IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 431 documents. Displaying 25 entries per page.


Progress report on "Studies on the effect of salinity on the growth and mortality of teredinids"
1976 - IRG/WP 418
An open flow aquarium was constructed at Forest Products Research Centre in 1972 in order to study the effect of salinity on the growth and mortality of teredinids. To determine the reliability of results obtained during salinity experiments, the growth rate of teredinids in the aquarium were compared with the growth rate of the same species living under natural conditions in the harbour in 1973. ...
S M Rayner


The association of bacteria with the increased permeability of water-stored spruce wood
1973 - IRG/WP 325
A microbiological investigation was undertaken to check our earlier work on patterns of bacterial counts and pH changes in water-stored wood. A survey of industrial activity was conducted upstream from the storage site with a view to explaining the existing bacterial flora. Further experiments were carried out with spruce bolts in enclosed tanks, using lake water with its natural bacterial flora a...
J A Dunleavy, J P Moroney, S E Rossell


Laboratory evaluation of water repellents as antisapstain treatment additives
1986 - IRG/WP 3382
Water repellent formulations consisting of five paraffin wax emulsions, three polyethylene wax emulsions, two polybutadiene resin emulsions, a polyester emulsion, and a ß-pinene polymer emulsion were subjected to water repellency tests on radiata pine sapwood. With one exception, the parafin wax emulsions were more effective water repellents than the alternative formulations and one of the paraff...
D V Plackett, C M Chittenden


The development of a new boron-based wood preservative
1995 - IRG/WP 95-30085
The paper describes a new boron based wood preservative for the treatment of green timber. The product offers many benefits over conventional boron diffusion treatment including: 1. high viscosity, high concentration formulation; 2. permits dip treatment of a wide range of sawn board and pole sizes at ambient temperatures; 3. permits full cross section diffusion of borates without block stacking a...
P Turner, D Conradie


Feeding response of field populations of Coptotermes species to softwood blocks treated with non-toxic water-proofing and anti-microbial products.
2003 - IRG/WP 03-10487
The feeding response of field populations of the subterranean termite, Coptotermes lacteus, to Pinus radiata wood blocks (50 x 40 x40 mm) treated with various combinations of non-toxic and odourless water-proofing materials based on natural high molecular weight esters (TimberTreatÒ) and a new water insoluble quaternary ammonium compound (‘anti-microbial’) is described. Treated wood blocks we...
J R J French, T Pynsent, M Susic


A technique for determining the efficacy of water diffusible preservative plugs for implanting in joinery in service
1987 - IRG/WP 2291
A technique is described for determining the efficacy of soluble, diffusible preservative plugs for eradicating decay in joinery. It uses blocks of Scots pine sapwood or heartwood adjusted to known moisture contents prior to the establishment of the test fungus Coniophora puteana, from a single longitudinal dowel and the subsequent introduction of the preservative plugs. Prevention of decay, eradi...
J K Carey, A F Bravery


The degradation of wood surfaces by dilute acids
1985 - IRG/WP 3326
Thin radial/longitudinal sections(~100 µ) of Corsican Pine (Pinus nigra) and Lime (Tilia vulgaris), were exposed to Sulphuric, Sulphurous, nitric, acetic, and formic acid at 40°C in the pH range 2-6. After about 3 months exposure to Sulphuric, nitric, acetic and formic acid at pH 2.0 Pine lost some 20-25% of its tensile strength. Losses in tensile strength due to sulphurous acid were greater bei...
P D Evans, W B Banks


Protection of cellulose string with biocide/water repellent mixtures
1997 - IRG/WP 97-30148
Protecting cellulosic materials in soil contact poses a formidable challenge. Many soil inhabiting bacteria and fungi that cannot degrade wood can nevertheless rapidly depolymerize cellulose once its protective lignin matrix is removed. As a result, cellulose based materials are rarely used in direct contact with soil. One exception, however, is the use of cellulose string to support climbing vine...
A B Chang, J J Morrell


Methods to determine the efficacy of three water repellent additives in waterborne preservatives
1997 - IRG/WP 97-30142
The paper describes the methods used to determine the efficacy of three different water repellent additives in waterborne preservatives. The wooden samples used are pine (Pinus sylvestris) and spruce (Picea abies) that are treated with 9 different waterborne preservatives in retention for hazard class 3 (above ground commodities). There are two sample sizes exposed, cladding boards (19 x 148 mm) w...
F G Evans, B Nossen, K M Jenssen, L R Wilhelmsen, G Fuglum


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic applications. Part 1: Laboratory scale investigation
1995 - IRG/WP 95-50046
In order to investigate the applicability of current prestandard leaching test methods, a series of experiments has been performed on CCA impregnated wood dealing with the influence of pH, temperature and agitation of the surrounding water. The leaching method used in this first part of the investigation is the European prestandard drafted by CEN/TC38/WG11, a short term dynamic leaching test under...
G M F Van Eetvelde, R J Orsler, G E Holland, M Stevens


Compatibility of deltamethrin with wood adhesives
1993 - IRG/WP 93-30031
This work presents the studies conducted on the compatibility of deltamethrin when mixed with wood adhesive to manufacture plywood in order to protect the wood against wood-borers insects and termites. The following types of adhesive were tested: PVA, Urea-formaldehyde, phenol-formaldehyde and a formulation based on tannin. The experiments were made in the adhesive manufacturers' laborato...
A M F Oliveira


Aquatic toxicity research of structural materials
1998 - IRG/WP 98-50114
Continuing from preliminary results reported on the aquatic toxicity of some tropical hardwoods under high hazard conditions, a more comprehensive research study is set-up in order to assess the environmental toxicology of various structural materials in water applications. Hazard class 4 preservative treated wood is tested for its toxic response on a battery of aquatic test organisms, next to con...
G M F Van Eetvelde, S De Geyter, P Marchal, M Stevens


PCP in aquatic environments arising from historic contamination at wood processing and preservation sites
1995 - IRG/WP 95-50040-14
Three different studies are reported that assess the impacts of Pentachlorophenol (PCP) in aquatic environments arising from its historic use at sawmilling and wood preservation sites. These studies involved New Zealand wood processing facilities, and collectively they aimed to measure the transport of PCP from sawmill sites into the aquatic environment, determine the background environmental conc...
J S Gifford, P N McFarlane, M C Judd, S M Anderson


Influence of water soluble extractives on CCA fixation and leaching performance of red maple and red oak
1997 - IRG/WP 97-30133
We have observed several peculiarities in relation to CCA fixation in red maple and red oak woods such as high variability in fixation rates and leaching performance in maple and precipitate formation in solutions expressed from CCA treated red oak wood blocks at different stages of fixation. We have postulated that the extractives could be the factor of influence, as this has already been reporte...
T Stevanovic-Janezic, P A Cooper, Y T Ung


IRG/COIPM INTERNATIONAL MARINE TEST - To determine the effect of timber substrate on the efectiveness of different preservatives in sea-water: Coding scheme
1976 - IRG/WP 420
It was agreed in Wildhaus on 15 May 1976 that preparations for the test detailed in Document No: IRG/WP/414 should commence immediately, but that initially only two water-borne preservatives should be used - a copper/chrome/arsenic (CCA) and a copper/chrome/boron (CCB) formulation respectively. PRL, England (R Cockcroft) would be responsible for supplying only the reference species treated with th...
Anonymous


Moisture content of logs under sprinklers
2000 - IRG/WP 00-40157
Logs are kept under sprinklers during storage for avoiding the development of sapstain fungi. According to literature, sapstain fungi do not develop if the moisture content is above 120%. It is supposed that, the water sprinklers maintain the log's moisture content above this value, but, very often, sapstain is found on sawn lumber cut from these logs. Logs are harvested and transported t...
M C Rose, A M Briones, M Fernández


A substantively bonded water repellent treatment based on chromium carboxylates
1985 - IRG/WP 3344
Chromium carboxylates soluble in toluene have been synthesised and applied to Scots pine (Pinus sylvestris) sapwood. Without any further treatment, the compounds may be readily leached from wood surfaces with toluene. After a period of heating however, they become fixed to the cell wall, substantial amounts being resistant to leaching even under reflux conditions for several hours. Treatment of wo...
J K Wright, W B Banks, W J Eilbeck


Melamine resins as preservatives results of biological testing
1996 - IRG/WP 96-40061
Based on previous work of the authors on resins, the upgrading of wood with a true solution of a methanol etherificated melamine resin in low aqueous concentration was performed. For the relative assessment of the biological resistance against brown and white-rot fungi were used not only untreated controls of pine sapwood (Pinus sylvestris L.), but also heartwood of European larch (Larix decidua M...
A O Rapp, R-D Peek


The effect of oil-borne preservative treatments on the shear strength of FRP/wood composite adhesive bonds
2003 - IRG/WP 03-40265
Reinforcement of structural wood components with Fiber Reinforced Polymer (FRP) will enhance the beam’s strength, but actual data on long-term durability is sparse, not well documented or not readily accessible. In this study, bond properties of FRP-wood composite materials were investigated following treatment with creosote or copper naphthenate preservatives. The properties investigated inclu...
B Herzog, B Goodell, R Lopez-Anido


A field trial to assess the potential of antisapstain chemicals for long-term protection of sawn radiata pine
1986 - IRG/WP 3375
Seven chemical formulations were tested as antisapstain treatments for freshly sawn radiata pine sapwood (90x50 mm²). Each formulation was used with and without a water-repellent additive and was sprayed on to 1 m long boards. The boards were then stacked into "mini" packets and stored unprotected from the weather for 6 months. Haipen 50w (at 0.2 or 0.4% active) and NaPCP (1% active) plus 1.5% bo...
J A Drysdale


Prevention of sapstain in logs using water barriers
1997 - IRG/WP 97-30147
Placing logs in ponds or under water sprinklers to keep moisture levels high enough to prevent oxygen tensions rising above inhibitory levels, is a proven method of preventing sapstain. The objective of this experiment was to determine if water barriers significantly reduce the rate of sapstain penetration into logs by maintaining moisture contents, and consequently oxygen tensions, at inhibitory ...
R N Wakeling, D R Eden, C M Chittenden, B Carpenter, I Dorset, J Wakeman, R Kuluz


Water transfer in wood in relation to fungal attack in building - Effect of condensation and diffusion
1992 - IRG/WP 92-1543
Wood is continuously exchanging moisture with the surrounding atmosphere, the temperature and relative humidity are important factors. Wood moisture in this case is not enough to provoque decay by fungi. However, when, during the night, condensation appears cyclically, wood absorbs water and moisture content may be sufficiently high to allow development if drying does not take place. The water tra...
D Dirol, J-M Vergnaud


A study of methanogenesis and sulphate-reduction: A possible source of explosive gas mixtures in a gold mine
1989 - IRG/WP 1399
Previous work isolated anaerobic bacteria from timbers and drainage water in a gold mine. The present work identifies the predominant methanogen in the mine ecosystem as Methanobacterium bryantii and sulphate-reducing isolates as Desulphovibrio desulphuricans and Desulphotomaculum antarcticum. Laboratory studies using model systems evaluate the activity of methanogenic and sulphate-reducing bacter...
L D Abraham, J F Putterill, A A W Baecker


Wood cement composites using spent CCA treated wood
1999 - IRG/WP 99-50126
The feasibility of using spent or out-of-service CCA treated wood as a component of wood/cement composites was evaluated. Cold pressed wood particle cement boards were made using CCA treated particles from a red pine (Pinus resinosa Ait.) pole removed from service and from untreated red pine wood from a new pole. Boards were manufactured using a range of wood to cement ratios and water to cement r...
Chen Huang, P A Cooper


A novel method for evaluating the performance of water repellents
1987 - IRG/WP 2279
Application of water repellent formulations to timber surfaces offers protection from the weather, reducing degrade and movement. A novel test method has been developed to evaluate the comparative efficacy of such formulations when samples are exposed to weather. The method uses sapstain free sapwood of defect free, untreated, seasoned Radiata pine, (Pinus radiata D. Don.) Water Repellency was det...
A R Moffat


Previous Page | Next Page