IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 500 documents. Displaying 25 entries per page.


Working plan: Second international collaborative field trial
1995 - IRG/WP 95-20056
This paper describes the scope, objectives, and approaches to be used in the second international collaborative field trial approved by the Scientific Programme Committee for partial funding in 1994. The trial is designed to develop a broad data base on causal mechanisms, interactions, and factor affecting the performance of treated wood in ground contact. The trial encompasses 12 different field ...
H M Barnes, T L Amburgey


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 22: Report on the conditions of specimens at Sekondi, Ghana after 60 months
1986 - IRG/WP 4123
The results of the third inspection of CCA and CCB treated test panels exposed at Sekondi, Ghana in June 1980 are presented. None of the panels still in test, i.e. panels of Pinus sylvestris treated with CCA at 3 and 10%, Alstonia scholaris treated with CCA at 10%, Fagus sylvatica treated with CCA at 10%, and Erythrophleum ivorense and Mitragyna stipulosa both treated with CCB at 10%, shows any ex...
F F K Ampong, N Asare-Nyadu


Performance of water-borne pressure treated fence posts - A practical application of the new Canadian field test data base
1988 - IRG/WP 2305
50 years of test plot data acquisition have been recently set up as a computerized database. The new database which contains information on the service life of a great number of non durable Eastern Canadian wood species treated with various preservatives and many application processes is presented. As an example for its use, a summary of the performance of fence posts treated with waterborne prese...
E E Doyle, R Dubois, J P Hösli


Future insecticidal treatments for wood products
1980 - IRG/WP 3140
Protective measures involving chemical treatment of wood use only a narrow range of toxic materials which are divisible into two groups, (i) those that are water-soluble, (ii) those that are soluble only in organic solvents. It is generally true to say that, as far as protection against insects is concerned, the former are stomach poisons while the latter are largely (though not exclusively) conta...
D J Cross


Microdistribution of water-borne preservatives in blue gum treated by full-cell process
1990 - IRG/WP 3617
The present work deals with the study of the microdistribution of copper, chrome and arsenic elements in Eucalyptus globulus Labill. sapwood, treated with a CCA water-borne preservative by full-cell process, with the help of scanning electron microscopy together with energy dispersion X-ray analysis technique. The work shows that the retention of CCA elements is high in vessels and vasicentric par...
D De Sousa Castro Reimão, J M Palacios


Influence of water-borne preservatives on water repellency and the impact of addition of water repellent additives
1992 - IRG/WP 92-3704
The primary goal of a desirable wood preservative system is to effectively control decay fungi and other biodeteriogens in service. The water repellent nature of a given system may play an important role in the protection of wood. In this study, the water repellency of several water-borne preservative systems has been evaluated by measurements of tangential swelling during immersion. The systems i...
L Jin, D M Roberts, A F Preston


Wood protecting chemicals for the 21st century
1993 - IRG/WP 93-30018
After assessing the past research with protection chemicals, this paper proposes future avenues for research and development in wood protection. Three scenarios are put forward for consideration. First, more is not better and future systems will emphasize combination formulations which enhance properties while providing biological efficacy. Second, current systems, especially those based on copper...
H M Barnes


Penetration and absorption of water-borne preservatives in conifers from the Western United States: A preliminary report
1988 - IRG/WP 3475
The treatment of most softwoods from the western United States with waterborne chemicals poses a major challenge. Although many of these species are commercially treated with waterbornes, there is considerable debate about their treatability. At present, there is little or no information on the treatability of western wood species with waterborne chemicals. The lack of accurate treatability inform...
S Kumar, J J Morrell


The future for chromium in wood preservation
1985 - IRG/WP 3332
Most water-borne preservatives contain CrVI compounds, originally to reduce corrosion although now also to improve toxicant fixation. Chromium contributes to preservation and this is recognised in, for example, New Zealand and USA where chromium contents are included in calculations of overall preservative activity of CCA formulations, but chromium may also have anti-stain and joinery (millwork) p...
B A Richardson, T R G Cox


Leaching of components from CCF treated timber in ground contact
1998 - IRG/WP 98-50108
In order to investigate the depletion of different CCF-salts during service small stakes (10*10*450mm³) were treated with five water-borne wood preservatives and after fixation brought into ground contact for several years. After failing some of the broken down stakes were used to determine the remaining concentration of relevant ions and their distribution in different segments of the stakes. A...
E Melcher


The potential of high pressure pulsation processes to treat white spruce lumber with water-borne preservatives
1988 - IRG/WP 3471
Laboratory work using end sealed 4x8x46 cm³ white spruce samples has been done to explore the suitability of three variants of a 2.1 MPa pulsation process for the impregnation of white spruce with CCA. The results showed that the process improved significantly the penetration of the preservatives and reduced significantly cell collapse, when compared with the results of treatment using a 2.1 MPa ...
J P Hösli, J N R Ruddick


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 17: Report of fifth inspection (4 years) in Italy
1983 - IRG/WP 4103
The wood samples of Alstonia scholaris, Fagus sylvatica, Pinus sylvestris were submerged in the sea at Follonica, Italy, in April 1977. Follonica, latitude 42°55' North and longitude 10°45' East, is situated on the Tyrrhenian coast. The recorded temperature varies from 13°C to 25°C, salinity 37-38% and pH about 8. The inspections were carried out after 6 months (10/1977), 12 ...
A Gambetta, E Orlandi


Soft rot in heartwood of preservative-treated pole stubs of Eucalyptus cypellocarpa L. Johnson
1983 - IRG/WP 1204
Pole stubs of Eucalyptus cypellocarpa L. Johnson, treated in the sapwood with certain waterborne preservatives and exposed for 21 to 23 years in a dry tropical region were severely soft-rotted in the heartwood, as well as the sapwood. They broke with a brash fracture when stress tested (loaded as a cantilever) in the field. The severe soft rot in the heartwood was not detected by the knife test or...
J E Barnacle, G C Johnson, M A Tighe


Enhancing the Performance of Transparent Coatings by UV Protective Pre-treatments
2006 - IRG/WP 06-30399
Most industry observers anticipate a change from copper-based preservatives to metal-free combinations of organics for residential treated wood products in North America within the next one to five years. While the chromium copper provide considerable protection against UV, metal-free formulations will need UV protection in the form of additives or coatings. While transparent coatings can be made ...
P I Morris, S McFarling


Growth and succession of mould on commercial paint systems in two field sites
2007 - IRG/WP 07-30421
Discolouring fungi reduce the service life of coated wooden claddings in façades and increase the total cost of ownership due to shorter maintenance intervals. It is of major importance to find paint systems for wood which are durable and have a high resistance to mould growth. A total of 15 paint systems from 9 different manufacturers were exposed on two field sites, Sørkedalen and Birkenes, ...
L Ross Gobakken, K M Jenssen


Preservative treatment of Golla cane (Daemonorops jenkinsiana) by pressure process
2007 - IRG/WP 07-40379
The feasibility of preservative treatment of golla cane (Daemonorops jenkinsiana (Griff) Mart). by pressure process has been studied using water borne preservatives CCB (copper-chrome-boron). Cane samples of three different lengths 1m, 2m and 3 m. were treated at different pressure and time period to evaluate the extent of penetration and retention of preservative chemicals. It was observed that t...
K Akhter, M Hoque Chowdhury


Selection of an appropriate coating system for wooden boats to be used in fresh water
2009 - IRG/WP 09-40472
Properties of several, most commonly used protective low-price coatings, which are used by the pletnja boat owners in Bled, Slovenia, were extensively studied. The aim of this professional, practically oriented study was to compare various coating systems, and to recommend the most suitable one to the boat owners. Regarding specific use conditions, the following properties, including their resista...
M Petrič, B Kričej, A Logar, M Pavlič


Water uptake of wood surfaces with and without coating: influence of weathering
2012 - IRG/WP 12-40580
The objective of this study was to compare liquid water absorption of wood surfaces with and without coating, before and after artificial weathering. Samples of spruce, oak and sapelli were exposed to the EN 927-6 cycle for 1500 and 1850 hours and to the weathering produced by the Garner wheel for 1000 hours. Two highly pigmented coatings (solventborne and waterborne) and two semi-transparent stai...
L Podgorski, S Collignan, J D Lanvin


Protective nanoparticle coating reducing water absorption of wood species
2012 - IRG/WP 12-40614
Nanoparticle coatings were deposited onto different tropical wood samples for controlling the surface hydrophobicity. The styrene(maleimide) nanoparticles were synthesized in aqueous dispersions under pure conditions or in combination with 70 wt.-% palm oil. A first evaluation of the non-coated wood surfaces indicates a high dependence between the water contact angles, the average surface roughnes...
P Samyn, A Paredes, G Becker, H Van den Abbeele, L Vonck, D Stanssens


Influence of coatings on water uptake of wood surfaces before and after natural and artificial weathering
2013 - IRG/WP 13-40641
Liquid water absorption of wood surfaces with and without coating, before and after exposure to artificial and natural weathering has been studied. Spruce, oak and sapele samples have been exposed to the cycle of EN 927-6, to the cycle of the Gardner wheel and to natural weathering. Five coatings were tested including solventborne and waterborne, semi-transparent and opaque products. Exposure to w...
L Podgorski, S Collignan, J-D Lanvin


Relative efficacy of various oxine copper formulations against brown-rot fungi
2019 - IRG/WP 19-30741
This paper investigates the relative resistance of three different oxine copper formulations (oil-borne, water-borne, water-borne with pH-adjustment) as a preservative treatment for wood against brown-rot fungi. Impregnated southern pine sapwood cubes were exposed to R. placenta and G. trabeum cultures in a soil-block test. After eight weeks, the weight losses of the cubes were examined in relatio...
M Petruch, J Lloyd, A Taylor


Performance of a water-borne stain on beech, spruce, MDF and OSB improved by plasma pre-treatment
2020 - IRG/WP 20-40897
Coatings are an important part of wood protection, especially for outdoor applications. In order to provide a good protection, protective coatings need to exhibit good adhesion, mechanical resistance, and weathering resistance. Plasma pre-treatments are an established method to increase the performance of existing coatings including those on wood and wood-based substrates. Moreover, plasma deposit...
S Dahle, J Žigon, I Uranjek, M Petrič


Treatability of South African-grown Eucalyptus grandis with water-borne copper azole and disodium octaborate tetrahydrate wood preservatives
2021 - IRG/WP 21-40920
This study investigated the treatability of the sapwood and heartwood of sawn Eucalyptus grandis with copper-azole (CuAz) and disodium octaborate tetrahydrate (DOT) water-borne preservatives towards improving its durability for enhanced use in structural solid wood applications. The results obtained showed that, at a moisture content of 12 ± 1%, sawn E. grandis sapwood can be impregnated to a mea...
A A Alade, Z Naghizadeh, C B Wessels


Evaluation of weathering and termite resistance of the Myoung-oil as a Korean traditional coating agent
2022 - IRG/WP 22-10996
This study investigated the applicability of Myoung-oil (MO) as an eco-friendly preservative of Korean wooden cultural properties and buildings. Wood test specimens painted with various concentrations of MO were exposed in the external environment. Then color change and wettability of the wood surface were evaluated and compared depending on the exposure time. As a result of exposure for 12 months...
S-M Yoon, Y Park, W-S Jeon, H-M Lee, J-G Park, K Dal Nam, W-J Hwang


Management of the wood and additives wastes in the wood processing industries: Problematics and technical answers review
1996 - IRG/WP 96-50073
Management pathways for pure wood subproducts are well known and used; but as soon as additives like preservatives, glues, varnishes or coatings are present within the wood wastes, their disposal or valorization becomes more tricky. The different kinds of mixed wood wastes of the wood processing industries, from the sawmill to the furniture manufacture, are identified herewith and their diversity ...
S Mouras, G Labat, G Deroubaix


Previous Page | Next Page