Micro-Distribution of Metals in Wood Treated with a Nano-Copper Wood Preservative
2007 - IRG/WP 07-40360
The microdistribution of copper in southern pine treated with a newly-developed nano-copper wood preservative was examined to determine if it differed from that reported for wood treated with conventional copper-based wood preservatives. Field Emission Scanning Electron Microscopy (FE-SEM) in combination with x-ray microanalysis (EDX) revealed the presence of nano-sized copper and iron particles i...
H Matsunaga, M Kiguchi, P Evans


Water repellency and dimensional stabilIty of wodd treated with waterborne resin acids/TOR
2007 - IRG/WP 07-40364
Wood used in above ground applications such as decking undergoes undesired dimensional changes leading to the lumber warping, cupping, splitting, etc. This is a major concern to consumers but it can be reduced by treating lumber with a water repellent. The ability of resin acids, hydrophobic compounds naturally present in southern yellow pines, was examined as a possible water repellent. A wate...
T P Schultz, D D Nicholas, J Shi


Effect of barriers on moisture content of treated and non-treated utility poles
2007 - IRG/WP 07-40369
The potential for non-biocidal barriers to slow moisture sorption was investigated using butt treated western redcedar poles immersed in either water or moist soil over a 2 year period. Moisture sorption was initially slowed by the barriers, but openings at the bottoms of the barriers eventually allowed moisture to migrate upward. Moisture levels in wrapped poles eventually reached those found in...
C S Love, J J Morrell


Comparative Laboratory Leaching Test Methods to Study Post-Treatment Storage Period Impacts on CCA Leachability and Fixation in Treated Kempas (Koompassia malaccensis) Heartwood
2007 - IRG/WP 07-20376
Three laboratory leaching test methods were compared to determine the effects of different post-treatment storage fixation periods on leachability/fixation of CCA components from treated kempas (Koompassia malaccensis) permeable heartwood. End-sealed test wood blocks of permeable were treated with CCA to target retention of 5.6 kg/m3, immediately stored to fix at ambient conditions for 0 and 48 ho...
A H H Wong, H C Lai


Durability of some alternatives to preservative-treated wood. Progress report 2: Results from field tests after 5 years’exposure
2007 - IRG/WP 07-30442
A number of alternatives to preservative-treated wood have been tested according to EN 252 (stake test) and a specially designed ground-proximity field test, the latter in Sweden as well as in Hawaii, USA. Seven untreated wood species and four alternative wood treatments labelled as environmentally friendly (acetylation, linseed oil, heat treatment, vinyl polymer) were included in the study. Four ...
M-L Edlund, J Jermer


Development of preservative treatment method using sub and super critical carbon dioxide
2007 - IRG/WP 07-40385
Significant efforts have been devoted for developing biocide impregnation method into wood materials using supercritical fluid. Developing better understandings of fluid phase and its effect on treatment results would facilitate a more rational development of supercritical fluid (SCF) impregnation. In this project, the preservative treatabilities under super- and sub-critical fluid conditions we...
Myeung-Won Cho, Sung-Mo Kang, Gyu-Hyeok Kim


Performance of softwood preservative treated stakes after 4 years exposure in-ground to decay fungi and termites in tropical Australia
2008 - IRG/WP 08-10643
This field study was based on the 1993 IUFRO method and designed as a graveyard (in-ground) test in the tropical region of the Northern Territory to examine the efficacy of novel preservative formulations developed as alternative protection for softwood timber against decay fungi and termites for Hazard Class 3 and 4. This study was supported by the Forest and Wood Products Research and Develop...
B M Ahmed (Shiday), J R J French, S R Przewloka, P Vinden, J A Hann, P Blackwell


Water Absorption of Various Building Materials and Mold Growth
2008 - IRG/WP 08-10657
Mold growth is a major problem for house owners, as it often occurs on the surface of building materials in damp houses. The principal method to control mold growth on building materials is to prevent water penetration into the materials. A study was recently conducted to determine water absorption rates of different wood species and panel materials used as building materials, when water intrusi...
Dian-Qing Yang


Relationship between coating properties and their performance on treated wooden decks
2008 - IRG/WP 08-30454
Preservative treated wood benefits from the application of a surface coating to protect it from weathering (UV and rain). Different preservative formulations may affect surface properties of treated wood differently; therefore compatibility of coatings with different preservative treated wood types should be considered. This paper examines coatings characteristics and their weathering performance ...
M Ahmadinejad, P A Cooper


Hydrophobic characteristics of pyrolysis oil
2008 - IRG/WP 08-30458
Hydrophobic behavior of pyrolysis oils obtained by pyrolysis of Scots pine wood (Pinus sylvestris L.) by using extruder type pyrolyzer at 450, 550 and 600 ºC was the objective of the study. Sapwood specimens (15×25×50 mm along the grain) were impregnated with the obtained pyrolysis oils by full- and empty cell treatment. The results indicated that wood impregnated with the studied pyrolysis o...
A Temiz, M Hakki Alma, N Terziev


Mechanical strength of wood from the Vasa shipwreck
2008 - IRG/WP 08-20381
Samples from three ancient ship wrecks (Vasa, Elefanten, and Gröne Jägaren) and recent oak samples as reference were examined with regard to mechanical strength using the high-energy multiple impact (HEMI) - test method, which delivers the resistance to impact milling (RIM) of a material. Adoption and optimisation of the test method for the particular sample size of the wooden drilling cores was...
A O Rapp, C Brischke, C R Welzbacher, T Nilsson, C Björdal


A preliminary note on the role of moisture absorption rate in durability assessment
2008 - IRG/WP 08-20383
The rate of moisture uptake was studied in 15 wood species using vermiculite at varying moisture levels as the exposure medium. As might be expected, moisture uptake varied widely among the species studied. While some of the more durable wood species were also resistant to moisture uptake, this was not always true. The results are discussed in relation to performance in under varying environmenta...
J J Morrell, L P Francis


Wood preservation by a mixed anhydride treatment: Using simple models of polymeric wood compounds
2008 - IRG/WP 08-30457
Treatment of wood by a mixed aceto/oleic (or other fatty acid residue) anhydride promoted as a safe and environment friendly wood preservation system has been examined quantitatively by liquid phase 13C NMR and solid phase MAS-DEC (proton decoupling) 13C NMR through all its different stages to determine which reactions occur with simple model compounds of the polymeric constituents of wood. The p...
F Lyon, M-F Thevenon, A Pizzi, G Tondi, A Despres, J Gril, S Rigolet


Primary Study on Compressed Preservative-treated Wood (CPW) for Outdoor Applications
2008 - IRG/WP 08-40412
In this study, the compressed wood samples pre-treated with hot water bath or water spraying were immersed in the ammoniacal copper quat –type D (ACQ-D) preservative solution to get compressed preservative-treated wood (CPW). The liquid absorption and the recovery rate of compression deformation of the compressed wood was determined, as well as the surface hardness, the distribution of density a...
Jinzhen Cao, Jia Mao


Above and Below-Ground Copper-Azole and Copper, Chrome Arsenate Depletion from Pinus radiata and Fagus sylvatica at Thirteen New Zealand & Australian Sites
2008 - IRG/WP 08-30460
The objective was to determine the significance of site on preservative depletion from Pinus radiata D. Don and Fagus sylvatica L. 20 x 20 x 500 mm field test stakes treated with a ground contact retention of copper amine plus tebuconazole (CuAz) and copper chrome arsenate (CCA) after approximately 5 years exposure to widely different soil and climate conditions. Site, wood species and their inter...
R Wakeling


The role of chromium in wood preservatives under BPD - a review and the current situation in Europe
2008 - IRG/WP 08-30468
Already during the IRG-meeting in Trømso a paper was presented to give an overview regarding the situation on chromium (JÜNGEL et al. 2006). Already in that year there was an increased attempt to achieve a science-based correct and harmonised solution in Europe regarding the chromium-question by the European Commission. Nevertheless the competent authorities (CAs) and the industry were similarly...
P Jüngel, S Hellkamp


Formation and Structure of Metal Azole Complexes
2008 - IRG/WP 08-30469
Divalent copper and zinc complexes with metal:azole ratio 1:2 were readily formed at room temperature with the fungicides tebuconazole and propiconazole. The structure of copper and zinc tebuconazole acetate and zinc cis-propiconazole chloride were examined by X-ray crystallography. In copper tebuconazole acetate, the copper atom lies on a crystallographic inversion centre and is coordinated to tw...
P D Evans, K J Schmalzl, C M Forsyth, G D Fallon, S Schmid, B Bendixen, S Heimdal


Preservative treatment of strips of Bambusa balcooa by soaking process using Borax-Boric acid
2008 - IRG/WP 08-30478
Bamboo strips made from Borak bamboo (Bambusa balcooa) were treated with 10% borax-boric acid aqueous solution by soaking process. The moisture contents of the bamboo strips were 12%, 20% and 30%. The strips were soaked for one, two, three, four and five days. The penetration of the solution was investigated by colour test after soaking and drying. Full penetration was observed after three days ...
K Akhter, M W Sheikh, M M Rahman, T A Chowdhury, M H Chowdhury


The effect of gamma radiation on selected wood properties
2008 - IRG/WP 08-40394
As an easy, fast, and effective sterilisation method, gamma irradiation changes molecular structures not only in pest’s living cells, but also in wooden cell walls. Radiation-induced depolymerisation causes significant changes in some properties of wood crucial for restoration and for laboratory testing of wood-preservative effectiveness. The influence of gamma radiation concerning total amount ...
R Despot, M Hasan, A O Rapp, C Brischke, C R Welzbacher


Preliminary investigation of biological resistance, water absorption and swelling of thermally compressed pine wood panels
2008 - IRG/WP 08-40396
Wood can be modified by compressive, thermal and chemical treatments. Compression of wood under thermal conditions is resulted in densification of wood. This study evaluated decay and termite resistance of thermally compressed pine wood panels at either 5 or 7 MPa and at either 120 or 150?C for one hour. The process caused increases in density and decreases in thickness of the panels; however, lab...
Ö Ünsal, S N Kartal, Z Candan, R Arango, C A Clausen, F Green III


Bending Properties of Southern Pine Treated with Micronized Preservative Systems
2008 - IRG/WP 08-40414
This study indicates that treatment of southern pine with micronized copper systems have no deleterious effect on the residual strength property values. No statistical differences between wood treated with micronized systems and water-treated controls were noted when means were compared using either Tukey’s test or S-N-K mean comparison tests. Using the more discriminating Least Squares anal...
H M Barnes, G B Lindsey, J Hill, M Pompeo, R Hodge


The Effect of Heat Treatment on Water Absorption and Dimensional Stability of Anatolian Chestnut (Castanea sativa Mill.) wood
2008 - IRG/WP 08-40407
The heat treatment of wood is an environment-friendly method for wood preservation. This process improves wood’s resistance to decay and its dimensional stability. However, mechanical properties decrease in different ration because of density loss as a result of heat treatment. In this study, the effect of heat treatment on water absorption and dimensional stability at different relative humidit...
G Gunduz, D Aydemir


Effect of steam on fixation of Cu-amine preservative treated wood
2008 - IRG/WP 08-50251
The rates of copper fixation in copper amine preservative treated wood were investigated with different fixation conditions (20° with drying and 50° without drying) and post-steaming. We also measured the degree of leaching for other biocide components (azoles, quatz, and Cu-HDO). Treatments conditioned at 20° with drying required 50 days or more to fix in woods. While copper was stabilized i...
Sung-Mo Kang, In-Yong Hwang, Suk-Kuwon Kim


Thermochemical Remediation of Preservative-Treated Wood
2008 - IRG/WP 08-50254
Remediation methods continue to be developed and refined for CCA-treated wood in order to divert this material from landfills and create secondary products from the wood fiber. A two-step thermochemical remediation method was developed to assess the efficiency of metal removal from CCA-treated spruce flakes. Nearly all the metals (As, Cr, and Cu) were thermochemically extracted from chromated copp...
R Sabo, C A Clausen, J E Winandy


Measurement of wood decay by dynamic MOE in an accelerated soil contact test
2008 - IRG/WP 08-20390
Current laboratory and field testing of preservatives involves various techniques to determine the extent of fungal attack, including visual inspection, mass loss, and static bending and compression strength measurements. The objective of this study was to compare decay measurement by conventional compression strength versus dynamic MOE, employing small wood stakes in an accelerated laboratory so...
Gan Li, D D Nicholas, T P Schultz