Differential behaviour of wood rotters at water repellent Rubberwood
2000 - IRG/WP 00-10386
Rubberwood samples treated with different concentration of aqueous solution of chromic acid has induced significant increase in water repellency and attains dimensional stability. Though water repellency and dimensional stability was achieved by treatment, the fungal invasion could not be completely controlled. Differential level of decay of brown and white rot in wood treated with water repellent...
H C Nagaveni, S S Chauhan, K S Rao


Performance of treated spruce in Canadian field test sites
1989 - IRG/WP 3506
Spruce material under test in Canadian field test sites is performing better than anticipated. From the comparison of the performance of spruce treated with various preservatives, it appears that penetration may be far more important on durability performance than the preservative itself or the retention of preservatives in the wood. However, there is still insufficient data on the influence of pe...
J P Hösli, E E Doyle


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic conditions. Part 2: Semi-industrial investigation
1995 - IRG/WP 95-50040-13
In continuation of previous leaching research on the quantification and modelling of metal elements released from CCA treated timber, a series of experiments has been carried out dealing with the influence of temperature and pH of the relative aquatic environment. The leaching method used is the Dutch prestandard for building materials, a long term static leaching test simulating practical bank-sh...
G M F Van Eetvelde, W J Homan, H Militz, M Stevens


Some observations on miniaturised soil/block tests
1988 - IRG/WP 2317
Results are presented for miniaturised soil/block tests carried out in 120 ml capacity glass jars. The four test fungi (Coniophora puteana, Coriolus versicolor, Gloeophyllum trabeum and Poria placenta) reacted differently to different moisture regimes established by varying the soil moisture content. Acceptable levels of decay were achieved by the three brown rot fungi with soil at 110% whc; howev...
J K Carey


The use of zirconium as an inert fixative for borates in preservation
2001 - IRG/WP 01-30256
Stand-alone borates have been used in internal protected situations as wood preservatives for about 60 years. They have not been deemed acceptable for external situations because of their leaching characteristics. Work carried out to reduce the leachability of borates has been reviewed briefly here, and a specific fixation agent based on zirconium has been tested in standard leaching and decay tes...
J D Lloyd, J L Fogel, A Vizel


Patterns of long-term performance - How well are they predicted from accelerated tests and should evaluations consider parameters other than averages?
1998 - IRG/WP 98-20130
This paper is a discussion of whether different service-life distribution patterns of products treated with unlike preservatives can be predicted, modeled, characterized, or even anticipated from accelerated laboratory tests. Graphic displays of data from Forest Products Laboratory field plots with preservative-treated and fire-retardant-treated stakes demonstrate the importance of local environme...
R C De Groot, J W Evans


Risk assessment and the approval of wood preservatives in the United Kingdom
1995 - IRG/WP 95-50040-23
An approval system operates in the United Kingdom (UK) for the regulation of wood preservatives. The regulatory authority uses a risk assessment approach to evaluate how far the potential for harm to people and the environment from wood preservatives is likely to be realised in practise, and hence the controls required for products to be, used safely. The evaluation for approval purposes also take...
R M Turner


Available iron promotes brown rot of treated wood
1992 - IRG/WP 92-1526
Exposure of treated wood blocks to rusting iron increased the toxic threshold of chromated copper arsenate and ammoniacal copper arsenate to a brown-rot fungus Leucogyrophana sp. This supports the hypothesis that the movement of iron ions into wood contributes to the unexpectedly high decay rate of treated wood at the stake test site at Westham Island BC. To what extent this phenomenon may occur e...
P I Morris


Report of activity of CEN/TC 38: Test Methods for Wood Preservatives
1987 - IRG/WP 2287
G Castan


The proposal for optimalization of the agar-block method for wood preservatives fungitoxic evaluation
1995 - IRG/WP 95-20065
On the base of own research and other scientists results the proposal for optimalization of agar-block method was presented by: - selection of test fungal species and strains and central distribution of their pure cultures, - change of the treatment and control samples exposure procedure, - application of mathematical estimation of toxic value results, - shortening the duration of fungitoxic t...
J Wazny


A bibliography of organic solvent-based wood preservatives
1973 - IRG/WP 313 E
H Alliot


Questionnaire on the state of pollution control in the field of wood preservation
1974 - IRG/WP 52
H Willeitner


Literature survey on the permanence and distribution of salt-type wood preservatives
1969 - IRG/WP III 1B
The objective of this survey is generally to review some of the more important published work dealing with the distribution and permanence of salt-type waterborne wood preservatives in treated timber. The survey is limited to the major chrome-containing formulations and the classification system proposed by Becker (1964) has been adopted throughout. CK - chromium, copper (copper, chrome); CKA - c...
Anonymous


Preservatives treatment and field test monitoring of spruce pole stock: CCA and fumigant treatments
1990 - IRG/WP 3619
The fumigants trichloronitromethane (chloropicrin) and sodium N-methyldithiocarbamate (SNMDC) were used to treat red spruce pole stock, either CCA treated or untreated, through holes bored through the pole's center. The poles were analyzed for the presence of microorganisms immediately before ground installation and again after installation at a pole test site. Monitoring of fumigant move...
A J Pendlebury, B Goodell


Agenda Special Seminar: Screening techniques for potential wood preservative chemicals
1978 - IRG/WP 2115
IRG Secretariat


Developments in wood preservation processing techniques in New Zealand
1980 - IRG/WP 3143
P Vinden, A J McQuire


Bamboo preservation in Vietnam
2009 - IRG/WP 09-40457
This paper presents the current state of bamboo preservation in Vietnam. The report focuses on the importance of bamboo preservation in relation to the bamboo resource and utilization, the major methods for preservation (such as non chemical und chemical methods), and emphasises the today’s pressing problems of research, standards as well as information for the bamboo preservation industry in Vi...
Tang Thi Kim Hong


The Effect of Soil pH on the pH of Treated Southern Pine in Ground Contact after 12 Months
2011 - IRG/WP 11-50281
Southern pine samples treated with soluble and particulate copper solutions were subjected to three soils that had been amended to provide acidic, neutral and alkaline conditions. Wood pH was measured prior to, and after 6 and 12 months after being placed in the soil to determine the effect of soil pH on wood pH....
L Jin, C Schauwecker, C Vidrine, P Walcheski, A Preston


Methods of treatment of wood preservatives. The selection of appropriate preservation process with particular reference to mixed tropical forest resources. A key address
1982 - IRG/WP 3177
All wood is biodegradable. Many timber species have, however, sufficient natural durability to permit their use, particularly in protected situations, without any special precautions. Many others, of course, are readily attacked by insects and where there is sufficient moisture and air, by wood-decaying fungi. It is these timber species which benefit most from treatment with wood preservatives. Ev...
C R Levy


Development of a method for testing wood preservatives with soft rot fungi
1975 - IRG/WP 250
Although the first publications on experimental soft rot attack date back 20 years ago, so far no test method for evaluating the efficacy of wood preservatives against soft rot attack (Ascomycetes and Fungi Imperfecti) has been generally accepted. The reasons are diverse and the shortcomings and the disadvantages of the methods described are well known and have repeatedly been discussed. The soil ...
M Gersonde, W Kerner-Gang


Field and laboratory studies on anti-sapstain preservatives
1982 - IRG/WP 3205
The field tests included 11 different anti-sapstain preservatives and were carried out at different sawmills in southern Sweden. Drying conditions, climate and the local fungus flora were not identical for the different preservatives and comparisons between the preservatives should therefore be made with caution. Results obtained in the field tests are, however, in relatively good agreement with t...
M-L Edlund, B Henningsson


Evaluation and approval of wood preservatives in Japan
1988 - IRG/WP 2303
Japanese standardized decay test methods, performance requirements and approving system are briefly described. JIS (Japanese Industrial Standard) A 9302, which is related to a testing method for evaluating effectiveness of wood preservatives when applied to pressure treatment, is fundamentally a sand-block laboratory test method. According to performance requirements in JIS A 9201, mean percentage...
K Tsunoda


Incorporating insect behaviour in standard tests of wood preservatives - A possible way to reduce pesticide loadings
2000 - IRG/WP 00-20190
The application of wood preservatives to protect timber against insect infestation is common practice world wide. The effectiveness of wood protecting insecticides is usually determined in various standard tests. Depending on the target pest species and the test method, larvae of different developmental stages and sizes or adult insects are exposed artificially to the insecticide-treated commodity...
H Hertel, R Plarre


Natural durability of some common Indian timbers and marine plywood against biodeterioration in Kochi waters (India)
1992 - IRG/WP 92-4177
Panels of thirty-eight timber species and marine plywood were tested in Kochi harbour (South-west India) for periods ranging from 3 to 21 months, so as to evaluate their natural resistance against marine borers. Results indicate that all the timber species studied are non-durable, 6 of them having undergone more than 50% internal destruction within 3 months; 14 species in 6 months, 13 species and ...
L N Santhakumaran, M V Rao


Leaching of inorganic wood preservatives – Investigating the relationship between leachability, dissociation characteristics and long-term leaching potential
2003 - IRG/WP 03-50199
Estimation of the leaching properties of preservative components is greatly affected by the leaching test method applied since not all methods equally consider the physical components responsible for leaching. These include: wetting of the wood and penetration of water (affected by dimensions, amount of end grain, permeability, duration and nature of water exposure); solution of preservative comp...
L Waldron, Y T Ung, P A Cooper