The micro-distribution of copper/chrome/arsenate in Acer pseudoplatanus and Eucalyptus maculata
1973 - IRG/WP 319
The excellent field performance of copper-chrome-arsenate (CCA) treated timber has been accepted for many years. The preservative loadings used in practice have been based on field trial results, backed by service tests. The performance of treated hardwoods in trials and practice indicated that provided the required loading and penetration could be achieved the performance would be good. Recent un...
D J Dickinson


Moisture content of logs under sprinklers
2000 - IRG/WP 00-40157
Logs are kept under sprinklers during storage for avoiding the development of sapstain fungi. According to literature, sapstain fungi do not develop if the moisture content is above 120%. It is supposed that, the water sprinklers maintain the log's moisture content above this value, but, very often, sapstain is found on sawn lumber cut from these logs. Logs are harvested and transported t...
M C Rose, A M Briones, M Fernández


The future for chromium in wood preservation
1985 - IRG/WP 3332
Most water-borne preservatives contain CrVI compounds, originally to reduce corrosion although now also to improve toxicant fixation. Chromium contributes to preservation and this is recognised in, for example, New Zealand and USA where chromium contents are included in calculations of overall preservative activity of CCA formulations, but chromium may also have anti-stain and joinery (millwork) p...
B A Richardson, T R G Cox


A substantively bonded water repellent treatment based on chromium carboxylates
1985 - IRG/WP 3344
Chromium carboxylates soluble in toluene have been synthesised and applied to Scots pine (Pinus sylvestris) sapwood. Without any further treatment, the compounds may be readily leached from wood surfaces with toluene. After a period of heating however, they become fixed to the cell wall, substantial amounts being resistant to leaching even under reflux conditions for several hours. Treatment of wo...
J K Wright, W B Banks, W J Eilbeck


A field trial to assess the potential of antisapstain chemicals for long-term protection of sawn radiata pine
1986 - IRG/WP 3375
Seven chemical formulations were tested as antisapstain treatments for freshly sawn radiata pine sapwood (90x50 mm²). Each formulation was used with and without a water-repellent additive and was sprayed on to 1 m long boards. The boards were then stacked into "mini" packets and stored unprotected from the weather for 6 months. Haipen 50w (at 0.2 or 0.4% active) and NaPCP (1% active) plus 1.5% bo...
J A Drysdale


Prevention of sapstain in logs using water barriers
1997 - IRG/WP 97-30147
Placing logs in ponds or under water sprinklers to keep moisture levels high enough to prevent oxygen tensions rising above inhibitory levels, is a proven method of preventing sapstain. The objective of this experiment was to determine if water barriers significantly reduce the rate of sapstain penetration into logs by maintaining moisture contents, and consequently oxygen tensions, at inhibitory ...
R N Wakeling, D R Eden, C M Chittenden, B Carpenter, I Dorset, J Wakeman, R Kuluz


Leaching of components from CCF treated timber in ground contact
1998 - IRG/WP 98-50108
In order to investigate the depletion of different CCF-salts during service small stakes (10*10*450mm³) were treated with five water-borne wood preservatives and after fixation brought into ground contact for several years. After failing some of the broken down stakes were used to determine the remaining concentration of relevant ions and their distribution in different segments of the stakes. A...
E Melcher


Water transfer in wood in relation to fungal attack in building - Effect of condensation and diffusion
1992 - IRG/WP 92-1543
Wood is continuously exchanging moisture with the surrounding atmosphere, the temperature and relative humidity are important factors. Wood moisture in this case is not enough to provoque decay by fungi. However, when, during the night, condensation appears cyclically, wood absorbs water and moisture content may be sufficiently high to allow development if drying does not take place. The water tra...
D Dirol, J-M Vergnaud


A study of methanogenesis and sulphate-reduction: A possible source of explosive gas mixtures in a gold mine
1989 - IRG/WP 1399
Previous work isolated anaerobic bacteria from timbers and drainage water in a gold mine. The present work identifies the predominant methanogen in the mine ecosystem as Methanobacterium bryantii and sulphate-reducing isolates as Desulphovibrio desulphuricans and Desulphotomaculum antarcticum. Laboratory studies using model systems evaluate the activity of methanogenic and sulphate-reducing bacter...
L D Abraham, J F Putterill, A A W Baecker


Wood cement composites using spent CCA treated wood
1999 - IRG/WP 99-50126
The feasibility of using spent or out-of-service CCA treated wood as a component of wood/cement composites was evaluated. Cold pressed wood particle cement boards were made using CCA treated particles from a red pine (Pinus resinosa Ait.) pole removed from service and from untreated red pine wood from a new pole. Boards were manufactured using a range of wood to cement ratios and water to cement r...
Chen Huang, P A Cooper


A novel method for evaluating the performance of water repellents
1987 - IRG/WP 2279
Application of water repellent formulations to timber surfaces offers protection from the weather, reducing degrade and movement. A novel test method has been developed to evaluate the comparative efficacy of such formulations when samples are exposed to weather. The method uses sapstain free sapwood of defect free, untreated, seasoned Radiata pine, (Pinus radiata D. Don.) Water Repellency was det...
A R Moffat


Fixation of chromated wood preservatives through technical drying
1990 - IRG/WP 3623
Twin samples of sawn timber of Pinus sylvestris and Picea sp. were treated with copper-chromate-containing wood preservatives and subsequently kiln resp. air dried. After drying, the distribution of preservative and rate of fixation were determined. Drying of freshly treated wood in a condenser type kiln at temperatures of 60°C and 80°C and in a vacuum type kiln at 55°C with a pressure of about...
R-D Peek, H Klipp


Experimental variations in the distribution of CCA preservative in lignin and holocellulose as a function of treating conditions (temperature, concentration, pH, species, and time)
1984 - IRG/WP 3277
The exact distributions between lignin and holocellulose and retentions on wood of copper, chromium and arsenic as a function of various sets of conditions in a 3x3x4x2 factorial experiment in which combinations of three temperatures of treatment, three CCA solution concentrations, four pH's of the initial CCA solution and two timber species, namely Pinus radiata and Eucalyptus grandis, a...
A Pizzi, E Orovan, M Singmin, A Jansen, M C Vogel


The potential of high pressure pulsation processes to treat white spruce lumber with water-borne preservatives
1988 - IRG/WP 3471
Laboratory work using end sealed 4x8x46 cm³ white spruce samples has been done to explore the suitability of three variants of a 2.1 MPa pulsation process for the impregnation of white spruce with CCA. The results showed that the process improved significantly the penetration of the preservatives and reduced significantly cell collapse, when compared with the results of treatment using a 2.1 MPa ...
J P Hösli, J N R Ruddick


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 17: Report of fifth inspection (4 years) in Italy
1983 - IRG/WP 4103
The wood samples of Alstonia scholaris, Fagus sylvatica, Pinus sylvestris were submerged in the sea at Follonica, Italy, in April 1977. Follonica, latitude 42°55' North and longitude 10°45' East, is situated on the Tyrrhenian coast. The recorded temperature varies from 13°C to 25°C, salinity 37-38% and pH about 8. The inspections were carried out after 6 months (10/1977), 12 ...
A Gambetta, E Orlandi


Soft rot in heartwood of preservative-treated pole stubs of Eucalyptus cypellocarpa L. Johnson
1983 - IRG/WP 1204
Pole stubs of Eucalyptus cypellocarpa L. Johnson, treated in the sapwood with certain waterborne preservatives and exposed for 21 to 23 years in a dry tropical region were severely soft-rotted in the heartwood, as well as the sapwood. They broke with a brash fracture when stress tested (loaded as a cantilever) in the field. The severe soft rot in the heartwood was not detected by the knife test or...
J E Barnacle, G C Johnson, M A Tighe


Interactions between soft rot fungi and CCA preservatives in Betula verrucosa
1988 - IRG/WP 1367
Ultrastructural investigations were carried out to obtain information on the cell wall distribution of CCA elements during soft rot decay of 4% K33 CCA preservative treated birch (Betula verrucosa) wood. TEM observations on fibres at various stages of S2 cavity formation by mutabilis showed a distinct pattern of electron dense materials to occur within the S2 cell wall region. These materials (gra...
G F Daniel, T Nilsson


Note and literature survey on the "Eucalyptus borer" Phoracantha semipunctata F. (Col.; Cerambycidae), a pest in between forest and wood
1984 - IRG/WP 1228
In the Eucalyptus-forests of Huelva, Spain, Phoracantha semipunctata appears as a severe forest-pest fatal to trees impaired by drought. The population snowballed in two and a half years, millions of larvae reduce the value of wood to "papermill-quality''. One of the intentions of the paper is to collect knowledge for help and cure. A literature survey forms the main part of the ...
S Cymorek


Factors affecting the resistance of fibre building boards to fungal attack
1975 - IRG/WP 252
Fungal decay is initiated at lower moisture contents in standard and tempered hardboards (18%) than in pine sapwood (26%). In contrast, in a saturated atmosphere, the equilibrium moisture contents of standard hardboard (14%) and of tempered hardboard (12.5%) are much lower than the moisture content permitting decay initiation whilst the equilibrium moisture content of pine sapwood (25.1%) approach...
C Grant, J G Savory


Effects of hard water, sea water and humic acid on the release of CCA components from treated wood
2005 - IRG/WP 05-50228
Leaching medium is an important factor affecting release of preservative components from treated wood because physical and chemical characteristics of medium increase or decrease the solubility of fixed preservative components. This study evaluated the leaching properties of copper, chromium and arsenic elements from chromated copper arsenate (CCA)-treated wood specimens subjected to laboratory le...
S N Kartal, W J Hwang, Y Imamura


The resistance of wood coated with different water-borne paints against colonisation by decay fungi
1996 - IRG/WP 96-10165
The susceptibility of wood painted with model paints of known composition to decay fungi was tested without previous weathering. Included in the study were five alkyd emulsion paints and five acrylic paints; one linseed oil paint and two solvent-borne alkyd paints. It was found that several components influenced the susceptibility of these paints. The results of the present study indicate that the...
J Bjurman


A questionnaire survey to establish the perceptions of UK specifiers concerning the key material attributes of timer for use in marine and fresh water engineering
2004 - IRG/WP 04-10519
Engineers have a key role in making informed decisions on the type of materials to be used in the schemes they design and construct. Currently, in England and Wales, it is believed that some £500m per year is invested in flood and coastal defence engineering. There is a lack of centralised data in the UK holding information on timber for usage in fluvial and, particularly coastal engineering. A...
J R Williams, G S Sawyer, S M Cragg, J Simm


A field evaluation of chromated fluoride as a remedial treatment for creosoted wooden distribution poles
1989 - IRG/WP 3556
A commercial chromated fluoride formulation was applied by injection process to previously inoculated creosoted wooden distribution pole sections at a field site in Scotland and appraisal of the efficacy of the formulation against Lentinus lepideus was undertaken at two month and fifteen month intervals. Preliminary results suggest a rapid elimination of organisms from colonised areas. The usage o...
B King, A Bruce


Detection of termite attack in wood using acoustic emission
1989 - IRG/WP 2331
Acoustic emission (AE) is the elastic wave produced by the strain energy released in the process of fracture of a material and propagates through it. The object of this report is to detect AEs produced by the termite activities and to evaluate the possibility of using an AE monitoring test to nondestructively detect the termite attack in wood. It was revealed that AEs were detected from the specim...
Y Fujii, M Noguchi, Y Imamura, M Tokoro


Alkyl dimethyl benzyl ammonium chloride: toxicity to Coniophora puteana when formulated in water and organic solvent
1986 - IRG/WP 2250
Results from agar block tests using Coniophora puteana demonstrate that the biological activity of alkyl dimethyl benzyl ammonium chloride is affected by the nature of the carrier solvent in which it is applied. In contrast to some earlier work, an alkyl ammonium compound in organic solvent formulation was identified that had significantly greater activity than its aqueous equivalent. A simple sol...
D P Blow