Lab and field test results for wood treated with polymeric alkylphenol polysulfide
2001 - IRG/WP 01-30268
A new wood preservative based on polymeric alkyphenol polysulfide (PXTS-A) is being evaluated in a series of laboratory and field tests and the results continue to show promise. A modified formulation (PXTS-B), which contains additives to reduce the viscosity, is being evaluated along with the original formulation. Soil block decay tests comparing PXTS-B with CCA-C indicate that PXTS-B is equally ...
J Goswami, A Abramson, R Buff, D D Nicholas, T Schultz


Durability aspects of (hydro)thermal treated wood
2000 - IRG/WP 00-40160
Samples of several wood species were treated in a two steps process, subsequently hydrothermal and dry heat-treated, by the so-called PLATO-process and analysed for their resistance against fungal attack. Both PLATO-treated and dry heat-treated specimen were prepared and analysed, in order to study the influence of moisture during hydrothermal treatment of wood. The resistance against all of the s...
B F Tjeerdsma, M Stevens, H Militz


Relative merits of laboratory and field tests for assessing wood decay resistance
1993 - IRG/WP 93-20009
Laboratory and field trials have long been employed for assessing natural durability of a variety of wood species, but there is a continuing debate concerning the relative merits of approach. While laboratory tests provide carefully controlled conditions for decay, they are often criticized for being too artificial to produce meaningful results. Conversely, field trials often vary widely between t...
T C Scheffer, J J Morrell


Cell wall microdistribution of chloropicrin and methylisothiocyanate in treated spruce
1989 - IRG/WP 3548
Chloropicrin and methylisothiocyanate (MIT) residues were observed using SEM/EDXA and TEM/EDXA in treated spruce wafers that had been exposed to the vapors of the two fumigant preservatives. Chlorinated residues from chloropicrin were found throughout the wood cell wall, even in acetone extracted material. The residues were most heavily concentrated in extractive materials in the rays, but unlike ...
G F Daniel, B Goodell


Movement of borates in a range of timber species at various moisture contents
1998 - IRG/WP 98-30181
Borate-based wood preservatives are used in industrial pre-treatment as well as remedial treatment of timbers in situ. In both of these areas, understanding the mobile nature of these compounds is important in optimizing the main benefits of borates. Considerable work has been conducted on movement of borates in dip-diffusion treatment of freshly felled wood, as well as focusing on subsequent diff...
M W Schoeman, J D Lloyd, M J Manning


Determination methods of phytotoxic effect of wood preservatives
1990 - IRG/WP 2349
The phytotoxic effect of wood preservatives so widely used plays a considerable role in the protection of natural environment. A review was made of the existing methods with which to assess the phytotoxicity of the above chemicals and some suggestions were given concerning the methods most appropriate for their unification. Two areas of research are proposed: 1) estimating the direct effect on ind...
A Kundzewicz, J Wazny


Sampling and analysis of NeXgen-treated timber
1998 - IRG/WP 98-20134
Green sawn timber surfaces of the softwood Caribbean pine and the hardwood white cheesewood were treated by dipping, spraying, and precise spiking with the antisapstain product NeXgen. After storing for either two hours or two weeks, the treated surfaces were sampled by one of four alternative protocols, which included two involving a square wad sampling punch (one hit or six hits), one involving ...
M J Kennedy, D E Ferlazzo, T L Woods, M H Freeman


Differences in pH, electrical resistance, cation composition and NIR spectra of red spruce wood during early stages of brown rot degradation
2002 - IRG/WP 02-10449
Red spruce sapwood was exposed to degradation by the brown rot fungi Coniophora puteana, Postia placenta, Gloeophyllum trabeum and Serpula lacrymans for 0, 1, 2 or 3 weeks using a modified soil block assay design. Average weight losses over time ranged from 0-8.9% during this time period. Detectable changes in pH, electrical resistance and cation compostion were observed in the wood as early as 1 ...
J Jellison, S Kelley, B Goodell, D Hui, A Ostrofsky


Färbeverfahren zur Unterscheidung von Holzzonen mit unterschiedlichem Absorptionsvermögen, insbesondere bei Fichtenholz (Picea abies Karst.). [Staining method for distinguishing zones of wood with different absorption behaviour, particularly in spruce (Picea abies Karst.)]
1980 - IRG/WP 3163
A simple regressive staining method for crosscut wood surfaces is described. Phloroglucinol-hydrochloric acid serves as stain; flowing water and a solution of sodium carbonate are used for development and fixation of a picture showing the differences of absorption. Hydrophobic zones and, contrary to this, zones with a high water content can also be shown. Comparing green spruce wood before and dur...
S Cymorek


Cytoplasmic and extracellular localization of manganese II dependent peroxidase(s) in white rot fungi during degradation of woody materials
1989 - IRG/WP 1416
The manner by which lignin is degraded in-situ in natural substrates by white rot fungi still remains a controversial issue particularly the distribution and role(s) played by lignin degrading enzymes (i.e. manganese II peroxidase and lignin peroxidase). In the present study, use was made of anti-manganese II peroxidase and immunolabelling techniques in conjunction with transmission electron micro...
G F Daniel, B Pettersson, T Nilsson, J Volc


Micromorphology of decay in Keruing heartwood by the basidiomycetes Phellinus contiguus and Dacrymyces stillatus
2002 - IRG/WP 02-10454
This study aimed to characterise the micromorphology of fungal decay in a wooden handrailing in an above ground exposure at the Thames embankment in London. Keruing heartwood (Dipterocarpus spp.) was determined as the construction timber and the two basidiomycetes Phellinus contiguus and Dacrymyces stillatus identified as main decay organisms. Their decay patterns within Keruing heartwood were...
G Kleist, M Ray, R J Murphy


Synergistic combination of an antioxidant and wood preservative: a preliminary study
1998 - IRG/WP 98-30172
We previously proposed that extractives in highly durable angiosperm heartwood may protect wood against white-rot fungal colonization and subsequent degradation by a dual mechanism: extractives have some fungicidal activity and are also free radical scavengers (antioxidants) and thus interfere with the fungal free radical degradative mechanisms. We tested this hypothesis using the commercial bioci...
T Schultz, D D Nicholas, J Minn, K D McMurtrey, T H Fisher


Accelerated diffusion treatment of sawn Sitka spruce grown in the UK
1986 - IRG/WP 3395
The treatment of 'green' sapwood and heartwood of Sitka spruce by diffusion methods was investigated. Steam/dip treatment processes gave increased solution uptakes and depths of penetration of copper in comparison with a simple dip treatment. Further investigation is required to reduce diffusion gradients with copper based formulations and to improve the penetration of '...
R J Murphy, D J Dickinson


Sawn timber of fir (Abies alba Mill.) - Treatability and usability for the Hazard Classes 3 and 4
1999 - IRG/WP 99-40147
Within a national research project, tests on the treatability on sawn timber of fir (Abies alba Mill.) in oscillation pressure, vacuum pressure and double-vacuum processes have been worked out with 95 trunks taken from 3 different altitude levels (up to a height of 590 metres, 600 to 990 metres and over 1000 metres) and from 4 different regions of Switzerland. As the treatability of round wood can...
E Graf, T Bör


Microscopic analysis of southern pine utility pole core segments
1992 - IRG/WP 92-1542
Fifteen macroscopic core descriptive categories were evaluated by microscopic analysis for accuracy in detecting decay and judging decay severity. Five categories were good indicators of decay as decay was detected in 28 of 48 samples. Five categories were possible indicators of early decay as decay was detected in 6 of 40 core segments and an additional 18 contained hyphae. The remaining five cat...
S E Anagnost, C J K Wang, M Wright


Improved preservative penetration of spruce after pre-treatment with selected fungi. II. Creosote treatment, analysis and strength testing
1998 - IRG/WP 98-40106
This paper describes the creosote treatment and analysis of logs pre-treated with selected fungal agents as a method of increasing the porosity of the wood prior to preservative treatment. The paper also reports the subsequent strength testing of the timber to evaluate the effects of the fungal pre-treatment on the structural integrity of the wood. European spruce logs were pre-treated with eithe...
E J Tucker, A Bruce, H J Staines, B Rosner, K Messner


Mechanistic aspects of the reactions of copper complexes with lignin in the presence of hydrogen peroxide and lipid hydroperoxide model compounds as proposed for white rot fungi
2001 - IRG/WP 01-10399
The structural principles and the oxidative reactions of the catalytic system consisting of copper, hydroperoxides, and copper coordination compounds that contain aromatic nitrogen atoms are similar to those of catalytic centers of oxidative enzymes involved in delignification reactions of white rot fungi. The system is capable of selectively degrading lignin and its low molecular weight would all...
K Fackler, P Lamaipis, E Srebotnik, M Humar, C Tavzes, F Pohleven, M Sentjurc, T Watanabe, K Messner


Improved preservative penetration of spruce after pre-treatment with selected fungi. I. Fungal pre-treatment of pole sections
1998 - IRG/WP 98-40117
European spruce logs were pre-treated with either Phanaerochete chrysosporium, Dichomitus squalens, Trichoderma viride and Trichoderma aureoviride for incubation periods of between 1-4 weeks prior to pressure treatment with creosote in a commercial treatment plant and analysed for strength and creosote uptake (see part II Tucker et al.). A method to pre-treat logs was optimised. The pole sections ...
B Rosner, K Messner, E J B Tucker, A Bruce


Fruitbody formation and basidiosporogenesis by the white rot fungus Pycnoporus cinnabarinus
1988 - IRG/WP 1348
Conditions for fruitbody formation by the white rot fungus Pycnoporus cinnabarinus in vitro were outlined. A marked difference in substrate requirements in comparison to previously tested brown rot fungi was revealed. Agar media containing Walseth cellulose and NH4 tartrate at 1 g/l permit profound production of basidiospores particularly at 15°C but only under light treatment. Higher NH4 tartrat...
J Bjurman


The nature of osmiophilic particles and their distribution during different stages of brown and white rot decay
1983 - IRG/WP 1213
The distribution of osmiophilic particles during the course of brown and white rot decay was investigated by applying transmission electron microscopic (TEM) methods. It was found that it correlates with the brown and white rot pattern.The osmiophilic particles are produced by the fungus and are supposed to be wood rotting enzymes....
K Messner, H Stachelberger


Influence of surface coating on the leachability of boric acid and bifluorides from spruce wood
1995 - IRG/WP 95-50050
In the Netherlands, window joinery made from non-durable timber species (spruce) are widely protected with preservative rods. These rods contain non-fixing wood preservatives (e.g. bifluorides or boric acid). This reseach was performed to show the possible influence of a coating system to hinder the leaching of the active ingredients. The results of the leaching tests show, that bifluorides and ev...
W J Homan, H Militz


Evaluation of the natural durability and ultrasonic method for decay detection of some european hardwood and softwood species
2004 - IRG/WP 04-10537
This paper presents the first part of an investigation on the natural durability of mixed plywood made of durable and non durable plies from the following selected timbers : Cedrus atlantica, Cupressus sempervirens, Castanea sativa, Populus sp. I 214 and Fagus sylvatica. In order to carry out this study, the natural durability of the massive wood used to manufacture the plywood panels was asses...
F Faraji, M-F Thévenon, B Thibaut


Redox regulation of enzyme activity during wood decay
1996 - IRG/WP 96-10172
A potential strategy in the search for alternative wood preservatives against fungal decay is to target the extracellular wood-decay process itself, rather than the decay organisms. This presents novel targets for selective disruption and possibly without the broad-spectrum toxicity associated with conventional wood preservatives. The enzymes of white rot decay are mechanistically diverse (e.g. hy...
P J Kersten, B Kurek, J W Whittaker


Natural Durability studies and Changes in wood chemistry of some Ghanaian hardwoods during decay by white- and brown-rot fungi
2004 - IRG/WP 04-10542
The natural decay resistance of Esa (Celtis mildbraedii), Wawabima (Sterculia rhinopetela) and Dahoma (Piptadeniastrum africanum) obtained from Ghana was determined according to BS EN 113 (1997). Esa was found not durable to the white-rot, but very durable to the brown-rot; Wawabima was very durable to both white- and brown-rots; and Dahoma was durable to the white-rot, and very durable to the bro...
Zeen Huang, K Maher, S A Amartey


Ammoniacal wood preservatives for use in non-pressure treatment of spruce and aspen poplar. Part 2
1984 - IRG/WP 3274
A series of thermal diffusion treatments were carried out on unseasoned white spruce (Picea glauca (Moench) Voss) lumber and air dry aspen poplar (Populus tremuloides Michx.) timbers using an ammoniacal copper arsenate wood preservative. Under the specific conditions described, certain charges of lumber met the present Canadian Standards Association Wood Preservation Committee's requireme...
C D Ralph, J K Shields