IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 828 documents. Displaying 25 entries per page.


Effects of Borax and Boric Acid as Fire Retardants on the Resistance of Pterygota macrocarpa Wood to Fire Tests
2022 - IRG/WP 22-30770
The combustible nature of wood as a building material, when exposed to hazards of fire underscores the reason for fire retardant treatments. Pterygota macrocarpa wood is commonly used by builders in Nigeria for roof and other structural applications. Therefore, this study was carried out to assess the effect of Borax and Boric acid on the fire-retardant properties of P. macrocarpa wood. Wood sampl...
J M Owoyemi, O Apogbona, T O Akinwamide


Field tests of different tropical wood species in sea water
2022 - IRG/WP 22-30773
A number of tropical timbers have been tested according to EN 275 at Kristineberg Marine Research Station in Sweden since 1999. Most of these tests have started during the last 5-8 years. Wood species included have been Lophira alata (Azobé/Ekki), Minquartia guianensis (Manwood/Acaria), Chlorocardium rodiei (Greenheart), Cyclodiscus gabonensis (Okan/Denya), Shorea spp. (Bankirai), Dicorynia guia...
M Westin, P Larsson Brelid


A novel wood preservation technology improving durability and water-related properties
2022 - IRG/WP 22-40926
A newly developed silicone oil (Archroma Management GmbH, Switzerland) was tested for wood modification purposes. Scots pine sapwood was treated with aqueous solutions of this silicone oil and showed a penetration of the modification agent into the wood cell wall. Both, biological durability and moisture-related properties, experienced significant improvements by the modification. Besides, the mod...
L Emmerich, H Militz, M Vila


Environmentally Friendly Wood Modification based on Tannin-Furfuryl alcohol - Effect on stabilisation, mechanical properties and decay durability
2022 - IRG/WP 22-40929
Furfurylation is a well-known wood modification technology. This paper studied the effect of tannin addition on the wood furfurylation. Three kinds of dicarboxylic acids, adipic acid, succinic acid, and tartaric acid, as well as glyoxal as a comparing agent, were used to catalyse the polymerisation of furanic or tannin-furanic solutions during wood modification. Impregnation of furanic or tannin-f...
M Mubarok, E Azadeh, F O Akong, S Dumarçay, A Pizzi, C Charbonnier-Gérardin, P Gérardin


Steam Pre-conditioning Treatment Prior to Acetylation: Impact on Dimensional Stability, Moisture Response Behaviour, and White-Rot Fungal Resistance of Hevea brasiliensis and Mitragyna ciliata Wood
2022 - IRG/WP 22-40930
The effect of steam pre-conditioning treatment on the dimensional stability, moisture response behaviour, and durability against white-rot fungus P. chrysosporium of acetylated Hevea brasiliensis and Mitragyna ciliata wood species were assessed. Defect-free specimens of both species from the top, middle, and base positions were selected, prepared according to ASTM D143-09 & ASTM D-2017 standards a...
E Uchechukwu Opara, J Mayowa Owoyemi, J Adeola Fuwape


The influence of thermal modification and surface charring to different levels on wettability of Norway spruce wood
2022 - IRG/WP 22-40942
The wood can alternatively be protected from water absorption by thermal modification and charring. Both techniques cause certain chemical and physical changes in the wood, the extent of which depends on the level of temperature applied. The objective of this study was to determine how the combination of charring to different levels and thermal modification affects the chemical, morphological, and...
J Žigon, C Gerardin, M E P Wålinder, P Gerardin


The Resistance of Some Commercially Thermally Modified American Hardwoods to Termites and Fungi
2022 - IRG/WP 22-40944
Thermally Modified Wood (TMW) is now being produced in the United States but there are few data on the durability of these materials. In this study, commercially-produced thermally modified yellow poplar (Liriodendron tulipifera), red maple (Acer rubrum), and white ash (Fraxinus americana) were evaluated for fungal and termite resistance. The resistance of the three TMW species against Gloeophyllu...
B Cortes, B Bond, A Taylor, J Lloyd


Effect of densification of Eucalyptus nitens and E. obliqua on moisture uptake, swelling, decay resistance, and fire performance
2022 - IRG/WP 22-40946
Some Australian Eucalyptus species that are abundantly available have low natural durability and poor resistance to fire. These same species are also extremely difficult to treat with preservatives or fire retardants using conventional pressure treatment methods due to a large proportion of refractory heartwood. The aim of this research was to understand whether thermo-mechanical densification had...
B Hassan, J J Morrell, F Wiesner, W Wu, B Belleville, K C Wood


Phenol formaldehyde modification and termite resistance under laboratory testing
2022 - IRG/WP 22-40952
The development of phenol formaldehyde (PF) resins as a means of impregnating solid wood is one that has been explored for several decades, both in terms of conventional impregnation processing (Impreg) or compressional impregnation (Compreg). However, it is only recently with advances in processing conditions that the method truly affords a means of achieving conventional modification for solid t...
L Nunes, A Pitman, M Duarte, B Stefanowski, D Jones


Evaluation of Decay Resistance for the Larch Wood Heat-treated with Superheated Steam
2022 - IRG/WP 22-40956
Heat-treatment of wood is a process that involves applying heat ranging 160–260°C to improve its physico-mechanical properties and resistance against wood rot fungi. The level of the changes in the wood properties by heat-treatment differs depending on the temperature and duration of heat-treatment, as well as the types of heat transfer media used for heat-treatment. The heat-treatment on wood ...
Y Park, S-M Yoon, H Kim, W-J Hwang


A novel method for assessing radial variation in termite resistance of timber
2023 - IRG/WP 23-11005
Australia has many timbers whose heartwood is highly resistant to fungal and termite attack; however, changing public policies have resulted in restricted access to many native forests where these species are found. Plantations of these same species are expected to replace these resources, but there are questions concerning whether timber from these trees will have the same resistance as the nati...
S Kleinschmidt, R McGavin


Biological durability and wood-water interactions of sorbitol and citric acid modified wood – Effects on the expected service life
2023 - IRG/WP 23-40960
A high level of research activities on sorbitol and citric acid (SorCA) modified wood has been recognized in Europe over the last few years. As this treatment is close to entering an industrial-scale production, it is of interest to investigate how such treated wood performs upon long-term outdoor exposure. Hence, in this study Scots pine (Pinus sylvestris L.) sapwood was modified with aqueous sol...
K Kurkowiak, L Emmerich, H Militz


Resistance of phenol formaldehyde impregnated beech (Fagus sylvativa L.) LVL against biodegradation in soil contact
2023 - IRG/WP 23-40965
Alternatives to preservative impregnation are emphasized in Germany and other European countries. Even though these treatments significantly improve wood's resistance to decay, they often do not have a beneficial impact on the dimensional stability. One alternative product, which may be used in ground contact for items like poles and railway sleepers, could be beech (Fagus sylvatica L.) laminated ...
M Slabohm, C Brischke, S Bicke, H Militz


New wood-modification process based on grafted urethane groups: Durability of carbamamylated Scots pine (Pinus sylvestris L.) wood
2023 - IRG/WP 23-40974
Substituting commonly used toxic preservatives with wood modification treatments can make the wood material less prone to water and moisture uptake. This approach favours a more sustainable protection of wood against biodegradation. In this study, Scots pine sapwood was full-cell impregnated with an aqueous solution of urea (30%), dried at 40°C for 24h, and subsequently heat-treated at 150°C for...
C-F Lin, O Myronycheva, O Karlsson, D Jones, D Sandberg


Short-term absorption of water and coatings on thermally modified blue-stained spruce wood
2023 - IRG/WP 23-40984
The importance of wood has been increasing in the last decades. Among conifers, predominantly spruce (Picea abies) wood is often used in building constructions in Europe. Namely for construction and facades of buildings, decking and fences. Due to the increased public concerns about biocides, alternative techniques for protection, such as thermal modification and protection by construction, are ga...
R Hasanagic, M Bahmani, M Humar, L Fathi, L Cai


Evaluation of the effectiveness of soaking of high-temperature plywood in low-temperature oil-based wood
2023 - IRG/WP 23-40991
We conducted a preliminary investigation to determine if soaking high-temperature plywood in a low-temperature preservative solution could achieve deeper penetration of the preservative, even in plywood made with refractory wood species such as Japanese larch. Specimens cut from commercial plywood (Japanese larch) were stored at various temperatures before being soaked in the preservative solution...
T Miyauchi, S Isaji, H Shibui, N Furuta, J Miyazaki, H Matusnaga


Characterization of cell wall morphology and water-soluble extractives in Japanese larch decayed by white-pocket-rot fungi
2024 - IRG/WP 24-11034
Porodaedalea chrysoloma (Fr.) Fiasson & Niemelä is a basidiomycete that can cause white-rot decay in Japanese larch (Larix kaempferi) heartwood. P. chrysoloma is a white-rot fungus with a unique pattern that causes white-pocket-rot in the xylem of Japanese larch. However, the mechanism by which P. chrysoloma yields the pattern of white-pocket-rot in Japanese larch heartwood remains unclear. Thus,...
Y Mori, H Arai, T Ito, H Hashitani, K Yamashita, Y Ota, M Kiguchi


Do naturally sequestered biocidal metals contribute to the marine borer resistance of turpentine?
2024 - IRG/WP 24-11036
Turpentine wood is renowned for its resistance to attack by molluscan marine borers. This resistance is thought to be due to its high silica content, and possibly the presence of other, as yet unknown, compounds. Silica in turpentine wood is present as particles in rays, but in many plant species silica also occurs in cell walls. We hypothesized that Si is present in cell walls of turpentine, but ...
P D Evans, H Matsunaga, D Feng, M Turner, C Kewish


Enhancing UV resistance and decay resistance of wood by nanoparticle dispersed linseed oil nanoemulsion
2024 - IRG/WP 24-20706
Enhancing increasing demand for eco-friendly and cost-effective wood coatings and preservatives has led to the development of water-borne formulations and use of non-toxic and natural materials such as vegetable oils and waxes. The aim of this study was to improve the UV resistance and decay resistance of wood by nanomaterial dispersed linseed oil emulsions. Highly stable nanoemulsions of linseed ...
R Bansal, R Kumar, K K Pandey


Influence of the substitution of phenol with lignin cleavage products in phenol-formaldehyde impregnation resins for wood modification on the fungal decay resistance and impregnation depth
2024 - IRG/WP 24-30805
The impregnation modification of wood with phenol-formaldehyde (PF) resins increases the woods dimensional stability and resistance against fungal decay. However, to decrease the usage of non-renewable resources, the substitution of phenol has been a topic of scientific interest. Lignin is a currently underutilized resource with a chemical structure that contains phenolic units. For adhesive appli...
J Karthäuser, L Tarentino, A Treu, H Militz, G Alfredsen


A novel treatment for increasing UV stabuility of wood based on citric acid and urea
2024 - IRG/WP 24-30811
Wood, a fundamental material in the Built Environment, faces challenges related to durability and weathering, notably UV degradation leading to colour changes. This study explored a novel treatment method utilising citric acid and urea to enhance the UV stability of wood. The reaction between these compounds forms fluorescent species and insoluble nanoparticles upon thermal treatment. Two treatmen...
S Jué, A Scharf, C-F Lin, R Moutou Pitti, D Sandberg, D Jones


International joint field trial on the moisture performance of wood – Set up and first results
2024 - IRG/WP 24-40996
Wood durability to decay stems from its inherent resistance to fungi resistance to fungi. In this regard, wood's ability to withstand moisture uptake plays an important role as the lower threshold for wood decay is a moisture content of 25%. However, the aspect of moisture resistance is not yet sufficiently emphasized as a durability factor, both in the assessment of durability as a material prope...
C Brischke, et al. (33 co-authors)


Evaluation of the water exclusion ability and inherent bioactivity of heartwood against decay in Japanese and European wood species via above-ground exposure and water absorption tests
2024 - IRG/WP 24-40998
The natural durability of wood has been thought to mainly depend on bioactive extractives and the water exclusion ability. To clarify the contribution of each factor to wood durability, above-ground exposure tests were conducted on Japanese and European wood species. A double-layer test was carried out using heartwood specimens of four wood species, i.e., Japanese cedar, Japanese cypress, Scots pi...
T Osawa, R Noda, K Yamamoto


Outdoor termite resistance performance of zinc borate (Borogard® ZB) treated parallel strand lumber (PSL) – 15 years field test results
2024 - IRG/WP 24-40999
This report discloses the outdoor termite resistance performance of PSL samples treated with zinc borate at a dosage of 0.85% BAE and 1.72% BAE in Wuxi, China. The outdoor field trial lasted for 15 years and observations were made after 6 months, 3 years, 5 years 1 month, 6 years 6 months and 15 years. The retaining rates of B2O3 and ZnO in the final samples were also tested, and the hypothesis wa...
S Shi, E Laval, K Lung, F Ascherl, R Williams, W Li, X Li


Durability of Malaysian plybamboo to mold
2024 - IRG/WP 24-41014
Durability of 3-layer plybamboo fabricated from two Malaysian bamboo species, Gigantochloa levis (beting) and Gigantochloa scortechinii (semantan) using three different adhesives - urea formaldehyde (UF), melamine urea formaldehyde (MUF) and phenol resorcinal formaldehyde (PRF) was evaluated in this study. Samples were exposed to the mold, Aspergillus brasiliensis for 4-week following the ASTM D44...
S Lipeh, A Mustapha, A S Yusoh, M K A Uyup


Previous Page | Next Page