IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1007 documents. Displaying 25 entries per page.


In-situ experimental treatment and consolidation of degraded timber elements from a XIX century building
2012 - IRG/WP 12-10767
This paper presents the in situ experimental conservation work performed on three timber structural elements from a XIX century building: two floor beams and one roof beam. The palace was built in 1877 in the centre of Lisbon initially with residential purposes. It has four floors, with timber structural horizontal elements, stairs and roof beams (generally of Pinus sylvestris L.). The exterior wa...
D F Henriques, J de Brito, L Nunes


Preliminary laboratory bioassay to evaluate engineered Fibre-boards against subterranean termites C. acinaciformis (Isoptera: Rhinotermitidae)
2012 - IRG/WP 12-10768
In Australia, laboratory bioassays with subterranean termites typically contain groups of workers and soldiers in a substrate of moist mound material. This termite substrate may affect termite consumption, and the test materials create a favorable termite condition for the test. The main purpose of this test is to examine the effect of a melamine formaldehyde treatment of wood panels to evaluate t...
B M Ahmed (Shiday), H Militz, B Ozarska, I Ali, L Kloeser


A survey on Bio-Resistance of Oak and Elm in Caspian Sea Water
2012 - IRG/WP 12-20483
Logs of Oak (Quercus castanifolia) and Elm (Zelkova carpinifolia) have been cut to lumbers with dimensions of 300×100×30 mm. The oven dried samples have been impregnated with CCA (Chrome–Cupper-Arsenic). Treated and untreated (natural as a control) woods have been established for 3, 6, 9 and 12 months in Amirabad beach of Behshare under fishing environment. The observation results shows that i...
S M Kazemi


Performance superiority of CCA-C treated wooden jetty poles and piles used for 30 years in Bangladesh against marine borers
2012 - IRG/WP 12-30582
Observational study along with previous investigation and records revealed that chromated copper arsenate type C (CCA-C) impregnated southern pine poles and piles of jetty constructed in most vulnerable brackish water in Bangladesh are stable and resistant to attack of all types of marine borers after 30 years of use. It is evident from the service records of other construction materials that CCA-...
A K Lahiry


Mold Control for Treated Lumber in Block-Stack Storage Conditions
2012 - IRG/WP 12-30588
The mold development and control for freshly treated and block-stacked wood have been evaluated using a green house mold testing method. The results for the mold resistance of several commonly used water boron preservative treatment systems, such as ACQ, Copper Azole, and borates with and without inclusion of mold inhibitors are presented. The data suggest that the different preservative treatme...
L Jin, P Walcheski, A Preston


Supercritical impregnation of wood with siloxane
2012 - IRG/WP 12-30595
This paper describes the effect of supercritical impregnation with siloxane on the water repellency of Scots pine (Pinus sylvestris) sapwood samples. Samples were impregnated with a low amount of siloxane dissolved in supercritical carbon dioxide using isopropanol as a co-solvent. Siloxane retention (i.e. weight percent gain (WPG)) of the treated samples was 1.3 % (w/w) as found by mass balance. T...
A Kjellow, F Imsgard, J Fernandes, O Henriksen, E Klaassen, R Wagner, J Delis


Effects of oil types and treatment temperature on the properties of wood subjected to thermal modification in oil medium
2012 - IRG/WP 12-40574
The effect of the use of oil as a medium of heat transfer during thermal modification of different species of wood has been widely investigated with different results accruing with regards to the various end-use properties of the materials. However very little have been done on the effect of oil types as well as its interaction with treatment temperature on the resultant properties of the material...
L Awoyemi, M M Apetogbor, A A Oteng-Amoako


Effects of Nano-Zycosil on Liquid and Gas Permeability of MDF
2012 - IRG/WP 12-40578
Effects were studied of zycosil nanoparticles, with size range from 30 to 90 nm, on liquid and gas permeability of medium density fiberboard. 100 g of nanozycosil was added to each kg of dry fibers. Density was kept constant at 0.67 g/cm3. The obtained results indicated that addition of zycosil to the mat resulted in a significant increase in gas permeability due to the lower fiber-content in the ...
H Reza Taghiyari, K Heidarhaee, P Noori, A Karimi


The effect of press time on springback and water absorption of acetylated particleboard
2012 - IRG/WP 12-40579
In this study the effect of press time on springback, thickness swelling and water absorption was investigated. After 24 hours soaking in acetic anhydride, in order to achieving WPG 17%, acetylated particles were heated in an oven at 120 0C for 360 minutes. Acetylated and nonacetylated (control) particleboards were produced with 10% melamine urea formaldehyde (based on the oven-dry weight of part...
F Bavaneghi, M Ghorbani, A Kargarfard


Water uptake of wood surfaces with and without coating: influence of weathering
2012 - IRG/WP 12-40580
The objective of this study was to compare liquid water absorption of wood surfaces with and without coating, before and after artificial weathering. Samples of spruce, oak and sapelli were exposed to the EN 927-6 cycle for 1500 and 1850 hours and to the weathering produced by the Garner wheel for 1000 hours. Two highly pigmented coatings (solventborne and waterborne) and two semi-transparent stai...
L Podgorski, S Collignan, J D Lanvin


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and Russian imported spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


Influence of heat treatment intensity on the structural integrity of 14 timber species
2012 - IRG/WP 12-40586
Thermally modified timber (TMT) is characterized by improved durability and dimensionally stability, but strength properties, especially the dynamic ones, are compromised at the same time. Because dynamic standard tests require high efforts and time, the high-energy multiple impact (HEMI) –test was developed for the fast and reliable characterisation of the structural integrity of TMT, showing a...
C R Welzbacher, C Brischke, G Maier


Relationships between heat treatment intensity and some conferred properties of different European softwood and hardwood species
2012 - IRG/WP 12-40593
Effect of treatment intensity on conferred properties like elemental composition, durability, anti swelling efficiency (ASE) and equilibrium moisture content (EMC) of different European softwood and hardwood species subjected to mild pyrolysis at 230°C under nitrogen for different durations has been investigated. Independently of the wood species studied, elemental composition is strongly correl...
M Chaouch, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Effects of nano-wollastonite impregnation on fire resistance and dimensional stability of Poplar wood
2012 - IRG/WP 12-40595
The fire-retardant properties of Nano-Wollastonite (NW) in poplar wood (Populus nigra) were determined in this study. Some physical properties such as water absorption, volumetric swelling and Anti-Swelling Efficiency (ASE) were also measured. Specimens were prepared according to the ISO 11925 standard for the fire-retarding properties, and ASTM D4446-2002 standard for the physical properties. Imp...
A Karimi, A Haghighi Poshtir, H Reza Taghiyari, Y Hamzeh, A Akbar Enayati


Post-Manufacture Biocide Treatment of Engineered Wood I-Joists
2012 - IRG/WP 12-40596
Engineered wood I-joists, fabricated from laminated veneer lumber (LVL) flanges and oriented strand board (OSB) webs, offer many advantages over solid sawn lumber joists in residential and light commercial construction. With the expanded use of these products has come an increasing need to be able to treat them with biocides to prevent attack from decay fungi and termites during service. Historic...
A S Ross, R W Clawson


Mechanical Properties of Hydrothermally Treated Beech Wood in Buffered Mediums
2012 - IRG/WP 12-40597
Hydrothermal treatment of beech wood in buffered mediums was carried out by aim of controlling the destructive effect of acids formed by degradation of carbohydrates on strength properties. Different mediums (water, buffer5, 7 and 8) and temperatures (160 and 180 °C) were used. Mechanical properties of specimens including modulus of rupture (MOR), modulus of elasticity (MOE) and toughness were de...
A Talaei A Karimi, K Yaghoobi, A Talaei


Corrosion of fasteners in heat-treated wood – progress report after nine years’ exposure outdoors
2012 - IRG/WP 12-40601
The corrosion of common fastener materials now in use - mild steel, zinc-coated steel, aluminium and Sanbond Z-coated steel – has been evaluated after nine years’ exposure outdoors in untreated and heat-treated (thermally modified) spruce (Picea abies). Spruce from south-western Sweden was used. The heat-treatment was carried out in Finland by Stora-Enso Oy according to the ThermoWood process ...
J Jermer, B-L Andersson


Chemical Analysis of Hydrothermally Treated Beech Wood in Buffered Mediums
2012 - IRG/WP 12-40604
Hydrothermal treatment of beech wood in buffered mediums was carried out to study the effect of different mediums of heat treatment on crystallinity index of treated specimens due to degradation of carbohydrates. Different mediums (water, buffer5, 7 and 8) and temperatures (160 and 180 °C) were used. ATR spectra focusing on indexes of carbohydrates degradation obtained and analyzed. Results showe...
A Talaei, A Karimi


The effect of nanozycosil on the water absorption and dimensional stability of Beech wood
2012 - IRG/WP 12-40606
Zycosil is a clear penetrating water repellent. This product works by penetrating into the substrate and modifying the surface tension to inhibit water intrusion. Beech wood (Fagus orientalis) was modified by treatment with nanozycosil. Then water absorption and dimensional stability in terms of volumetric swelling percent and anti-swelling efficiency were determined and found to be improved on t...
M Ghorbani, F Bavaneghi


Environmental safeness of 60% and 72% concentrated CCA-C solution and paste for wood treatment
2012 - IRG/WP 12-50284
In this study 30-years practical and observational experience of the present author about using of 72% concentrated CCA-C paste for preparing treating solutions and for treating wooden poles, anchor logs and cross arms has revealed that the 60% concentrated CCA-C solution is superior to the 72% concentrated CCA-C paste regarding solubility, homogeneity, cleanliness, treatability, sludge formation,...
A K Lahiry


Tar-oil uptake vs time in immersion treatment of short pine posts: A simple technique applicable to rural communities of Papua New Guinea
2012 - IRG/WP 12-40608
Pinus caribaea and Araucaria cunninghamii logs ca. 100 mm in diameter were shortened to lengths 25-30 cm, conditioned to at/below fibre saturation point (FSP) for immersion/dip treatment using a hot- and- cold bath open- tank process. Before oven-drying and subsequent treatment, individual test specimens were numbered, their green weights and volumes, and dry weights recorded for basic density, vo...
B K Gusamo, R Tulo


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and imported Russian spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


Copper naphthenate treatment for wood pols - a review and update
2012 - IRG/WP 12-30600
This paper reviews copper naphthenate (CuNap) and its utility as a treatment for wooden utility poles. One of the principal reasons that CuNap has gained market acceptance, in addition to its efficacy against decay fungi and wood-destroying insects, is its low mammalian toxicity. CuNap is a well-proven non-restricted use preservative, used extensively and specified for environmental reasons by ut...
J A Brient, M H Freeman


Study of the use of organosolv lignin as bio-preservative of wood
2012 - IRG/WP 12-30603
The service life of wood depends on the species, use and environmental conditions of exposure. The treatment of wood protects it against degradation by xylophagous agents, enhancing the durability of material up to 10 times, and reducing the deforestation around 12.5%. In this way, the use of treatments is necessary because increases the service life of material and protect against xylophagous age...
P S B dos Santos, A Garcia, P H G de Cademartori, D A Gatto, J Labidi


Treating Bambusa vulgaris with neem seed oil against basidiomycetic biodegradation
2012 - IRG/WP 12-30608
Realising maximum benefits from bamboo stems/culms in Nigeria are presently constrained by their almost non-acceptance for applications in most structural and construction purposes, except in comparatively low quality and some temporary applications, such as scaffolding, owing to their susceptibility to easy destruction by agents of biodegradation as a result of their poor inherent natural durabil...
A A Erakhrumen


Previous Page | Next Page