Decay Resistance of Maple (Acer Insigne) Wood Against White Rot
2010 - IRG/WP 10-10740
In this study, the decay resistance of maple (Acer insigne) in natural state and treated with ACC (Acid copper chromate) was investigated against the white rot fungus (Coriolus versicolor). ACC is a kind of water borne preservatives that was used in this study for treating specimens under vacuum and pressure (Bethell procedure) with 3 percent concentration. In conducting mentioned evaluation, koll...
V Tazakor Rezaei


Analyzing hyphal growth of the bio incising fungus Physisporinus vitreus with light-, confocal laser scanning- and, Synchrotron X-ray tomographic microscopy
2010 - IRG/WP 10-20438
Norway spruce wood is an important building material for the forest and wood industry. To improve wood permeability and uptake of wood modification substances Physisporinus vitreus is employed as a bioincising agent. In this study wood specimens were incubated with P. vitreus to assess hyphal colonisation and structural alterations of Norway spruce wood. After different incubation periods, semi-th...
C Stührk, M Fuhr, M Schubert, F W M R Schwarze


Kinetic Water Vapour Sorption of Sitka Spruce at Variable Temperature Using the Parallel Exponential Kinetics Model
2010 - IRG/WP 10-40512
In this study the water vapour sorption of Sitka spruce (Picea sitchensis (Bongard) Carr.) was measured using a Dynamic Vapour Sorption (DVS) apparatus and then analysed using the parallel exponential kinetics (PEK) model. The water vapour sorption rate of wood quickly increased when the relative humidity was changed. With the elapse of time, the sorption rate gradually decreased within any specif...
Yanjun Xie, C Hill


Study of Microscopy Properties of Modified Wood During Weathering Process
2010 - IRG/WP 10-40517
In this study spruce (Picea excelsa) and Beech (Fagus orientalis) wood acetylated and has been subjected of artificial weathering in difference times (0, 50,150&300 h), then wood surface analyzed using Scanning Electron Microscopy (SEM). The SEM results shown that the surface of wood exposed to weathering undergoes distinct physical changes and the surface degradation appears to be directly propor...
M Akhtari


Testing of decay resistance of sapwood and heartwood of thermally modified Scots pine and Norway spruce
2010 - IRG/WP 10-40523
Thermal modification at elevated temperatures changes the chemical, biological and physical properties of wood. One of the main targets of thermal modification is to increase the biological durability and decay resistance of wood. Although the effects of thermal modification on wood have been widely studied, the significance of sapwood and heartwood on the resistance of thermally modified wood has...
H Viitanen, S Metsä-Kortelainen


Effect of Coatings on the Durability of Birch and Spruce Plywood. Part 1: Weathering Performance
2010 - IRG/WP 10-40526
Several different coated birch and spruce plywood types were investigated in Finland using outdoor weathering. The weather performance of the tested coated birch plywood was good compared with uncoated birch and spruce plywood. The paint base film coated and painted birch plywood performed well in outdoor testing at VTT's test site. Phenol film coated plywood was sensitive to UV light, but on...
A Nurmi, H Viitanen


Effect of Coatings on the Durability of Birch and Spruce Plywood. Part 2: Biological Durability
2010 - IRG/WP 10-40527
Several different coated birch and spruce plywood types were investigated in Finland using the combination of outdoor weathering and decay test EN 12038. The most important factor to affect on the biological performance of birch plywood, coated and uncoated, was edge sealing. For spruce plywood edge sealing had a smaller effect. However, in spite of positive effect against decay, edge sealing did ...
A Nurmi, H Viitanen


Biological resistance of acetylated particleboards exposed to white (Trametes versicolor (and brown (Coniophora puteana) rot fungi
2010 - IRG/WP 10-40534
This research was conducted to investigate the effect of acetylation on bioresistance of particleboard produced from acetylated wood chips of Fagus orientalis exposed to white (Trametes versicolor (and brown (Coniophora puteana) rot fungi. After 12 hours soaking in acetic anhydride, in order to achieve three level of weight gains, 5, 9 and 16%, acetylated particles were heated in an oven at 120 c...
M Ghorbani kokandeh, K Doosthoseini, A N Karimi, B Mohebby, H Asghari


Decay resistance attributes of teak (Tectona grandis L. f.) wood: comparison of the fungicidal activities of quinones
2011 - IRG/WP 11-10752
The implication of quinones in decay resistance of teak wood is controversial. To better understand the role of individual quinone in this property, we studied the correlations between this latter and the content of 2-(hydroxymethyl)anthraquinone, tectoquinone, anthraquinone-2-carboxylic acid, 1,4-naphthoquinone, lapachol and the new compound 4’,5’-dihydroxy-epiisocatalponol found in teak wood...
F B Niamké, N Amusant, N Lemenager, G Chaix, M-F Thévenon, C Baudassé, S Kati-Coulibaly, A Amissa Adima, I Gossan Ado, C Jay-Allemand


Wood protection by nano silver against white rot
2011 - IRG/WP 11-30554
This research was done with the aim of investigation on the natural durability of poplar (populous deltoides) in natural situation and treated with nano silver against the white rot. Testing samples was treated with the method of modified soaking and nano silver in 3 treating level of 0,200 and 400ppm. In this study effect of coriolus versicolor fungus (identificated as white rot) on populous del...
V Tazakor Rezai, A Usefi, M Soltani


Influence of wood swelling agents on penetration and copper leaching of copper-ethanolamine based wood preservatives
2011 - IRG/WP 11-30556
Copper ethanolamine based preservatives are currently the most important solutions for impregnation of wood in ground contact in Europe. One of the issues related to those and similar water based solutions is insufficient penetration to refractory wood species like Norway spruce. In order to elucidate this issue, commercial copper ethanolamine based solution was supplemented with five different wo...
M Humar, N Thaler, B Lesar


Adsorption boundary curve influenced by step interval of relative humidity investigated by Dynamic Vapour Sorption equipment
2011 - IRG/WP 11-40547
The adsorption of water vapour from dry conditions by Norway spruce sapwood has been investigated using Dynamic Vapour Sorption (DVS) instrumentation. This equipment allows a fast and easy data acquisition as well as enables detailed studies of sorption properties using very small sample masses. In this study, particular focus was paid to the effect of step size on the sorption isotherms. Furtherm...
E Tang Engelund, M Klamer, T Mark Venås


Study of the durability of the Maderon® against wood decay fungi and insects
2011 - IRG/WP 11-40548
Many industries produce residues that are not easily degradable. One of these is nut husks which, due to their high level of resistance to biological and environmental degradation, have become an ecological problem. Maderón® is a material invented and patented in Spain employed as an ecological substitute and a modern alternative to certain uses of wood. At present, Maderón® is commercialized ...
M T Troya, F Llinares, P Jiménez, J I Fernández-Golfín, M Conde, R Díaz


A Review of Radial Flow of the Refractory Softwoods: An Example of Sitka Spruce
2011 - IRG/WP 11-40564
As one of the refractory softwood species, the major problems in the preservative treatment of spruce based on the radial flow relate to the anatomical structure of the wood material. The most important morphological features influencing this were the amount of the nature and the condition of both ray tracheids and ray parenchyma cells, and the cross-field pits in particular. The conducting pathwa...
Ilker Usta, Radovan Despot


Influence of soil moisture, Sarawak soil types and decay types on decay susceptibility of rubberwood and kelempayan
2012 - IRG/WP 12-10780
Wood and soils are important natural resources of the land, the former widely used as structural supports in contact with the latter. Many low durability wood species exposed to soil contact has reportedly high incidence of decay failures in poorly treated and untreated materials depending on soil types, properties and soil microbial virulence. This paper probes the relationship of the main soil t...
A H.H. Wong, P K.F. Chong, J Sabang


In-ground variability of decay intensity within a test field
2012 - IRG/WP 12-20496
Timber exposed in the ground faces most severe conditions in terms of exposure to wetting and fungal decay in the terrestrial environment, therefore wood durability tests are often conducted in test fields preferably ensuring the occurrence of all relevant decay organisms. One can also expect differences in decay within an individual field-test site due to localized distribution of certain organis...
C Brischke, S Olberding, L Meyer, T Bornemann, C R Welzbacher


Evaluation of Five Novel Organotin(IV) Complexes as Wood Preservatives
2012 - IRG/WP 12-30590
Three selected non durable tropical wood species namely Alstonia scholaris (pulai), Macaranga triloba (mahang) and Hevea brasiliensis (rubber) were chemically impregnated with five novel organotin(IV) complexes using vacuum-pressure treatment method. The objectives of this study were to determine the treatability and efficacy of novel organotin(IV) complexes against white and brown rot decay fungi...
M M Rahman, I Jusoh, M A Affan, A Husaini


Antifungal activities of acetone-soluble Eusideroxylon zwageri and Potoxylon melagangai crude extracts against white rot
2012 - IRG/WP 12-30591
The development of natural wood extracts as a wood preservative is a potentially attractive prospect for the wood preservation industry. This study attempts to evaluate the toxicity of Eusideroxylon zwageri and Potoxylon melagangai extractives as potential wood preservatives. These two species are well-known as among the heaviest and very durable timbers. It has been established that natural durab...
I Jusoh, A Tida Henry, Z Assim, F Badruddin Ahmad, S Ujang


Performance of wood treated with linseed and tung oil against wood decay fungi and wetting
2012 - IRG/WP 12-30598
Most of the European wood species does not have durable wood. In order to use it in outdoor conditions nondurable material has to be protected. Nowadays, non-biocidal solutions for wood protection are attracting a lot of attention, particularly in use class 2 and 3 applications. One of the non-biocidal techniques is treatment of wood with water repellents like wax emulsions and oils. Linseed oil a...
M Humar, B Lesar


Classifying white rot decay resistance of some hardwoods from Sarawak and Peninsular Malaysia and correlations with their tropical in-ground durability
2012 - IRG/WP 12-10788
White rot wood decay under Malaysian (humid tropical) terrestrial conditions pose more serious threats to the in-ground service life of hardwoods than other common fungal decay types. A study is made on decay resistance variation for a total combined list of 30 Peninsular Malaysian and Sarawak timber species (plus 6 exotic reference temperate commercial woods for comparison) using the laboratory s...
A H H Wong, J M E Jem, Lai Jiew Kok


Field-testing of Norway Spruce Claddings with Monitoring of Moisture Content, Material Temperature and Microclimate
2012 - IRG/WP 12-20502
The physical function of a cladding is to protect the interior construction. Under normal circumstances the performance requirements can be met for a very long time, meaning that the technical service life of a wooden cladding can be very long. Since the cladding is a major part of the facade, it also has visual requirements that may define the aesthetic service life, and often it is much shorter ...
G I Vestøl, L Ross Gobakken


Wood-leather panels – A biological, fire retardant building material
2012 - IRG/WP 12-40615
The poor flame retardant properties of wood-based products are among the severest obstacles, hindering its use in the commercial building sector. Recently, some attempts to improve the fire properties, relying on inflammable salts or reactive halogen compounds, have been presented, although they either cause problems with machining or embody harmful compounds (halogen derivates). In this paper, ...
S Wieland, U Stöckl, T Grünewald, S Ostrowski, A Petutschnigg


Water absorption and desorption of non treated, pressure impregnated, and pine oil treated glulam made of small diameter Scots pine and Norway spruce
2012 - IRG/WP 12-40616
A growing proportion of harvested timber originates from the first or second commercial thinning stands in Finland, which means smaller average log volumes in comparison to final felling stands. Smaller log volume means challenging wood properties such as higher proportion of juvenile wood and sapwood. Due to these facts, products made of small diameter logs are prone to twist and check, and have ...
H Heräjärvi, V Möttönen, R Stöd


The influence of microclimate on the moisture conditions in a Norway spruce (Picea abies (L.) Karst.) joint exposed to artificial rain
2013 - IRG/WP 13-20505
Wood structures outdoors are susceptible to decay if they are exposed to high moisture contents during long periods of time. Structures with joints that act as water traps are especially exposed since high moisture contents are reached in such positions. This paper presents a part of a laboratory study that concerns the relationship between the microclimate and the material climate, i.e. the moist...
M Fredriksson, L Wadsö, P Johansson


Determination of the natural durability of solid wood against wood-destroying fungi - a European round-robin test
2013 - IRG/WP 13-20511
In Europe the durability of wood against wood-destroying basidiomycetes is tested according to CEN/TS 15083-1 (2005). Hitherto existing experience with this standard is quite heterogeneous and results from previous round-robin tests have stayed unreported or have been reported incompletely. In particular the need for natural pre-weathering of the test specimens to allow potential detoxification of...
C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar, K Plaschkies, W Scheiding, G Alfredsen, J Van Acker, I De Windt