were treated, along with boards of 'light' and 'dark' meranti. ...
L J Cookson, A Trajstman


The development of blue stain in service in sapwood of European softwood species
1997 - IRG/WP 97-10236
The utilisation of softwood species for window joinery applications is gaining importance in countries frequently using tropical hardwood species up to now. Since wood preservation is not always part of the total concept of window frames manufactured from sapwood containing wood elements it is essential to know the impact of durability on the performance. Moisture content control is a major tool i...
J Van Acker, R Klaassen, H Militz, M Stevens


Preliminary desk research in the Netherlands on development of a Knowledge Based System for Life Cycle Assessment of wood products
1997 - IRG/WP 97-50093
TNO is currently coordinating an EC-project (LIFE-SYS WOOD) to develop a consistent approach to Life Cycle Assessment (LCA) of wood products. Existing and new LCA-inventory data of six wood products will be evaluated on reliability and consistency. After validation, LCA-results will be made available through a Knowledge Based System (by 1998-1999). The aim of the KBS is to make LCA-results availab...
P Esser, D Robson, R Vanhauten


Material properties of furfurylated wood for window production
2009 - IRG/WP 09-40480
Wood modification with furfuryl alcohol is an extensively investigated process and already produced commercially. Furfurylated wood is in the focus of a European project on its use for the production of high performance windows. Different wood species were treated with furfuryl alcohol and tested on water uptake, dimensional changes, leaching in water, resistance to fungal degradation, and ecotoxi...
A Treu, A Pilgård, S Puttmann, A Krause