IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3208 documents. Displaying 25 entries per page.


Synergistic effects between 2-HPNO, Irganox 1076 and EDTA on the inhibition of wood degradation by Coriolus versicolor
2004 - IRG/WP 04-30331
The efficiency of 2-hydroxypyridine-N-oxide (2-HPNO) as wood preservative has been investigated. As shown using classical experiments as well as using response surface methodology, the efficiency of 2-HPNO as wood preservative is strongly improved in presence a chelator like EDTA and/or of Irganox 1076 an industrial antioxidant. In these conditions, wood preservative efficiency of the mixture the ...
A Mabicka, S Dumarçay, N Rouhier, M Linder, J P Jacquot, P Gérardin, E Gelhaye


Microscopic characteristics of Pinus radiata wood veneers weathered outdoors for one yea
1993 - IRG/WP 93-10018
Radiata pine (Pinus radiata) wood veneers glued to solid wood hacking strips were exposed outdoors at 45° north-facing for one year and then examined by light microscopy (LM) and transmission electron microscopy (TEM). As expected, the exposed wood surfaces were colonised by a variety of microorganisms; however, wood decay was not observed. Ultlaviolet (UV light) radiation and water were the main...
A P Singh, R A B Sweeney, E A Dunningham, D V Plackett


On the problem "House Longhorn Beetle" in hardwoods and an aid to distinguish between Hylotrypes bajulus and Hesperophanes cinereus larvae
1981 - IRG/WP 1141
S Cymorek


Influence of storage on mould susceptibility of wood at relative humidity values lower than 100%
1989 - IRG/WP 1413
It is well known that wood material changes with time because of different environmental influences. The effects of such changes on the subsequent mould susceptibility are less known. In this paper we report on increased mould susceptibility of pine wood after storage. Mould growth was detected by indirect methods....
J Bjurman


Natural resistance of twenty-six Guianese wood species against marine borers
1988 - IRG/WP 4144
This note is a contribution on the study of the natural resistance of some wood species from French Guiana, some of which could be found too in the neighbourhood. Here are presented the results after one year exposure in the marine environment....
L N Trong


Report on a field demonstration of methods for detecting defects in wood poles
1984 - IRG/WP 2232
P I Morris, H Friis-Hansen


Long-term performance of a "wax" type additive for use with water-borne pressure preservative treatments
2000 - IRG/WP 00-40159
Field performance results are updated for matched CCA treated decking boards with and without an emulsion water repellent additive incorporated with the initial pressure treatment. Decks have been exposured for over 9 years in Harrisburg, NC. Boards were evaluated for in-service and laboratory performance for water repellent efficacy, as well as additive loadings in the boards after this exposure....
A R Zahora


Marine borers as wood degraders in Bangladesh and their protection
1996 - IRG/WP 96-10186
Field study on timber piles used in Bangladeshi brackish waters revealed that untreated and pentachlorophenol treated piles drastically degraded by the attack of molluscs and pholads (marine borers). Adequately CCA-C impregnated (30 kg/m³ or 6% W/W dry oxide retention) timber piles can protect the attack of molluscs. It is very difficult to protect pholads which can invade naturally very durable ...
A K Lahiry


Migration of active ingredients from treated timber into fresh water
1991 - IRG/WP 3669
Spruce roundwoods and segments were treated with three different wood preservatives. Two of them containing copper and chromium the other one free of chromium. After fixation (3 weeks, 20°C) the specimens were leached by using artifical rain or by shaking the segments for one hour in contact with demineralized water. The water was analysed for the relevant elements of the preservative tested. Lea...
H Klipp, H Willeitner, K Brandt, A Müller-Grimm


Detection of brown rot decay in wood by ion mobility spectrometry
1991 - IRG/WP 2377
A test method for the detection of brown rot decay in wood is described and involves a two-step procedure: thermal release of vapours from wood samples followed by analysis using Ion Mobility Spectrometry (IMS), with results being obtained in 5-10 seconds. The advantages, limitations as well as the detection limit of the technique are presented....
A H Lawrence, T Nilsson


Preventive action against fungal decay: A comparative experiment on the effects of natural and artificial infection of wood by Basidiomycetes
1981 - IRG/WP 2160
M Fougerousse


Report on Sub-group 5 in Raleigh, 6 May 1980
1980 - IRG/WP 1123
S Cymorek


United States Federal Committee on Wood Protection
1971 - IRG/WP 43
A C Jewett


Elimination of alternative explanations for the effect of iron on treated wood
1993 - IRG/WP 93-30006
Amounts of iron which had previously been found in stakes removed from ground contact reduced decay of untreated wood by four brown-rot fungi. This suggested that the effect of iron may be on the preservative. Analysis of the leachates from CCA- and ACA-treated wood blocks first exposed to rusting iron, then to a brown-rot fungus, showed that the increased decay found in the laboratory for wood ex...
P I Morris, J K Ingram, D L Gent


A note on testing the efficacy of wood preservatives above ground
1995 - IRG/WP 95-20078
A number of test methods have been used to evaluate the performance of wood preservatives in above ground situations. These have included EN 113 tests following natural exposure weathering (NEWT), L-joint or T-joint tests, lap-joint tests, and decking tests. A new test referred to as the A-frame test has been developed and is under evaluation. This is based on a sandwich-type test in which a thin ...
G R Williams, J A Drysdale, R F Fox


The effects of heat treament on the specific gravity of beech and spruce wood
2003 - IRG/WP 03-40254
The effects of heat treatment on specific gravity of beech (Fagus orientalis) and spruce wood (Picea orientalis) naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 2 x 2 x 3 cm. Heat treatment was than applied to the wood samples at four different temperatures (130 °C, 150 °C, 180 °C and 200 °C) and three different durations...
S Yildiz, Ü C Yildiz, G Colakoglu, E D Gezer, A Temiz


An introduction to environmental aspects of groundwater arsenic and CCA treated wood poles in Bangladesh
1997 - IRG/WP 97-50081
The environment comprises biosphere, lithosphere, atmosphere and hydrosphere. Therefore, environmental science is a multi-disciplinary study, includes life sciences, physical sciences, chemical sciences, geology, geography, meteorology, forestry, agriculture, soil science, hydrology, ecology, public health, engineering etc. Tremendous industrial and mining activities, deforestation and population ...
A K Lahiry


Changed susceptibility of the chemically and thermally degraded spruce wood to its attack by the dry rot fungus Serpula lacrymans
1999 - IRG/WP 99-10322
In buildings, some intentional or unintended situations can occur at which some wood products are exposed to aggressive chemicals and also to higher temperatures. Occasional activity of fungi on such pre-attacked wood products can be either higher or lower. This paper deals with changes in the susceptibility of spruce wood (Picea abies L. Karst.) to attack by the dry rot fungus Serpula lacrymans, ...
L Reinprecht


Depletion of wood preservatives after four years' marine exposure in Mt. Maunganui harbour, NZ
1994 - IRG/WP 94-50036
This paper reports on chemical analysis of marine test samples exposed in Mt. Maunganui harbour, New Zealand from 1977 to 1981. Depletion data for a Class II CCA, a CCA-A formulation, acid copper chromate and ammoniacal copper arsenate are presented. The results suggest differences in the rate of loss of individual preservative components among the four formulations and redistribution of individua...
K J Archer, A F Preston, C M Chittenden, D R Page


The Fifth Annual Report of the International Research Group on Wood Preservation 1973-1974
1974 - IRG/WP 531
IRG Secretariat


Model questionnaire for preparation of monographic cards for wood-destroying fungi
1972 - IRG/WP 103
C Jacquiot


In-situ pressure injection for preservation of rubber wood (Hevea brasiliensis Muel Arg.)
1992 - IRG/WP 92-3688
Rubber wood is widely used for the manufacture of furniture, doors for housing and packing cases. However in an untreated condition it is highley susceptible to sapstain and decay fungi and borers. Its utility gets considerably reduced if the wood is not treated well in time. Preservative treatment has to be given within the period of felling and transport to prevent not only loss of structural pr...
H S Ananthapadmanabha, V R Sivaramakrishnan


Inorganic wood preservative levels in soil near a noise barrier treated with different preservatives after 8 years in service
2005 - IRG/WP 05-50234
In March 1996 nine test sections of a noise barrier were installed near Stockholm Sweden. The test sections include untreated Scots pine, spruce and larch and Scots pine, treated with different wood preservatives. After 8 years in service, the untreated spruce, pine and larch boards in contact with the soil were significantly decayed, with an estimated service life of about 5-10 years, while the u...
P A Cooper, Y T Ung, M-L Edlund, J Jermer, O Söderström


Report of an investigation of damage by wood ants in buildings in Sweden
1976 - IRG/WP 148
Wood ants in buildings occur everywhere in Sweden, particularly in maritime districts and in vicinity of larger lakes. The damage caused by Camponotus herculeanus does not differ from that caused by Camponotus ligniperda. The former occurs in all Sweden, the latter only in southern Sweden. The damage is to be found almost exclusively in dwelling houses (week-end cabins and "all-the-year round" hou...
V Butovitsch


A bibliography of organic solvent-based wood preservatives
1973 - IRG/WP 322
H Alliot


Previous Page | Next Page