The Effect of Heat Treatment on Water Absorption and Dimensional Stability of Anatolian Chestnut (Castanea sativa Mill.) wood
2008 - IRG/WP 08-40407
The heat treatment of wood is an environment-friendly method for wood preservation. This process improves wood’s resistance to decay and its dimensional stability. However, mechanical properties decrease in different ration because of density loss as a result of heat treatment. In this study, the effect of heat treatment on water absorption and dimensional stability at different relative humidit...
G Gunduz, D Aydemir


Near infrared spectroscopy for the quantification of wood preservatives
2008 - IRG/WP 08-20391
Near infrared (NIR) spectroscopy is a rapid, flexible, inexpensive and non-destructive technology that has many applications, including the evaluation of many wood properties. Initial studies have indicated the potential to apply NIRS for the quantification of wood preservatives. However, further evaluation with borate and azole preservative systems has revealed that NIRS technology is challenged ...
A M Taylor, Seung H Baek, Myong K Jeong, J D Lloyd, J J Morrell


Mold fungi - Major impediments to cleaning/repairing flood and rain-damaged homes
2008 - IRG/WP 08-40427
Damage to homes by hurricanes that make landfall in the south and southeastern United States, or sub-tropical and tropical regions, during the hot, humid summer months is compounded by the growth of mold fungi on wetted building materials. Most homeowners are better equipped to deal with construction problems associated with storm damage than to control the growth of mold fungi. Following hurrican...
T L Amburgey


Wood preservative obtained by recycling – preliminary selection of leaching inhibitor
2008 - IRG/WP 08-50252
Based on recycling of used household batteries, a process was developed to enable the recovery of major manufacturing components, leading to a solution of zinc (32 g.l-1) and manganese (15 g.l-1) salts, free of heavy metals. The potential use of the above solution as wood preservative was demonstrated by means of assays both of fungicidal activity -using white and brown rot fungi- and of insectici...
C Ibáñez, C Mantero, G Cecchetto, M Rabinovich, M Cerdeiras


Comparison of laboratory and natural exposure leaching of copper from wood treated with three wood preservatives
2008 - IRG/WP 08-50258
Standard and non-standard laboratory and field leaching tests were used to compare copper leaching from wood treated to above ground and ground contact specified retentions for three wood preservative systems, CCA-C, ACQ-D and a micronized copper formulation with quat DDAC as co-biocide. Copper leaching was highest for the ACQ formulation. Percent leaching was lowest for the micronized copper sy...
P A Cooper, Y T Ung


Moisture adsorption isotherms of wood studies using a dynamic vapour sorption apparatus
2009 - IRG/WP 09-20398
Five types of wood including two Malaysian hardwoods acacia mangium (Acacia mangium) and sesenduk (Endospermum malaccense), two temperate softwoods, Sitka spruce (Picea sitchensis), radiata pine (Pinus radiata) and Accoya (commercially modified wood) were studied to determine their moisture sorption behaviour using a Dynamic Vapour Sorption (DVS) apparatus. The isotherm plot for each species teste...
J Zaihan, C A S Hill, S Curling


A theoretical-industrial correlation and perspective on copper-based wood preservatives - a review of thermodynamic and kinetic aspects on copper-wood fixation mechanism
2009 - IRG/WP 09-30499
Copper was and it will continue to remain one of the key active component in wood protection industry. Over the past decades, a significant effort from R&D teams in industry, academia and research institutes was directed toward understanding the copper-wood fixation mechanism, optimising the copper retentions in the wood and reduce leaching in order to maximized performance, prolong the lifetime o...
R Craciun, M Maier, J Habicht


Antifungal Activities of Three Supercritical Fluid Extracted Cedar Oils
2009 - IRG/WP 09-30501
The antifungal activities of three supercritical CO2 (SCC) extracted cedar oils, Port-Orford-cedar (POC) (Chamaecyparis lawsoniana), Alaska yellow cedar (AYC) (Chamaecyparis nootkatensis), and Eastern red cedar (ERC) (Juniperus virginiana L), were evaluated against two common wood decay fungi, brown-rot fungi (Gloeophyllum trabeum) and white-rot fungi (Trametes versicolor). The statistical analysi...
Tianchuan Du, T F Shupe, Chung Y Hse


Effects of new fixative additives on leachability of boron wood preservatives
2009 - IRG/WP 09-30507
Borates are well known with their protective capacity against both fungi and insects with low mammalian toxicity and environmental acceptable. However, boron itself does not ensure the appropriate protection for wood in the exterior applications because of their easily depletion from the treated wood under wet conditions. In this study, the potential use of monoglyceride and polyvinyl alcohol prod...
A Mohareb, J Henry, E Wozniak, P Gérardin


Micronized Copper Preservative Systems: Observations on the Release of Cupric ion (Cu2+) from Treated Wood and Performance against Wood Decay Fungi
2009 - IRG/WP 09-30519
In an attempt to address the mechanism of action of micronized copper preservatives, a 20-week continuous water leaching study was conducted. The leaching results indicated that, once impregnated in wood, micronized copper preservatives continuously release cupric ion, and the levels of cupric ion released from micronized copper treated wood are higher than those released from CCA treated wood, a...
J Zhang, R Ziobro


Enhanced uptake of wood modification agents in “bioincised” wood
2009 - IRG/WP 09-40445
The permeability of refractory wood species e.g. Picea abies and Abies alba is reduced resulting in a radial penetration of chemical solutions of only a few millimetres. Exploitation of these wood species is therefore not possible for many applications. A novel biotechnological method (European patent 05027812.6) based on the pre-treatment of wood with the white-rot fungus Physisporinus vitreus si...
F W M R Schwarze, M Schubert


Environmental Emission of Wood Preservatives: Interpretation of Data Relevant to BPD Risk Assessments
2009 - IRG/WP 09-50259
The risk assessments for the use of wood preservatives proposed by the OECD and used under the Biocidal Products Directive (BPD) (98/8/EC) require the derivation of leaching rates for active substances. These rates are to be used as input data in to agreed exposure scenarios. The leaching rates can be derived from laboratory testing and from field testing. The relationship between laboratory and f...
D G Cantrell


Leaching of the copper component from full scale decking boards during one summer season
2009 - IRG/WP 09-50260
The leaching of copper has been tested in laboratory and in outside exposure for freshly treated pine sapwood samples with three different copper preservatives, Cu HDO, copper quat and copper triazoles. We found in the laboratory leaching test that a fixation with warming to 60 °C (140 °F) for 48 hours without drying and then drying in the laboratory in room temperature gave the lowest leaching of copper. We also found that surface treatments with wood oils reduced the leaching, and that washing of the surface before testing had no effect. Full scale decking board samples (0.25 m2) were then exposed outdoors for rain. The rain water was collected and analysed for copper. After one summer season (about 600 mm rain) we found that the leaching differ for the three preservatives. All samples with a water borne surface treatment had the lowest leaching, about half the amount of untreated.
F G Evans


Modification of Wood by a Water-Repellent Compound Used in the Textile Industry: Boron Release and Termite Resistance
2009 - IRG/WP 09-40447
In the study, wood specimens were treated with disodium octoborate tetrahydrate (DOT) and a commercial water and oil repellent compound, FORGUARD M®, a weak cationic emulsion containing dipropylene glycol monomethylether, water and solids in its formulation and used in the textile industry. There were two different processes for preservative treatments: double and single treatments. The leaching ...
S N Kartal, E Terzi, B Erilkun, Y Imamura


Selection of an appropriate coating system for wooden boats to be used in fresh water
2009 - IRG/WP 09-40472
Properties of several, most commonly used protective low-price coatings, which are used by the pletnja boat owners in Bled, Slovenia, were extensively studied. The aim of this professional, practically oriented study was to compare various coating systems, and to recommend the most suitable one to the boat owners. Regarding specific use conditions, the following properties, including their resista...
M Petrič, B Kričej, A Logar, M Pavlič


Physical and Mechanical Properties of Bamboo Oriented Strand Board Treated with Copper-based Preservatives
2009 - IRG/WP 09-40482
Oriented strand board (OSB) has been gradually accepted, used and developed in China. Bamboo is a renewable and potential non-wood fibre resource for making OSB. But the nature of bamboo makes its products including bamboo OSB (BOSB) more prone to decay and mold. Protection BOSB from biodegradation is the key both to efficiently using bamboo resource and to improving the durability of the final pr...
Juwan Jin, Daochun Qin


Microscopy evaluation of microbial decay patterns in wood stakes after 6 years in soil contact
2010 - IRG/WP 10-10715
Most studies on wood modification have so far been concerned with service life predictions rather than investigating the decay protection mechanism. Very little is known about the mode of action of these new treatments and about the strategies used by wood degraders in order to utilize the wood material despite a treatment. Access to such knowledge would allow further modification and improvement ...
A Pilgård, C G Björdal


The brown rot of oak wood submerged for 6 months in the Baltic sea
2010 - IRG/WP 10-10736
The natural wood submerged or partially immersed in sea water is commonly affected by certain microorganisms. The bacteria and marine borers that decay the wood totally submerged in sea water and above sea level other microorganisms as fungi, algae, insects may attacked wood. The sea water may affect and change the properties of wood. We have tried to determine the susceptibility to decay caused b...
A Fojutowski, A Kropacz, I Pomian


Methods for Studying Penetration Depth of Wood Protection Products
2010 - IRG/WP 10-20432
EN 152 is an accepted standard in Europe for measuring how deep a wood protection product penetrates into the surface of treated pine wood. The method has provided consumers with a wide assortment of products that meet the specifications outlined in the standard. Because the test takes 8 or more months to carry out, artificial ageing procedures have evolved in order to standardize and speed up the...
K Hansen, L Sites, D D Nicholas


Determination of a fixation time of wood preservatives: A discussion paper
2010 - IRG/WP 10-20436
The intention of that paper is to initiate a discussion on the basis of a French method in combination with a German approach regarding the need of a method for the determination of a fixation time and especially to obtain input as well as ideas concerning a possible test design. Since no harmonised European approach exists up to now concerning the determination of a fixation time, CEN TC 38 (2009...
E Raphalen, E Melcher


Synthesis of novelty borate compounds for wood preservatives: Laboratory test of leachability and decay resistance
2010 - IRG/WP 10-30520
A novel series of ammonium tetraphenylborate (ATB) and borate chemical compounds (BBC) were synthesized as wood preservatives. The leaching rates and decay resistance of boron formulations containing ATB and BBC were conducted. The laboratory leaching results showed that boron leaching rate of treated wood by ATB formulations was from 2.1% - 6.7%, while that of BBC formulations from 23.3% -59.0%. ...
Zhiqiang Li, Mingliang Jiang, Xingxia Ma


Effects of polyvinyl alcohol on leachability and efficacy of boron wood preservatives against fungal decay and termites attack
2010 - IRG/WP 10-30526
In this study, the use of polyvinyl alcohol (PVA) as boron fixative agent was investigated. Two levels of PVA (2.5 and 4%) were evaluated with disodium octaborate tetrahydrate (DOT) at three concentrations (1, 2 and 4% boric acid equivalent (BAE) using a double vacuum impregnation processes on Scots pine sapwood specimens. Leaching was performed according to a laboratory leaching procedure. Boron ...
A Mohareb, M F Thévenon, E Wozniak, P Gérardin


Effects of Cunninghamia Lanceolata Heartwood Extracts on the Growth of Wood Decay Fungi
2010 - IRG/WP 10-30527
China-fir (Cunninghamia lanceolata) wood is well known for its good durability. This species is native to China and has been extensive planted there. Mainly, extractives are responsible for the wood resistance to decay fungi. In this paper, the extractives of China-fir heartwood were studied for their effects on various wood decay fungi. Sequential extraction of heartwood in hexane, ethyl acet...
Shujun Li, Jing Wang, Jian Li


Degradation of Carbon-Based Preservatives by Black-stain Fungi
2010 - IRG/WP 10-30533
Some black-stain fungi are known to exhibit resistance to carbon-based preservatives. However, the cause of this resistance is unclear. The fungi may have mechanisms to tolerate these chemicals, or they may be able to degrade and detoxify them. Fungi capable of degrading carbon-based preservatives are of interest for possible bioremediation of carbon-based preservative-treated wood at the end of i...
R Stirling, P I Morris


Treatment of Scots pine wood with oil in water and water in oil emulsion systems: Effects on boron leaching and water absorption
2010 - IRG/WP 10-30535
The aim of this study was to investigate the water absorption and water repellent efficiency of oils and oil water emulsions [oil-in-water (O/W) and water-in-oil (W/O)] and possibilities of reducing the amount of boron leaching from treated wood. Scots pine wood samples treated with waste or sunflower oil and water formulations contained 3%BA. The level of water absorption and water repellent effi...
E D Tomak, Ü C Yildiz, A Can