Photostabilization of Wood with Higher Molecular Weight UV Absorbers
2010 - IRG/WP 10-30524
Higher molecular weight UV absorbers were created by reacting the epoxy-functionalized UV absorber 2-hydroxy-4(2,3-epoxypropoxy)-benzophenone (HEPBP) with maleic, phthalic or succinic anhydride. The ability of the UV absorbers to photostabilize wood was then examined. FTIR-spectroscopy confirmed that HEPBP reacted with phthalic anhydride to create a polyester that preserved the UV-absorbing benzop...
P D Evans, M J Chowdhury


Effects of polyvinyl alcohol on leachability and efficacy of boron wood preservatives against fungal decay and termites attack
2010 - IRG/WP 10-30526
In this study, the use of polyvinyl alcohol (PVA) as boron fixative agent was investigated. Two levels of PVA (2.5 and 4%) were evaluated with disodium octaborate tetrahydrate (DOT) at three concentrations (1, 2 and 4% boric acid equivalent (BAE) using a double vacuum impregnation processes on Scots pine sapwood specimens. Leaching was performed according to a laboratory leaching procedure. Boron ...
A Mohareb, M F Thévenon, E Wozniak, P Gérardin


Effects of Cunninghamia Lanceolata Heartwood Extracts on the Growth of Wood Decay Fungi
2010 - IRG/WP 10-30527
China-fir (Cunninghamia lanceolata) wood is well known for its good durability. This species is native to China and has been extensive planted there. Mainly, extractives are responsible for the wood resistance to decay fungi. In this paper, the extractives of China-fir heartwood were studied for their effects on various wood decay fungi. Sequential extraction of heartwood in hexane, ethyl acet...
Shujun Li, Jing Wang, Jian Li


Treatment of Scots pine wood with oil in water and water in oil emulsion systems: Effects on boron leaching and water absorption
2010 - IRG/WP 10-30535
The aim of this study was to investigate the water absorption and water repellent efficiency of oils and oil water emulsions [oil-in-water (O/W) and water-in-oil (W/O)] and possibilities of reducing the amount of boron leaching from treated wood. Scots pine wood samples treated with waste or sunflower oil and water formulations contained 3%BA. The level of water absorption and water repellent effi...
E D Tomak, Ü C Yildiz, A Can


The Effects of Some Fire Retardant Chemicals on the Decay Resistance of Medium Density Fiberboard (MDF)
2010 - IRG/WP 10-30536
The objective of this study was to determine the decay resistance of Medium Density Fiberboard (MDF) treated with 5% and 10% concentration of various fire retardant (FR) chemicals. Experimental panels were produced using by melamine-urea-formaldehyde (MUF) resins having 10%, 15% and 20% of melamine content. MDF specimens were subjected to decay resistance test performed according to modified EN 11...
D Ustaömer, M Usta, Ü C Yildiz, S Yildiz, E D Tomak


Copper preservative systems: A rapid investigation into effects of co-biocides and used treating solutions
2010 - IRG/WP 10-30541
The efficacy of various micronized and amine copper preservative systems was evaluated using soil block testing with the copper tolerant brown rot fungi, Postia placenta. The American Wood Protection Association E22 protocol was used to compare the relative efficacy of preservatives by monitoring compressive strength losses of the systems in southern pine wood. As information, the weight losses ...
T F Shupe, K Ragon, Q Wu, M H Freeman, C R McIntyre


Comparison of colour change in wood clear-coating systems including inorganic and organic UV absorbers for exterior use
2010 - IRG/WP 10-40499
The aim of this work is to compare the performance of inorganic and organic UV absorbers used in a wood coating application against weathering. Our study has investigated the colour changes of selected UV absorbers; hombitec 402 RM from the Sachtleben Company as an inorganic UV absorber, tinuvin 477 DW from the Ciba Company as an organic UV absorber. The study was carried out on two wood species; ...
Ö Özgenç, B Forsthuber, A Teischinger, C Hansmann


Performance of selected types of coated and uncoated modified wood in artificial and natural weathering
2010 - IRG/WP 10-40510
The objective of the present work was to investigate the influence of commercial wood modification methods on weathering behaviour and coating performance. It was aimed to compare modification methods and to set up maps of weathering behaviour for these methods with and without a semi-transparent wood stain. Artificial and natural weathering trials were carried out with a selection of different ty...
G Grüll, L Podgorski, M Truskaller, I Spitaler, V Georges, S Bollmus, A Steitz


Study of Microscopy Properties of Modified Wood During Weathering Process
2010 - IRG/WP 10-40517
In this study spruce (Picea excelsa) and Beech (Fagus orientalis) wood acetylated and has been subjected of artificial weathering in difference times (0, 50,150&300 h), then wood surface analyzed using Scanning Electron Microscopy (SEM). The SEM results shown that the surface of wood exposed to weathering undergoes distinct physical changes and the surface degradation appears to be directly propor...
M Akhtari


Impact of wood species on the performance of exterior wood coatings
2010 - IRG/WP 10-40519
To prolong the service life of a wooden construction the protective function of a coating is of utmost importance. The chemical composition as well as the wood-coating interface affects the performance of this protective layer and obviously wood species have an impact too. This paper discusses the influence of wood species on the overall coating performance. Therefore, a range of opaque waterborne...
I De Windt, J Van den Bulcke, J Van Acker


Effect of Coatings on the Durability of Birch and Spruce Plywood. Part 1: Weathering Performance
2010 - IRG/WP 10-40526
Several different coated birch and spruce plywood types were investigated in Finland using outdoor weathering. The weather performance of the tested coated birch plywood was good compared with uncoated birch and spruce plywood. The paint base film coated and painted birch plywood performed well in outdoor testing at VTT's test site. Phenol film coated plywood was sensitive to UV light, but on...
A Nurmi, H Viitanen


Effect of Coatings on the Durability of Birch and Spruce Plywood. Part 2: Biological Durability
2010 - IRG/WP 10-40527
Several different coated birch and spruce plywood types were investigated in Finland using the combination of outdoor weathering and decay test EN 12038. The most important factor to affect on the biological performance of birch plywood, coated and uncoated, was edge sealing. For spruce plywood edge sealing had a smaller effect. However, in spite of positive effect against decay, edge sealing did ...
A Nurmi, H Viitanen


Effects of global climate change on mould growth - Interactions of concern
2010 - IRG/WP 10-50270
An evident change in climate the last decades has been recorded, and combined effects of increased CO2, elevated temperature and altered precipitation regimes have been observed to represent a change to the fundamental drivers within ecosystems. Growth of moulds, both in nature and on man-made constructions and objects, will most likely increase due to changes in the climate. The survival, the rep...
L Ross Gobakken


Effects of intumescent formulation of vinyl acetate-based coating on flame-retardancy of thin painted red lauan (Parashorea spp.) plywood
2011 - IRG/WP 10-40537
Using intumescent coatings on wood-based materials is an effective method for fire safety. The intumescent coatings consist of four major components: (1) binder resin (BR), (2) carbonizing substance (CS), (3) foam producing substance (FPS) and (4) dehydrating agent (DA). Previous studies have demonstrated that the formulation of the four components strongly influences the performance of coatings. ...
Chih-Shen Chuang, Kuang-Chung Tsai, Te-Hsin Yang, Ming-Kuang Wang, Chun-Han Ko


The effects of acetylation level on the growth of Postia placenta
2011 - IRG/WP 11-10751
To understand the defence mechanisms utilized by decay fungi when exposed to different wood protection systems the study of gene expression can give us some answers. When the DNA sequences are known, primers can be designed to detect transcripts of genes with gene products related to basic cellular processes and hyphal growth. The characteristic gene products induced in different fungi by differen...
A Pilgård, G Alfredsen, C G Fossdal, C J Long II


The Effectiveness of Machined Profiles at Reducing the Checking of Wooden Decking
2011 - IRG/WP 11-40541
This study tests the hypothesis that ‘the ability of surface profiling to reduce checking of deck boards exposed to weathering will vary with wood species and profile type’. Southern pine (Pinus sp.) and Pacific silver fir (Abies amabilis) deck boards were machined to produce three different types of surface profiles: flat (control), ribbed (V-shaped grooves), and rippled (U-shaped grooves). B...
P Evans, I Cullis, P Morris


Evaluation of an optimized industrial process aiming to improve the natural durability and mechanical behavior of bamboo for outdoor use
2011 - IRG/WP 11-40554
Mao Bamboo (Phyllostachys pubescens) is characterized by high contents of sugar and starch and by high hygroscopicity, which makes it susceptible to biodegradation, and specifically to fungal decay. Still, many bamboo based products regularly enter the European wood construction market, competing with traditional solid wood products used for outdoor decking and cladding. The performance of a heat ...
F Simon, M Kutnik, I Le Bayon, G Moisset, V Gatimel


Effects of Heat-Treatment in Hot Water and Steam Mediums on Gas Permeability of Beech Wood
2011 - IRG/WP 11-40557
Heat-treatment, as a major method of wood modification, improving dimensional stability, and natural durability, has been studied greatly from different aspects. The effect of heat-treatment on gas permeability, as an important physical property of wood, in two different mediums of hot water and steam, as well as in two buffers of 7 and 8, is the main topic of the present study. Hydrothermal treat...
H Reza Taghiyari, A Talaei, A Karimi


Moisture protection and performance during 5 years exposure of 19 wood coating systems on a cladding in Vienna
2011 - IRG/WP 11-40561
A cladding with vertical boards of Norway spruce (Picea abies) comprising different coating systems had been exposed to natural weathering oriented south west in Vienna for 5 years. Weathering behaviour of the boards was assessed in intervals and wood moisture content was measured over the first 22 months of exposure. The moisture protective properties of the coating systems were assessed using la...
G Grüll, I Spitaler, M Truskaller


Wet and dry adhesion of coatings on modified and unmodified wood: influence of 18 months of natural weathering on the pull-off test and cross-cut test results
2011 - IRG/WP 11-40569
The objective of this paper is to study the influence of several types of modification (acetylation, furfurylation, heat treatment) on coatings adhesion after 18 months of natural weathering according to EN 927-3 in Vienna (Austria). The paper compares two methods for assessing the adhesion: the cross-cut test (EN ISO 2409) which is the conventional method used and recommended in EN 927-3 and th...
L Podgorski, G Grüll, M Truskaller, J D Lanvin, S Bollmus


Effects of nano-silver on brittleness of heat-treated solid woods
2011 - IRG/WP 11-40572
The present study is aimed at the effect of heat-treatment of normal as well as nano-silver-impregnated Populus nigra, Populus deltoides, and Fagus orientalis on brittleness. Specimens were impregnated with 200 ppm water-based solution of nano-silver particles under 3 bars in a pressure vessel using empty-cell process. For heat treatment, both nano-silver-impregnated and normal specimens were kept...
H Reza Taghiyari, B Moradi Malek, A Karimi


Use of Variable Pressure Scanning Electron Microscopy for in situ Observation of Degradation of Wood Surfaces during Artificial Weathering
2012 - IRG/WP 12-20489
Variable pressure scanning electron microscopy (VPSEM) is capable of observing electrically non-conductive materials like wood without the need to render the surface conductive by applying a coating of gold, platinum or carbon. Hence, there is the possibility that VPSEM could be used to non-destructively follow the structural changes occurring at wood surfaces during weathering, because specimens ...
F Hatae, Y Kataoka, M Kiguchi, H Matsunaga, J Matsumura


Effects of microclimate, wood temperature and surface colour on fungal disfigurement on wooden claddings
2012 - IRG/WP 12-20490
Wooden claddings are common in façades in Norway, and Norway spruce (Picea abies) is the most frequently used species. The cladding is a major part of the facade, and it has visual requirements that may define the aesthetic service life. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more of...
L Ross Gobakken, G I Vestøl


Effects of oil types and treatment temperature on the properties of wood subjected to thermal modification in oil medium
2012 - IRG/WP 12-40574
The effect of the use of oil as a medium of heat transfer during thermal modification of different species of wood has been widely investigated with different results accruing with regards to the various end-use properties of the materials. However very little have been done on the effect of oil types as well as its interaction with treatment temperature on the resultant properties of the material...
L Awoyemi, M M Apetogbor, A A Oteng-Amoako


Effects of Nano-Wollastonite on Ignition Time Reduction in MDF
2012 - IRG/WP 12-40576
Effects of wollastonite nano-fibers on ignition time reduction in medium density fiberboard were studied. Nanowollastonite was applied at 5, 10, 15, and 20 g/kg dry weight basis of wood fibers and compared with control specimens. Two application methods of nanowollastonite were used: surface application, and internal application. Specimens of 150×130×9 mm were prepared and the ignition times wer...
H Reza Taghiyari, H Rangavar, P Noori, A Karimi


Previous Page | Next Page