High-frequency monitoring of mass loss due to brown rot degradation of modified wood
2016 - IRG/WP 16-10862
Fungi growing in liquid culture undergoes three separate phases in which they i) adapt to the new environment, ii) grow unrestrictedly and exponentially, and iii) are inhibited to increase in number/mass due to lack of nutrients etc. Filamentous fungi have been shown to exhibit similar growth phases in a solid food substrate and have been modelled to grow in this way also in solid wood. In modifie...
R Ringman, A Pilgård, K Richter


Moisture induced risk and fungal development in various field test set-ups in and above ground
2016 - IRG/WP 16-20577
A high number of studies on the decay performance of wood in outdoor exposure have been conducted in the past. However, no testing methodology for wooden components exposed above ground reflecting the variety of different loads has been established so far. Many test protocols were modified in different ways throughout the years and results were often published in an encoded or incomplete way. This...
L Meyer-Veltrup, C Brischke


Bundle tests - Simple alternatives to standard above ground field test methods
2016 - IRG/WP 16-20581
Within this study we applied different new above ground test set ups to untreated Norway spruce (Picea abies Karst.) and Scots pine sapwood (Pinus sylvestris L.) which are frequently used as reference or control species in wood durability field tests. The overall aim of this study was to find a simple alternative method to the few standardized above ground field test methods, such as the L-joint a...
C Brischke, L Meyer-Veltrup


Measurement of Cell Wall Moisture in Acetylated Radiata Pine Using Low-Field Nuclear Magnetic Resonance
2016 - IRG/WP 16-20583
Understanding the interaction of water with acetylated wood is necessary to explain how the protective mechanism of acetylation functions. Low-field nuclear magnetic resonance is one technique for assessing water in wood. Pinus radiata earlywood sapwood samples were acetylated to various weight percentage gains and then analysed with this method. Increased levels of acetylation showed significantl...
H G Beck, C A S Hill


Evaluation of advanced tannin-boron preservative in unsterile soil-bed tests
2016 - IRG/WP 16-30693
In Europe, boron compounds are facing restrictions, and due to their natural solubility into water, the only way to keep using them for wood protection is to fix them into the wood, at very low level (Obanda et al. 2008). In the meantime, the idea of protecting wood with natural preservatives has been back into favour (Lotz and Hollaway 1988, Nakayama et al. 2001, Singh and Singh 2012). Tannin a ...
Jinbo Hu, Yiqiang Wu, Shanshan Chang, Guangming Yuan, G Tondi, M-F Thévenon


10 year Report on COST E37 Round Robin Tests – Comparison of results from laboratory and field tests
2017 - IRG/WP 17-30718
A round robin involving 15 European participants was set up in 2006. The round robin consisted of both a field test according to the double layer test method and a laboratory test with two different preconditioning methods. The laboratory test results were reported in an earlier IRG paper (IRG/WP13-20535) but are included also in this paper in order to facilitate the comparison with the field test...
M Westin, E Conti, J Creemers, P-O Flæte, A Gellerich, I Irbe, M Klamer, E Melcher, R Moeller, L Nunes, S Palanti, L Reinprecht, E Suttie, H Viitanen


Redwood Durability in NZ – Can pure culture laboratory tests predict outdoor service life
2017 - IRG/WP 17-20610
Coast Redwood (Sequoia sempervirens) is an alternative species in New Zealand to the large scale Pinus radiata plantations. Redwood is classified as moderately durable but its durability is extremely variable. In order to reduce this variability in future stock, understanding growth conditions, clone, and tree age effects are important however this involves many samples and is not suitable for ass...
D O’Callahan, C Chittenden, J van der Waals, D Meason, T Singh


Monitoring Diversity and Colonization Patterns of Wood-Inhabiting Fungi Using Field Stake Tests
2017 - IRG/WP 17-20614
Advances in molecular identification of microbial communities enabling rapid microorganism determination have allowed ecological data to be increasingly incorporated into standardized wood performance tests. Combining standard field tests with molecular methods to study wood-associated microflora can help to better understand fungal colonization and decay processes of wood in service. The potentia...
P Torres-Andrade, J Cappellazzi, J J Morrell


Activity of Two Strobilurin Fungicides Against Three Species of Decay Fungi in Agar Plate Tests
2017 - IRG/WP 17-30704
The objective of this study was to examine the toxicity of strobilurin fungicides against wood decay fungi in order to assess their potential to act as a co-biocide for copper-based wood protection. Two strobilurin fungicides, Heritage (50% azoxystrobin active ingredient) and Insignia (20% pyraclostrobin active ingredients), and copper sulfate pentahydrate were tested against one white rot fungus...
J D Tang, T Ciaramitaro, M Tomaso-Peterson, S V Diehl


Hybrid green composites manufactured with glass fiber and jute fabric skin by VARTM process: Fungal, mold, and termite resistance tests
2017 - IRG/WP 17-40780
Hybrid green composites are increasingly used in building applications due to the development of new production approaches. Biological performance of such composites is needed when they are employed in extreme conditions. Hybrid composite panels were manufactured by wood furnish, glass fiber, and jute fabric skin by the vacuum assisted resin transfer molding (VARTM). Petri dish test method was fol...
S N Kartal, E Terzi, M Muin, A H Hassanin, T Hamuoda, A Kilic, Z Candan


Markers of quality in self-bonded beech boards
2017 - IRG/WP 17-40820
A self-bonding phenomenon takes place when five layers of beech (Fagus Sylvatica L.) veneers are pressed at temperatures higher than 200ºC. If the pressing temperature between veneer surfaces reaches at least 225ºC during pressing and if the pressure applied is optimal, water-resistant bonds are formed between veneers. This study investigates the relation of thickness reduction (marker of compre...
C Cristescu, D Sandberg, O Karlsson


Natural resistance of Bambusa vulgaris to termite and powder-post beetle attack in laboratory and graveyard tests
2018 - IRG/WP 18-10925
Deterioration is the major setback to the utilisation of bamboo products. To enhance bamboo utilization, an understanding of the level of resistance to degradation is important. In this study, level at which Bambusa vulgaris will naturally resistant attack by subterranean termites and powder-post beetles were evaluated. B. vulgaris aged 2, 3 and 4 years were subjected to attack by subterranean ter...
N A Sadiku, S O Bada


Testing the durability of timber products above ground using the block-test method – A critical review
2018 - IRG/WP 18-20637
The block-test method for testing the durability of wood and wood products above ground is reviewed critically with respect to practical aspects, moisture loads, corresponding decay development, and the possibilities of assessing test specimens by determining the dynamic modulus of elasticity (MOEdyn) of wood. In total, 36 blocks representing different modifications of the original set-up and a wi...
C Brischke, A Gellerich, H Militz


Performance of acetylated wood in aquatic applications
2018 - IRG/WP 18-40822
Acetylation of wood to enhance its resistance against wood decaying fungi and insects has been studied extensively under both laboratory and terrestrial field trials. Also several studies are investigating the performance of acetylated wood in marine and fresh water exposures. This paper updates nine year marine tests with acetylated radiata pine in Hejlsminde (Denmark) and presents data on 3 year...
F Bongers, S Palanti, A Gellerich, J J Morrell, J Creemers, J Hague


Resistance of modified wood to termite attack assessed in laboratory and field testing: A review of internal research
2018 - IRG/WP 18-40824
Within the past decades, new wood modification technologies have been investigated in order to improve certain wood characteristics and enable the use of timber products for outdoor applications. Some of these non-biocidal technologies have been developed and commercialized recently. Thus, various material properties were studied intensively and shown to be improved. To a great extent, previous re...
L Emmerich, P Gascón-Garrido, H Militz


Long-term performance of DMDHEU-treated wood exposed in ground, above ground and in the marine environment
2018 - IRG/WP 18-40825
Chemical wood modification with N-methylol compounds such as 1.3-dimethylol-4.5-dihydroxyethyleneurea (DMDHEU) has been studied intensively since the 1990s. Research of the past years focused on treatment of Scots pine (Pinus sylvestris L.) and European beech wood (Fagus sylvatica L.) and was shown to be applicable to improve specific material properties. A high resistance against wood-destroying ...
L Emmerich, H Militz, C Brischke


Identifying the fungal community on western redcedar (Thuja plicata) wood in field tests above and in ground contact exposure: preliminary results
2019 - IRG/WP 19-10939
Western redcedar (Thuja plicata) is a high value species in the Canadian forest industry due in large part to the natural durability of its heartwood. Western redcedar heartwood contains extractives that are inhibitory to the growth of many fungi responsible for decay. In order to gain insights into which extractives are important in long term durability, and which fungi are important to decay of ...
A Dale, S Kus, R Stirling


Performance of untreated timbers in above ground decking tests: Preliminary results from an international collaborative trial
2019 - IRG/WP 19-10940
The ability to accurately predict wood decay risks under varying environmental conditions has long been of interest to timber users. Accurate predictions are difficult owing to the myriad of variables associated with the decay process including wood species, wood inhabiting organisms, timber building element design and environmental conditions. Despite these difficulties, decay predictions have be...
L P Francis, J Norton, E Melcher, A H H Wong, J Kok Lai, M Klamer, M J Konkler, J J. Morrell


From fungal detoxification systems to wood durability in neotropical forests
2019 - IRG/WP 19-10946
White-rot fungi are able to mineralize all the wood components due in particular to an efficient detoxification system. We hypothesised that components of this detoxification systems, glutathione transferases, could be used as tools to explore the natural durability of neotropical wood species. Analysis of the interactions between six glutathione transferases of Trametes versicolor and extracts of...
T Perrot, G Salzet, N Amusant, J Duchene, E Gelhaye


Using X-ray micro-CT to evaluate density loss in anobiid infested wood
2019 - IRG/WP 19-10956
Considering the relevance of wood borers in construction, the present study had as main objective the evaluation of the impact of anobiid damage on timber elements by establishing an empirical correlation between lost material percentage (LM%, consumed by beetles) and apparent density (original – OTD and residual – RTD). Since the beetles’ attack produces a diffuse damage with a set of tunne...
J L Parracha, M F Pereira, A Maurício, P Faria, L Nunes


Validation by micro-computed tomography of an assessment method to measure the residual strength of anobiids infested timber
2019 - IRG/WP 19-20650
In this article a quantitative correlation study of pine timber structural elements, which have been subject to attack by anobiids, is presented. The main objective of the study was to establish a valid empirical correlation between the lost material percentage (consumed by beetles) and original/residual apparent density. Since the beetles’ attack produces a diffuse damage with a set of tunnels ...
J L Parracha, M F Pereira, A Maurício, P Faria, L Nunes


Durability classification of preservative treated and modified wood
2019 - IRG/WP 19-20659
EN 350 (2016) allows formally to determine durability classes (DC) for wood products and wood-based materials, which was previously only possible for untreated wood in the form of natural durability. In a first study, the University of Goettingen carried out the durability classification of chemically modified (modified with 1,3-dimethylol-4,5-dihydroxyethyleneurea, DMDHEU) and preservative-treate...
S Bollmus, L Bachle, C Brischke, H Militz


Exploring the use of X-ray micro CT as a tool for the monitoring of moisture production and mass loss during lab-based fungal degradation testing
2019 - IRG/WP 19-20654
Bio-based building materials, such as wood and wood-engineered products, are susceptible to degradation by decay fungi. In-depth knowledge on the intricate material-fungus relationship as well as performance data for many bio-based building materials are still lacking, and especially knowledge on how a material’s structure and moisture properties affect the degradation process is missing. Althou...
L De Ligne, J Van den Bulcke, A De Muynck, J M Baetens, B De Baets, L Van Hoorebeke, J Van Acker


Alternative fumigants to Methyl Bromide for wood products: Review of the development and preliminary tests of Ethane Dinitrile (EDN) in Canada
2019 - IRG/WP 19-30743
This paper reviews recent developments and updates in the search for alternative fumigants to ozone-depleting methyl bromide, for wood products fumigation. The absence of alternative treatments may result in significant market disruption if further restrictions on methyl bromide are imposed. This paper reviews key challenges and key attributes of an ideal fumigant and also the status of standardis...
A Uzunovic


Gloss and hardness variations as early indicators of wood coating failure during weathering tests
2019 - IRG/WP 19-40866
The objective was to track early changes which ultimately will lead to coating failure when exposed to artificial weathering. Two different coatings (one waterborne acrylic paint and one solventborne alkyd stain) were exposed to artificial weathering for 2016 hours according to EN 927-6. Every 168 hours, samples were removed from the artificial weathering device for assessment (general appearance,...
L Podgorski