Above ground testing at tropical test sites, what have we learned?
2011 - IRG/WP 11-20473
Three different above ground test methods have been utilized at a selection of five tropical and sub-tropical test sites with a variety of treated and untreated material. The results show that a multi-site approach to above ground field tests presents the opportunity for exposure to un-predicted biodeterioration hazards, which may be important for developmental products of poorly characterized fu...
A Preston, A Zahora, Y Cabrera, L Jin, C Schauwecker, P Walcheski


A comparative study and evaluation of methodologies used for determining wood preservative penetration
2011 - IRG/WP 11-20475
A series of methods for determining penetration of wood preservatives into the wood structure have been developed for either quality control (QC) or research and development purposes. QC methods range from monitoring the solution uptake, applying colour indicators or sampling specific wood samples followed by wood acid digestion/atomic absorption spectroscopy (AAS) or solvent extraction/chromatogr...
R Craciun, R Moeller, J Wittenzellner, T Jakob, J Habicht


The durability of acetylated radiata pine sapwood (Accoya). Results from five years testing
2011 - IRG/WP 11-30560
New Zealand grown radiata pine sapwood was modified using the Accsys PLC acetylation process (Accoya). Following treatment, various test samples were exposed in the Scion Accelerated Field Test facility (Fungus Cellar) and in exterior ground contact field tests. In the Fungus Cellar, performance was compared with that of radiata pine treated with CCA to Hazard Classes H3.2 (0.37% m/m Cu+Cr+As) and...
M Hedley, D Page, J van der Waals, K Nasheri, G Durbin


Novel Approaches to the Development and Testing of Anti After-glow Additives for CCA-based Treatments of Poles
2011 - IRG/WP 11-30561
In this paper, a field fire stake testing screen method is described. This method uses stake samples from matched wood sources allowing replicates from different boards to be included. The method is easy to control and can provide quick comparative fire resistance test results. The parameters measured from the tests are percentage weight loss, minimum residual circumference and residual thicknes...
L Jin, P Walcheski, A Preston


Comparison of rates of wood decay from four different field test protocols following 4-5 years exposure at a site in New Zealand
2011 - IRG/WP 11-30565
The rate of decay of Pinus radiata was evaluated using four different field test protocols at a site near New Plymouth, New Zealand. The average Scheffer index was 86 over the five year period of testing. The field tests were an in-ground stake test (AWPA Std E7-01) and three above ground tests – lap-joint (AWPA Std E16-98), decking (AWPC protocol) and ground proximity tests (AWPA Std E18-06) T...
P Lobb, K Day, A Siraa


Challenges and new developments in testing electro osmotic pulsing technology (PLEOT) by means of conventional laboratory methods
2011 - IRG/WP 11-40555
A new wood protection system, electro-osmotic pulsing technology, called PLEOT, is tested in lab trials using different test setup. The technology is tested on Scots pine sapwood and beech wood samples exposed to brown- and white rot fungi. Mass loss and moisture content is calculated after testing and a chitin analysis are performed on the sample powder. Two different electrodes are used in ord...
A Treu, E Larnøy


Durability of modified wood in UC3 and UC4. Results from lab tests and 5 years testing in 3 fields
2011 - IRG/WP 11-40562
In 2005 an extensive test program including field tests was set up in order to obtain more data on the durability and long term performance of modified wood and semi-durable wood species. One of the main challenges for modified wood is to predict accurate service life time in UC3 (use class 3, above ground) and UC4 (use class 4, in soil or fresh water contact). So far, data from in-service condi...
M Westin, G Alfredsen


Extractives in Norwegian-Grown and North American-Grown Western Redcedar and Their Relation to Durability
2012 - IRG/WP 12-10762
The extractives responsible for the natural durability of western redcedar (WRC) are not well understood. Recent work by the Norwegian Institute of Wood Technology and the Norwegian Forest and Landscape Institute has evaluated the natural durability of Norwegian wood species and reference species, including Norwegian-grown WRC and North American-grown WRC, in a series of decay tests. The availabil...
R Stirling, P O Flæte, G Alfredsen, P I Morris


Above Ground Field Evaluation and GC-MS Analysis of Naturally Durable Wood Species
2012 - IRG/WP 12-10764
Nine wood species are being evaluated in above ground field studies in Mississippi and Wisconsin. Candidate naturally durable wood (NDW) species are being rated at yearly intervals for resistance to decay, cupping, and checking. Field ratings after 12 months exposure are presented. To date, Paulownia tomentosa (PAW) and southern yellow pine (SYP) are least durable and cedars are the most durable i...
G T Kirker, A B Blodgett, S T Lebow, C A Clausen


Use of the durable species Coast Redwood as a reference system for field testing of Wood Protection systems
2012 - IRG/WP 12-20486
Data is provided and discussed for a number of field exposure tests where the naturally durable wood species Coast redwood, Sequoia sempervirens, was included along with untreated pine and standard preservative treatments. In general, there is potential for higher variability of results with this naturally durable species, but it does suggest that redwood can be a useful reference material for te...
A Zahora, A Preston, L Jin


Evaluation of fungal infestation and decay in a simulated use class 3 situation (block test) after some years of exposure
2012 - IRG/WP 12-20487
The so named “block test” was designed as part of the assessment methodology for testing the behaviour of natural and modified wood used under use class 3 (EN 335-2) conditions. The test was developed to expose the wood close to the ground to an environment with high humidity and high biological activity, but not in soil contact. The present study describes the evaluation of fungal infestatio...
A Gellerich, K Röhl, S Adamopoulos, H Militz


Moisture performance based wood durability testing
2012 - IRG/WP 12-20495
In the frame of a scientific cooperation within the Swedish research program ‘WoodBuild’ comparative field and laboratory durability studies have been carried out by the Technical Research Institute of Sweden SP and Leibniz University Hannover. One objective was to improve test methods as well as evaluation systems in order to facilitate the use of (field) testing for service life prediction. ...
L Meyer, C Brischke, A Pilgård


Performance of Wood Protection Systems at Multiple Field Test Sites Using the Ground Proximity Test Method
2012 - IRG/WP 12-20499
A series of preservative systems were used to treat southern pine ground proximity test samples which were then exposed at a range of test sites located throughout the world. The sites were chosen on the basis of having vastly different Scheffer Climate decay indices. After almost 14 years exposure, distinct differences are apparent in how different preservative systems perform at the different ...
A Zahora, A Preston, L Jin


Testing service life for use class 3: accelerated L-joint performance of commodities
2012 - IRG/WP 12-20500
Above ground testing is considered important for the assessment of treated wood intended for use class 3. Laboratory testing of efficacy of biocides as well as of natural durability focussing on such applications has to be linked to performance and service life. An accelerated L-joint test was some 15 years ago developed at the Ghent University to allow worst case assessment under semi-controlled ...
J Van Acker, J Van den Bulcke, I De Windt, L De Vetter


Field-testing of Norway Spruce Claddings with Monitoring of Moisture Content, Material Temperature and Microclimate
2012 - IRG/WP 12-20502
The physical function of a cladding is to protect the interior construction. Under normal circumstances the performance requirements can be met for a very long time, meaning that the technical service life of a wooden cladding can be very long. Since the cladding is a major part of the facade, it also has visual requirements that may define the aesthetic service life, and often it is much shorter ...
G I Vestøl, L Ross Gobakken


Statistical analysis of durability tests - Part 1: Principles of distribution fitting and application on laboratory tests
2013 - IRG/WP 13-20504
Service life prediction is an important topic in wood research, especially with regard to the Construction Products Regulation (CPR). Both laboratory tests as well as in-service performance testing are therefore essential in combination with proper monitoring and analysis tools. A crucial concept is variability in testing and analysis, especially for a biological material such as wood. The larger ...
I De Windt, J Van den Bulcke, C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar,


Quasi-in-situ durability tests on oak timber bridges
2013 - IRG/WP 13-20510
This study aims on developing a method for determination of wood durability on samples taken from real structures in service. Therefore quasi-in-situ durability tests have been conducted exemplarily on timber bridges made from English oak (Quercus robur L.). Drilling cores were found to be a feasible alternative to standard specimens for laboratory durability tests against pure cultures of Basidio...
C Brischke, C J Behnen, M-T Lenz, K Brandt, E Melcher


Statistical analysis of durability tests - Part 2: Principles of time-to-failure and application on field test data
2013 - IRG/WP 13-20512
Service life prediction is an important topic in wood research, especially with regard to the Construction Products Regulation (CPR). Both laboratory tests as well as in-service performance testing is therefore essential, in combination with proper monitoring and analysis tools. A crucial concept is variability and the incorporation of variability in tests and analysis. In this paper we focus on t...
J Van den Bulcke, I De Windt, C Brischke, C R Welzbacher, A O Rapp, J Van Acker


Testing the performance of timber using 27 different field test methods
2013 - IRG/WP 13-20517
Numerous test methods to determine the durability of timber and timber products have been described in relevant literature. However, only some of these methods have been standardized and thus only very few are regularly used for resistance tests in the field. Since results from extensive comparative field studies have shown differences in moisture performance between different test methods, the ai...
L Meyer, C Brischke, J Rieken


Image analysis for mould and sapstain detection on wood
2013 - IRG/WP 13-20519
Laboratory tests for mould growth on wood products are time consuming and rely on visual assessments of specimens utilizing subjective rating systems. Accelerated laboratory methods are needed that can provide rapid, quantitative assessment of mould and sapstain growth on solid and composite wood products. Image analysis of scanned spore imprints from southern pine or oriented strandboard (OSB) sp...
C A Clausen, V W Yang


Accelerated H3 above-ground decay testing
2013 - IRG/WP 13-20520
An above-ground H3 fungal field trial was installed at two sites in Australia and one in New Zealand, as well as in two Accelerated Field Simulators. The aim was to find a method that would shorten the time required for evaluating new preservatives and protection systems. One-quarter H3 retentions were installed, as first results suitable for registration occur when these reach 70% soundness. Twel...
L J Cookson, D Page, T Singh


Visual Inspection – How Important is the Influence of the Evaluator?
2013 - IRG/WP 13-20521
Visual inspection is often a crucial means of judging the efficacy and performance of a preservative. It is used in non-destructive testing in long term exposure trials or simply, when the practical use and precision of the human eye is a good means of measure. As for the procedure described in EN 252, the impression of softness due to decay of the wood has also to be considered. Although, a thumb...
M Klamer, P Larsson Brelid, I Stephan


Predicting the Rate of Decay, and the Potential for Misinterpretation of Proper Scientific Method
2013 - IRG/WP 13-20525
Predicting the rate of fungal attack in wood-based materials and its effect on properties remains the holy grail of wood products pathologists; however, achieving this goal is difficult because of the many variables associated with the process. This paper reviews some of the more important aspects of the decay process in relation to test methodology and then discusses how data are sometimes used b...
B S Goodell, J J Morrell


Micronized Copper Wood Preservatives: Strong Indications of the Reservoir Effect
2013 - IRG/WP 13-30609
Micronized copper wood preservative systems were launched commercially in May 2006. Now, over 75% of the residential lumber produced in the USA is treated with micronized wood preservative formulations. Although considered controversial at first, the mode of action of micronized copper has been clearly defined by multiple authors over the years, as well as a need for a co-biocide in water-borne sy...
M H Freeman, C R McIntyre


Performance testing of DMDHEU-modified wood in Australia
2013 - IRG/WP 13-30613
Chemical wood modification with dimethyloldihydroxy-ethyleneurea (DMDHEU) or its derivatives has been researched for many years and shown to be applicable to improve certain wood properties to both solid lumber and wood-based composites. Earlier research proved a high biological resistance of DMDHEU-modified wood against biological degradation in laboratory and field tests in Europe. Due to the ve...
H Militz, J Norton