Environmentally benign wood preservatives based on organic biocide antioxidant combinations: A brief review of laboratory and field exposure results and discussion of a proposed mechanism
2004 - IRG/WP 04-30335
The combination of various organic biocides with commercial antioxidants generally increased the biocides’ efficacy 2-3 fold against wood-destroying fungi in short-term laboratory decay tests, and some positive results have been obtained after 2-4 years of outdoor exposure. The two antioxidants principally examined, propyl gallate and butylated hydroxytoluene, are low cost and, since both are f...
T Schultz, D D Nicholas, W Henry, C Pittman, D Wipf, B Goodell


Comparison of Temporal Changes in Metal Leaching and Aquatic Toxicity from Wood Treated with CCA and Alternative Preservatives
2005 - IRG/WP 05-50236
This study compares the temporal variation of chemical leaching and aquatic toxicity of wood treated with chromated copper arsenate (CCA) and other copper-based wood preservatives (alkaline copper quaternary (ACQ), copper boron azole (CBA), copper citrate (CC) and copper dimethyldithiocarbamate (CDDC)). Treated wood blocks were leached for 21 days and the leachate collected was analyzed for prese...
B Dubey, T G Townsend, G Bitton, H M Solo-Gabriele


Copper based water-borne preservatives: Copper adsorption in relation to performance against soft rot
1987 - IRG/WP 3452
As part of a fundamental study concerned with the performance of copper based water-borne preservatives the adsorption of copper from aqueous solutions by 4 hardwood and 1 softwood species has been studied. Experiments were conducted to determine the influence of solution pH, solution concentration and solution temperature. The results obtained were consistent with an acid form ion-exchange mechan...
P M S Rennie, S M Gray, D J Dickinson


Industrial fixation of chromium based wood preservatives
1990 - IRG/WP 3630
Fixation is an abstract and non-defined process. Nevertheless it is a specified requirement in most impregnation standards. The impregnation industry is facing increased pressure to deliver fixed products and to increase the safety of the handling of impregnated products. Industrial fixation of impregnated wood can be obtained by using different methods. The purpose of the process is to transform ...
T Christensen


Resistance of acrylic paints on wood against growth of the rot fungus Dacrymyces stillatus
1990 - IRG/WP 2345
In the last few years the presence of the rot fungus Dacrymyces stillatus has been repeatedly confirmed in external wood panels, particularly from wood painted with water based paints. A laboratory method for testing of the fungal resistance of paint films on wood has been developed.This method has been used to test the efficacy of the fungicides Parmetol DF 18 and Parmetol HF 25 against attack by...
J Bjurman


Preservatives stains as exterior wood finishes
1977 - IRG/WP 389
For many years wood preservatives and paints have been used as the only treatment for exposed wood surfaces. Because of the inherent color of the preservatives, such as creosote, the wood surface was stained as well as protected from attack by micro-organisms. Paints protect surfaces from weathering, but recently, with an increased interest in maintaining the more natural appearance of exterior wo...
D W French


Future insecticidal treatments for wood products
1980 - IRG/WP 3140
Protective measures involving chemical treatment of wood use only a narrow range of toxic materials which are divisible into two groups, (i) those that are water-soluble, (ii) those that are soluble only in organic solvents. It is generally true to say that, as far as protection against insects is concerned, the former are stomach poisons while the latter are largely (though not exclusively) conta...
D J Cross


Changes of EPR spectra of wood, impregnated with copper based preservatives, during exposure to Antrodia vaillantii
2000 - IRG/WP 00-10355
Spruce wood (Picea abies) samples were impregnated with two different aqueous solutions: copper(II) octanoate with ethanolamine or copper(II) sulfate (cCu = 1,0 x 10-2 mol/l). Impregnated and unimpregnated test pieces were exposed to wood rotting fungus Antrodia vaillantii. Some strains of this fungus are known as copper tolerant. After four weeks of exposure to A. vaillantii, we could not detect ...
M Humar, M Petric, F Pohleven, M Šentjurc


The development of a new boron-based wood preservative
1995 - IRG/WP 95-30085
The paper describes a new boron based wood preservative for the treatment of green timber. The product offers many benefits over conventional boron diffusion treatment including: 1. high viscosity, high concentration formulation; 2. permits dip treatment of a wide range of sawn board and pole sizes at ambient temperatures; 3. permits full cross section diffusion of borates without block stacking a...
P Turner, D Conradie


Technologies for the Management of Wood Waste Containing Metals-Based Preservatives
2005 - IRG/WP 05-50224-16
Disposal of the metals from preservative treated wood can occur through two general strategies: “removal and confinement” or “dilution”. The acceptability of each of these two choices is typically dictated through the disposal regulations of a particular region. A considerable amount of research has been conducted to develop new and innovative “removal and confinement” technologies...
H M Solo-Gabriele, T G Townsend


Copper based wood preservative - A new approach using fixation with resin acids of rosin
2000 - IRG/WP 00-30249
Copper soaps with carboxylic acid groups of resin acids of rosin were shown to be potential long-term wood preservatives. The principle involved is the attachment of copper to the network formed by the inorganic part of the preservative (rosin) through the -COOH groups. The mechanisms of fixation have been studied, and it has been shown that this association could be obtained : (1) by forming the ...
C Roussel, J P Haluk, A Pizzi, M-F Thévenon


Wood protecting chemicals for the 21st century
1993 - IRG/WP 93-30018
After assessing the past research with protection chemicals, this paper proposes future avenues for research and development in wood protection. Three scenarios are put forward for consideration. First, more is not better and future systems will emphasize combination formulations which enhance properties while providing biological efficacy. Second, current systems, especially those based on copper...
H M Barnes


Leaching Characteristics of Alder Wood Treated with Copper Based Wood Preservatives
2005 - IRG/WP 05-50225
In this study, it was designed for determining leaching characteristics of CCA and alternatives wood preservatives. Alder wood blocks were treated with CCA (1 % and 2 %), ACQ-1900 (2 % and 3 %), ACQ-2200 (1 % and 2 %), Tanalith E 3491 (2 % and 2.8 %), Wolmanit CX-8 (% 1 and 2 %). Leaching studies were conducted according to AWPA E11-97. Copper analyses of leachate were determined Atomic absorption...
A Temiz, Ü C Yildiz, E D Gezer, S Yildiz, E Dizman


The future for chromium in wood preservation
1985 - IRG/WP 3332
Most water-borne preservatives contain CrVI compounds, originally to reduce corrosion although now also to improve toxicant fixation. Chromium contributes to preservation and this is recognised in, for example, New Zealand and USA where chromium contents are included in calculations of overall preservative activity of CCA formulations, but chromium may also have anti-stain and joinery (millwork) p...
B A Richardson, T R G Cox


Leaching of components from CCF treated timber in ground contact
1998 - IRG/WP 98-50108
In order to investigate the depletion of different CCF-salts during service small stakes (10*10*450mm³) were treated with five water-borne wood preservatives and after fixation brought into ground contact for several years. After failing some of the broken down stakes were used to determine the remaining concentration of relevant ions and their distribution in different segments of the stakes. A...
E Melcher


Fungal degradation of wood treated with metal-based preservatives. Part 1: Fungal tolerance
1996 - IRG/WP 96-10163
In recent years, concerns have arisen about the leaching of heavy metals from wood treated with chromated copper arsenate (CCA), particularly because of the large amount of CCA treated wood that will be discarded in the coming years. The long term objectives of this work are to determine the fate of copper, chromium and arsenic with the aging and potential decay of CCA-treated wood, and to develop...
B Illman, T L Highley


The Use of Modulus of Elasticity and Modulus of Rupture to Assess Wood Decay in Laboratory Soil-Bed Test
2006 - IRG/WP 06-20338
The efficacy of wood preservatives were determined in a soil-bed test. Samples of alder wood sapwood (Alnus glutinosa subsp. barbata) (5x10x100 mm) were treated with Solutions of CCA (1 % and 2 %), ACQ-1900 (2 % and 3 %), ACQ-2200 (1 % and 2 %), Tanalith E 3491 (2 % and 2.8 %), Wolmanit CX-8 (% 1 and 2 %). Modulus of Elasticity, modulus of rupture, mass loss and decay rate according to AWPA E7 wer...
A Temiz, Ü C Yildiz


Preliminary screening of a boron based wood preservative for biological efficacy (fungicidal) in treated timber
2006 - IRG/WP 06-30396
The resistance of Pinus radiata D.Don sapwood blocks, treated with a boron based preservative, to attack by five wood destroying fungi (Fomitopsis lilacino-gilva, Coniophora olivacea, Gloeophyllum abietinum (boron resistant), Serpula lacrymans and Perenniporia tephropora) was investigated. A phenyl pyrazole termiticide (fipronil) was also incorporated into the formulation to examine if its presen...
S R Przewloka, J A Hann, P Vinden


Addition of boron compounds and octanoic acid for improvement of biocidal properties and copper fixation at copper-ethanolamine based wood preservatives
2006 - IRG/WP 06-30408
Copper-ethanolamine based wood preservatives became important active substance (formulation) for wood protection, novelty. As copper itself can not ensure sufficient protection against wood destroying organisms and fixation in wood we combine it with other biocides like ethanolamine, boron and octanoic acid. This investigates were performance on spruce wood impregnated with different combination o...
F Pohleven, M Humar


Some textile auxiliaries as wood protective agents
2007 - IRG/WP 07-30417
This study evaluated some textile auxiliaries applicable for wood protection. Commercial alkoxysilane quarternary ammonium formulation and fluorocarbon based water-oil repellent were tested for their ability to provide hydrophobicity and antifungal effect to solid wood samples. Scots pine (Pinus sylvestris L.) sapwood samples were impregnated with 25, 50 and 100 % concentrations of the above menti...
E Dizman, A Temiz, N Terziev, Ü C Yildiz


Amine Oxides for Use in Wood Protection: II: Water Repellent Agents for Wood
2007 - IRG/WP 07-30426
Wood treated with cetyl and stearyl amine oxides was evaluated to determine its long term water repellency. Comparative water uptake data, generated during two years of outdoor exposure, illustrated that Lonza’s products, Barlox® 18S (N-octadecyl-N, N-dimethylamine oxide) and Barlox® 16S (N-hexadecyl-N, N-dimethylamine oxide), were effective water repellent agents, imparting lasting water res...
Xiao Jiang, L Walker


Synthesis of boric acid ammonium oleate salt for wood preservation: Leachability and termite resistance test
2007 - IRG/WP 07-30435
A new chemical compound coupling boric acid and oleic acid through a joint of ammonium salt has been produced and its synthesis followed and validated by Fourier Transformed Infra Red (FTIR). This compound named ammonium borate oleate (BAO) combining biocidal properties of boron and water repellence of fatty acids has then been studied as a wood preservative. Synthesis of BAO involved different...
F Lyon, A Pizzi, Y Imamura, M F Thevenon, S N Kartal, J Gril


Evaluation of Water Repellency of Treated Wood Using Several Alternative Methods
2009 - IRG/WP 09-20419
In this study, the results of water repellency testing using a digital swellometer method for water-borne organic-preservative systems with water repellent additives are reported. The findings suggest that the traditional method of using matched untreated controls as a reference developed from historic solvent-based treatments for determination anti-swelling efficacy (ASE) may underestimate the a...
L Jin, A F Preston


A theoretical-industrial correlation and perspective on copper-based wood preservatives - a review of thermodynamic and kinetic aspects on copper-wood fixation mechanism
2009 - IRG/WP 09-30499
Copper was and it will continue to remain one of the key active component in wood protection industry. Over the past decades, a significant effort from R&D teams in industry, academia and research institutes was directed toward understanding the copper-wood fixation mechanism, optimising the copper retentions in the wood and reduce leaching in order to maximized performance, prolong the lifetime o...
R Craciun, M Maier, J Habicht


Methods for Studying Penetration Depth of Wood Protection Products
2010 - IRG/WP 10-20432
EN 152 is an accepted standard in Europe for measuring how deep a wood protection product penetrates into the surface of treated pine wood. The method has provided consumers with a wide assortment of products that meet the specifications outlined in the standard. Because the test takes 8 or more months to carry out, artificial ageing procedures have evolved in order to standardize and speed up the...
K Hansen, L Sites, D D Nicholas


Previous Page | Next Page