IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 515 documents. Displaying 25 entries per page.


The relationship between preservative type and surface degrade in Pinus radiata
1980 - IRG/WP 3158
Samples of Pinus radiata D. Don were impregnated with one of two preservative types, a copper chrome arsenic salt and a light organic solvent preservative. The panels were exposed to the weather for 4-5 years at a site near Sydney, Australia. Macroscopic and microscopic examinations showed different rates and patterns of weathering between the samples treated with each preservative and an untreate...
R S Johnstone, R K Bamber


Borates as wood preserving compounds: The status of research in the United States
1989 - IRG/WP 3542
This paper describes the extensive, on-going cooperative research effort among government and university research laboratories and industry to fully evaluate the potential for borates as wood preservatives in the United States. Research is discussed in terms of laboratory evaluations, field testing and mill trials, pilot plant pressure treatment studies, and remedial treatments. Future research pl...
H M Barnes, T L Amburgey, L H Williams, J J Morrell


Statement on laws relating to wood preservation in Brazil
1977 - IRG/WP 399
A set of copies of the laws relating to wood preservation in Brazil (in Portuguese) have been deposited with the IRG Secretariat. Generally speaking, it can be said that all public constructions have to comply with the laws that have been laid down. All organisations (governmental and private) which produce or apply wood preservatives are registered. The private sector is not obliged to abide by t...
P Karstedt


Blue stain in timber in service. Preliminary results of the IRG collaborative tests to compare natural and artificial weathering
1978 - IRG/WP 286
The collaborative programme was initiated at IRG Meetings in Wildhaus, 1976. The six collaborators were BAM (Berlin), Cuprinol Ltd (UK), EMPA (Switzerland), GORI (Denmark), PRL (UK) and Imperial College (UK). Experimental plans were finalised in December 1976 and panels treated by Cuprinol Ltd early in 1977. Natural weathering was carried out by BAM, Cuprinol, EMPA, GORI and PRL during April-Septe...
A F Bravery, D J Dickinson


Preservatives stains as exterior wood finishes
1977 - IRG/WP 389
For many years wood preservatives and paints have been used as the only treatment for exposed wood surfaces. Because of the inherent color of the preservatives, such as creosote, the wood surface was stained as well as protected from attack by micro-organisms. Paints protect surfaces from weathering, but recently, with an increased interest in maintaining the more natural appearance of exterior wo...
D W French


Progress report on "Studies on the effect of salinity on the growth and mortality of teredinids"
1976 - IRG/WP 418
An open flow aquarium was constructed at Forest Products Research Centre in 1972 in order to study the effect of salinity on the growth and mortality of teredinids. To determine the reliability of results obtained during salinity experiments, the growth rate of teredinids in the aquarium were compared with the growth rate of the same species living under natural conditions in the harbour in 1973. ...
S M Rayner


The association of bacteria with the increased permeability of water-stored spruce wood
1973 - IRG/WP 325
A microbiological investigation was undertaken to check our earlier work on patterns of bacterial counts and pH changes in water-stored wood. A survey of industrial activity was conducted upstream from the storage site with a view to explaining the existing bacterial flora. Further experiments were carried out with spruce bolts in enclosed tanks, using lake water with its natural bacterial flora a...
J A Dunleavy, J P Moroney, S E Rossell


Laboratory evaluation of water repellents as antisapstain treatment additives
1986 - IRG/WP 3382
Water repellent formulations consisting of five paraffin wax emulsions, three polyethylene wax emulsions, two polybutadiene resin emulsions, a polyester emulsion, and a ß-pinene polymer emulsion were subjected to water repellency tests on radiata pine sapwood. With one exception, the parafin wax emulsions were more effective water repellents than the alternative formulations and one of the paraff...
D V Plackett, C M Chittenden


The development of a new boron-based wood preservative
1995 - IRG/WP 95-30085
The paper describes a new boron based wood preservative for the treatment of green timber. The product offers many benefits over conventional boron diffusion treatment including: 1. high viscosity, high concentration formulation; 2. permits dip treatment of a wide range of sawn board and pole sizes at ambient temperatures; 3. permits full cross section diffusion of borates without block stacking a...
P Turner, D Conradie


Feeding response of field populations of Coptotermes species to softwood blocks treated with non-toxic water-proofing and anti-microbial products.
2003 - IRG/WP 03-10487
The feeding response of field populations of the subterranean termite, Coptotermes lacteus, to Pinus radiata wood blocks (50 x 40 x40 mm) treated with various combinations of non-toxic and odourless water-proofing materials based on natural high molecular weight esters (TimberTreatÒ) and a new water insoluble quaternary ammonium compound (‘anti-microbial’) is described. Treated wood blocks we...
J R J French, T Pynsent, M Susic


A technique for determining the efficacy of water diffusible preservative plugs for implanting in joinery in service
1987 - IRG/WP 2291
A technique is described for determining the efficacy of soluble, diffusible preservative plugs for eradicating decay in joinery. It uses blocks of Scots pine sapwood or heartwood adjusted to known moisture contents prior to the establishment of the test fungus Coniophora puteana, from a single longitudinal dowel and the subsequent introduction of the preservative plugs. Prevention of decay, eradi...
J K Carey, A F Bravery


The degradation of wood surfaces by dilute acids
1985 - IRG/WP 3326
Thin radial/longitudinal sections(~100 µ) of Corsican Pine (Pinus nigra) and Lime (Tilia vulgaris), were exposed to Sulphuric, Sulphurous, nitric, acetic, and formic acid at 40°C in the pH range 2-6. After about 3 months exposure to Sulphuric, nitric, acetic and formic acid at pH 2.0 Pine lost some 20-25% of its tensile strength. Losses in tensile strength due to sulphurous acid were greater bei...
P D Evans, W B Banks


Protection of cellulose string with biocide/water repellent mixtures
1997 - IRG/WP 97-30148
Protecting cellulosic materials in soil contact poses a formidable challenge. Many soil inhabiting bacteria and fungi that cannot degrade wood can nevertheless rapidly depolymerize cellulose once its protective lignin matrix is removed. As a result, cellulose based materials are rarely used in direct contact with soil. One exception, however, is the use of cellulose string to support climbing vine...
A B Chang, J J Morrell


Methods to determine the efficacy of three water repellent additives in waterborne preservatives
1997 - IRG/WP 97-30142
The paper describes the methods used to determine the efficacy of three different water repellent additives in waterborne preservatives. The wooden samples used are pine (Pinus sylvestris) and spruce (Picea abies) that are treated with 9 different waterborne preservatives in retention for hazard class 3 (above ground commodities). There are two sample sizes exposed, cladding boards (19 x 148 mm) w...
F G Evans, B Nossen, K M Jenssen, L R Wilhelmsen, G Fuglum


Glue-line additives for protecting plywood. A review
1978 - IRG/WP 2102
The conclusions of this review are: 1) Insecticidal glue-line additives can be used satisfactorily to protect plywood against insect attack. 2) It is uncertain, in spite of some claims, wether fungicidal glue-line additives can be similarly used to protect plywood against fungi under damp conditiones. There is a need for further work to validate the mycological tests that may be used to investigat...
R Cockcroft


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic applications. Part 1: Laboratory scale investigation
1995 - IRG/WP 95-50046
In order to investigate the applicability of current prestandard leaching test methods, a series of experiments has been performed on CCA impregnated wood dealing with the influence of pH, temperature and agitation of the surrounding water. The leaching method used in this first part of the investigation is the European prestandard drafted by CEN/TC38/WG11, a short term dynamic leaching test under...
G M F Van Eetvelde, R J Orsler, G E Holland, M Stevens


Aquatic toxicity research of structural materials
1998 - IRG/WP 98-50114
Continuing from preliminary results reported on the aquatic toxicity of some tropical hardwoods under high hazard conditions, a more comprehensive research study is set-up in order to assess the environmental toxicology of various structural materials in water applications. Hazard class 4 preservative treated wood is tested for its toxic response on a battery of aquatic test organisms, next to con...
G M F Van Eetvelde, S De Geyter, P Marchal, M Stevens


Influence of water soluble extractives on CCA fixation and leaching performance of red maple and red oak
1997 - IRG/WP 97-30133
We have observed several peculiarities in relation to CCA fixation in red maple and red oak woods such as high variability in fixation rates and leaching performance in maple and precipitate formation in solutions expressed from CCA treated red oak wood blocks at different stages of fixation. We have postulated that the extractives could be the factor of influence, as this has already been reporte...
T Stevanovic-Janezic, P A Cooper, Y T Ung


IRG/COIPM INTERNATIONAL MARINE TEST - To determine the effect of timber substrate on the efectiveness of different preservatives in sea-water: Coding scheme
1976 - IRG/WP 420
It was agreed in Wildhaus on 15 May 1976 that preparations for the test detailed in Document No: IRG/WP/414 should commence immediately, but that initially only two water-borne preservatives should be used - a copper/chrome/arsenic (CCA) and a copper/chrome/boron (CCB) formulation respectively. PRL, England (R Cockcroft) would be responsible for supplying only the reference species treated with th...
Anonymous


Moisture content of logs under sprinklers
2000 - IRG/WP 00-40157
Logs are kept under sprinklers during storage for avoiding the development of sapstain fungi. According to literature, sapstain fungi do not develop if the moisture content is above 120%. It is supposed that, the water sprinklers maintain the log's moisture content above this value, but, very often, sapstain is found on sawn lumber cut from these logs. Logs are harvested and transported t...
M C Rose, A M Briones, M Fernández


A bioassay of remedially treated pole material
1987 - IRG/WP 3453
Stubs prepared from treated and untreated utility poles were installed in a test plot and pressure spade treated at the groundline with one of four preservative greases. At one and three year intervals, core samples were removed from the stubs and the improvement in the preservative efficacy due to the greases was assessed. The bioassay investigation showed that only bis(tributyltin) oxide (TBTO) ...
J N R Ruddick, L Parker


A substantively bonded water repellent treatment based on chromium carboxylates
1985 - IRG/WP 3344
Chromium carboxylates soluble in toluene have been synthesised and applied to Scots pine (Pinus sylvestris) sapwood. Without any further treatment, the compounds may be readily leached from wood surfaces with toluene. After a period of heating however, they become fixed to the cell wall, substantial amounts being resistant to leaching even under reflux conditions for several hours. Treatment of wo...
J K Wright, W B Banks, W J Eilbeck


The effect of oil-borne preservative treatments on the shear strength of FRP/wood composite adhesive bonds
2003 - IRG/WP 03-40265
Reinforcement of structural wood components with Fiber Reinforced Polymer (FRP) will enhance the beam’s strength, but actual data on long-term durability is sparse, not well documented or not readily accessible. In this study, bond properties of FRP-wood composite materials were investigated following treatment with creosote or copper naphthenate preservatives. The properties investigated inclu...
B Herzog, B Goodell, R Lopez-Anido


A field trial to assess the potential of antisapstain chemicals for long-term protection of sawn radiata pine
1986 - IRG/WP 3375
Seven chemical formulations were tested as antisapstain treatments for freshly sawn radiata pine sapwood (90x50 mm²). Each formulation was used with and without a water-repellent additive and was sprayed on to 1 m long boards. The boards were then stacked into "mini" packets and stored unprotected from the weather for 6 months. Haipen 50w (at 0.2 or 0.4% active) and NaPCP (1% active) plus 1.5% bo...
J A Drysdale


Prevention of sapstain in logs using water barriers
1997 - IRG/WP 97-30147
Placing logs in ponds or under water sprinklers to keep moisture levels high enough to prevent oxygen tensions rising above inhibitory levels, is a proven method of preventing sapstain. The objective of this experiment was to determine if water barriers significantly reduce the rate of sapstain penetration into logs by maintaining moisture contents, and consequently oxygen tensions, at inhibitory ...
R N Wakeling, D R Eden, C M Chittenden, B Carpenter, I Dorset, J Wakeman, R Kuluz


Previous Page | Next Page