Hydroponic Phytoremediation of Chromated Copper Arsenate (CCA) and Copper Contaminated Water
2014 - IRG/WP 14-50304
The removal of selected metals by duckweed (Lemna minor) and parrotfeather (Myriophyllum aquaticum) from a simulated aqueous environment contaminated with Chromated Copper Arsenate (CCA) and copper sulfate was studied in a controlled laboratory experiment. The duckweed and parrotfeather’s tissues were analyzed to evaluate the removal of copper (Cu), chromium (Cr), and arsenic (As) from CCA cont...
C Keith, H Borazjani, S Diehl, Y Su, Fengxian Han, B Baldwin


Nano-Zycosil in MDF. Part I: Gas and Liquid Permeability
2014 - IRG/WP 14-40652
Effects were studied of zycosil nanoparticles, with size range from 20 to 80 nm, on liquid and gas permeability of medium density fiberboard. Nanozycosil was used at four consumption levels of 0, 50, 100, and 150 g/kg dry wood fibers. Density of all treatments was kept constant at 0.67 g/cm3. The obtained results indicated that the addition of zycosil to the mat resulted in a significant increase...
H Reza Taghiyari, A Karimi, P M D Tahir, O Schmidt, E Bari, P Nouri , A Jahangiri


Decay resistance of wood-plastic composites reinforced with extracted or delignified wood flour
2014 - IRG/WP 14-40655
The moisture and decay resistance of wood-plastic composites (WPCs) reinforced with extracted or delignified wood flour (WF) was investigated. Three different extractions were preformed: toluene/ethanol (TE), acetone/water (AW), and hot water (HW). Delignification (DL) was performed using a sodium chlorite/acetic acid solution. All WPCs specimens were made with 50% by weight HDPE and WF, first com...
R E Ibach, Yao Chen, N M Stark, M A Tshabalala, Yongming Fan, Jianmin Gao


Effect of Nano-Wollastonite on Water Absorption in Particleboard
2014 - IRG/WP 14-40662
Effects of wollastonite nanofibers on physical properties of particleboard were studied. Nano-wollastonite (NW) was applied at 5, 10, 15, and 20 g/kg, based on the dry weight of wood-chips, and compared with control specimens. Two application methods of NW were used: surface application (SA), and internal application (IA). Density was kept constant at 0.68 g/cm3 for all treatments. Tests were carr...
S Karimi, H Reza Taghiyari, A Karimi, P M Tahir, J Abdul Halip


Modern Instrumental Methods to Investigate the Mechanism of Biological Decay in Wood Plastic Composites
2014 - IRG/WP 14-40674
Various instrumental techniques were used to study the fungal decay process in wood plastic composite (WPC) boards. Commercial boards exposed near Hilo, Hawaii (HI) for eight years in both sun and shadow locations were inspected and tested periodically. After eight years of exposure, both boards were evaluated using magnetic resonance imaging (MRI), while a selected area of the board exposed in sh...
G Sun, R Ibach, M Gnatowski, J Glaeser, M Leung, J Haight


The Physical Properties of Heat Treated Fir Wood and Outdoor Durability
2014 - IRG/WP 14-40677
Wood might be easily susceptible to degrade by biotic and abiotic factors. Therefore, wood should be protected from fungi, insects and other degradation factors by applying treatment methods. Especially, for the wood have used in the external environment. Chemical treatment methods have some disadvantages such as use of toxic chemicals (Arsenic and chromium) and treatability of refractory wood spe...
O E Özkan, H Vurdu, A Temiz, G Köse


Experiences with an industrial system for controlled thermal wood modification in pressurized unsaturated steam
2014 - IRG/WP 14-40678
Thermal wood modification in pressurized reactors has a long history, but these processes are to date industrially scarcely used, because of the relatively complicated process equipment, compared to the more common high-temperature processes in kilns at atmospheric pressure. However, based on our practical experience with the FirmoLin® process, supported by recent scientific findings, it is foun...
W Willems


Leachability and Dimensional Stability of Nanosilver-Steamed Densified Poplar
2014 - IRG/WP 14-40684
This study was aimed to investigate leachability and dimensional stability of nanosilver impregnated poplar (Popolus alba), steamed before hot compression. Wood samples were impregnated with nanosilver suspension (200 and 400 ppm) under pressure of 4 bar for 20 minutes. Steam treatment was carried out at 150°C for 2 hours. Then samples were compressed (33%) radially in a hot press at 170°C for 3...
G Rassam, A Talaei, A Ahmadi


Repellency of Schinus molle L. leaf extracts onto Reticulitermes flavipes Kollar (Isoptera: Rhinotermitidae)
2015 - IRG/WP 15-10850
Reticulitermes flavipes Kollar (Isoptera: Rhinotermitidae), is a subterranean termite which damage wood and it is a pest in several countries, where the economic losses are huge. In Chile there have been foci of infestation in the Metropolitan Region and in the Region of Valparaíso with a big expansion in the last years. This study evaluated in laboratory the repellence effect of extracts from Sc...
A Huerta Fuentes, S Constenla Cáceres, Í Chiffelle Gómez


Influence of artificial and natural weathering on water exclusion efficacy of wood
2015 - IRG/WP 15-20559
Water exclusion efficacy (WEE) is one of the most important properties of wood that contributes to the overall performance of naturally durable wood species in outdoor above ground applications. WEE is in strong correlation with moisture dynamics of wood, its hydrophobicity and can indicates susceptibility against wood decay fungi. Despite of the importance of this parameter, WEE is not completely...
M Žlahtič, M Humar


Development of a rapid screening method to determine the susceptibility to mould growth of novel construction and insulation products
2015 - IRG/WP 15-20562
Wood-based materials are commonly used in building construction/insulation as a replacement for solid timber. However, these materials are susceptible to microbiological growth and different environmental conditions influence the vulnerability of wood-based materials. Moulds are a common problem found within homes and cause aesthetic damage, health problems and can increase material vulnerability ...
B K Stefanowski, S F Curling, E Mansour, G A Ormondroyd


Some comments on durability testing of WPC according to EN 15534-1
2015 - IRG/WP 15-40695
The standard EN 15534-1 (2014) gives advice for broad characterization of WPC materials and products. It contains instructions for test procedures concerning different properties e.g. mechanical properties, thermal properties, as well as durability. In this paper some WPC materials from the market were tested for their resistance against brown rot. Furthermore, the water uptake and bending prope...
S Bollmus, A Gellerich, H Militz


Buffered Amine Oxide Treatment Systems for Imparting Water Based Azoles/Insecticides in Douglas Fir and Eucalyptus
2015 - IRG/WP 15-40707
In today’s world, wood remains the most versatile, practical and sustainable building material. In contemporary countries, wood is a well-managed renewable resource that has a remarkably small carbon footprint compared to those of steel, aluminium, composites, and concrete. These alternative materials have continued to emerge as viable building materials given the durability issues of untreate...
R W Clawson Jr


Effect of Nano-Silane on Permeability in MDF as a Result of Susceptibility to Moulds and Fungi
2016 - IRG/WP 16-40716
Effects were studied of vapor chamber on specific gas permeability of nanosilane-treated medium-density fiberboards (MDF). Size range of nanoparticles was 20 – 80 nm. Nano-silane (NS) was used at four consumption levels of 0, 50, 100, and 150 g/kg dry wood fibers. Density of all treatments was kept constant at 0.67 g/cm3. Specimens were kept for 18 weeks in vaporized chamber; their specific gas ...
H R Taghiyari, J Norton, A Moradiyan, M Sadegh Taher Tolou Del, H Siahposht, B Moradi-Malek, M Noferesti


Superhydrophobic treatment of Norway spruce wood for improvement of its resistance against brown rot and moulds
2016 - IRG/WP 16-40734
Water repellence of wood can be increased and its some other properties influenced by introduction of hydrophobic chemicals into and on cell walls without affecting the wood’s bulk density due to lumen filling. Herein, a simple dipping method to insert octadecyltrichlorosilane (OTS) into cell walls and to deposit the self-assembled hydrophobic monolayers (SAMs) of OTS is reported. It was found o...
A Kumar, P Ryparová, P Hajek, B Kričej, M Pavlič, A S Škapin, M Šernek, J Tywoniak, J Žigon, M Petrič


Encapsulation of poles to prevent moisture uptake – a laboratory test
2016 - IRG/WP 16-40753
Premature failure of utility poles due to decay in soil contact is the main reason for early removal of utility poles, a measure that implies extra costs for utilities. Remedial treatments and barriers are common methods to prolong the service life of utility poles. The first part of this paper gives an overview of mode of action and commercial application of barrier systems as described in the li...
K-C Mahnert, U Hundhausen


The effect of acetylation on physical properties of beech (Fagus orientalis) and Alder (Alnus subcordata) wood
2016 - IRG/WP 16-40759
In this study the effect of acetylation on physical properties such as water absorption, volumetric swelling and anti-shrink efficiency (ASE) of beech and alder were investigated. After 24 hours soaking in acetic anhydride, in order to achieving two surface of weight gains, acetylated samples were heated in oven at 120 0C for 90 and 360 minutes. Then water absorption and dimensional stability in...
M Akhtari, M Arefkhani


A Treatability Study of Western Wood Species with Water Based Azoles and Insecticides Using Buffered Amine Oxides
2016 - IRG/WP 16-40766
The use of Western U.S. Wood Species remains small in today’s global wood product market when compared to the use of other commercially available softwoods. One reason that other fiber sources, those that may be less naturally durable or exhibit slightly inferior mechanical properties, are utilized is ease of treatment. In an attempt to ensure adequate penetration in commercially important an...
R W Clawson Jr, C N Cheeks, K A Cutler


Efficacy of Erythropleum suaveolens (potrodom) and Distemonanthus benthamianus (bonsamdua) water extractives on the durability of five Ghanaian less used timber species of varying perviousness and retentiveness
2017 - IRG/WP 17-30705
Conventional wood preservatives are not only toxic to target bio-deterioration organisms but also to humans, other organisms and the environment. In an effort to find preservatives that are less toxic or non-toxic to man, other organisms and the environment, efficacy of branch bark and heartwood water extracts (0.65 g/ml) of Erythropleum suaveolens (potrodom) and Distemonanthus benthamianus (bonsa...
A Asamoah, K Frimpong-Mensah, C Antwi-Boasiako


Copolymers of tannin extracts as wood protection agents
2017 - IRG/WP 17-30709
Wouldn´t be a dream to preserve wood with the substances which the nature already synthesizes for protecting itself? The idea we would like to pursue is simple: Increase the concentration of these substances, the tannins, trying to fix them properly in wood. It appears easy but it is not. Sensibility against leaching, fungal decay and weathering were observed. In this paper new flavonoid co-polym...
G Tondi, L Sommerauer, A Oberle, A Petutschnigg, M-F Thevenon


Water absorption characteristics of CLT
2017 - IRG/WP 17-40817
CLT is initialism of Cross Laminated Timber. CLT is generally large-sized panel which can use many woods efficiently, so it is attracted attention recently in Japan. Therefore, many studies about CLT are carried out. However, there are few studies about durability of CLT. Avoiding water infiltration is important for durability of wooden building. CLT has many edge-glued points which has risk of w...
D Yokoi, H Ishiyama, Y Hirano


Influence of sea water on timber and metal joints
2017 - IRG/WP 17-40818
In the Great East Japan Earthquake that occurred in March 2011, many buildings suffered from seawater immersion caused by the tsunami. Saito's study revealed that corrosion progresses on metal plate that experienced seawater immersion 1). However, the detailed mechanism of corrosion progresses has not yet been clarified. Therefore, in this study, salinity which is one of causes of corrosion w...
T Nishimura, H Ishiyama, F Hirose, N Wada


The Impact of Cryopreservation Techniques and of Water Quality on the Wood Degrading Ability of Fungal Strains: Recommendations for Maintenance and Culturing Procedures
2018 - IRG/WP 18-20636
In order to establish an optimal cryopreservation method, strains of Basidiomycete and Ascomycete fungi, which are among the most frequently used for wood durability testing, were evaluated using three cryopreservation procedures at -80°C. The main objective was to prevent decrease of the fungal virulence that may occur due to repeated routine sub-culturing procedures and to optimize the reactiva...
A Stum, M Montibus, I le Bayon, M Kutnik


Material Resistance and Chemical Composition of Italian Stone Pine (Pinus pinea)
2018 - RG/WP 18-20645
Relevant properties of stone pine (Pinus pinea) wood have been only fragmentarily addressed in the past, which has been recognized as a limiting factor for its potential applications. The amount of the respective wood species on the market will likely increase in the future. The sorption properties, permeability to water, extractives content and durability against fungi of Pinus pinea sapwood and ...
M Humar, M De Angelis, M Romagnoli, V Vek, I Poljanšek, P Oven, N Thaler, B Lesar, D Kržišnik


Performance of acetylated wood in aquatic applications
2018 - IRG/WP 18-40822
Acetylation of wood to enhance its resistance against wood decaying fungi and insects has been studied extensively under both laboratory and terrestrial field trials. Also several studies are investigating the performance of acetylated wood in marine and fresh water exposures. This paper updates nine year marine tests with acetylated radiata pine in Hejlsminde (Denmark) and presents data on 3 year...
F Bongers, S Palanti, A Gellerich, J J Morrell, J Creemers, J Hague