A review of the current status of the estimation of emissions from preserved wood and their use in the environmental risk assessment of wood preservatives under the Biocidal Products Directive
2005 - IRG/WP 05-50224-7
A review and update of the status of the issues concerning the estimation of emissions from preserved wood (e.g. amendments to the proposed ‘OECD Guidelines’), and the environmental risk assessment of wood preservatives under the Biocidal Products Directive (e.g. compartmental sizes, emissate ecotoxicity testing)....
E F Baines


The use of organic wood preservatives in ground contact and the suitability of laboratory test procedures to determine their efficacy
1999 - IRG/WP 99-20175
Organic fungicides, such as propiconazole, have proven to be highly effective when used as a co-biocide in recently developed wood preservative formulations. They have however been ineffective when used as a stand alone preservative, particularly when used in ground contact (European Hazard class 4). Previous research, using the test methods of ENV 807 (1993), provided conflicting evidence regardi...
I J Herring, D J Dickinson


The extraction of boron from treated wood for quantitative analysis: A comparison of procedures
1992 - IRG/WP 92-2414
The extraction of boron preservative from treated rubberwood and scots pine samples was compared using methods based on refluxing and extraction in 1N NaOH or distilled water at 80°C. The extract solutions were analysed by Inductively Coupled Plasma spectroscopy (ICP/AES). A simple extraction procedure based on immersion of wood samples of approximate dimension 2 x 1 x 1 cm³ in distilled water a...
R J Murphy, D J Dickinson, P W McCormack, M K Lung


Co-operative tests concerning the influence of solvent and drying method on the toxic limit of wood preservatives against Coniophora cerebella
1972 - IRG/WP 216
In the working group II of the IRG it was agreed that more knowledge was necessary concerning the influence of the solvent on the toxic limit of organic solvent types of wood preservatives against Basidiomycetes. A test program was drawn up and after discussion in the mentioned working group the final program was accepted by the co-operating institutes in 1969. In the test program two fungicides, ...
T Hof


Water transfer in wood in relation to fungal attack in building - Effect of condensation and diffusion
1992 - IRG/WP 92-1543
Wood is continuously exchanging moisture with the surrounding atmosphere, the temperature and relative humidity are important factors. Wood moisture in this case is not enough to provoque decay by fungi. However, when, during the night, condensation appears cyclically, wood absorbs water and moisture content may be sufficiently high to allow development if drying does not take place. The water tra...
D Dirol, J-M Vergnaud


Bethoguard; A new wood protecting fungicide for use in metal free ground contact wood preservatives
2002 - IRG/WP 02-30301
Research has identified the limitations in both the spectrum of activity and permanence of organic biocides placed in wood in high hazard environments, particularly in the absence of heavy metals such as copper. More specifically, the control of soft rot decay in wood in soil contact has proven to be most problematic. The new organic biocide, Bethoguard; an oxathiazine, has demonstrated excellen...
S C Forster, G R Williams, M Van Der Flaas, M Bacon, J Gors


Changes of copper and chromium content after leaching in wood impregnated with the CCB and CB preservatives
2000 - IRG/WP 00-50147
The objective of the study was impregnated with CCB and CB preservatives pine wood of moisture content varying from 12% to 55% subjected to leaching. Losses of copper and chromium were determined for individual layers of wood up to 3 cm from the girth. The results were compared to the total amount of metals determined in water extracts. The degree of leaching of metal ions from wood of 55% moistur...
B Mazela


Wood preservation in Croatia
2004 - IRG/WP 04-30360
Croatia, as all the other countries in transition, however also because of its specific and well-known reasons, is on a path to gradual drawing nearer to the European standards. Only the scientists working at the Faculty of Forestry in Zagreb are engaged in scientific work relating to wood preservation. The construction and wood industry, which should enhance the chemical industry, also have subs...
R Despot, M Hasan


Wood cement composites using spent CCA treated wood
1999 - IRG/WP 99-50126
The feasibility of using spent or out-of-service CCA treated wood as a component of wood/cement composites was evaluated. Cold pressed wood particle cement boards were made using CCA treated particles from a red pine (Pinus resinosa Ait.) pole removed from service and from untreated red pine wood from a new pole. Boards were manufactured using a range of wood to cement ratios and water to cement r...
Chen Huang, P A Cooper


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 4: Conversion reactions during storage
1974 - IRG/WP 332
Precipitates simulating those produced in wood by preservative fixation reactions were prepared by the reduction of Boliden K 33 and Celcure AP solutions with hydrogen peroxide and hydrazine. The pH changes on aging at 20 and 50°C were studied and related to the chemistry of fixation previously described. Hydrolysis of copper arsenates may render arsenic acid temporarily water soluble pending pre...
S-E Dahlgren


Fixation of chromated wood preservatives through technical drying
1990 - IRG/WP 3623
Twin samples of sawn timber of Pinus sylvestris and Picea sp. were treated with copper-chromate-containing wood preservatives and subsequently kiln resp. air dried. After drying, the distribution of preservative and rate of fixation were determined. Drying of freshly treated wood in a condenser type kiln at temperatures of 60°C and 80°C and in a vacuum type kiln at 55°C with a pressure of about...
R-D Peek, H Klipp


Penetration of oil-borne preservatives in American elm
1975 - IRG/WP 355
Pressure treatment of elm posts and cants by Rueping schedules resulted in erratic penetration. Instead of the expected gradual decrease in retention from surface inward in posts, inner zones frequently contained more preservative than the surface quarter inch. Heartwood was found penetrated when sapwood was not. There were numerous skips in treated zones. The prevalence and possible causes were i...
E A Behr


Regulations of wood preservatives in Finland
1978 - IRG/WP 3124
Toxic wood preservatives are covered by the Poison Act (No. 309/69). The act came into force in May 1969 and was supplemented by the Statute on Poisons (No. 612/69). The act and the statute contain the regulations on the production, commerce and handling of poisons. Already when issued they were complained to contain some defects and obscurities. However, only minor alteration in them have been ma...
T Vihavainen


Evaluation of hydroxamates as wood preservatives
2004 - IRG/WP 04-30330
Fungicidal activity of different hydroxamates was investigated by laboratory malt-agar block tests to evaluate their potential as wood preservatives. Results obtained indicate that benzohydroxamic acids substituted or not on the aromatic nuclei were unable to protect wood blocks against the white rot fungus Coriolus versicolor while 2-hydroxypyridine-N-oxide (2-HPNO) possesses an interesting activ...
P Gérardin, S Dumarçay, E Gelhaye, A Mbamba, V Mussavu


The potential of high pressure pulsation processes to treat white spruce lumber with water-borne preservatives
1988 - IRG/WP 3471
Laboratory work using end sealed 4x8x46 cm³ white spruce samples has been done to explore the suitability of three variants of a 2.1 MPa pulsation process for the impregnation of white spruce with CCA. The results showed that the process improved significantly the penetration of the preservatives and reduced significantly cell collapse, when compared with the results of treatment using a 2.1 MPa ...
J P Hösli, J N R Ruddick


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 17: Report of fifth inspection (4 years) in Italy
1983 - IRG/WP 4103
The wood samples of Alstonia scholaris, Fagus sylvatica, Pinus sylvestris were submerged in the sea at Follonica, Italy, in April 1977. Follonica, latitude 42°55' North and longitude 10°45' East, is situated on the Tyrrhenian coast. The recorded temperature varies from 13°C to 25°C, salinity 37-38% and pH about 8. The inspections were carried out after 6 months (10/1977), 12 ...
A Gambetta, E Orlandi


Information on a project about the conditions of admissibility of wood-protecting agents in connection with environmental protection in Poland
1974 - IRG/WP 57
Wood-protecting agents are compounds acting toxically on fungi and insects. If handled improperly or carelessly, they may exert an action harmful to health and safety of men. This action is concerning: a) workers employed at the production of wood-protecting agents; b) workers employed at the impregnation, or at the transport and handling of impregnated wood; c) inhabitants of buildings with impre...
J Wazny


Soft rot in heartwood of preservative-treated pole stubs of Eucalyptus cypellocarpa L. Johnson
1983 - IRG/WP 1204
Pole stubs of Eucalyptus cypellocarpa L. Johnson, treated in the sapwood with certain waterborne preservatives and exposed for 21 to 23 years in a dry tropical region were severely soft-rotted in the heartwood, as well as the sapwood. They broke with a brash fracture when stress tested (loaded as a cantilever) in the field. The severe soft rot in the heartwood was not detected by the knife test or...
J E Barnacle, G C Johnson, M A Tighe


The effect of stack height on the performance of preservatives used for the prevention of sapstain on seasoning wood
1997 - IRG/WP 97-10192
The performance of three anti-sapstain preservatives was investigated under field conditions in south east England. The preservatives under test were: copper-8-quinolinolate (Mitrol PQ8) trimethylalkylammoniumchloride and sodium hexanoate (Sinesto B) and chlorothalonil (Tuff Brite). The preservatives were tested on Corsican Pine grown in south east England. The field trial was set up to investigat...
J R Williams, D J Dickinson, J F Webber


A novel technique for comparative toxicity studies of potential insecticidal wood preservatives
1983 - IRG/WP 2198
For some years now a device has been under development at the New Zealand Forest Research Institute, the purpose of which is to study the effects of sub-lethal amounts of stomach poisons (but also of fumigants and contact active materials) on the co-ordinative abilities of a cerambycid larva. This insect is Prionoplus reticularis - indigenous to New Zealand its larvae feed in decaying logs and are...
D J Cross


A combined method for drying and preserving wood in a single step process
2000 - IRG/WP 00-40183
Based on a convective dryer, this process allows to dry and treat wood blocks with diffusible preservatives in the same time. A boric acid solution (heated to fix the wet temperature of the system) is pumped and introduced in the flow system through a venturi, where the air coming back from the drying cell also arrives. The role of the venturi is to create a dispersion of boric acid solution micro...
O Colin, C Dupuis, E Mougel, A Zoulalian, M-F Thévenon


Wood preservation in the Netherlands
1985 - IRG/WP 3324
This report gives some information on the production, import and use of timber in the Netherlands and, in more detail, about the country's wood preservation industry. As the country's production of wood that is useful for its manufacturing industries is very limited, the position of wood in the building industry is not too important. Architects think first in terms of bricks, con...
N Burgers, R Cockcroft, D De Jong


Comparative study on the leaching of wood preservatives between natural exposure and accelerating laboratory conditions
1999 - IRG/WP 99-50134
Impregnated specimens with CCA, ACQ, and BAAC were subjected to leaching tests. Specimens of 2x2x1 cm3 in size were used for the laboratory leaching test for 10 days according to JIS K 1571. Specimens of 25x1 x1 cm3 were used for outdoor leaching test for 6 months. Total leaching amounts of boron per cm3 of specimens treated with BAAC were 325 µg in the laboratory test and 206 µg in the outdoor ...
K Yamamoto, S Motegi, A Inai


Evaluation of rapid methods for detecting wood preservatives in waste wood
1994 - IRG/WP 94-50024
For the disposal of wood waste under ecological sound conditions information about its hazardous potential is required. Several analytical methods are available for the detection of most elements in wood preservatives. Industrial process conditions, however, demand methods with very short turn around times. In this research several methods of analysis were judged on their speed and accuracy. A num...
W J Homan, H Militz


Effects of hard water, sea water and humic acid on the release of CCA components from treated wood
2005 - IRG/WP 05-50228
Leaching medium is an important factor affecting release of preservative components from treated wood because physical and chemical characteristics of medium increase or decrease the solubility of fixed preservative components. This study evaluated the leaching properties of copper, chromium and arsenic elements from chromated copper arsenate (CCA)-treated wood specimens subjected to laboratory le...
S N Kartal, W J Hwang, Y Imamura