Effect of long-term immersion in fresh and salt water on mould growth on Scots pine (Pinus Sylvestris L.) wood
2020 - IRG/WP 20-10962
Wood exposed outdoors will eventually be degraded by fungi, depending on exposure and material characteristics. Numerous wooden constructions in the Røros municipality have existed since the 17th century, but wood used in recent repairs have decayed faster than expected. Before 1970 timber was mainly transported by log driving or rafting, and the logs were immersed in water for longer or shorter ...
M Sand Austigard, J Mattsson


Water interactions in wood polyesterified with sorbitol and citric acid
2020 - IRG/WP 20-40888
Polyesterifcation of wood with sorbitol and citric acid seems to be a promising chemical wood modification technique that is both low-cost and produced from bio-based chemicals. An interesting aspect of the modification is the interaction of water with the polyesterified wood since the relationship with moisture appears to be unique compared to other wood modification systems. This communication p...
G Beck, A Treu, E Larnøy


Studying amount, location and state of water in modified wood at moisture levels relevant for fungal degradation
2020 - IRG/WP 20-40889
Water is an essential parameter for fungal degradation of wood, but degradation primarily occurs at high moisture levels at water potential in the range of -4 to -0.1 MPa, which corresponds to 97-99.9% relative humidity. At these moisture levels, water is present in the wood structure both in and outside of cell walls. The majority of previous studies on the interaction between wood and water for ...
M Fredriksson, E Engelund Thybring, Ramunas Digaitis


Performance of a water-borne stain on beech, spruce, MDF and OSB improved by plasma pre-treatment
2020 - IRG/WP 20-40897
Coatings are an important part of wood protection, especially for outdoor applications. In order to provide a good protection, protective coatings need to exhibit good adhesion, mechanical resistance, and weathering resistance. Plasma pre-treatments are an established method to increase the performance of existing coatings including those on wood and wood-based substrates. Moreover, plasma deposit...
S Dahle, J Žigon, I Uranjek, M Petrič


Comprehensive protection of timber in seawater
2020 - IRG/WP 20-10970
The hazard of wood in seawater can be divided into two areas: Below the water level, shipworm (Teredo navalis) and gribble (Limnoria lignorum) can attack non-resistant or insufficiently protected wood; above the water level, there is a risk by wood-destroying fungi and, to a lesser extent, insects. In a national project funded by the Deutsche Bundesstiftung Umwelt (DBU, German Federal Environmenta...
E Melcher, J Müller, T Huckfeldt


Monitoring uptake and penetration of pesticides during impregnation of pine (Pinus sylvestris) and spruce (Picea abies) wood with bio-based microemulsion gel formulations
2020 - IRG/WP 20-30756
Even in dry state wood is susceptible to biological degradation. Preservation against biological decay in exposed conditions is conventionally achieved by impregnating the wood with pesticides applied at professional and industrial levels. Impregnation of wood with preservatives is a complex process that involves wood macro- and microstructure, and the physical characteristics of woods. Here we fo...
D Messaoudi, K Ruel, J-P Joseleau


Silicate coatings for wood substrates
2020 - IRG/WP 20-40906
Silicate coatings are surface finishing products containing alkali metal silicates or ethyl silicates as main binders. They are traditionally designed and well established for mineral substrates or corrosion protection of steel. The interest for these coatings in wood field is growing because of the benefits they could provide such as high durability, weathering resistance and fireproofing and sus...
A M Cheumani Yona, M Pavlič, M Petrič


Surface morphology and short-term water uptake of charred and coated wood
2021 - IRG/WP 21-40916
Charring of the wood surface represents a traditional alternative surface treatment technique with the purpose of aesthetics and protection. By the treatment with flame the surface of wood becomes carbonized and a few millimetres thick charred layer is formed on the top of the wooden element. Further, the charred layer can be removed by brushing, which accentuates the structure of the surface. Add...
J Zigon


Studies on the material resistance and moisture dynamics of Douglas fir and Sitka spruce from Slovenia
2021 - IRG/WP 21-20677
Wood in outdoor applications is subject to various decomposition factors. Wood degradation can be prevented by construction details, biocide protection of wood, wood modification, or selection of naturally durable wood species. Unfortunately, the majority of timber species in Europe do not have naturally durable wood. Imported tree species represent a new pool from which we can draw wood species w...
M Humar, B Lesar, D Krzisnik, E Kerzic, R Brus


Development of software to automate the quantification of the extent of penetration of treated wood
2021 - IRG/WP 21-20678
In Japan, Japanese Agricultural Standard (JAS) by the Ministry of Agriculture, Forestry and Fisheries and Approved Quality (AQ) by the Japan Housing and Wood Technology Center have established the penetration standard for treated wood. In our company, we measure the degree of penetration by either visual assessment or image processing. In the visual assessment, the degree of penetration is determi...
Y Susa, D Watanabe, T Shigeyama, Y Sugai


Preliminary investigation for preservation method of CLT using non-pressure treatment
2021 - IRG/WP 21-40919
Cross-laminated Timber (CLT) is increasingly being used in residential and non-residential construction around the world, and some of these areas are at high risk of biodeterioration. Addition to moisture management of construction, preservative treatment of CLT may be needed to prevent decay and termite attack in the area. Pressure treatment being most reliable, is not feasible due to the large d...
T Miyauchi, Y Ohashi, J Miyazaki, R Takanashi, H Shibui, S Isaji, T Shigeyama, Y Sugai, A Yamamoto, T Hramiishi, T Mori, H Matsunaga


Treatability of South African-grown Eucalyptus grandis with water-borne copper azole and disodium octaborate tetrahydrate wood preservatives
2021 - IRG/WP 21-40920
This study investigated the treatability of the sapwood and heartwood of sawn Eucalyptus grandis with copper-azole (CuAz) and disodium octaborate tetrahydrate (DOT) water-borne preservatives towards improving its durability for enhanced use in structural solid wood applications. The results obtained showed that, at a moisture content of 12 ± 1%, sawn E. grandis sapwood can be impregnated to a mea...
A A Alade, Z Naghizadeh, C B Wessels


Effect of a Water Repellent Treatment on Moisture Behavior of Three Australian Hardwoods: A Preliminary Report
2021 - IRG/WP 21-40921
Wood is inherently hygroscopic and will sorb moisture either directly from the atmosphere or via capillary action. Moisture can have marked effects on wood properties and repeated wetting and drying creates dimensional changes that lead to physical damage. Exposure to elevated moisture levels also increases the risk of fungal attack. Wood preservatives have long been used to minimize the risk of ...
B Hassan, J J Morrell, K Wood


Evaluation of weathering and termite resistance of the Myoung-oil as a Korean traditional coating agent
2022 - IRG/WP 22-10996
This study investigated the applicability of Myoung-oil (MO) as an eco-friendly preservative of Korean wooden cultural properties and buildings. Wood test specimens painted with various concentrations of MO were exposed in the external environment. Then color change and wettability of the wood surface were evaluated and compared depending on the exposure time. As a result of exposure for 12 months...
S-M Yoon, Y Park, W-S Jeon, H-M Lee, J-G Park, K Dal Nam, W-J Hwang


Properties of Iron (II) Sulphate treated Norway Spruce
2022 - IRG/WP 22-30765
Exterior wood is exposed to various environmental factors that cause weathering. Weathering is important primarily from an aesthetic standpoint. However, not all parts of the building are equally susceptible to weathering. Parts exposed to moisture will discolour faster than protected parts, such as wood under roof overhangs. To achieve fast and uniform artificial greying, a surface treatment with...
B Lesar, M Humar, M Škamlec


Field tests of different tropical wood species in sea water
2022 - IRG/WP 22-30773
A number of tropical timbers have been tested according to EN 275 at Kristineberg Marine Research Station in Sweden since 1999. Most of these tests have started during the last 5-8 years. Wood species included have been Lophira alata (Azobé/Ekki), Minquartia guianensis (Manwood/Acaria), Chlorocardium rodiei (Greenheart), Cyclodiscus gabonensis (Okan/Denya), Shorea spp. (Bankirai), Dicorynia guia...
M Westin, P Larsson Brelid


A novel wood preservation technology improving durability and water-related properties
2022 - IRG/WP 22-40926
A newly developed silicone oil (Archroma Management GmbH, Switzerland) was tested for wood modification purposes. Scots pine sapwood was treated with aqueous solutions of this silicone oil and showed a penetration of the modification agent into the wood cell wall. Both, biological durability and moisture-related properties, experienced significant improvements by the modification. Besides, the mod...
L Emmerich, H Militz, M Vila


The influence of thermal modification and surface charring to different levels on wettability of Norway spruce wood
2022 - IRG/WP 22-40942
The wood can alternatively be protected from water absorption by thermal modification and charring. Both techniques cause certain chemical and physical changes in the wood, the extent of which depends on the level of temperature applied. The objective of this study was to determine how the combination of charring to different levels and thermal modification affects the chemical, morphological, and...
J Žigon, C Gerardin, M E P Wålinder, P Gerardin


Synergized pyrethrins insecticide as a spot treatment option for West Indian drywood termites
2023 - IRG/WP 23-11004
Pyrethrin is a natural biopesticide with relatively low mammalian toxicity. Two identical products in Australia contain pyrethrin in liquid CO2-propelled aerosol, Pestigas from BOC international and SupaPy Supagas. In the current study, the toxicity of SupaPy was tested against West Indian drywood termite Cryptotermes brevis as an option for spot treatment of this pest. Termites were exposed to wo...
B Hassan, C J Fitzgerald


Assessment of the Material Durability and Structural Integrity of the Wooden Velodrome in Češča vas, Slovenia
2023 - IRG/WP 23-11012
Wood is a widely used material in the construction industry, and it has been utilized for thousands of years to create buildings and other structures. When wooden structures are designed, built, and maintained properly, they can be safe and long-lasting. Sports facilities, which provide athletes with a space to train, compete, and improve their abilities, are crucial in creating a strong and susta...
D Kržišnik, M Humar, B Lesar


Sensitivity of copper indicators for detecting preservative penetration
2023 - IRG/WP 23-20701
Chrome azurol S (CAS), 1-(2-pyridylazo)-2-naphthol (PAN), and rubeanic acid (RA) are the three copper indicators currently used by the timber industry to assess preservative penetration. Although only the American Wood Protection Association (AWPA) standards specify indicator sensitivity, it is unclear how those limits were developed. The sensitivity of each copper indicator was determined in solu...
T Yi, J Norton, S Meldrum, J J Morrell


Analytical retentions of active ingredients in H2F treated framing over a 12-year period
2023 - IRG/WP 23-20702
The H2F hazard class in Australia was developed to treat internal framing timber with a surface application of an insecticide, to control mainly termites. Two of the actives approved in AS 1604.1-2010 (and subsequent revisions) for this hazard class are bifenthrin and imidacloprid. The penetration zone of both actives is 0 – 2 mm from the wood surface. Radiata pine sapwood framing timber wa...
A Siraa


Establishing the minimum effective penetration of wood preservatives in the refractory heartwood of E. nitens
2023 - IRG/WP 23-30780
Conventional pressure treatment of many Australian hardwoods results in little to no penetration of heartwood and a non-uniform envelope treatment of <5 mm surrounding a mostly untreated core. This is a major issue for many of the low durability plantation hardwood timbers that are grown in Tasmania, which contain high percentages of heartwood. Long term studies on softwoods such as spruce decking...
J R Vargas, J J Morrell, L Yermán, K C Wood


Biological durability and wood-water interactions of sorbitol and citric acid modified wood – Effects on the expected service life
2023 - IRG/WP 23-40960
A high level of research activities on sorbitol and citric acid (SorCA) modified wood has been recognized in Europe over the last few years. As this treatment is close to entering an industrial-scale production, it is of interest to investigate how such treated wood performs upon long-term outdoor exposure. Hence, in this study Scots pine (Pinus sylvestris L.) sapwood was modified with aqueous sol...
K Kurkowiak, L Emmerich, H Militz


The appropriateness of central one-ninth or core retentions as a means of demonstrating penetration compliance
2023 - IRG/WP 23-40976
Treatment quality is in general terms dependent upon the preservative retention, and how the preservative is distributed throughout the cross-section of the treated article in question, i.e. the penetration of the preservative. Of these two fundamental qualities that are intrinsically linked to treatment quality, penetration is in general terms the most subjective. The determination of retention i...
D Humphfrey, B Skewes