A study of the decay type potential of seven soils
1992 - IRG/WP 92-1539
The aim of this experiment was to determine the significance of the fungal inoculum potential and physico-chemical properties of five field trial test site soils, a garden compost known to cause white rot in copper treated fence palings, and soil from a zone between 2 and 15 centimetres from a CCA treated post with brown rot, in causing differential decay type in Pinus radiata and Poplus deltoides...
R N Wakeling


Biochemical aspects of white-rot and brown-rot decay
1987 - IRG/WP 1319
This paper presents an overview of the decomposition of wood by white- and brown-rot fungi - the most important and potent of known wood-decay fungi. These organisms are unique among cellulose destroyers because of their strong capability to enzymatically degrade lignified material. Special emphasis is given to the following aspects of wood decomposition by white- and brown-rot fungi: (1) effects...
T L Highley


Preliminary studies to assess the effects of aeration and lowered humidity on the decay capacity, growth and survival of the dry rot fungus Serpula lacrymans (Wulf ex. Fr.)
1997 - IRG/WP 97-10208
Novel microcosms were used to test separately the effects of aeration and humidity on the decay capacity, linear spread and survival of Serpula lacrymans. The application of a pumped air supply resulted in an effective cessation of fungal activity when all but the lowest of the air flow rates was used. Furthermore, the lowest air flow rate caused marked growth tropisms away from the stress. In sep...
G A Low, J W Palfreyman, N A White, H J Staines, A Bruce


Hygroscopicity of decayed wood - Implications for weight loss determinations
1996 - IRG/WP 96-20085
Hygroscopicity changes were observed in red maple blocks subjected to brown rot, white rot and soft rot. Brown rot reduced hygroscopicity, soft rot increased hygroscopicity, and white rot showed only a very slight increase in hygroscopicity. The effect of these changes on weight loss tests is a slight overestimation of weight loss for brown rot and a slight underestimation for soft rot and white r...
S E Anagnost, W B Smith


A light and electron microscopic study of decayed CCA-treated radiata pine (Pinus radiata) wood from a cooling tower
1994 - IRG/WP 94-10056
An inspection of an industrial cooling tower in New Zealand showed surface decay of 12 year old Pinus radiata wood panels treated with CCA preservative to a retention of around 15 kg/m³ of salt. Wood decay micromorphology typical of that caused by soft rot fungi, white rot fungi, 'stripy' and 'v-shaped' erosion bacteria and cavitation bacteria were all commonly...
A P Singh, R N Wakeling, D R Page


Ability of chitosans to limit wood decay under laboratory conditions.
2004 - IRG/WP 04-30339
Chitosans have recently been explored for controlling a number of plant pathogenic fungi and have shown some promise for controlling stain fungi on wood. The potential for using chitosans either alone or in combination with copper sulfate to protect wood from fungal decay was explored using maple veneers. Chitosan treatment reduce weight losses caused by two brown rot and one white rot fungi, howe...
M Maoz, J J Morrell


Statistical evaluation of 'micro-bending' samples for classification of wood attacking fungi
1992 - IRG/WP 92-1544
Micro-specimens from both hardwood and softwood were exposed to selected species of field isolated fungi. The strength reduction and weight loss caused by these fungi were determined. A statistical procedure was then developed to classify the fungi into brown-, white-rot, or non-decay fungal categories based on these data. The procedure reveals the extent of hazard a fungus poses to wood members. ...
B Goodell, Jing Liu, A Homola, J Jellison, J Shottafer


Influence of CCA and TnBTO on wood decay, under different oxygen levels and various initial moisture content
2001 - IRG/WP 01-10415
Fagus sylvatica (beech) and Pinus sylvestris (Scots pine) were impregnated by TnBTO (tributyl-tin oxide) and CCA (chromated copper arsenate). In wood blocks two levels of moisture content (50% and 100% of saturation point) were used. Three levels of oxygen concentrations (10, 21, and 50%) were chosen. Treated and untreated wood were exposed to three fungi (C. versicolor a white rot, C. puteana, a ...
S M Kazemi, R J Murphy, D J Dickinson


Extracellular hydrogen peroxide producing and hydrogen peroxide reducing compounds of wood decay fungi
1991 - IRG/WP 1516
Extracellular H2O2-producing and H2O2-reducing compounds were isolated from wood-containing cultures of all the white-rot and brown-rot fungi and Ascomycetes which well degraded wood, but were not detected in the culture of the fungi which degraded little wood. The compounds are glycopeptides with a low molecular weight, require H2O2 for one-electron oxidation, catalyze the redox reaction between ...
A Enoki, G Fuse, H Tanaka


Decay resistance of Platanus acerifolia wood against White Rot Fungi (Coriolus versicolor)
2002 - IRG/WP 02-10431
Degradation of the lignocellulose complex in wood varies on the microorganism causing decay and chemical composition of wood. The weight loss of Platanus acerifolia wood after decay by white rot fungus (Coriolus versicolor) for period 16 weeks were evaluated according to European standard EN 113 and beech wood as a control. The samples were collected in October 2000 from Nantes, France. The aim of...
M Irmouli, O Duchelier, N Ayadi, B Charrier


Micromorphology of Schizophyllum commune attack in pine (Pinus sylvestris) wood
1983 - IRG/WP 1184
The decay pattern caused by Schizophyllum commune in pine latewood tracheids was studied using both light and transmission electron microscopy. The attack began as isolated concentric slits within the S2 layer with extensive lamellation and separation of individual wall layers observed in subsequent stages of decay. The slits resulting from attack appeared to be formed in thin, regular concentric ...
T Nilsson, G F Daniel


Lab and field test results for wood treated with polymeric alkylphenol polysulfide
2001 - IRG/WP 01-30268
A new wood preservative based on polymeric alkyphenol polysulfide (PXTS-A) is being evaluated in a series of laboratory and field tests and the results continue to show promise. A modified formulation (PXTS-B), which contains additives to reduce the viscosity, is being evaluated along with the original formulation. Soil block decay tests comparing PXTS-B with CCA-C indicate that PXTS-B is equally ...
J Goswami, A Abramson, R Buff, D D Nicholas, T Schultz


Relative merits of laboratory and field tests for assessing wood decay resistance
1993 - IRG/WP 93-20009
Laboratory and field trials have long been employed for assessing natural durability of a variety of wood species, but there is a continuing debate concerning the relative merits of approach. While laboratory tests provide carefully controlled conditions for decay, they are often criticized for being too artificial to produce meaningful results. Conversely, field trials often vary widely between t...
T C Scheffer, J J Morrell


Cytoplasmic and extracellular localization of manganese II dependent peroxidase(s) in white rot fungi during degradation of woody materials
1989 - IRG/WP 1416
The manner by which lignin is degraded in-situ in natural substrates by white rot fungi still remains a controversial issue particularly the distribution and role(s) played by lignin degrading enzymes (i.e. manganese II peroxidase and lignin peroxidase). In the present study, use was made of anti-manganese II peroxidase and immunolabelling techniques in conjunction with transmission electron micro...
G F Daniel, B Pettersson, T Nilsson, J Volc


Micromorphology of decay in Keruing heartwood by the basidiomycetes Phellinus contiguus and Dacrymyces stillatus
2002 - IRG/WP 02-10454
This study aimed to characterise the micromorphology of fungal decay in a wooden handrailing in an above ground exposure at the Thames embankment in London. Keruing heartwood (Dipterocarpus spp.) was determined as the construction timber and the two basidiomycetes Phellinus contiguus and Dacrymyces stillatus identified as main decay organisms. Their decay patterns within Keruing heartwood were...
G Kleist, M Ray, R J Murphy


Microscopic analysis of southern pine utility pole core segments
1992 - IRG/WP 92-1542
Fifteen macroscopic core descriptive categories were evaluated by microscopic analysis for accuracy in detecting decay and judging decay severity. Five categories were good indicators of decay as decay was detected in 28 of 48 samples. Five categories were possible indicators of early decay as decay was detected in 6 of 40 core segments and an additional 18 contained hyphae. The remaining five cat...
S E Anagnost, C J K Wang, M Wright


The nature of osmiophilic particles and their distribution during different stages of brown and white rot decay
1983 - IRG/WP 1213
The distribution of osmiophilic particles during the course of brown and white rot decay was investigated by applying transmission electron microscopic (TEM) methods. It was found that it correlates with the brown and white rot pattern.The osmiophilic particles are produced by the fungus and are supposed to be wood rotting enzymes....
K Messner, H Stachelberger


Evaluation of the natural durability and ultrasonic method for decay detection of some european hardwood and softwood species
2004 - IRG/WP 04-10537
This paper presents the first part of an investigation on the natural durability of mixed plywood made of durable and non durable plies from the following selected timbers : Cedrus atlantica, Cupressus sempervirens, Castanea sativa, Populus sp. I 214 and Fagus sylvatica. In order to carry out this study, the natural durability of the massive wood used to manufacture the plywood panels was asses...
F Faraji, M-F Thévenon, B Thibaut


Redox regulation of enzyme activity during wood decay
1996 - IRG/WP 96-10172
A potential strategy in the search for alternative wood preservatives against fungal decay is to target the extracellular wood-decay process itself, rather than the decay organisms. This presents novel targets for selective disruption and possibly without the broad-spectrum toxicity associated with conventional wood preservatives. The enzymes of white rot decay are mechanistically diverse (e.g. hy...
P J Kersten, B Kurek, J W Whittaker


Natural Durability studies and Changes in wood chemistry of some Ghanaian hardwoods during decay by white- and brown-rot fungi
2004 - IRG/WP 04-10542
The natural decay resistance of Esa (Celtis mildbraedii), Wawabima (Sterculia rhinopetela) and Dahoma (Piptadeniastrum africanum) obtained from Ghana was determined according to BS EN 113 (1997). Esa was found not durable to the white-rot, but very durable to the brown-rot; Wawabima was very durable to both white- and brown-rots; and Dahoma was durable to the white-rot, and very durable to the bro...
Zeen Huang, K Maher, S A Amartey


Efficacy of waterborne copper naphthenate as preservative for northern hardwood species
1995 - IRG/WP 95-30091
Northern red oak (Quercus rubra) and red maple (Acer rubrum) cubes pressure treated with waterborne formulation of copper naphthenate were evaluated for resistance to attack by brown fungi Gloeophyllum trabeum (Pers. ex Fr.) Murr. (Madison 617 ATCC 11539) and Poria placenta (Fr.) Cooke (Madison 698, ATCC 11538), white rot fungi Trametes versicolor (L. ex Fr.) Pilat (R-105 from Jeff Morrell), Irpex...
D P Kamdem, R Fair, M H Freeman


Colonization of treated and untreated ponderosa pine exposed in Hilo, Hawaii
1995 - IRG/WP 95-20068
The rate of decay in above ground exposures is largely controlled by rainfall and temperature, factors which can be used to construct a climate index of decay hazard in above ground exposures. Developers of new biocide formulations have utilized this knowledge by establishing test sites in sub-tropical regions such as the Gulf Coast of the United States. More recently, field sites have been locate...
C M Freitag, J J Morrell, K J Archer


Method of embedding and staining of wood after biological testing to support the identification of decay type
1998 - IRG/WP 98-20131
A method for preparing wood for microscopic analysis after decay testing is described, with special regard to a novel fast simultaneous staining, which helps to identify different types of decay. The novel staining process is explained as well as the embedding of heavily decayed samples in polyethylene glycol (PEG) and picking up of sections by transparent adhesive tape. Special feature of the int...
A O Rapp


Occurrence and importance of various types of fungal and bacterial decay in CCA-treated horticultural pine posts in New Zealand
1984 - IRG/WP 1234
A detailed microscopical examination has been carried out on samples taken from CCA-treated pine posts exposed in horticultural soils. The following decay types were observed: white rot, brown rot, soft rot, tunnelling bacteria, cavitation bacteria, and bacterial erosion. The occurrence and importance of the various decay types between different regions, and plots within a specific region, varied ...
T Nilsson


Extracellular osmiophilic particles in connection with brown rot and white rot
1982 - IRG/WP 1157
The way of attack on Pine woodblocks of two brown-rot fungi (Fomitopsis pinicola, Coniophora puteana) differing in their cellulase activities, and one white-rot fungus (Trametes hirsuta) has been investigated by transmission electron microscopy. Even at early stages of decay, osmiophilic particles were found with all the fungi investigated. In the brown-rotted wood, the osmiophilic particles occur...
K Messner, H Stachelberger


Previous Page | Next Page