IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 846 documents. Displaying 25 entries per page.


Termite resistance of timber envelope treated with imidacloprid then modified by typical building site operations
2011 - IRG/WP 11-30570
Imidacloprid is a new envelope insecticide approved by Australian regulatory authorities for framing timber. It is a non repellent insecticide. Results are reported for timber envelope treated with imidacloprid and altered post treatment with typical building site operations to expose untreated surfaces. These modifications included, cutting, notching and drilling. Pinus radiata timber samples w...
K Day, A Siraa, P Lobb


Effectiveness of Water Based Bentonite-Borate Slurry for In-situ Remedial Protection of Historic Wooden Piles: The Eurobor Protocol, Part 2
2011 - IRG/WP 11-30574
The study of the biocide product Eurobor®, water mixture of boric acid, borax and sodium bentonite, aimed to verify previous findings regarding borates penetration from a clay-water mixture of foundation timber. The product was applied on samples from 100 year old timber foundation from the city of Göteborg. Although in ground for this long the timber was in acceptable god condition due to groun...
M. Theorin, K. Fimmerstad, K-M. Bandh


The resistance to Basidiomycetes fungi of chipboard 35 years after their industrial preservation with wood preservative on fluoroborate basis
2011 - IRG/WP 11-40546
The research on wood-based panels’ (WBP) behaviour towards fungi impact demonstrated rather low resistance of wood-based materials to wood rotting fungi. However, these materials are used in construction under conditions favourable to fungi growth. In such conditions WBP treated with wood preservatives should be used. Preservation durability is of great importance in such cases. The resistance o...
A Fojutowski, A Kropacz


Adsorption boundary curve influenced by step interval of relative humidity investigated by Dynamic Vapour Sorption equipment
2011 - IRG/WP 11-40547
The adsorption of water vapour from dry conditions by Norway spruce sapwood has been investigated using Dynamic Vapour Sorption (DVS) instrumentation. This equipment allows a fast and easy data acquisition as well as enables detailed studies of sorption properties using very small sample masses. In this study, particular focus was paid to the effect of step size on the sorption isotherms. Furtherm...
E Tang Engelund, M Klamer, T Mark Venås


Decay resistance of a commercial pistachio twig-plastic composite
2011 - IRG/WP 11-40553
In this research, the decay resistance of commercial extruded pistachio twig flour-plastic composite was investigated against the white-rot fungi Trametes versicolor and the brown-rot fungus Coniophora puteana. The composite specimens containing 60% pistachio twig flour were exposed to a decay test according to modified ASTM standard for 3 months. The results showed that the composite could be d...
M R M Farahani, M Safarzadeh


Evaluation of an optimized industrial process aiming to improve the natural durability and mechanical behavior of bamboo for outdoor use
2011 - IRG/WP 11-40554
Mao Bamboo (Phyllostachys pubescens) is characterized by high contents of sugar and starch and by high hygroscopicity, which makes it susceptible to biodegradation, and specifically to fungal decay. Still, many bamboo based products regularly enter the European wood construction market, competing with traditional solid wood products used for outdoor decking and cladding. The performance of a heat ...
F Simon, M Kutnik, I Le Bayon, G Moisset, V Gatimel


Effects of Heat-Treatment in Hot Water and Steam Mediums on Gas Permeability of Beech Wood
2011 - IRG/WP 11-40557
Heat-treatment, as a major method of wood modification, improving dimensional stability, and natural durability, has been studied greatly from different aspects. The effect of heat-treatment on gas permeability, as an important physical property of wood, in two different mediums of hot water and steam, as well as in two buffers of 7 and 8, is the main topic of the present study. Hydrothermal treat...
H Reza Taghiyari, A Talaei, A Karimi


Effect of Nano-silver Treatment on Densified Poplar Wood Properties. Part Two: Spring Back, Compression set, Impact Load Resistance and Hardness
2011 - IRG/WP 11-40568
This paper is the second part of the study of applying nano-silver treatment before densification of poplar wood (Popolus alba). The specimens were prepared in four groups of: 1) nano-silver impregnated 2) water impregnated 3) dried with no impregnation and 4) the control specimens. The impregnation process was done by empty cell process. Then, the groups of 1 to 3 were compressed in a hot press a...
G Rassam, H Reza Taghiyari, B Jamnani, M Ali Khajeh


Eastern redcedar included sapwood: Resistance to mold and termites under laboratory conditions
2012 - IRG/WP 12-10765
The heartwood of eastern redcedar (Juniperus virginiana) frequently contains areas of light-colored wood. This “included sapwood” is considered to be a defect by some manufacturers. In this study, sapwood, included sapwood and heartwood samples from five eastern redcedar trees were exposed to mold fungi or to subterranean termites in a no-choice feeding test. Extractives content was also measu...
C Köse, A M Taylor


Laboratory and Field evaluation on Natural Resistance and Feeding Preference of Different Wood Species to Subterranean Termites (Isoptera: Rhinotermitidae, Termitidae) in Pakistan
2012 - IRG/WP 12-10769
The resistance of twenty four different woods to attack and damage by subterranean termite species Heterotermes indicola (Wasmann) and Coptotermes heimi (Wasmann) was evaluated by choice and no choic in laboratory and field trials. Mean wood mass loss was calculated for both laboratory and field trials results using Analysis of Variance (ANOVA). Mean percentage termite mortality was calculated fo...
S A Malik; F Manzoor, B M Ahmed (Shiday)


Influence of soil moisture, Sarawak soil types and decay types on decay susceptibility of rubberwood and kelempayan
2012 - IRG/WP 12-10780
Wood and soils are important natural resources of the land, the former widely used as structural supports in contact with the latter. Many low durability wood species exposed to soil contact has reportedly high incidence of decay failures in poorly treated and untreated materials depending on soil types, properties and soil microbial virulence. This paper probes the relationship of the main soil t...
A H.H. Wong, P K.F. Chong, J Sabang


Coconut lumber for wood decks (Cocos nucifera L.): decay resistance against Basidiomycetes fungi
2012 - IRG/WP 12-10784
Since a couple of years, manufactured products of coconut wood for outdoor uses like wood decks have been proposed on the European market. These are presented as an alternative for traditional tropical timbers. In the past, coconut wood was neglected and burned for sanitary reasons and lack of interest at industrial scale. Plantation coconut trees at end of production of copra constitute a renewab...
B Jourez, C Verheyen, J Van Acker


Durability of timber products – Part 2: Proposal for an IRGWP - Durability Database
2012 - IRG/WP 12-20497
A proposal for a web-based platform for scientific exchange of test data in the field of wood durability and wood protection has been made. The overall aim of the durability data base is to improve the usability of existing test data and to create an added value for durability research and service life prediction. The database allows for test results from standardized and non-standardized laborat...
C Brischke, L Meyer, G Alfredsen, M Humar, L Francis


Durability of timber products –Part 1: Inventory and evaluation of above ground data
2012 - IRG/WP12-20498
The material-inherent resistance of wood is one of the most important qualities influencing the durability of timber. Hence, it has also a major effect on the service life to be expected from a timber construction. In addition, design details and the respective climatic conditions determine durability and make it impossible to treat wood durability as an absolute value. Moreover, the reference mag...
C Brischke, L Meyer, G Alfredsen, M Humar, L Francis, P O Flæte, P Larsson Brelid


Performance superiority of CCA-C treated wooden jetty poles and piles used for 30 years in Bangladesh against marine borers
2012 - IRG/WP 12-30582
Observational study along with previous investigation and records revealed that chromated copper arsenate type C (CCA-C) impregnated southern pine poles and piles of jetty constructed in most vulnerable brackish water in Bangladesh are stable and resistant to attack of all types of marine borers after 30 years of use. It is evident from the service records of other construction materials that CCA-...
A K Lahiry


Mould resistance of bamboo timber treated with tebuconazole-loaded micells
2012 - IRG/WP 12-30586
In this paper both anti-mould test through inhibition zone and mould resistance test on bamboo samples were carried out evaluate mould resistant effect of tebuconazole (TBA) loaded micells. Results showed that TBA loaded micells prepared with a ratio of TBA to PEG113-b-PCL28 50:25 had the best mould resistance, followed by micells prepared with a ratio of TBA to PEG113-b-PCL28 50:50. PEG113-b-PCL2...
Sun Fangli, Chen Anliang, Bao Binfu, Zhou Yueying, Zhang Shaoyong, Zhang Xu


Tannin resin-boron associations: Leaching and biological resistance
2012 - IRG/WP 12-30587
The easy leaching of boron in wood preservation formulations has allowed to use this fungicide only for short term applications. The recently discovered adduct with flavonoids allows boron to resist longer periods of time within wood and consequently extend its life. Two different leaching treatments were compared and the fungal and termite decay was examined. The biological tests have shown extre...
G Tondi, S Wieland, N Lemenager, A Petutschnigg, A Pizzi, M-F Thevenon


Mold Control for Treated Lumber in Block-Stack Storage Conditions
2012 - IRG/WP 12-30588
The mold development and control for freshly treated and block-stacked wood have been evaluated using a green house mold testing method. The results for the mold resistance of several commonly used water boron preservative treatment systems, such as ACQ, Copper Azole, and borates with and without inclusion of mold inhibitors are presented. The data suggest that the different preservative treatme...
L Jin, P Walcheski, A Preston


Termite resistance of copper-based preservative supplemented aspen strandboards
2012 - IRG/WP 12-30594
Termite resistance of aspen strandboards treated with various copper-based preservative systems was evaluated in field exposure tests. Five copper-based chemicals or zinc borate were blended into aspen furnish at three retention levels prior to pressing. Tebuconazole or 4,5-dichloro-2-N-octyl-4-isothiazolin-3-one (DCOI) were added as co-biocides to selected copper-based treatments. Sections from...
J J Morrell, C Vidrine, A Preston, L Jin


Supercritical impregnation of wood with siloxane
2012 - IRG/WP 12-30595
This paper describes the effect of supercritical impregnation with siloxane on the water repellency of Scots pine (Pinus sylvestris) sapwood samples. Samples were impregnated with a low amount of siloxane dissolved in supercritical carbon dioxide using isopropanol as a co-solvent. Siloxane retention (i.e. weight percent gain (WPG)) of the treated samples was 1.3 % (w/w) as found by mass balance. T...
A Kjellow, F Imsgard, J Fernandes, O Henriksen, E Klaassen, R Wagner, J Delis


Effect of preservative treatment on dimensional stability of plywood made of treated simul (Bombax ceiba) veneer
2012 - IRG/WP 12-40575
The dimensional stability such as thickness swelling and water absorption of plywood made of treated simul (Bombax ceiba) veneers were investigated after 2 hours and 24 hours soaking under water. The veneers were treated with hot water and cold water solution of borax-boric acid (1:1), neem leaves and mahogany seeds of different concentration (1:10, 1:20, and 1:40) at different treatment duration....
K Akhter, M Mahabubur Rahaman, A Ara


Effects of Nano-Zycosil on Liquid and Gas Permeability of MDF
2012 - IRG/WP 12-40578
Effects were studied of zycosil nanoparticles, with size range from 30 to 90 nm, on liquid and gas permeability of medium density fiberboard. 100 g of nanozycosil was added to each kg of dry fibers. Density was kept constant at 0.67 g/cm3. The obtained results indicated that addition of zycosil to the mat resulted in a significant increase in gas permeability due to the lower fiber-content in the ...
H Reza Taghiyari, K Heidarhaee, P Noori, A Karimi


The effect of press time on springback and water absorption of acetylated particleboard
2012 - IRG/WP 12-40579
In this study the effect of press time on springback, thickness swelling and water absorption was investigated. After 24 hours soaking in acetic anhydride, in order to achieving WPG 17%, acetylated particles were heated in an oven at 120 0C for 360 minutes. Acetylated and nonacetylated (control) particleboards were produced with 10% melamine urea formaldehyde (based on the oven-dry weight of part...
F Bavaneghi, M Ghorbani, A Kargarfard


Water uptake of wood surfaces with and without coating: influence of weathering
2012 - IRG/WP 12-40580
The objective of this study was to compare liquid water absorption of wood surfaces with and without coating, before and after artificial weathering. Samples of spruce, oak and sapelli were exposed to the EN 927-6 cycle for 1500 and 1850 hours and to the weathering produced by the Garner wheel for 1000 hours. Two highly pigmented coatings (solventborne and waterborne) and two semi-transparent stai...
L Podgorski, S Collignan, J D Lanvin


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and Russian imported spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


Previous Page | Next Page