Relative merits of laboratory and field tests for assessing wood decay resistance
1993 - IRG/WP 93-20009
Laboratory and field trials have long been employed for assessing natural durability of a variety of wood species, but there is a continuing debate concerning the relative merits of approach. While laboratory tests provide carefully controlled conditions for decay, they are often criticized for being too artificial to produce meaningful results. Conversely, field trials often vary widely between t...
T C Scheffer, J J Morrell


Resistance of acetylated wood to biological degradation. Evaluation of field test
1997 - IRG/WP 97-30139
Acetylated wood samples were tested in ground contact (stake test) at two test fields, one in Simlångsdalen, Sweden, and one in Viikki, Finland, according to European standard EN 252. The test samples were inspected annually and their condition was compared with that of untreated controls and of samples treated with two reference CCA preservatives. The use of untreated controls and preservative t...
P Larsson Brelid, R Simonson, Ö Bergman


Comparative field performance of CCA and CCA-water repellent treated Southern pine lumber
1995 - IRG/WP 95-30089
This paper describes the field performance of end-matched southern pine boards treated with either CCA type C or CCA type C containing an emulsion water repellent (WR) additive. Boards were either kiln or air-dried after treatment, constructed into decks, and exposed for over 3 years at Harrisburg, NC. During this exposure, matched boards were monitored for internal moisture content, cupping at mi...
A R Zahora


Resistance of six timber species, treated with CCA and CCB, against marine borer attack in Goa waters (India)
1991 - IRG/WP 4166
Panels of Lagerstroemia speciosa, Toona ciliata, Olea dioica, Pinus insignis, Acrocarpus fraxinifolius and Borassus flabellifer, pressure-treated with a 6.6% solution of Copper-Chrome-Arsenic (CCA) and 6% solution of Copper-Chrome-Boric (CCB), were exposed along with untreated controls, in triplicate, in Goa waters to, assess their resistance to damage by marine borers. The control panels were all...
L N Santhakumaran, R V Krishnan


Detection of methanogenic bacteria in mining timber
1988 - IRG/WP 1352
Methane explosions in gold mines have been attributed to spontaneous ignition of methane/air mixtures. Biogenesis of methane in the heartwood of diseased trees has been shown, but never in timber in service. Studies were therefore undertaken to establish whether methanogens were present in wooden pit props. Core samples were removed by Pressler increment borer from props in disused areas 2,600 m d...
L D Abraham, K Westlake, R I Mackie, J F Putterill, A A W Baecker.


Interactions between water-borne preservatives and emulsion additives that influence the water repellency of wood
1991 - IRG/WP 2374
Incorporation of non-polar additives into water-borne treatments through of emulsion technology can greatly improve the physical characteristics of wood in service. Of specific interest with these emulsions is their effectiveness in reducing the rate of wood swelling. We have observed that the presence or absence of preservatives can often significantly influence the resultant effectiveness of the...
A R Zahora


Occurrence of wood-boring pholads in Kochi harbour waters (south-west coast of India)
1992 - IRG/WP 92-4175
The paper reports the occurrence of four species of wood-boring pholads (Pholadidae: Martesiinae), namely Martesia (Martesia) striata (Linnaeus), Martesia (Martesia) fragilis Verrill and Bush. Martesia (Particoma) nairi Turner and Santhakumaran and Lignopholas fluminalis (Blanford), in the Kochi back-waters, south-west coast of India. Of these Martesia nairi and Lignopholas fluminalis are now reco...
L N Santhakumaran, M V Rao


Differences in pH, electrical resistance, cation composition and NIR spectra of red spruce wood during early stages of brown rot degradation
2002 - IRG/WP 02-10449
Red spruce sapwood was exposed to degradation by the brown rot fungi Coniophora puteana, Postia placenta, Gloeophyllum trabeum and Serpula lacrymans for 0, 1, 2 or 3 weeks using a modified soil block assay design. Average weight losses over time ranged from 0-8.9% during this time period. Detectable changes in pH, electrical resistance and cation compostion were observed in the wood as early as 1 ...
J Jellison, S Kelley, B Goodell, D Hui, A Ostrofsky


Influences of the hydro-thermal treatment on physical properties of beech wood (Fagus orientalis)
2005 - IRG/WP 05-40303
Influences of the hydro-thermal treatment on physical properties of beech wood were studied. Wood specimens (2×2×2cm) were treated in two steps. At first step, samples were treated at 160,180 & 200ºC for 4, 5 & 6 hours. At second step, treated samples were cured based on their first step treatment temperatures (160,180 & 200ºC) for 16 hours. The treated samples were soaked in water...
B Mohebby, I Sanaei


Tebuconazole - A new triazole fungicide for wood preservation
1990 - IRG/WP 3629
The main cause of economic damage to timber and millwork worldwide are Basidiomycetes (brown and white rot). After testing a wide range of triazole derivatives for their effectiveness against decay fungi, Tebuconazole, a triazole compound, was selected. The physico-chemical, toxicological and ecotoxicological data of this substance are described. Tebuconazole is unleachable, light-stable, heat-sta...
R Gründlinger, O Exner


Some aspects of testing water repellents
1998 - IRG/WP 98-40113
Several test methods are used to determine the efficiency of water repellent treatments on wood. The most common are: contact angle measurement, swelling rate of samples immersed under water and, the increase in mass of wood samples with time or after a fixed period of time either fully immersed under, or partially immersed in or floating on water. In this paper, some fundamental aspects of the l...
D Lukowsky, M Farnow, T Rypstra


Movement of water through quaternary ammonium treated wood
1987 - IRG/WP 3440
Radiata pine sapwood stakes were treated with didodecyl methyl 1, 3 dichloropropenyl ammonium chloride and distearyl dimethyl ammonium chloride. Various ratios of these two chemicals were, tested to determine the extent of water movement through the treated wood. Measurements were taken of the amount of water moved through the wood, degree of wetting of various sectors of the stakes, and the distr...
P J Hayward, J Duff


The high decay resistance in the sapwood of the naturally durable Malaysian hardwood Belian (Eusideroxylon zwageri)
2001 - IRG/WP 01-10410
It has long been assumed that the observed natural durability of the heartwood in certain timbers is perhaps associated with a relatively lower decay susceptibility also of the sapwood of these species. While the heartwood of Belian is reputedly highly decay resistant among the tropical hardwoods of Southeast Asia, laboratory decay tests reported in this paper have also confirmed the high decay re...
A A H Wong, A P Singh


Protection of buildings, other structures and materials in ground contact from attack by subterranean termites with a physical barrier - a fine mesh of high grade stainless stee
1993 - IRG/WP 93-10014
A new type of physical barrier for the prevention of attack by subterranean termites on buildings, other structures and materials in ground contact - a fine mesh of highalloy (originally 304, now 316) stainless steel - has recently been developed and patented worldwide by industry in Australia. The termite resistance of the material was assessed by CSIRO in laboratory and field trials. In the labo...
M Lenz, S Runko


Ponding of radiata pine (Pinus radiata) - 2. The effect of ponding on coating penetration into wood
1998 - IRG/WP 98-10249
Radiata pine (Pinus radiata) wood panels which had been ponded for periods ranging from 2 to 12 weeks, dried and subsequently coated with a primer and examined by light microscopy after staining sections with Sudan IV to enhance the contrast of the primer material. A correlation between the extent of ponding and the extent of coating penetration into wood was observed. The coating penetration var...
A P Singh, S S Gallagher, U Schmitt, B S Dawson, Yoon Soo Kim


Laboratory Evaluation of the Formosan Subterranean Termite Resistance of Borate-treated Rubberwood Chipboard
2004 - IRG/WP 04-30359
Both no-choice and two-choice 4-week AWPA laboratory tests were performed to evaluate the resistance of borate-treated rubberwood (Hevea brasiliensis) chipboard prepared from a commercial mill run, against the Formosan subterranean termite Coptotermes formosanus. Boric acid (technical granular) was incorporated into the boards during manufacture to achieve loadings of 1.0% or 1.1% boric acid equiv...
A H H Wong, J K Grace


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 14: Report of sixth inspection (60 months) in Australia
1983 - IRG/WP 499
The IRG/COIPM International Marine Test was installed at Goat Island, Sydney Harbour, in December, 1977. The results of inspections made at 6, 12, 24, 36 and 48 months have previously been reported. This document records the data obtained on the 16.12.82, i.e. after 60 months exposure, at which time only 4 of the test frames remained in test. The surface water temperature at the time of inspection...
L J Cookson, J E Barnacle


The Effect on Biological and Moisture Resistance of Epichlorohydrin Chemically Modified Wood
2002 - IRG/WP 02-40224
Southern pine solid wood and fiber were chemically modified with epichlorohydrin to help in understanding the role of moisture in the mechanism of biological effectiveness of chemically modified wood. The solid wood had weight gains from 11% to 34%, while the fiber had weight gains from 9% to 75%. After modification, part of the specimens were water leached for 2 weeks or extracted for 2 hours ...
R E Ibach, B-G Lee


Window test. Direct testing of wood resistance to decay: A study of its fitness, its reliability and its accelerating factor
1984 - IRG/WP 2219
This is the results of an experiment using the window-test specimens, exposing the specimens to three different types of testing procedure: 1. Natural infestation in the open air; 2. Artificial infestation and exposure in the open air; 3. Artificial infestation in a green-house. The results show good similiraties of the three parallel tests in term of decay, and assess the reliability of the windo...
G R Y Déon, L N Trong


Dimensional stabilization and decay resistance of wood treated with brown-rotted lignin and copper sulfate
1990 - IRG/WP 3608
The objective of this study was to evaluate the potential usefulness of brown-rotted lignin (BRL) as a dimensional stabilization and copper complexing agent for wood treatment. For dimensional stabilization, aqueous solutions of the lignin extract were combined with either copper sulfate, glyoxal or other additives. Anti-shrink efficiency (ASE) values as high as 42% were obtained with wood treated...
L Jin, D D Nicholas, T Schultz


Accelerated termicidal performance data for new water-based copper linoleate formulations
1996 - IRG/WP 96-30104
An organic solvent based copper linoleate (Culin) has proved itself as an effective wood preservative in long term field trials in South Africa over a period of 30 years. Whilst the organic solvent based product offers good wood preservative performance, primary industrial interest has been in an emulsified version of the product. The objective of this study was to evaluate the influence of two di...
D Conradie, P Turner


Remedial treatment of creosoted railway sleepers of redwood by selective application of boric acid
1980 - IRG/WP 3134
An ideal preservative for remedial treatment must primarily be characterized by two requirements. First, it must have an ability to diffuse and distribut evenly into the wood and secondly, it must be fixed properly so that it does not leach out too fast. However, these two characteristics conflict with each other, and the choice of preservative must of necessity be a compromise. Wood preservatives...
C Bechgaard, L Borup, B Henningsson, J Jermer


Termite resistance of twenty-eight Indonesian timbers
1982 - IRG/WP 1150
A comparative study of termite resistance of 28 Indonesian wood species has been conducted using small samples measuring 5 x 10 x 20 mm³. The drywood termite Cryptotermes cynocephallus (Kalotermitidae) and the subterranean termite Coptotermes curvignathus (Rhinotermitidae) were used in the study. A resistance classification was derived on the basis of cluster analysis. The result reveals that Alb...
Nana Supriana, P E Howse


Leaching from CCA-treated wood submerged in seawater: Effect of high loadings, and a comparison between laboratory and marine conditions
1996 - IRG/WP 96-50080
This study of leaching examined the following variables: CCA loading; marine versus laboratory exposure and length of submergence. Blocks of Pinus sylvestris were treated to a range of nominal retentions from 15 to 50 kg/m³. Each block was then divided into three cubes and all transverse faces were sealed. All cubes were allowed to fix at ambient temperature for a minimum of one week. One set of ...
R M Albuquerque, S M Cragg, J D Icely


Microemulsion formulations for wood protection chemicals
1993 - IRG/WP 93-30030
A microemulsion is a thermodynamically stable oil-water dispersion system. As a formulation it provides many unique features such as water compatibility for water-insoluble chemicals, formulation stability, good bioavailability and environmental acceptance. This paper discusses the major criteria for the formulations of water-insoluble wood biocides and the comparison in properties between convent...