Biosorption of metals for wood waste effluent clean up
1997 - IRG/WP 97-50090
The common filamentous fungi can sorb metal ions from aqueous solutions. The biosorption of metal ions like copper Cu2+, chromium Cr6+ and arsenic As5+ by dead fungal mycelia was investigated. Two industrial fermentation byproducts are tested: Mucor miehei and Aspergillus oryzae. The adsorption of metal ions depends on parameters such as chemical treatment of fungi before biosorption (acid or basi...
S Legay, G Labat


Comparison of Temporal Changes in Metal Leaching and Aquatic Toxicity from Wood Treated with CCA and Alternative Preservatives
2005 - IRG/WP 05-50236
This study compares the temporal variation of chemical leaching and aquatic toxicity of wood treated with chromated copper arsenate (CCA) and other copper-based wood preservatives (alkaline copper quaternary (ACQ), copper boron azole (CBA), copper citrate (CC) and copper dimethyldithiocarbamate (CDDC)). Treated wood blocks were leached for 21 days and the leachate collected was analyzed for prese...
B Dubey, T G Townsend, G Bitton, H M Solo-Gabriele


CCFZ, a new type of water-borne wood preservative for vacuum pressure impregnation
1991 - IRG/WP 3643
By combination of CCF-Salt types with zinchexafluorosilicate a remarkable improvement of efficacy is achieved. In the same time the ecotoxicoligical data become more save. As well as the efficacy against wood-destroying organisms (Basidiomycetes, Soft rot and Long horn beetle) the basic data to evaluate the ecotoxicological behaviour of a CCFZ-Salt are described and compared with the properties of...
W Metzner, D Seepe, H-W Wegen


Preservatives stains as exterior wood finishes
1977 - IRG/WP 389
For many years wood preservatives and paints have been used as the only treatment for exposed wood surfaces. Because of the inherent color of the preservatives, such as creosote, the wood surface was stained as well as protected from attack by micro-organisms. Paints protect surfaces from weathering, but recently, with an increased interest in maintaining the more natural appearance of exterior wo...
D W French


Methods to determine the efficacy of three water repellent additives in waterborne preservatives
1997 - IRG/WP 97-30142
The paper describes the methods used to determine the efficacy of three different water repellent additives in waterborne preservatives. The wooden samples used are pine (Pinus sylvestris) and spruce (Picea abies) that are treated with 9 different waterborne preservatives in retention for hazard class 3 (above ground commodities). There are two sample sizes exposed, cladding boards (19 x 148 mm) w...
F G Evans, B Nossen, K M Jenssen, L R Wilhelmsen, G Fuglum


Algal growth resistance of paints for coating of wood; a laboratory study
1997 - IRG/WP 97-10213
Twelve paints were tested for resistance against algae. In addition, one algicidal compound commercially used for remedial treatments of algal growth on paints was tested for its effectiveness for prevention of algal growth. An agar diffusion bioassay was employed in which paint films on filter paper discs were placed on mineral salt medium and sprayed with an algal suspension containing a mixture...
J Bjurman


IRG/COIPM INTERNATIONAL MARINE TEST - To determine the effect of timber substrate on the efectiveness of different preservatives in sea-water: Coding scheme
1976 - IRG/WP 420
It was agreed in Wildhaus on 15 May 1976 that preparations for the test detailed in Document No: IRG/WP/414 should commence immediately, but that initially only two water-borne preservatives should be used - a copper/chrome/arsenic (CCA) and a copper/chrome/boron (CCB) formulation respectively. PRL, England (R Cockcroft) would be responsible for supplying only the reference species treated with th...
Anonymous


The effect of oil-borne preservative treatments on the shear strength of FRP/wood composite adhesive bonds
2003 - IRG/WP 03-40265
Reinforcement of structural wood components with Fiber Reinforced Polymer (FRP) will enhance the beam’s strength, but actual data on long-term durability is sparse, not well documented or not readily accessible. In this study, bond properties of FRP-wood composite materials were investigated following treatment with creosote or copper naphthenate preservatives. The properties investigated inclu...
B Herzog, B Goodell, R Lopez-Anido


Penetration of oil-borne preservatives in American elm
1975 - IRG/WP 355
Pressure treatment of elm posts and cants by Rueping schedules resulted in erratic penetration. Instead of the expected gradual decrease in retention from surface inward in posts, inner zones frequently contained more preservative than the surface quarter inch. Heartwood was found penetrated when sapwood was not. There were numerous skips in treated zones. The prevalence and possible causes were i...
E A Behr


The resistance of wood coated with different water-borne paints against colonisation by decay fungi
1996 - IRG/WP 96-10165
The susceptibility of wood painted with model paints of known composition to decay fungi was tested without previous weathering. Included in the study were five alkyd emulsion paints and five acrylic paints; one linseed oil paint and two solvent-borne alkyd paints. It was found that several components influenced the susceptibility of these paints. The results of the present study indicate that the...
J Bjurman


Resistance of pine and spruce heartwood against decay - The effect of wood chemical composition and coating with water-borne wood oil product
2006 - IRG/WP 06-10597
Natural durability of wood has been widely studied, but the combination of the natural durability and different treatments has not been the focus of many studies. The durability of wooden products is mainly based on the water permeability and the resistance against organisms. In this study, the water absorption and decay resistance of sapwood and heartwood of Scots pine and Norway spruce were exam...
H Viitanen, S Metsä-Kortelainen, T Laakso


Photo-degradation of modified and non-modified wood, coated with water borne acrylic coatings during artificial light exposure
2007 - IRG/WP 07-30416
A series of experiments were carried out to investigate photo-degradation of thermally modified (at 210oC and – 0.9 bars for two hours) and non-modified spruce wood (Picea abies L (Karst)), coated with transparent and semitransparent (with 3% pigment content) acrylic coatings during artificial UV light irradiation for 200 hours. Photo-degradation was evaluated in terms of colour changes througho...
M Deka, M Tomažic, M Petric


Growth and succession of mould on commercial paint systems in two field sites
2007 - IRG/WP 07-30421
Discolouring fungi reduce the service life of coated wooden claddings in façades and increase the total cost of ownership due to shorter maintenance intervals. It is of major importance to find paint systems for wood which are durable and have a high resistance to mould growth. A total of 15 paint systems from 9 different manufacturers were exposed on two field sites, Sørkedalen and Birkenes, ...
L Ross Gobakken, K M Jenssen


Preservative treatment of Golla cane (Daemonorops jenkinsiana) by pressure process
2007 - IRG/WP 07-40379
The feasibility of preservative treatment of golla cane (Daemonorops jenkinsiana (Griff) Mart). by pressure process has been studied using water borne preservatives CCB (copper-chrome-boron). Cane samples of three different lengths 1m, 2m and 3 m. were treated at different pressure and time period to evaluate the extent of penetration and retention of preservative chemicals. It was observed that t...
K Akhter, M Hoque Chowdhury


Synthesis of boric acid ammonium oleate salt for wood preservation: Leachability and termite resistance test
2007 - IRG/WP 07-30435
A new chemical compound coupling boric acid and oleic acid through a joint of ammonium salt has been produced and its synthesis followed and validated by Fourier Transformed Infra Red (FTIR). This compound named ammonium borate oleate (BAO) combining biocidal properties of boron and water repellence of fatty acids has then been studied as a wood preservative. Synthesis of BAO involved different...
F Lyon, A Pizzi, Y Imamura, M F Thevenon, S N Kartal, J Gril


Evaluation of Water Repellency of Treated Wood Using Several Alternative Methods
2009 - IRG/WP 09-20419
In this study, the results of water repellency testing using a digital swellometer method for water-borne organic-preservative systems with water repellent additives are reported. The findings suggest that the traditional method of using matched untreated controls as a reference developed from historic solvent-based treatments for determination anti-swelling efficacy (ASE) may underestimate the a...
L Jin, A F Preston


Efficacy of Erythropleum suaveolens (potrodom) and Distemonanthus benthamianus (bonsamdua) water extractives on the durability of five Ghanaian less used timber species of varying perviousness and retentiveness
2017 - IRG/WP 17-30705
Conventional wood preservatives are not only toxic to target bio-deterioration organisms but also to humans, other organisms and the environment. In an effort to find preservatives that are less toxic or non-toxic to man, other organisms and the environment, efficacy of branch bark and heartwood water extracts (0.65 g/ml) of Erythropleum suaveolens (potrodom) and Distemonanthus benthamianus (bonsa...
A Asamoah, K Frimpong-Mensah, C Antwi-Boasiako


Relative efficacy of various oxine copper formulations against brown-rot fungi
2019 - IRG/WP 19-30741
This paper investigates the relative resistance of three different oxine copper formulations (oil-borne, water-borne, water-borne with pH-adjustment) as a preservative treatment for wood against brown-rot fungi. Impregnated southern pine sapwood cubes were exposed to R. placenta and G. trabeum cultures in a soil-block test. After eight weeks, the weight losses of the cubes were examined in relatio...
M Petruch, J Lloyd, A Taylor


Performance of a water-borne stain on beech, spruce, MDF and OSB improved by plasma pre-treatment
2020 - IRG/WP 20-40897
Coatings are an important part of wood protection, especially for outdoor applications. In order to provide a good protection, protective coatings need to exhibit good adhesion, mechanical resistance, and weathering resistance. Plasma pre-treatments are an established method to increase the performance of existing coatings including those on wood and wood-based substrates. Moreover, plasma deposit...
S Dahle, J Žigon, I Uranjek, M Petrič


Danish wood preservatives approval system with special focus on assessment of the environmental risks associated with industrial wood preservatives
2001 - IRG/WP 01-50166-01
The following is a description of the procedure used by the Danish Environmental Protection Agency to assess the environmental risks associated with preservatives used in the pressure impregnation of wood. The risk assessment covers issues considered to be of significance for the environment and which are adequately documented so as to allow an assessment. Such issues are persistence and mobility ...
J Larsen


Finishes for outdoor timbers
1975 - IRG/WP 378
Anonymous


Management of the wood and additives wastes in the wood processing industries: Problematics and technical answers review
1996 - IRG/WP 96-50073
Management pathways for pure wood subproducts are well known and used; but as soon as additives like preservatives, glues, varnishes or coatings are present within the wood wastes, their disposal or valorization becomes more tricky. The different kinds of mixed wood wastes of the wood processing industries, from the sawmill to the furniture manufacture, are identified herewith and their diversity ...
S Mouras, G Labat, G Deroubaix


Proposed method for out-of-ground contact trials of exterior joinery protection systems
1981 - IRG/WP 2157
Methods for testing the efficacy of preservative treatments for exterior joinery are described using the format of a European Standard. Commercially used treatments applied to jointed test units (L-joints) which are then protected by conventional finishes are exposed to normal outdoor hazards out of ground contact. Assessment is made a) by determining eventual failure through decay and b) by destr...
J K Carey, D F Purslow, J G Savory


JWPA method for testing effectiveness of surface coatings with preservatives against decay fungi
1981 - IRG/WP 2164
In 1979 JWPA established a new method for testing effectiveness of surface coatings in accordance with practical use of preservative-treated lumber. Comparing the new testing method with JIS A 9302, a few new trials - size of wood specimen, weathering procedure, and decay-test procedure - are incorporated....
K Tsunoda


Wood preservation in Poland
2004 - IRG/WP 04-30362
Dynamic growth of market demand for wooden elements and articles, generated in Poland increase of interest in industrial preservation. Today, Poland is a substantial producer and exporter of wood made products. Majority of exported wood - approximately 70% - is scotch pine (Pinus silvestris L.), which, due to its natural durability, requires preservation....
A Kundzewicz


Previous Page | Next Page