IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 978 documents. Displaying 25 entries per page.


Soft rot - Soil burial - Tests. Influence of the water content of the soil on wood decay
1972 - IRG/WP 212
The decay of wood samples buried in the soil is influenced by various factors. Decisive are the water content, the content of organic substances, pH-value content of mineral nutritive substances etc. of the soil. For the tests, carried out by the EMPA until now, it was always started with a water content of 35%, refered to the dry weight of the EMPA-soil = 75% of its water capacity. In order to in...
O Wälchli


Environmentally benign biological wood preservatives by Streptomyces rimosus, SC-36
1997 - IRG/WP 97-10196
Microbiocides obtained from mutant culture Streptomyces rimosus SC-36 were evaluated for their abilities to inhibit the growth of brown-rot, soft-rot, white-rot, and sapstain fungi on wood. The test fungi were the brown-rot fungi Antrodia carbonica, Gloeophyllum trabeum, Neolentinus lepideus, and Postia placenta; soft-rot fungi Chaetomium globosum, Paecilomyces variotti, Phialocephala dimorphospor...
S C Croan


Preliminary results of the treatment of wood with chlorosilanes
1981 - IRG/WP 3172
It is clear from the initial data reported here that the treatment of pine sapwood with chlorosilanes under the reaction conditions employed did not significantly reduce the decay by both white rot and brown rot fungi. Only the dichlorosilane compounds showed to possess some protective action against fungal attack. Before drawing conclusions on the application of organosilicon compounds as potenti...
M Stevens


A preliminary assessment of the penetration into wood achieved by bodied mayonnaise emulsion wood preservatives
1992 - IRG/WP 92-3725
Five different commercial formulations of bodied mayonnaise emulsions were applied to samples of Scots pine (Pinus sylvestris) sapwood as recommended by the manufacturers. Penetration and loading characteristics were determined by measuring the distribution profiles of the active ingredients after various intervals of time. The changes in the general appearance of the emulsions on the surface of t...
G E Holland, R J Orsler


The effect of water-repellent additives on the leaching of CCA from simulated southern Yellow pine decks
2000 - IRG/WP 00-50158
End-matched SYP boards were pressure-treated with CCA or CCA in combination with commercial water repellent additives. After fixation and drying, the boards were placed in plastic boxes and exposed outside in Harrisburg, NC. Plastic supports were used to keep the boards above the water collected. Over a period of five months, rain run-off water from 14 natural rainfalls were collected and analyzed...
F Cui, P J Walcheski


Towards harmonisation of regional approaches for an International Standard for the approval of wood preservatives
1997 - IRG/WP 97-20122
Recent proposals from the European Standards body (CEN) for an ISO Standard on wood preservatives has initiated debate on whether there is any prospect of an acceptable common approach among ISO member countries, to a harmonised framework of hazard classes, with agreed supporting biological tests, leading to a unified rationale for demonstrating compliance with minimum performance standards for sp...
A F Preston, A F Bravery


In situ timber treatments by spraying. Distribution of preservative in wood
1991 - IRG/WP 3678
This study was carried out in order to make the Pest Control Operators able to achieve correct treatments and enhance their efficacy. It was carried out in two steps: 1) in laboratory, to learn the influence of various parameters like spraying pressure, use of repeated applications, distance from nozzle to wood; 2) in situ on roof timber of five buildings. In this case, the applications of the pre...
C Defoin, G Dupont, M Lamour, H Sageot, M-M Serment


Comparison of the effects of borate, germanate and tellurate on fungal growth and wood decay
1992 - IRG/WP 92-1533
The tetra-hydroxy borate ion is known to undergo complexation with polyols and has been shown to inhibit dehydrogenase enzymes in this way. It has been previously suggested that this complexation is responsible for the inhibition of fungal growth and the protection of boron treated timber. Other ions that have the ability to complex with polyols have also been shown to inhibit dehydrogenase activi...
J D Lloyd, D J Dickinson


Soluble nutrient content in wood and its susceptibility to fungal discoloration and decay in above ground and ground tests
2000 - IRG/WP 00-10336
The objective of this comprehensive study was to reveal the impact of soluble nutrients in wood on its susceptibility to fungal discoloration and decay in various tests, which is important for the test methodology and standardisation. Seven tests were carried out including pure culture above and ground contact tests, above ground field test and laboratory ground contact tests. The samples containi...
O M Caballero, N Terziev


Field testing of alkylammonium wood preservatives
1983 - IRG/WP 3248
The field test performance of five alkylammonium wood preservatives is described. The relative effectiveness of three unmodified formulations was determined by calculation of a Performance Index. Of the three, didecyldimethylammonium chloride was found to be superior to octyldecyldimethylammonium chloride, and both were more effective than alkyltrimethylammonium chloride. However, none were consid...
J N R Ruddick


Inorganic preservatives in wood dust - Cause of nasal cancer?
1997 - IRG/WP 97-50085
Since 1985 dust particles from beech and oak trees have been classified by the Senate Commission of the German Research Council (DFG) as being ,,working materials which are definitely carcinogenic to humans". All other wood dusts, including those from softwoods, are classified as being materials ,,with reasonable suspicion of carcinogenic potential". The carcinogenic principle of action continues ...
A O Rapp, K Brandt, R-D Peek, U Schmitt


Serpula lacrymans, The Dry Rot Fungus and its Tolerance towards Copper-based Wood Preservatives
2005 - IRG/WP 05-10555
Serpula lacrymans (Wulfen : Fries) Schröter, the dry rot fungus, is considered the most economically important wood decay fungus in temperate regions of the world i.e. northern Europe, Japan and Australia. Previously copper based wood preservatives were the most commonly used preservatives for pressure treatment of wood for building constructions. Because of a suspicion about tolerance toward cop...
A C Steenkjær Hastrup, F Green III, C A Clausen, B Jensen


Selective chromate elimination from the storage-drainage-water of a wood impregnation plant
1980 - IRG/WP 3153
With the Enviro-Chrom-Ex process it is possible to eliminate ecologically and economically hexavalent chromium (chromate) from water selectively. The process which is based on the principle of selective ion exchange works with different chromate concentrations and under the presence of other ions, irrespective of the water hardness. The values of water-offtake reach 0.1 mg CrVI at maximum, causing...
O Wälchli, R Ott, R Hugener, E Graf, B Lieberherr


Comparison of three methods for assessing the in-ground termite resistance of treated timber, durable timber and plastics at sites in Australia, USA and Thailand - First results
1998 - IRG/WP 98-20132
The in-ground resistance of materials to attack by subterranean termites is most commonly assessed with one form or another of the conventional graveyard method, despite the significant shortcomings of this method. In Australia, an alternative method, in which all samples of test materials are placed below-ground, has been in use for more than 10 years. The method provides reliable exposure of sam...
M Lenz, A F Preston, J W Creffield, K J Archer, B M Kard, C Vongkaluang, Y Sornnuwat


Determination of the water sorption properties and preliminary results from field tests above ground of thermally modified material from industrial scale processes
2004 - IRG/WP 04-40279
In this study the differences in moisture behavior and durability above ground of heat treated wood originating from different European industrial heat treatment plants by means of the water sorption properties as well as field tests were examined. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood (Premium wood)/ Finland and Menz Holz/ Germany, where Oil-...
C R Welzbacher; A O Rapp


A method for the preliminary assessment of timbers for their treatability with preservatives under pressure
1977 - IRG/WP 3100
President Maurice Fougerousse has provided the following references to a IUFRO report, published in English, French and German, which may be of interest to IRG members: 'A method for the preliminary assessment of timbers for their treatability with preservatives under pressure', PANS Vol 23, No 2, 153 158, June 1977. 'Une methode d'evaluation preliminaire de l...
M Fougerousse


Remedial treatments of glulam = diffusion of active ingredients through glue lines from solid wood diffusable preservatives
1996 - IRG/WP 96-30117
Diffusable preservatives are very suitable for use in remedial treatments of laminated beams in which too high moisture content involves the development of wood destroying fungi. The diffusion of active ingredients (boric acid, disodium octoborate, bifluoride) is well observed in solid wood but in a composite wood, the glue lines may appear not only as a barrier for the diffusion but also, may be ...
D Dirol, S Mouras


Accelerated laboratory testing of preservatives on 13 North American wood species
1999 - IRG/WP 99-30201
The ability of selected water and solvent based biocides to protect wood against fungal attack was evaluated on 13 North American wood species using 7 decay fungi in a modified soil block test. Most preservatives were capable of providing protection at their recommended above ground and soil contact use levels. Many decay fungi caused substantial weight losses on blocks treated with chlorothalonil...
J J Morrell, C M Freitag


An appraisal of methods for environmental testing of leachates from salt-treated wood; part 1
1998 - IRG/WP 98-50115
The magnitude and diversity of leaching tests with salt-treated wood, performed by institutes as well as industry, strongly appeal for harmonisation towards one single method. That procedure should be well-defined, cost- and time-effective and moreover be extended with a clear detection and interpretation scheme. The paper(s) presented here tend to evaluate 2 existing leaching methods, the ENV 12...
G M F Van Eetvelde, M Stevens, F Mahieu, H-W Wegen, A Platen


Observations on the performance of copper-based wood preservatives in fungal cellar (soil-bed) tests
1994 - IRG/WP 94-20047
Fungal cellar (soil-bed) tests are considered to be an important tool for the evaluation of the performance of ground contact wood preservatives. Facilities of this type have been established world wide although caution has been exercised in their introduction into standard testing methods for the approval of wood preservatives. This is the result of concerns over the variability in the biological...
G R Williams, D Rudolph, M E Hedley, J A Drysdale, R F Fox


Description of a trial with wood preservatives against marine wood boring organisms
1975 - IRG/WP 412
Wood situated in sea water along the Atlantic coasts of the Nordic countries is attacked by marine wood boring organisms. Timber constructions in these waters therefore must be preservative treated. In order to evaluate the effect of various preservatives against marine wood borers, the Nordic Wood Preservation Council (NWPC) organized a rather extensive trial in 1972. In the absence of and while ...
E Norman, B Henningsson


Vertical distribution of fouling and wood-boring organisms in the Trondheimsfjord (Western Norway)
1981 - IRG/WP 476
Results of a detailed study on the vertical distribution of fouling and wood-boring organisme of Trondheimefjord at an interval of 3 m from intertidal level to a depth of 30 m, has been presented, based on data collected from two series of panels, exposed from 15-3-1977 to 15-7-1977 (Series I) and from 22-7-1977 to 13-3-1978 (Series II). The intensity of fouling generally decreased with increasing...
L N Santhakumaran


Unsuitability of the limiting dose as a criterion for assessing the toxicity of preservatives to wood-destroying fungi
1974 - IRG/WP 243
In the majority of methods for investigating preservatives for wood-destroying fungi their toxicity is assessed by determining what is called the "limiting dose". This normally denotes a range of preservative solution concentrations or retentions of dry preservative in the timber, the lower value serving to indicate the amount of preservative at which is observed the expected effect, e.g. the grow...
D A Belenkov


The probable mechanism of action of boric acid and borates as wood preservatives
1990 - IRG/WP 1450
The tetrahydroxyborate ion [B(OH)4-] acts by complexation with poly-ols and probably attacks decay fungi through extracellular substrate sequestration; intracellular substrate sequestration; enzyme inhibition; and change in membrane function. Work was carried out to investigate this further and to try to explain certain phenomena observed in the area of boron preservation. The effect of Na borate ...
J D Lloyd, D J Dickinson, R J Murphy


Treatability of waterstored poles of Norway spruce by sap-displacement and pressure treatment with Boliden K33 and creosote
1973 - IRG/WP 328
Poles of windthrown Norway spruce were stored in bark under water sprinklers for 11-20 months or fully submerged in a lake for 3 years (tab. 1 and 2). Water content after storage is shown in fig. 1 and 8. Treatment with Boliden K33 by sap-displacement (open tank suction) gave a poor result. The Danish requirements of delivery claim a penetration of 20 mm and a net retention of 12 kg/m³ in outer 2...
P Moltesen, E Borsholt, B Bang


Previous Page | Next Page