Moisture sorption behaviour of poplar and thermally modified poplar using dynamic vapour sorption (DVS)
2022 - IRG/WP 22-40947
The moisture sorption behaviour of wood has a critical impact on service life. In Europe, softwood is mostly used to manufacture engineered wood products such as cross-laminated timber (CLT) or glue-laminated timber (GLT or glulam). Yet fast-growing and widespread tree species such as hybrid poplar with or without modification, have potential to meet the increasing demand. This study shows the moi...
X Jiang, J Van den Bulcke, L De Boever, M Minsart, A Mignon, J Van Acker


Phenol formaldehyde modification and termite resistance under laboratory testing
2022 - IRG/WP 22-40952
The development of phenol formaldehyde (PF) resins as a means of impregnating solid wood is one that has been explored for several decades, both in terms of conventional impregnation processing (Impreg) or compressional impregnation (Compreg). However, it is only recently with advances in processing conditions that the method truly affords a means of achieving conventional modification for solid t...
L Nunes, A Pitman, M Duarte, B Stefanowski, D Jones


Evaluation of Decay Resistance for the Larch Wood Heat-treated with Superheated Steam
2022 - IRG/WP 22-40956
Heat-treatment of wood is a process that involves applying heat ranging 160–260°C to improve its physico-mechanical properties and resistance against wood rot fungi. The level of the changes in the wood properties by heat-treatment differs depending on the temperature and duration of heat-treatment, as well as the types of heat transfer media used for heat-treatment. The heat-treatment on wood ...
Y Park, S-M Yoon, H Kim, W-J Hwang


A novel method for assessing radial variation in termite resistance of timber
2023 - IRG/WP 23-11005
Australia has many timbers whose heartwood is highly resistant to fungal and termite attack; however, changing public policies have resulted in restricted access to many native forests where these species are found. Plantations of these same species are expected to replace these resources, but there are questions concerning whether timber from these trees will have the same resistance as the nati...
S Kleinschmidt, R McGavin


Biological durability and wood-water interactions of sorbitol and citric acid modified wood – Effects on the expected service life
2023 - IRG/WP 23-40960
A high level of research activities on sorbitol and citric acid (SorCA) modified wood has been recognized in Europe over the last few years. As this treatment is close to entering an industrial-scale production, it is of interest to investigate how such treated wood performs upon long-term outdoor exposure. Hence, in this study Scots pine (Pinus sylvestris L.) sapwood was modified with aqueous sol...
K Kurkowiak, L Emmerich, H Militz


Resistance of phenol formaldehyde impregnated beech (Fagus sylvativa L.) LVL against biodegradation in soil contact
2023 - IRG/WP 23-40965
Alternatives to preservative impregnation are emphasized in Germany and other European countries. Even though these treatments significantly improve wood's resistance to decay, they often do not have a beneficial impact on the dimensional stability. One alternative product, which may be used in ground contact for items like poles and railway sleepers, could be beech (Fagus sylvatica L.) laminated ...
M Slabohm, C Brischke, S Bicke, H Militz


New wood-modification process based on grafted urethane groups: Durability of carbamamylated Scots pine (Pinus sylvestris L.) wood
2023 - IRG/WP 23-40974
Substituting commonly used toxic preservatives with wood modification treatments can make the wood material less prone to water and moisture uptake. This approach favours a more sustainable protection of wood against biodegradation. In this study, Scots pine sapwood was full-cell impregnated with an aqueous solution of urea (30%), dried at 40°C for 24h, and subsequently heat-treated at 150°C for...
C-F Lin, O Myronycheva, O Karlsson, D Jones, D Sandberg


Short-term absorption of water and coatings on thermally modified blue-stained spruce wood
2023 - IRG/WP 23-40984
The importance of wood has been increasing in the last decades. Among conifers, predominantly spruce (Picea abies) wood is often used in building constructions in Europe. Namely for construction and facades of buildings, decking and fences. Due to the increased public concerns about biocides, alternative techniques for protection, such as thermal modification and protection by construction, are ga...
R Hasanagic, M Bahmani, M Humar, L Fathi, L Cai


Evaluation of the effectiveness of soaking of high-temperature plywood in low-temperature oil-based wood
2023 - IRG/WP 23-40991
We conducted a preliminary investigation to determine if soaking high-temperature plywood in a low-temperature preservative solution could achieve deeper penetration of the preservative, even in plywood made with refractory wood species such as Japanese larch. Specimens cut from commercial plywood (Japanese larch) were stored at various temperatures before being soaked in the preservative solution...
T Miyauchi, S Isaji, H Shibui, N Furuta, J Miyazaki, H Matusnaga


Characterization of cell wall morphology and water-soluble extractives in Japanese larch decayed by white-pocket-rot fungi
2024 - IRG/WP 24-11034
Porodaedalea chrysoloma (Fr.) Fiasson & Niemelä is a basidiomycete that can cause white-rot decay in Japanese larch (Larix kaempferi) heartwood. P. chrysoloma is a white-rot fungus with a unique pattern that causes white-pocket-rot in the xylem of Japanese larch. However, the mechanism by which P. chrysoloma yields the pattern of white-pocket-rot in Japanese larch heartwood remains unclear. Thus,...
Y Mori, H Arai, T Ito, H Hashitani, K Yamashita, Y Ota, M Kiguchi


Do naturally sequestered biocidal metals contribute to the marine borer resistance of turpentine?
2024 - IRG/WP 24-11036
Turpentine wood is renowned for its resistance to attack by molluscan marine borers. This resistance is thought to be due to its high silica content, and possibly the presence of other, as yet unknown, compounds. Silica in turpentine wood is present as particles in rays, but in many plant species silica also occurs in cell walls. We hypothesized that Si is present in cell walls of turpentine, but ...
P D Evans, H Matsunaga, D Feng, M Turner, C Kewish


Enhancing UV resistance and decay resistance of wood by nanoparticle dispersed linseed oil nanoemulsion
2024 - IRG/WP 24-20706
Enhancing increasing demand for eco-friendly and cost-effective wood coatings and preservatives has led to the development of water-borne formulations and use of non-toxic and natural materials such as vegetable oils and waxes. The aim of this study was to improve the UV resistance and decay resistance of wood by nanomaterial dispersed linseed oil emulsions. Highly stable nanoemulsions of linseed ...
R Bansal, R Kumar, K K Pandey


Influence of the substitution of phenol with lignin cleavage products in phenol-formaldehyde impregnation resins for wood modification on the fungal decay resistance and impregnation depth
2024 - IRG/WP 24-30805
The impregnation modification of wood with phenol-formaldehyde (PF) resins increases the woods dimensional stability and resistance against fungal decay. However, to decrease the usage of non-renewable resources, the substitution of phenol has been a topic of scientific interest. Lignin is a currently underutilized resource with a chemical structure that contains phenolic units. For adhesive appli...
J Karthäuser, L Tarentino, A Treu, H Militz, G Alfredsen


A novel treatment for increasing UV stabuility of wood based on citric acid and urea
2024 - IRG/WP 24-30811
Wood, a fundamental material in the Built Environment, faces challenges related to durability and weathering, notably UV degradation leading to colour changes. This study explored a novel treatment method utilising citric acid and urea to enhance the UV stability of wood. The reaction between these compounds forms fluorescent species and insoluble nanoparticles upon thermal treatment. Two treatmen...
S Jué, A Scharf, C-F Lin, R Moutou Pitti, D Sandberg, D Jones


International joint field trial on the moisture performance of wood – Set up and first results
2024 - IRG/WP 24-40996
Wood durability to decay stems from its inherent resistance to fungi resistance to fungi. In this regard, wood's ability to withstand moisture uptake plays an important role as the lower threshold for wood decay is a moisture content of 25%. However, the aspect of moisture resistance is not yet sufficiently emphasized as a durability factor, both in the assessment of durability as a material prope...
C Brischke, et al. (33 co-authors)


Evaluation of the water exclusion ability and inherent bioactivity of heartwood against decay in Japanese and European wood species via above-ground exposure and water absorption tests
2024 - IRG/WP 24-40998
The natural durability of wood has been thought to mainly depend on bioactive extractives and the water exclusion ability. To clarify the contribution of each factor to wood durability, above-ground exposure tests were conducted on Japanese and European wood species. A double-layer test was carried out using heartwood specimens of four wood species, i.e., Japanese cedar, Japanese cypress, Scots pi...
T Osawa, R Noda, K Yamamoto


Outdoor termite resistance performance of zinc borate (Borogard® ZB) treated parallel strand lumber (PSL) – 15 years field test results
2024 - IRG/WP 24-40999
This report discloses the outdoor termite resistance performance of PSL samples treated with zinc borate at a dosage of 0.85% BAE and 1.72% BAE in Wuxi, China. The outdoor field trial lasted for 15 years and observations were made after 6 months, 3 years, 5 years 1 month, 6 years 6 months and 15 years. The retaining rates of B2O3 and ZnO in the final samples were also tested, and the hypothesis wa...
S Shi, E Laval, K Lung, F Ascherl, R Williams, W Li, X Li


Durability of Malaysian plybamboo to mold
2024 - IRG/WP 24-41014
Durability of 3-layer plybamboo fabricated from two Malaysian bamboo species, Gigantochloa levis (beting) and Gigantochloa scortechinii (semantan) using three different adhesives - urea formaldehyde (UF), melamine urea formaldehyde (MUF) and phenol resorcinal formaldehyde (PRF) was evaluated in this study. Samples were exposed to the mold, Aspergillus brasiliensis for 4-week following the ASTM D44...
S Lipeh, A Mustapha, A S Yusoh, M K A Uyup


Analysis and performance of spruce alternative species and discarded wood for windows production
2024 - IRG/WP 24-50386
Climate change is having a significant impact on European forestry, particularly on the softwood species used for window frames. This study investigates potential replacement tree species for spruce (Picea abies), the predominant material for window frames. We evaluate Douglas fir (Pseudotsuga menziesii), Scots pine (Pinus sylvestris), thermally modified poplar (Populus nigra) and discarded silver...
B Lesar, J Levanič, M Humar, A Treu


Determining the minimum water vapor permeability of exterior wood coatings by means of hygrothermal and decay models
2024 - IRG/WP 24-20717
The objective of this study was to determine the minimum water vapor permeability of exterior wood coatings for log homes using hygrothermal and decay modeling. The approach is based on a worst-case scenario assumption, namely a moisture trap at a given wood moisture content in a coated wall log. The minimum limit of vapor permeability of the coating system was determined by simulating the time re...
U Hundhausen, S Ullah, D Kraniotis


The durability and mechanical properties of 40 years old Black locust poles
2024 - IRG/WP 24-11042
This study investigates the durability and mechanical properties of 40-year-old black locust (Robinia pseudoacacia) poles harvested from a vineyard in Slovenia. Wood from these poles was compared to recently harvested black locust wood to determine possible reuse options. Visual inspection, hyperspectral imaging, and laboratory tests were conducted to assess decay, density, mechanical properties, ...
M Humar, J Malik, J Levanic, D Krzisnik, E Kerzic, B Lesar