The extraction of boron from treated wood for quantitative analysis: A comparison of procedures
1992 - IRG/WP 92-2414
The extraction of boron preservative from treated rubberwood and scots pine samples was compared using methods based on refluxing and extraction in 1N NaOH or distilled water at 80°C. The extract solutions were analysed by Inductively Coupled Plasma spectroscopy (ICP/AES). A simple extraction procedure based on immersion of wood samples of approximate dimension 2 x 1 x 1 cm³ in distilled water a...
R J Murphy, D J Dickinson, P W McCormack, M K Lung


Co-operative tests concerning the influence of solvent and drying method on the toxic limit of wood preservatives against Coniophora cerebella
1972 - IRG/WP 216
In the working group II of the IRG it was agreed that more knowledge was necessary concerning the influence of the solvent on the toxic limit of organic solvent types of wood preservatives against Basidiomycetes. A test program was drawn up and after discussion in the mentioned working group the final program was accepted by the co-operating institutes in 1969. In the test program two fungicides, ...
T Hof


Water transfer in wood in relation to fungal attack in building - Effect of condensation and diffusion
1992 - IRG/WP 92-1543
Wood is continuously exchanging moisture with the surrounding atmosphere, the temperature and relative humidity are important factors. Wood moisture in this case is not enough to provoque decay by fungi. However, when, during the night, condensation appears cyclically, wood absorbs water and moisture content may be sufficiently high to allow development if drying does not take place. The water tra...
D Dirol, J-M Vergnaud


Bethoguard; A new wood protecting fungicide for use in metal free ground contact wood preservatives
2002 - IRG/WP 02-30301
Research has identified the limitations in both the spectrum of activity and permanence of organic biocides placed in wood in high hazard environments, particularly in the absence of heavy metals such as copper. More specifically, the control of soft rot decay in wood in soil contact has proven to be most problematic. The new organic biocide, Bethoguard; an oxathiazine, has demonstrated excellen...
S C Forster, G R Williams, M Van Der Flaas, M Bacon, J Gors


A study of methanogenesis and sulphate-reduction: A possible source of explosive gas mixtures in a gold mine
1989 - IRG/WP 1399
Previous work isolated anaerobic bacteria from timbers and drainage water in a gold mine. The present work identifies the predominant methanogen in the mine ecosystem as Methanobacterium bryantii and sulphate-reducing isolates as Desulphovibrio desulphuricans and Desulphotomaculum antarcticum. Laboratory studies using model systems evaluate the activity of methanogenic and sulphate-reducing bacter...
L D Abraham, J F Putterill, A A W Baecker


Changes of copper and chromium content after leaching in wood impregnated with the CCB and CB preservatives
2000 - IRG/WP 00-50147
The objective of the study was impregnated with CCB and CB preservatives pine wood of moisture content varying from 12% to 55% subjected to leaching. Losses of copper and chromium were determined for individual layers of wood up to 3 cm from the girth. The results were compared to the total amount of metals determined in water extracts. The degree of leaching of metal ions from wood of 55% moistur...
B Mazela


Wood preservation in Croatia
2004 - IRG/WP 04-30360
Croatia, as all the other countries in transition, however also because of its specific and well-known reasons, is on a path to gradual drawing nearer to the European standards. Only the scientists working at the Faculty of Forestry in Zagreb are engaged in scientific work relating to wood preservation. The construction and wood industry, which should enhance the chemical industry, also have subs...
R Despot, M Hasan


Suitability of different termite species for laboratory testing
1982 - IRG/WP 1159
Different termite species were tested in the laboratory to evaluate the effectiveness of insecticides and wood preservatives in wood against termite attack. Determined were the optimum group size and composition, the matrix (vermiculite) volume and its moisture content. Choice feeding tests with fully impregnated wood blocks which are carried out according to a modified EN 117 procedure for Reticu...
U Kny, H Kühne


Wood cement composites using spent CCA treated wood
1999 - IRG/WP 99-50126
The feasibility of using spent or out-of-service CCA treated wood as a component of wood/cement composites was evaluated. Cold pressed wood particle cement boards were made using CCA treated particles from a red pine (Pinus resinosa Ait.) pole removed from service and from untreated red pine wood from a new pole. Boards were manufactured using a range of wood to cement ratios and water to cement r...
Chen Huang, P A Cooper


A novel method for evaluating the performance of water repellents
1987 - IRG/WP 2279
Application of water repellent formulations to timber surfaces offers protection from the weather, reducing degrade and movement. A novel test method has been developed to evaluate the comparative efficacy of such formulations when samples are exposed to weather. The method uses sapstain free sapwood of defect free, untreated, seasoned Radiata pine, (Pinus radiata D. Don.) Water Repellency was det...
A R Moffat


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 4: Conversion reactions during storage
1974 - IRG/WP 332
Precipitates simulating those produced in wood by preservative fixation reactions were prepared by the reduction of Boliden K 33 and Celcure AP solutions with hydrogen peroxide and hydrazine. The pH changes on aging at 20 and 50°C were studied and related to the chemistry of fixation previously described. Hydrolysis of copper arsenates may render arsenic acid temporarily water soluble pending pre...
S-E Dahlgren


Fixation of chromated wood preservatives through technical drying
1990 - IRG/WP 3623
Twin samples of sawn timber of Pinus sylvestris and Picea sp. were treated with copper-chromate-containing wood preservatives and subsequently kiln resp. air dried. After drying, the distribution of preservative and rate of fixation were determined. Drying of freshly treated wood in a condenser type kiln at temperatures of 60°C and 80°C and in a vacuum type kiln at 55°C with a pressure of about...
R-D Peek, H Klipp


Regulations of wood preservatives in Finland
1978 - IRG/WP 3124
Toxic wood preservatives are covered by the Poison Act (No. 309/69). The act came into force in May 1969 and was supplemented by the Statute on Poisons (No. 612/69). The act and the statute contain the regulations on the production, commerce and handling of poisons. Already when issued they were complained to contain some defects and obscurities. However, only minor alteration in them have been ma...
T Vihavainen


Evaluation of hydroxamates as wood preservatives
2004 - IRG/WP 04-30330
Fungicidal activity of different hydroxamates was investigated by laboratory malt-agar block tests to evaluate their potential as wood preservatives. Results obtained indicate that benzohydroxamic acids substituted or not on the aromatic nuclei were unable to protect wood blocks against the white rot fungus Coriolus versicolor while 2-hydroxypyridine-N-oxide (2-HPNO) possesses an interesting activ...
P Gérardin, S Dumarçay, E Gelhaye, A Mbamba, V Mussavu


Information on a project about the conditions of admissibility of wood-protecting agents in connection with environmental protection in Poland
1974 - IRG/WP 57
Wood-protecting agents are compounds acting toxically on fungi and insects. If handled improperly or carelessly, they may exert an action harmful to health and safety of men. This action is concerning: a) workers employed at the production of wood-protecting agents; b) workers employed at the impregnation, or at the transport and handling of impregnated wood; c) inhabitants of buildings with impre...
J Wazny


The effect of stack height on the performance of preservatives used for the prevention of sapstain on seasoning wood
1997 - IRG/WP 97-10192
The performance of three anti-sapstain preservatives was investigated under field conditions in south east England. The preservatives under test were: copper-8-quinolinolate (Mitrol PQ8) trimethylalkylammoniumchloride and sodium hexanoate (Sinesto B) and chlorothalonil (Tuff Brite). The preservatives were tested on Corsican Pine grown in south east England. The field trial was set up to investigat...
J R Williams, D J Dickinson, J F Webber


A novel technique for comparative toxicity studies of potential insecticidal wood preservatives
1983 - IRG/WP 2198
For some years now a device has been under development at the New Zealand Forest Research Institute, the purpose of which is to study the effects of sub-lethal amounts of stomach poisons (but also of fumigants and contact active materials) on the co-ordinative abilities of a cerambycid larva. This insect is Prionoplus reticularis - indigenous to New Zealand its larvae feed in decaying logs and are...
D J Cross


A combined method for drying and preserving wood in a single step process
2000 - IRG/WP 00-40183
Based on a convective dryer, this process allows to dry and treat wood blocks with diffusible preservatives in the same time. A boric acid solution (heated to fix the wet temperature of the system) is pumped and introduced in the flow system through a venturi, where the air coming back from the drying cell also arrives. The role of the venturi is to create a dispersion of boric acid solution micro...
O Colin, C Dupuis, E Mougel, A Zoulalian, M-F Thévenon


Interactions between soft rot fungi and CCA preservatives in Betula verrucosa
1988 - IRG/WP 1367
Ultrastructural investigations were carried out to obtain information on the cell wall distribution of CCA elements during soft rot decay of 4% K33 CCA preservative treated birch (Betula verrucosa) wood. TEM observations on fibres at various stages of S2 cavity formation by mutabilis showed a distinct pattern of electron dense materials to occur within the S2 cell wall region. These materials (gra...
G F Daniel, T Nilsson


Factors affecting the resistance of fibre building boards to fungal attack
1975 - IRG/WP 252
Fungal decay is initiated at lower moisture contents in standard and tempered hardboards (18%) than in pine sapwood (26%). In contrast, in a saturated atmosphere, the equilibrium moisture contents of standard hardboard (14%) and of tempered hardboard (12.5%) are much lower than the moisture content permitting decay initiation whilst the equilibrium moisture content of pine sapwood (25.1%) approach...
C Grant, J G Savory


Wood preservation in the Netherlands
1985 - IRG/WP 3324
This report gives some information on the production, import and use of timber in the Netherlands and, in more detail, about the country's wood preservation industry. As the country's production of wood that is useful for its manufacturing industries is very limited, the position of wood in the building industry is not too important. Architects think first in terms of bricks, con...
N Burgers, R Cockcroft, D De Jong


Fungal degradation of wood treated with metal-based preservatives. Part 1: Fungal tolerance
1996 - IRG/WP 96-10163
In recent years, concerns have arisen about the leaching of heavy metals from wood treated with chromated copper arsenate (CCA), particularly because of the large amount of CCA treated wood that will be discarded in the coming years. The long term objectives of this work are to determine the fate of copper, chromium and arsenic with the aging and potential decay of CCA-treated wood, and to develop...
B Illman, T L Highley


Comparative study on the leaching of wood preservatives between natural exposure and accelerating laboratory conditions
1999 - IRG/WP 99-50134
Impregnated specimens with CCA, ACQ, and BAAC were subjected to leaching tests. Specimens of 2x2x1 cm3 in size were used for the laboratory leaching test for 10 days according to JIS K 1571. Specimens of 25x1 x1 cm3 were used for outdoor leaching test for 6 months. Total leaching amounts of boron per cm3 of specimens treated with BAAC were 325 µg in the laboratory test and 206 µg in the outdoor ...
K Yamamoto, S Motegi, A Inai


Evaluation of rapid methods for detecting wood preservatives in waste wood
1994 - IRG/WP 94-50024
For the disposal of wood waste under ecological sound conditions information about its hazardous potential is required. Several analytical methods are available for the detection of most elements in wood preservatives. Industrial process conditions, however, demand methods with very short turn around times. In this research several methods of analysis were judged on their speed and accuracy. A num...
W J Homan, H Militz


Evaluation of extractives from African Padauk (Pterocarpus soyauxii Taub.) for protection of non decay resistant species
2002 - IRG/WP 02-10419
The development of a wood preservative made up of natural extracts is a potentially attractive prospect for the wood preservation industry. In this study, organic solvents were used to remove extractives from African padauk wood samples. The solvent was removed by rotoevaporation, and the total content of the viscous extracts determined to be 54.4mg/ml. The toxicity of various extracts concentrat...
P Nzokou, D P Kamdem