IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 460 documents. Displaying 25 entries per page.


Field Stake Tests with Copper-based Preservatives
2008 - IRG/WP 08-30459
The performance of field test stakes derived from commercially produced ground contact retention copper quat preservatives based on either soluble copper complexed with ethanolamine, or from a water-based suspension of particulate micronized copper compounds, as well as untreated southern yellow pine controls, is compared at two decay test sites. After less than one year in field test some of t...
A Preston, L Jin, D Nicholas, A Zahora, P Walcheski, K Archer, T Schultz


The Comparison of Fixation and Leachability of Bark, Fruit and Leaf Tannin Extracts with Boron Minerals
2008 - IRG/WP 08-30473
Tannins extracted from several plants have natural durability properties. Due to these properties, some of the researchers have studied them for protecting wood. In this study, Scots pine (Pinus sylvestris) and beech (Fagus orientalis) wood samples were treated with bark, fruit, and leaf extracts as well as water-based wood preservative salts at various concentrations to increase fixation. The pen...
S Sen, C Tascioglu, K Tirak


Treatment of Selected Lesser Used Timber Species against Subterranean Termites using Heartwood Extracts from Teak (Tectona grandis) and Dahoma (Piptadeniastrum africanum)
2008 - IRG/WP 08-30476
Lesser used timber species represent a valuable material for all-purpose uses. However, most of them are not durable. They are, for effective utilization, often treated with all manner of toxic synthetic substances to enhance their natural durability, especially in the tropics where conditions favour their deterioration. Most of these toxic synthetic substances often pose a threat to the environme...
A Asamoah, C Antwi-Boasiako, K Frimpong-Mensah


Preliminary investigation of biological resistance, water absorption and swelling of thermally compressed pine wood panels
2008 - IRG/WP 08-40396
Wood can be modified by compressive, thermal and chemical treatments. Compression of wood under thermal conditions is resulted in densification of wood. This study evaluated decay and termite resistance of thermally compressed pine wood panels at either 5 or 7 MPa and at either 120 or 150?C for one hour. The process caused increases in density and decreases in thickness of the panels; however, lab...
Ö Ünsal, S N Kartal, Z Candan, R Arango, C A Clausen, F Green III


The Effect of Heat Treatment on Water Absorption and Dimensional Stability of Anatolian Chestnut (Castanea sativa Mill.) wood
2008 - IRG/WP 08-40407
The heat treatment of wood is an environment-friendly method for wood preservation. This process improves wood’s resistance to decay and its dimensional stability. However, mechanical properties decrease in different ration because of density loss as a result of heat treatment. In this study, the effect of heat treatment on water absorption and dimensional stability at different relative humidit...
G Gunduz, D Aydemir


Laboratory Studies on Copper Availability in Wood Treated with Soluble Amine Copper and Micronized Copper Systems
2008 - IRG/WP 08-30489
A laboratory method has been employed to investigate the level of soluble copper in wood treated with various copper-based preservative systems, such as micronized copper (particulate copper) and amine copper solutions. This report describes the methodology and preliminary results on determination of the soluble copper in the treating solutions and the treated wood by these systems, as well as th...
L Jin, P Walcheski, A Preston


Mold fungi - Major impediments to cleaning/repairing flood and rain-damaged homes
2008 - IRG/WP 08-40427
Damage to homes by hurricanes that make landfall in the south and southeastern United States, or sub-tropical and tropical regions, during the hot, humid summer months is compounded by the growth of mold fungi on wetted building materials. Most homeowners are better equipped to deal with construction problems associated with storm damage than to control the growth of mold fungi. Following hurrican...
T L Amburgey


Moisture adsorption isotherms of wood studies using a dynamic vapour sorption apparatus
2009 - IRG/WP 09-20398
Five types of wood including two Malaysian hardwoods acacia mangium (Acacia mangium) and sesenduk (Endospermum malaccense), two temperate softwoods, Sitka spruce (Picea sitchensis), radiata pine (Pinus radiata) and Accoya (commercially modified wood) were studied to determine their moisture sorption behaviour using a Dynamic Vapour Sorption (DVS) apparatus. The isotherm plot for each species teste...
J Zaihan, C A S Hill, S Curling


Evaluation of Water Repellency of Treated Wood Using Several Alternative Methods
2009 - IRG/WP 09-20419
In this study, the results of water repellency testing using a digital swellometer method for water-borne organic-preservative systems with water repellent additives are reported. The findings suggest that the traditional method of using matched untreated controls as a reference developed from historic solvent-based treatments for determination anti-swelling efficacy (ASE) may underestimate the a...
L Jin, A F Preston


Potential synergy between natural product extracts for limiting fungal decay
2009 - IRG/WP 09-30495
Natural products often exhibit tremendous potential for inhibiting various microorganisms when they are tested in petri dish tests, but perform poorly when tested in vivo. The failures can often be attributed to a lack of broad spectrum activity against the range of organisms present in a natural environment. One method for overcoming this challenge is to use extracts from a number of sources with...
M Maoz, C Freitag, J J Morrell


Micronized Copper Preservative Systems: Observations on the Release of Cupric ion (Cu2+) from Treated Wood and Performance against Wood Decay Fungi
2009 - IRG/WP 09-30519
In an attempt to address the mechanism of action of micronized copper preservatives, a 20-week continuous water leaching study was conducted. The leaching results indicated that, once impregnated in wood, micronized copper preservatives continuously release cupric ion, and the levels of cupric ion released from micronized copper treated wood are higher than those released from CCA treated wood, a...
J Zhang, R Ziobro


Leaching of the copper component from full scale decking boards during one summer season
2009 - IRG/WP 09-50260
The leaching of copper has been tested in laboratory and in outside exposure for freshly treated pine sapwood samples with three different copper preservatives, Cu HDO, copper quat and copper triazoles. We found in the laboratory leaching test that a fixation with warming to 60 °C (140 °F) for 48 hours without drying and then drying in the laboratory in room temperature gave the lowest leaching of copper. We also found that surface treatments with wood oils reduced the leaching, and that washing of the surface before testing had no effect. Full scale decking board samples (0.25 m2) were then exposed outdoors for rain. The rain water was collected and analysed for copper. After one summer season (about 600 mm rain) we found that the leaching differ for the three preservatives. All samples with a water borne surface treatment had the lowest leaching, about half the amount of untreated.
F G Evans


Modification of Wood by a Water-Repellent Compound Used in the Textile Industry: Boron Release and Termite Resistance
2009 - IRG/WP 09-40447
In the study, wood specimens were treated with disodium octoborate tetrahydrate (DOT) and a commercial water and oil repellent compound, FORGUARD M®, a weak cationic emulsion containing dipropylene glycol monomethylether, water and solids in its formulation and used in the textile industry. There were two different processes for preservative treatments: double and single treatments. The leaching ...
S N Kartal, E Terzi, B Erilkun, Y Imamura


Estimating the heat treatment intensity through various properties of thermally modified timber (TMT)
2009 - IRG/WP 09-40459
The suitability of different measures for prediction of the heat treatment intensity was investigated. Therefore, the resistance to impact milling (RIM), the lightness L*, the equilibrium moisture content (EMC), the anti swelling efficiency (ASE) and the total amount of soluble carbohydrates (TSC) of heat treated specimens were correlated with corresponding fungal resistance achieved by heat treat...
C R Welzbacher, C Brischke, A O Rapp


Selection of an appropriate coating system for wooden boats to be used in fresh water
2009 - IRG/WP 09-40472
Properties of several, most commonly used protective low-price coatings, which are used by the pletnja boat owners in Bled, Slovenia, were extensively studied. The aim of this professional, practically oriented study was to compare various coating systems, and to recommend the most suitable one to the boat owners. Regarding specific use conditions, the following properties, including their resista...
M Petrič, B Kričej, A Logar, M Pavlič


The brown rot of oak wood submerged for 6 months in the Baltic sea
2010 - IRG/WP 10-10736
The natural wood submerged or partially immersed in sea water is commonly affected by certain microorganisms. The bacteria and marine borers that decay the wood totally submerged in sea water and above sea level other microorganisms as fungi, algae, insects may attacked wood. The sea water may affect and change the properties of wood. We have tried to determine the susceptibility to decay caused b...
A Fojutowski, A Kropacz, I Pomian


Methods for Studying Penetration Depth of Wood Protection Products
2010 - IRG/WP 10-20432
EN 152 is an accepted standard in Europe for measuring how deep a wood protection product penetrates into the surface of treated pine wood. The method has provided consumers with a wide assortment of products that meet the specifications outlined in the standard. Because the test takes 8 or more months to carry out, artificial ageing procedures have evolved in order to standardize and speed up the...
K Hansen, L Sites, D D Nicholas


Effects of Cunninghamia Lanceolata Heartwood Extracts on the Growth of Wood Decay Fungi
2010 - IRG/WP 10-30527
China-fir (Cunninghamia lanceolata) wood is well known for its good durability. This species is native to China and has been extensive planted there. Mainly, extractives are responsible for the wood resistance to decay fungi. In this paper, the extractives of China-fir heartwood were studied for their effects on various wood decay fungi. Sequential extraction of heartwood in hexane, ethyl acet...
Shujun Li, Jing Wang, Jian Li


Antifungal Effect of Bark and Wood Extracts of Condalia hookerii (Rhamnaceae), Ebenopsis ebano (Fabaceae) and Helietta parvifolia (Rutaceae) on Trametes versicolor
2010 - IRG/WP 10-30532
This research detail the growing inhibition effect on Coniophora puteana and Trametes versicolor fungi caused by hot water sawdust and bark extracts of three semi-arid land species Condalia hookerii, Ebenopsis ebano and Helietta parvifolia diluted in malt extract agar medium at 2000 ppm and 10000 ppm. After 12-14 days incubation the inhibition growing effect was measured based on the difference be...
A Carrillo, J G Marmolejo, F Garza, V Bustamante, M Garza


Treatment of Scots pine wood with oil in water and water in oil emulsion systems: Effects on boron leaching and water absorption
2010 - IRG/WP 10-30535
The aim of this study was to investigate the water absorption and water repellent efficiency of oils and oil water emulsions [oil-in-water (O/W) and water-in-oil (W/O)] and possibilities of reducing the amount of boron leaching from treated wood. Scots pine wood samples treated with waste or sunflower oil and water formulations contained 3%BA. The level of water absorption and water repellent effi...
E D Tomak, Ü C Yildiz, A Can


A Comparison of the Performance of Related Copper Based Preservatives against Soft Rot
2010 - IRG/WP 10-30540
The performance of pine and beech wood treated with either a soluble copper + quat (ACQ type D) preservative system or a particulate copper + quat system was evaluated in unsterile soil using the European standard ENV 807 soft rot decay test procedure. In addition, to compare soft rot performance of soluble and particulate copper directly without the influence of co-biocides, beech and pine test...
M Ray, D Dickinson, K Archer


Studies on Effect of pH on Copper Availability in Copper-Based Preservatives
2010 - IRG/WP 10-30549
Laboratory methods have been employed to investigate the pH effect on the copper solubility of basic copper carbonate. The pH was controlled using two different approaches. One was with the adjustment of pH of the solutions by acid or base using sulfuric acid or sodium hydroxide until the solution equilibriums were obtained for each defined pH. A second approach was to control pH with buffer sol...
L Jin, P Walcheski, A F Preston


An investigation on some physical properties of oil heat treated poplar wood
2010 - IRG/WP 10-40509
In this study some physical properties of small samples (20×20×20 cm) of poplar wood (Populus nigra var.pyramidalis) after oil heat treatment with linseed oil was investigated. Two time levels (4.5 & 6 hours) and three temperature stages (180,200 & 220°C) were selected. The results of this study showed significant differences in effects of treatment temperature on physical properties of wood....
B Bazyar, D Parsapajouh, H Khademiesalam


Kinetic Water Vapour Sorption of Sitka Spruce at Variable Temperature Using the Parallel Exponential Kinetics Model
2010 - IRG/WP 10-40512
In this study the water vapour sorption of Sitka spruce (Picea sitchensis (Bongard) Carr.) was measured using a Dynamic Vapour Sorption (DVS) apparatus and then analysed using the parallel exponential kinetics (PEK) model. The water vapour sorption rate of wood quickly increased when the relative humidity was changed. With the elapse of time, the sorption rate gradually decreased within any specif...
Yanjun Xie, C Hill


Biological degradation of acetylated wood after 18 years in ground contact and 10 years in marine water
2010 - IRG/WP 10-40522
This paper addresses the resistance to biological degradation of acetylated wood. Firstly, it presents results from an EN 252 test after 18 years’ exposure. The test is still running in Nordic NWPC test fields, Simlångsdalen in Sweden and Viikki in Finland. Results from this test were presented after 5 years’ exposure ( IRG/WP 97-30139), and showed that the resistance of acetylated wood wit...
P Larsson Brelid, M Westin


Previous Page | Next Page