IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1102 documents. Displaying 25 entries per page.


Occurrence of wood-boring pholads in Kochi harbour waters (south-west coast of India)
1992 - IRG/WP 92-4175
The paper reports the occurrence of four species of wood-boring pholads (Pholadidae: Martesiinae), namely Martesia (Martesia) striata (Linnaeus), Martesia (Martesia) fragilis Verrill and Bush. Martesia (Particoma) nairi Turner and Santhakumaran and Lignopholas fluminalis (Blanford), in the Kochi back-waters, south-west coast of India. Of these Martesia nairi and Lignopholas fluminalis are now reco...
L N Santhakumaran, M V Rao


Toxic values derived from EN 113 tests - are they determined by the virulence of a test fungus? - Results from a round robin test -
1999 - IRG/WP 99-20176
The virulence of Coniophora puteana BAM Ebw. 15, the obligatory test fungus on softwood in tests according to EN 113, is known to be rather inconstant at least in some laboratories. The mass losses of untreated Scots pine sapwood blocks in an EN 113 test may range from below 20% to up to more than 50%. Possible reasons for these differences as well as the impact of a low virulence on the toxic val...
H Leithoff, R-D Peek, H V Borck, R Goettsche, H Kirk, M Grinda


Differences in pH, electrical resistance, cation composition and NIR spectra of red spruce wood during early stages of brown rot degradation
2002 - IRG/WP 02-10449
Red spruce sapwood was exposed to degradation by the brown rot fungi Coniophora puteana, Postia placenta, Gloeophyllum trabeum and Serpula lacrymans for 0, 1, 2 or 3 weeks using a modified soil block assay design. Average weight losses over time ranged from 0-8.9% during this time period. Detectable changes in pH, electrical resistance and cation compostion were observed in the wood as early as 1 ...
J Jellison, S Kelley, B Goodell, D Hui, A Ostrofsky


Preliminary evaluations of a small wafer assay for screening potential biological control agents
1989 - IRG/WP 2332
Screening potential biological agents for controlling wood decay fungi poses a dilemma. The ideal test would eliminate as many variables as possible. Most tests utilize pure cultures of the test organism on an artificial media which in no way resembles wood. The use of sawdust improves this approach, but the sawdust increases fungal access to the lignocellulose matrix, potentially inflating the im...
C M Freitag, J J Morrell


The evaluation of the effectiveness of wood preservatives by means of IUFRO's method for field tests with wooden stakes
1985 - IRG/WP 3348
Pinus elliottii and Eucalyptus saligna stakes treated with CCA-A, CCA-C, CCB, Cashew Nut Shell Oil and Benzotar solutions were exposed in seven test sites in Sao Paulo State, Brazil. After five years of exposure, between oil-borne preservatives Benzotar show better performance than CNSL (cashew nut shell liquid), and within waterborne preservatives the performance of CCB is not so good as that of ...
G A C Lopez, A M F Oliveira, E S Lepage


Current status of AAC preservatives in New Zealand
1980 - IRG/WP 3141
Two types of alkylammonium compounds (AAC) have been approved as commercially acceptable wood preservatives by the NZ Timber Preservation Authority (TPA). They are alkyldimethylbenzyl ammonium chloride and alkyldimethylamine acetate, both of which must contain either (a) 70% alkyl chains of C12 + C14 and less than 10% of any other individual chain length, or (b) 85% alkyl chains of C12 + C14 with ...
J A Butcher


European standardization for wood preservation
1991 - IRG/WP 2365
Since the last IRG 21 conference in New-Zealand, there one meeting of the plenary committee and several meetings of working groups. The interprative documents prepared by CCE for expliciting the essential requirements of the CCE Directive on the construction products and specially: mechanical resistance and stability / hygiene, health and environment / safety in use are waited to valid the progra...
Anonymous


The high decay resistance in the sapwood of the naturally durable Malaysian hardwood Belian (Eusideroxylon zwageri)
2001 - IRG/WP 01-10410
It has long been assumed that the observed natural durability of the heartwood in certain timbers is perhaps associated with a relatively lower decay susceptibility also of the sapwood of these species. While the heartwood of Belian is reputedly highly decay resistant among the tropical hardwoods of Southeast Asia, laboratory decay tests reported in this paper have also confirmed the high decay re...
A A H Wong, A P Singh


Regulation of hyphal sheath formation iron-chelator production by the brown rot fungi Gloeophyllum trabeum and Postia placenta
1994 - IRG/WP 94-10074
Hyphal sheath formation and iron-chelator production by liquid cultures of the brown rot fungi Gloeophyllum trabeum and Postia placenta were monitored over time. The effects of incubation at various temperatures, pH's and concentrations of iron, manganese and nitrogen were determined. Hyphal sheath production was observed microscopically and quantified with JAVA video analysis. The hyphal...
Y Chen, J Jellison


Co-operative research project on L-joint testing. Progress report to March 1986
1986 - IRG/WP 2272
Further sets of data received from CTFT (France) after 18 months exposure, BAM (Germany) after 18 months exposure, STU (Sweden) after 9.5 months exposure and TI (Denmark) after 12 and 17.5 months exposure are presented and discussed in conjunction with data previously reported. The new data are generally in agreement with those presented previously and indicate the major difference between the co-...
J K Carey, A F Bravery


Results on field stake tests against termite – Maximum for 8 years examination at Kumamoto in Japan
2003 - IRG/WP 03-10463
Various preservative treated or modified wood and charcoal painting stakes were tested in field, maximum for eight years in Kumamoto, distributed two main termite species, Coptotermes formosanus and Reticulitermes speratus. After two years in field, untreated sapwood of sugi (Cryptomeria japonica) were observed severe attacks by termites, but the preservative treated stakes were observed no signif...
K Suzuki


The Effect on Biological and Moisture Resistance of Epichlorohydrin Chemically Modified Wood
2002 - IRG/WP 02-40224
Southern pine solid wood and fiber were chemically modified with epichlorohydrin to help in understanding the role of moisture in the mechanism of biological effectiveness of chemically modified wood. The solid wood had weight gains from 11% to 34%, while the fiber had weight gains from 9% to 75%. After modification, part of the specimens were water leached for 2 weeks or extracted for 2 hours ...
R E Ibach, B-G Lee


The Copper Tolerance of Mycelium vs. Spores for Two Brown Rot Fungi
2002 - IRG/WP 02-10422
The copper tolerance of two brown rot fungi, Gloeophyllum sepiarium and Oligoporus placentus, has been tested using both mycelia and basidiospores as inoculum sources. Mycelial growth of O. placentus on agar medium was shown to be much more tolerant to copper (as copper sulfate) than that of G. sepiarium. However, there was no difference in copper tolerance of basidiospores between the two specie...
S Choi, J N R Ruddick, P I Morris


Window test. Direct testing of wood resistance to decay: A study of its fitness, its reliability and its accelerating factor
1984 - IRG/WP 2219
This is the results of an experiment using the window-test specimens, exposing the specimens to three different types of testing procedure: 1. Natural infestation in the open air; 2. Artificial infestation and exposure in the open air; 3. Artificial infestation in a green-house. The results show good similiraties of the three parallel tests in term of decay, and assess the reliability of the windo...
G R Y Déon, L N Trong


Nasutitermes exitiosus and wood-rotting fungi in Eucalyptus regnans, E. acmenioides, E. wandoo, and E. marginata: force-feeding, laboratory study
1985 - IRG/WP 1231
Under a force-feeding regime, the termitid Nasutitermes exitiosus was fed on four eucalypt timbers infested with several fungal species to investigate the influence of such fungus-infested timbers on mass of wood lost, termite biomass, fat content and water content. The results showed that wood mass losses were markedly affected by species of fungi and timber. The interaction of fungi and timbers ...
D B A Ruyooka


A field test with anti-stain chemicals on sawn pine timber in Brazil
1989 - IRG/WP 3513
Field tests were carried out in São Paulo State - Brazil, to evaluate pre-treatment formulations of O-Phenyl-Phenol (OPP) based products. The Sodium Pentachlorophenate solution was used as a reference formulation. The treated test blocks were stacked in a covered shed, and in an uncovered place for air drying. The evaluation was done by measuring the percentage of stained surface on each test blo...
M B B Monteiro, S Brazolin


Suitability of cotton strip testing as a screening method for the development of wood preservative formulations
2003 - IRG/WP 03-20270
This paper outlines a simple and rapid test method for screening the efficacy of wood preservative formulations against microbiological attack using cotton strips. The method was evaluated against soft rot and was found to provide reliable information on the protection of lignocellulosic material against microbiological attack. The assessment is based on visual interpretation of decay and on a sim...
H Leithoff, I Stephan, H Härtner


Properties of cellulose degraded by the brown rot fungus, Postia placenta
1988 - IRG/WP 1350
To gain further understanding of the nature of the cellulose depolymerizing agent or agents of brown-rot fungi, brown-rotted cellulose was chemically and physically characterized. Various culture conditions, such as low nitrogen and elevated oxygen levels, did not induce degradation of cellulose by Postia placenta in liquid cultures. Therefore, brown-rotted cellulose for analysis was prepared by a...
T L Highley, R E Ibach, T K Kirk


Wood decay of Pinus sylvestris L. and Fagus sylvatica L. by marine fungi. Part 2
1991 - IRG/WP 1471
The water-logged wood conservation requires a good knowledge of the wood decay organims which produce the degradation. Previous conducted studies (ESCORIAL, TROYA, GARCIA DE LOS RIOS, 1990) have shown that the incubation times normally used for in vitro laboratory tests are not sufficients for a significant wood degradation. This has been the reason why the aim of this work was the study of such d...
M T De Troya, A M Navarrete, M C Escorial


Accelerated termicidal performance data for new water-based copper linoleate formulations
1996 - IRG/WP 96-30104
An organic solvent based copper linoleate (Culin) has proved itself as an effective wood preservative in long term field trials in South Africa over a period of 30 years. Whilst the organic solvent based product offers good wood preservative performance, primary industrial interest has been in an emulsified version of the product. The objective of this study was to evaluate the influence of two di...
D Conradie, P Turner


Developments in unsterile soil soft rot testing
1984 - IRG/WP 2210
Two unsterile soil test methods, the soil burial technique and a method using vermiculite burial with soil inoculation, were compared using different soils to determine their effectiveness in evaluation of wood preservatives against soft rot. Isolation of fungi and microscopy of decayed wood indicated that both methods produced accelerated soft rot attack in treated and untreated birch. Vermiculit...
P A McKaig


Artificial weathering as an aid to assessing the effectiveness of chemicals for preventing blue stain in service - a co-operative study
1984 - IRG/WP 2215
The paper reports co-operative studies carried out within Working Group II of the International Research Group on Wood Preservation to assess the effects of different artificial weathering systems on the performance of fungicides to control blue-stain in service. It has been shown that Atlas, Xenotest and Marr equipments operated according to particular standard schedules can give essentially the ...
A F Bravery, D J Dickinson


Extracellular hydrogen peroxide-producing and one-electron oxidation system of brown-rot fungi
1990 - IRG/WP 1445
Wood-component-degrading compounds involved in the initial degradation of the cellulose and lignin in wood were isolated from wood-containing culture of brown-rot fungi, Gloeophyllum trabeum and Tyromyces palustris and partially purified by gel filtration on Sephadex G-25 and DEAE-Sepharose ion-exchange chromatography. The compounds were glycoproteins. The molecular weights of the glycoproteins as...
A Enoki, S Yoshioka, H Tanaka, G Fuse


Leaching from CCA-treated wood submerged in seawater: Effect of high loadings, and a comparison between laboratory and marine conditions
1996 - IRG/WP 96-50080
This study of leaching examined the following variables: CCA loading; marine versus laboratory exposure and length of submergence. Blocks of Pinus sylvestris were treated to a range of nominal retentions from 15 to 50 kg/m³. Each block was then divided into three cubes and all transverse faces were sealed. All cubes were allowed to fix at ambient temperature for a minimum of one week. One set of ...
R M Albuquerque, S M Cragg, J D Icely


Growth of the copper tolerant brown rot fungus Antrodia vaillantii on different substrates
1995 - IRG/WP 95-10121
In recent years the copper tolerant brown rot fungus Antrodia vaillantii caused severe damages on impregnated wood in ground contact. The pattern of decay gave the impression that impregnated wood was even more severely attacked than unimpregnated. To investigate this question more closely laboratory tests were carried out. In a "choice test" Antrodia vaillantii grew preferably towards CC-impregna...
H Leithoff, I Stephan, M-T Lenz, R-D Peek