IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 340 documents. Displaying 25 entries per page.


Formation of biofinishes on outdoor exposed wood; the impact of wood-oil combination and geographical location
2016 - IRG/WP 16-10864
Growth of dark moulds enables the use of a decorative and protective biofinish for wood, showing advantages compared to traditional wood-coatings in terms of sustainability and self-repair. Based on the formation of a uniform mould covering on oil treated wood during outdoor exposure, the utilisation of a biofinish is in development. Basic information is lacking on the correlation between exposure...
E J van Nieuwenhuijzen, L Ross Gobakken, M F Sailer, R A Samson, O C G Adan


Identification of the key factors influencing development of the blue stain fungi
2016 - IRG/WP 16-10872
Service life of wood is more and more frequently affected by aesthetic requirements than functional ones. In order to elucidate various aspects of service life, model house with façade elements made of 22 materials was built on the field test site at Department of Wood Science and Technology in Ljubljana. Colour and fungal disfigurement is among other parameters monitored on this house. In parall...
D Kržišnik, B Lesar, N Thaler, M Humar


Simulation of surface climate and mould growth on wooden façades
2016 - IRG/WP 16-20585
The weathering of wooden surfaces is normally caused by mould growth, lignin deterioration and leaching of extractives. For well insulated buildings, the effect of the interior climate on the outer surface is small and sometimes negligible. This paper describes simple models for surface temperature and moisture conditions on a wooden façade that can further be used to model weather degradation an...
T K Thiis, I Burud, D Kraniotis, L Ross Gobakken


Expert versus multi-sensor evaluation of wood samples after short term weathering
2016 - IRG/WP 16-20587
Understanding the influence of weathering factors and the material degradation mechanisms are fundamental for modelling the weathering process of wood. The goal of this work was to investigate the combined effect of time and exposure on the physical-chemical mechanisms of wood weathering. Four exposure directions (North, South, East and West) were investigated. Experimental tests were performed fo...
A Sandak, J Sandak, I Burud, L Ross Gobakken, M Noël


Effects of fungal exposure on air and liquid permeability of nanosilver- and nanozincoxide-impregnated Paulownia wood
2016 - IRG/WP 16-30680
Effects of aqueous dispersion of silver and zinc-oxide nano-particles on air and liquid permeability of Paulownia wood exposed to T. versicolor were studied in the present research project. Specimens were also heat-treated at 100 and 150°C and compared with the control specimens. Permeability values were measured when the moisture content of the specimens was 12%. Results showed significant incre...
H R Taghiyari, A Kalantari, M Ghorbani Kookandeh, F Bavaneghi, M Akhtari


Accelerated Weathering Performance of Impregnated Wood Samples Coated with Zinc by Means of Plasma-Assisted Particle Deposition
2016 - IRG/WP 16-30682
Many different methods are currently applied for wood protection against outdoor conditions. The most important of these is the process of impregnation with liquid substances. However, this kind of wood preservatives cannot provide a long-term protection of wooden surfaces. Weathering-resistant surfaces can be obtained by applying UV absorbing agents. In this study, the influence of zinc particles...
A Can, H Sivrikaya


Effects of Bio-oil Obtained from Laurel (Laurus nobilis) Residues on Biological, Physical, and Mechanical Properties of Treated Wood
2016 - IRG/WP 16-30692
In this study, the effects of bio-oil obtained from Laurel (Laurus nobilis) residues on biological (decay, insect, termite resistance), physical (water absorption, tangential and radial swelling), and mechanical properties (MOE, MOR and CSPG) of treated wood samples were studied. The bio-oil used in this paper was produced by the help of fixed bed reactor type pyrolyzer. GC/MS analysis showed that...
S Akbas, A Temiz, N Terziev, M H Alma, S Palanti, E Feci


Fabrication and characterization of MicroPCMs filled wood-plastic composites: Effects of polyethylene glycol on melamine–formaldehyde shell material
2016 - IRG/WP 16-40728
Microencapsulated phase change materials (MicroPCMs) containing dodecanol were fabricated using melamine-formaldehyde (MF) or polyethylene glycol 200 modified melamine-formaldehyde (PMF) resin as the shell materials by in situ polymerization. Wood flour/high-density polyethylene (WF/HDPE) composites with MF shell MicroPCMs (MF-MicroPCMs) or PMF shell MicroPCMs (PMF-MicroPCMs) were prepared, respec...
Xi Guo, Jinzhen Cao


Colorant Treatments to Enhance the Weathering Resistance of Western Red cedar
2016 - IRG/WP 16-40737
Western redcedar is renowned for its decay resistance, but, like most wood products, it requires frequent maintenance in many exterior applications to maintain its appearance. To provide adequate long-term performance in exterior applications, it must be protected against light, water, and disfiguring fungal growth. Colorant treatments, with and without preservatives, were investigated for their a...
R Stirling, V Landry


Variation in coating hardness during the EN 927-6 weathering test: influence of pigmentation
2016 - IRG/WP 16-40739
The objective of the SERVOWOOD project is to develop and establish European Standards that will facilitate the prediction of service life for exterior wood coatings. Within this project an extensive round robin exercise has been carried out by five partners to establish the repeatability and reproducibility of the EN 927-6 artificial weathering test. This round robin included the exposure of the I...
L Podgorski, L Malassenet, C Reynaud


Fungal resistance and accelerated weathering of Wood-Plastic composites reinforced with Maritime pine wood flour
2016 - IRG/WP 16-40750
This study evaluates the durability of wood-polymer composites (WPCs) elaborated for use in cladding application from recycled polypropylene (rPP) and wood flour. Local Maritime pine wood flour derived from regional sawmills was used in the study to reduce the environmental impact associated with transport. Different wood-plastic ratios with and without UV stabilizers and biocide were tested. One ...
M Jebrane, T Fournier, N-E El Bounia, F Charrier-El Bouhtoury


Accelerated weathering and fungal resistance of wood modified with isopropenyl acetate
2016 - IRG/WP 16-40764
Chemical modification of Rubberwood (Heveabrasiliensis Müll.Arg) with isopropenyl acetate (IPA) in presence of anhydrous aluminum chloride and iodine as catalysts was carried out. Modified wood surfaces were exposed to UV light source in an accelerated weathering tester to evaluate UV resistance. Anti-swelling efficiency (ASE) and fungal resistance of modified wood were also evaluated. Modified w...
G B Nagarajappa, K K Pandey


Evaluation of the effects of different concentrations of Fipronil against Reticulitermes grassei (Blattodea: Rhinotermitidae)
2016 - IRG/WP 16-30702
A laboratory evaluation of the effect of different concentrations of Termidor (fipronil at 9.09%) has been carried out. Six concentrations (10,000; 1,000; 100; 50; 10 and 5 ppm) have been tested in two different colony models imitating an open environment. After five days treatment, mortality data were collected. The three higher concentrations showed nearly 100% mortality. At 50 ppm the mortalit...
J R Carbonero-Pacheco, R Molero, M E Alcaide, J Diz, M Gaju


Effects of wollastonite nanofibers on biological resistance of historical paper against Aspergillus niger
2017 - IRG/WP 17-10878
Effect of wollastonite nanofibers on biological resistance of historical paper against Aspergillus niger was studied. Specimens from A4 papers were also prepared for comparison purposes. Paper specimens were dipped in aqueous nanowollastonite (NW) with 10, 20, 30, and 40% concentrations and compared with control specimens. In order the nanofibers be fixed on paper specimens, 5% of polyvinyl acetat...
H R Taghiyari, A Kalantari, A Ershad-Langroudi, A Kalantari


Effects of climatic factors and material properties on mould growth on untreated wooden claddings
2017 - IRG/WP 17-10884
Mould growth is an important contributor to colour change of untreated wood exposed outdoors. Predicting the development of mould growth is therefore important to ensure successful use of untreated wood as a façade material. More knowledge about the factors affecting mould growth on outdoor exposed wood is required to give better predictions. In this study, climatic factors and material propertie...
S Karlsen Lie, G I Vestøl, O Høibø, L Ross Gobakken


Untreated and copper-treated wood soaked in sodium oxalate: Effects of decay by copper-tolerant and copper-sensitive fungi
2017 - IRG/WP 17-10888
Copper is widely used as the primary component in wood protectants because it demonstrates a broad range of biocidal properties. However, a key concern with using copper in wood preservative formulations is the possibility for brown-rot basidiomycetes to resist the toxic effect. Many brown-rot basidiomycetes have evolved mechanisms, like the production and accumulation of oxalate, which helps thes...
K M Ohno, G T Kirker, A B Bishell, C A Clausen


Fungal growth on coated wood exposed outdoors: influence of coating pigmentation, cardinal direction and inclination of wood surfaces
2017 - IRG/WP 17-10896
The objective of the SERVOWOOD project was to develop and establish European Standards that will facilitate the prediction of service life for exterior wood coatings. One of the objective of this project was to study fungal growth of the field exposed panels. Two coatings applied in 2 and 3 coats were exposed for one year outdoors at 45° south: one solventborne (alkyd based) and one waterborne (a...
L Podgorski, C Reynaud, M Montibus


Influence of Weathering on Moisture Performance of Wood
2017 - IRG/WP 17-20619
Water performance of wood is besides the inherent durability the most important factor that influences on the performance of wood in outdoor, above ground applications. Therefore it is of significant importance to optimize the methods that are able to predict the moisture behaviour of wood in outdoor applications. In order to elucidate this questions, samples were prepared of oak (Quercus), sweet ...
M Žlahtič-Zupanc, B Lesar, N Thaler, M Humar


Weathering protection of European hardwoods through double modification
2017 - IRG/WP 17-30715
Beech and poplar were thermally modified, treated with melamine resin and both treatments were combined. The weathering performance (cracks and general appearance) of modified beech and poplar was assessed in natural weathering and correlated to material properties such as work in bending (WB) and Brinell hardness. In addition, the equilibrium moisture content after exposure of 12 months and subse...
G Behr, A Gellerich, S Bollmus, H Militz


Effects of heat treatment on sound absorption coefficients in nanosilver-impregnated and normal solid woods
2017 - IRG/WP 17-40770
Effects of impregnation with silver nano-suspension as well as heat-treatment on sound absorption coefficients (AC) were studied in tangential direction of five different solid woods based on their importance. AC was measured at two frequencies of 250 and 500 Hz. A 400 ppm nanosuspension was used for the impregnation; silver nanoparticles had a size range of 30-80 nm. Based on the obtained results...
A Esmailpour, J Norton, H R Taghiyari, H Zolfaghari, S Asadi


Effects of Nano-Wollastonite Impregnation on Fire Properties of Some Thermally-Treated Solid Wood Species
2017 - IRG/WP 17-40771
The effects of nano-wollastonite (NW) suspension impregnation on the fire-retarding properties of heat-treated solid wood of three species (beech, poplar, fir) were studied. Heat treatment was performed at two temperatures of 180 °C and 200 °C. Impregnation was carried out at a pressure of 3 bars for 30 min. The fire properties included ignition time, glowing time, back-darkening, back-splitting...
H R Taghiyari, R Hossinpourpia, S Adamopoulos, A Jahangiri, D Rabie


The Comparison of Weathering Resistance of New Generation Wood-Coating Systems
2017 - IRG/WP 17-40789
In this study, the performance of wood-coating systems containing different UV absorbers was evaluated in artificial weathering conditions. Acrylic-based resin containing three different UV absorbers was applied on oriental beech and scots pine surfaces. Weathering conditions were sustained for 84 days. After the weathering test, the change of color and roughness on the wood surface was measured t...
Ö Özgenç, S Durmaz


The Effects of Pre-Microwave Treatment on Retention Levels And Some Mechanical Properties of Spruce Wood Treated with CCA
2017 - IRG/WP 17-40800
Microwave (MW) treatment of wood has been evaluated in recent years for different purposes by several scientists. Microwave conditioning improves permeability, reduces density and heat conductivity and changes dimensional stability. Furthermore, it could even improve the permeability of refractory wood species such as spruce and Douglas fir. In this study, MW pre-treatment was applied to spruce wo...
E D Gezer, S Kuştaş, S Durmaz


Surface Protection of Wood with Metal Acetylacetonates
2017 - IRG/WP 17-40802
Metal acetylacetonates are coordination complexes of metal ions and the acetylacetonate anion. They have diverse uses as catalysts, cross-linking and curing agents and adhesion promotors. Some metal acetylacetonates can photostabilise polymers whereas others are photocatalysts. We hypothesise that the ability of metal acetylacetonates to photostabilise wood will vary depending on the metal in the ...
Yuner Zhu, P D Evans


Studying Weathering Performance of Coatings on Thermally Modified Wood
2017 - IRG/WP 17-40805
Thermal modification and degree of improved properties depends on wood species and treatment parameters. Southern pine and spruce are the two common wood species for decking, fences and siding in North America. This study was the first to evaluate coating performance when applied on oil-heat-treated southern pine and spruce wood samples. Water uptake, colour and gloss changes of samples were analy...
M Nejad, M Dadbin, P Cooper


Previous Page | Next Page