Current state of world standardization in the toxicometric methods for testing of wood preservatives
2007 - IRG/WP 07-20354
The paper presents an outline of the history of forming standardized toxicometric methods for testing of wood preservatives in the world during last 100 years. Numerous studies resulted in three main methods which are currently used for official and basis assessment of biocides: - agar-block method in Europe (EN 113); - soil-block method in the USA and Pacific countries (ASTM D 1413); - modifi...
J Wazny


Detecting fungal DNA in treated and non-treated wood
2007 - IRG/WP 07-10621
Isolating fungi from wood has long involved culturing on selective media followed by identification using various keys. This process can be cumbersome, costly, and, most importantly, not always capable of detecting all of the fungi present. The recent development of molecular methods for isolation and identification of fungi has created tremendous opportunities for expanding our knowledge of the...
C Freitag, M Freitag, J Morrell


Accelerated Above-ground Testing of Wood Preservatives
2007 - IRG/WP 07-20358
The Canadian wood preservation industry is interested the introduction of new preservative formulations, some of which are intended only for above ground uses. Canada’s Pest Management Regulatory Agency requires data from field tests under Canadian conditions but these can take many years to generate results. Forintek has therefore developed an accelerated above ground test, under contract to a ...
P I Morris, S McFarling


Use of the Digital Refractometer for the On-site Analysis of Copper-based Preservative Systems
2007 - IRG/WP 07-20371
In some counties, there are no on-site chemical analysis methods available for treatment plants to use to determine the key active ingredients in the preservative treatment solutions. The complexity of the sophisticated methodology; cost of analytical instruments and training required for operating these instruments in treating plant level are the reasons for lacking such practice. In this paper...
L Jin, T Cashman, A Preston, J Trompetter, H Trompetter


Photo-degradation of modified and non-modified wood, coated with water borne acrylic coatings during artificial light exposure
2007 - IRG/WP 07-30416
A series of experiments were carried out to investigate photo-degradation of thermally modified (at 210oC and – 0.9 bars for two hours) and non-modified spruce wood (Picea abies L (Karst)), coated with transparent and semitransparent (with 3% pigment content) acrylic coatings during artificial UV light irradiation for 200 hours. Photo-degradation was evaluated in terms of colour changes througho...
M Deka, M Tomažic, M Petric


Protection of wood for above ground application through modification with a fatty acid modified N-methylol/paraffin formulation
2007 - IRG/WP 07-40378
Hydrophobic chemical modification can be regarded as an alternative approach to conventional wood preservation using biocides in order to protect wood in hazard class 3 according the European Standard EN 335-1. A formulation containing fatty acid modified N-methylol/paraffin and an aluminium salt catalyst was used to change the material properties of wood in order to protect wood from fungal dec...
Nguyen Hong Minh, H Militz, C Mai


The effect of brighteners on wood surface aesthetics – exploring the use of various organo-phosphonates based precursors
2007 - IRG/WP 07-30441
Freshly cut hardwood lumber such as white oak, red oak, beech, or redwood are rich in mineral stain (mostly iron and calcium), which provides a strong discoloration of the wood surface significantly influencing the aesthetic of the wood surface and strongly affecting the cost of this lumber. The influence of mineral stain on soft wood discoloration (Southern Yellow Pine, Douglas fir, etc.) is les...
R Craciun, P Mitchell


Refinement of emission values for preserved wood in the ‘Storage Scenario’, for use in the environmental risk assessment of Wood Preservatives under the Biocidal Products Directive
2007 - IRG/WP 07-50244
The evaluation of an active substance or a biocidal product under the Biocidal Products Directive (BPD) requires that an environmental risk assessment is carried out. The risk assessment for wood preservatives includes a scenario for the treated wood in storage after treatment, in which the predicted environmental concentration (PEC) in soil, surface water and groundwater is calculated, using emis...
E F Baines


Evaluatiang the potency of cinnamaldehyde as a natural wood preservatives
2007 - IRG/WP 07-30444
Since cinnamaldehyde, the major constituent of leaf essential oil from Cinnamomum osmophloeum, has significant antifungal and antitermitic activities, it is worthy of understanding whether cinnamaldehyde has potential to be used as a natural preservative for improving the durability of wood. In this study, the fungi and termite resistance of cinnamaldehyde-treated wood (CTW) were evaluated accordi...
Chun-Ya Lin, Chi-Lin Wu, Shang-Tzen Chang


Water Absorption of Various Building Materials and Mold Growth
2008 - IRG/WP 08-10657
Mold growth is a major problem for house owners, as it often occurs on the surface of building materials in damp houses. The principal method to control mold growth on building materials is to prevent water penetration into the materials. A study was recently conducted to determine water absorption rates of different wood species and panel materials used as building materials, when water intrusi...
Dian-Qing Yang


Validity of above ground testing according to ENV 12037
2008 - IRG/WP 08-20379
The standard ENV 12037 for testing of treated and untreated wood (lap-joint) exposed above ground was issued in 1996 by The European Committee for Standardization. A draft for the development of the standard was presented by CEN-TC 38/WG 25/DOC N 076 in 2002. For a test to become valid the median rating of decay for untreated control replicates (Scots pine sapwood) must be equal or greater than ...
Ö Bergman, U Råberg, N Terziev


Mechanical strength of wood from the Vasa shipwreck
2008 - IRG/WP 08-20381
Samples from three ancient ship wrecks (Vasa, Elefanten, and Gröne Jägaren) and recent oak samples as reference were examined with regard to mechanical strength using the high-energy multiple impact (HEMI) - test method, which delivers the resistance to impact milling (RIM) of a material. Adoption and optimisation of the test method for the particular sample size of the wooden drilling cores was...
A O Rapp, C Brischke, C R Welzbacher, T Nilsson, C Björdal


Development of a Weatherometer to Accelerate the Surface Checking of Wood
2008 - IRG/WP 08-20388
There is significant interest in developing preservatives that are better at preventing wood from checking. Currently, however, there is no accepted test methodology for accelerating the development of checks in wood samples so information on the effectiveness of treatments at restricting checking can be obtained more quickly. This paper describes the development of a new type of weatherometer (Ac...
R Ratu, P D Evans


Wood preservation by a mixed anhydride treatment: Using simple models of polymeric wood compounds
2008 - IRG/WP 08-30457
Treatment of wood by a mixed aceto/oleic (or other fatty acid residue) anhydride promoted as a safe and environment friendly wood preservation system has been examined quantitatively by liquid phase 13C NMR and solid phase MAS-DEC (proton decoupling) 13C NMR through all its different stages to determine which reactions occur with simple model compounds of the polymeric constituents of wood. The p...
F Lyon, M-F Thevenon, A Pizzi, G Tondi, A Despres, J Gril, S Rigolet


Field Stake Tests with Copper-based Preservatives
2008 - IRG/WP 08-30459
The performance of field test stakes derived from commercially produced ground contact retention copper quat preservatives based on either soluble copper complexed with ethanolamine, or from a water-based suspension of particulate micronized copper compounds, as well as untreated southern yellow pine controls, is compared at two decay test sites. After less than one year in field test some of t...
A Preston, L Jin, D Nicholas, A Zahora, P Walcheski, K Archer, T Schultz


Effect of amphiphilic antioxidant alkyl ammonium ascorbate on inhibition of fungal growth: Application to wood preservatives formulation
2008 - IRG/WP 08-30466
Amphiphilic surfactants were synthesized from ascorbic acid and different fatty amines and evaluated for formulation of wood preservation products. Characterization of physicochemical properties of the new compounds indicated classical behavior of cationic surfactants. Antioxidant properties, estimated using methyl linoleate oxidation inhibition method, were similar to that of ascorbic acid teste...
C Gérardin , T Koumbi Mounanga, P Gérardin


The role of chromium in wood preservatives under BPD - a review and the current situation in Europe
2008 - IRG/WP 08-30468
Already during the IRG-meeting in Trømso a paper was presented to give an overview regarding the situation on chromium (JÜNGEL et al. 2006). Already in that year there was an increased attempt to achieve a science-based correct and harmonised solution in Europe regarding the chromium-question by the European Commission. Nevertheless the competent authorities (CAs) and the industry were similarly...
P Jüngel, S Hellkamp


The Comparison of Fixation and Leachability of Bark, Fruit and Leaf Tannin Extracts with Boron Minerals
2008 - IRG/WP 08-30473
Tannins extracted from several plants have natural durability properties. Due to these properties, some of the researchers have studied them for protecting wood. In this study, Scots pine (Pinus sylvestris) and beech (Fagus orientalis) wood samples were treated with bark, fruit, and leaf extracts as well as water-based wood preservative salts at various concentrations to increase fixation. The pen...
S Sen, C Tascioglu, K Tirak


Performance of wood-based composites in a protected aboveground test in southern Japan
2008 - IRG/WP 08-40391
Five kinds of untreated wood-based composites (medium density fiberboard, hardwood plywood=HP, softwood plywood, particleboard and aspen oriented strand board, hereinafter abbreviated as MDF, HP, SP, PB and OSB, respectively) were exposed to subterranean termites and microbial (decay) attack under protected aboveground conditions in a southern part of Japan (Kagoshima Prefecture) for six years. An...
K Tsunoda


The effect of gamma radiation on selected wood properties
2008 - IRG/WP 08-40394
As an easy, fast, and effective sterilisation method, gamma irradiation changes molecular structures not only in pest’s living cells, but also in wooden cell walls. Radiation-induced depolymerisation causes significant changes in some properties of wood crucial for restoration and for laboratory testing of wood-preservative effectiveness. The influence of gamma radiation concerning total amount ...
R Despot, M Hasan, A O Rapp, C Brischke, C R Welzbacher


Preliminary investigation of biological resistance, water absorption and swelling of thermally compressed pine wood panels
2008 - IRG/WP 08-40396
Wood can be modified by compressive, thermal and chemical treatments. Compression of wood under thermal conditions is resulted in densification of wood. This study evaluated decay and termite resistance of thermally compressed pine wood panels at either 5 or 7 MPa and at either 120 or 150?C for one hour. The process caused increases in density and decreases in thickness of the panels; however, lab...
Ö Ünsal, S N Kartal, Z Candan, R Arango, C A Clausen, F Green III


The Effect of Heat Treatment on Water Absorption and Dimensional Stability of Anatolian Chestnut (Castanea sativa Mill.) wood
2008 - IRG/WP 08-40407
The heat treatment of wood is an environment-friendly method for wood preservation. This process improves wood’s resistance to decay and its dimensional stability. However, mechanical properties decrease in different ration because of density loss as a result of heat treatment. In this study, the effect of heat treatment on water absorption and dimensional stability at different relative humidit...
G Gunduz, D Aydemir


Near infrared spectroscopy for the quantification of wood preservatives
2008 - IRG/WP 08-20391
Near infrared (NIR) spectroscopy is a rapid, flexible, inexpensive and non-destructive technology that has many applications, including the evaluation of many wood properties. Initial studies have indicated the potential to apply NIRS for the quantification of wood preservatives. However, further evaluation with borate and azole preservative systems has revealed that NIRS technology is challenged ...
A M Taylor, Seung H Baek, Myong K Jeong, J D Lloyd, J J Morrell


Wood preservative obtained by recycling – preliminary selection of leaching inhibitor
2008 - IRG/WP 08-50252
Based on recycling of used household batteries, a process was developed to enable the recovery of major manufacturing components, leading to a solution of zinc (32 g.l-1) and manganese (15 g.l-1) salts, free of heavy metals. The potential use of the above solution as wood preservative was demonstrated by means of assays both of fungicidal activity -using white and brown rot fungi- and of insectici...
C Ibáñez, C Mantero, G Cecchetto, M Rabinovich, M Cerdeiras


Comparison of laboratory and natural exposure leaching of copper from wood treated with three wood preservatives
2008 - IRG/WP 08-50258
Standard and non-standard laboratory and field leaching tests were used to compare copper leaching from wood treated to above ground and ground contact specified retentions for three wood preservative systems, CCA-C, ACQ-D and a micronized copper formulation with quat DDAC as co-biocide. Copper leaching was highest for the ACQ formulation. Percent leaching was lowest for the micronized copper sy...
P A Cooper, Y T Ung


Previous Page | Next Page