IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 49 documents. Displaying 25 entries per page.


Status of wood preservation industry in India
2005 - IRG/WP 05-30388
The paper traces the history of wood preservation industry in India, listing various mile stones for creation of treating capacity. The preservation industry developed with the development of rail road system on the line of most other developed countries. The most popular wood preservatives are CCA, CCB, ACC, Creosote and recently LOSP have also appeared in the market. The major users of CCA is th...
S Kumar


Manual of a mini treating plant for waterborne preservative treatment of timber and bamboo
1999 - IRG/WP 99-40130
This contributional article includes machinaries and equipments necessary for a small wood treating plant for the pressure treatment of tim bers with waterborne preservatives along with the cost and design. The preservative treatment limitations, treatment schedules and specifications for different products have been described. The cost of a mini treating plant will be 6,00,000 Tk. (13,000 US$), s...
A K Lahiry


Collaborative soft rot tests: Programme and test method
1973 - IRG/WP 229
J G Savory, J K Carey


Iron promotes decay capacity of Serpula lacrymans
1993 - IRG/WP 93-10008
The influence of iron and iron compounds on the decay capacity of Serpula lacrymans was studied. Mass losses of pine wood caused by dry rot fungus were increased when FeSO4 was added into the culture medium or when there were iron nails or stone wool on the culture medium. This supports the hypothesis that iron in stone-based building materials is one reason for the increased decay capacity of Ser...
L Paajanen


Production of treated wood in Brazil in 1982 and 1983
1985 - IRG/WP 3327
The data of Brazilian production of treated sleepers, poles, crossarms, fence posts and other commodities are given for the years of 1982 and 1983. This report updates information given to the Group in Document No: IRG/WP/3321 Wood Preservation in Brazil, STU information no 445...
M S Cavalcante


Some observations on miniaturised soil/block tests
1988 - IRG/WP 2317
Results are presented for miniaturised soil/block tests carried out in 120 ml capacity glass jars. The four test fungi (Coniophora puteana, Coriolus versicolor, Gloeophyllum trabeum and Poria placenta) reacted differently to different moisture regimes established by varying the soil moisture content. Acceptable levels of decay were achieved by the three brown rot fungi with soil at 110% whc; howev...
J K Carey


A new laboratory technique devised with the intention of determining whether, related to practical conditions, there should be a relationship between growth rate and decay capacity (of different strains) of Serpula lacrymans
1989 - IRG/WP 1384
Most laboratory techniques for the determination of growth rate not only use a medium (agar) unrelated to practice, but also yield values that are often far less than those found in practice. Also, most laboratory techniques for the determination of decay capacity ensure that the whole of a small test block becomes fully surface-colonised within the first few days; whereas in Australian practice S...
J D Thornton


Report on the status of collaborative experiments within the Sub-group on Basidiomycete tests
1983 - IRG/WP 2194
This report summarises the results of co-operative work carried out within the Sub-Group on Basidiomycete tests up to December 1982. The principle findings are recorded in the Conclusions Section. Work intended between IRG-13 in Turkey and IRG-14 in Australia is cited under Future Programme. An Annex provides a response sheet for existing and new participants to notify their contributions....
A F Bravery


Testing wood in ground contact: An artificial soil
1977 - IRG/WP 280
This document is an interim report on the development of the artificial soil medium. It includes some information on the relationship between soil, wood and water which is of relevance in testing....
E F Baines, D J Dickinson, J F Levy


Copper binding capacity of modified wood flour
1992 - IRG/WP 92-3709
Wood flour was modified by reaction with oxidising agents and CCA preservative. The copper chromium and arsenic were removed from the CCA treated wood flour by an acid leaching procedure. The modified wood flours were allowed to react with copper acetate solution and the level of copper fixation achieved was determined. The modified wood flours had greater affinity for copper ions present in solut...
N C Milowych, W B Banks, J A Cornfield


Treating Eucalyptus tereticornis wood with boron: Optimizing treatment conditions
2005 - IRG/WP 05-40309
Even though Eucalyptus tereticornis wood is suitable for small timber purposes, being non-durable, it needs to be treated with preservative chemicals. As it is a heavy, hard and difficult to treat species, the possibility of using diffusible boron compounds was investigated. The present study explored the effect of impregnation conditions such as treatment schedule, concentration of treatment solu...
T K Dhamodaran, R Gnanaharan


Iron in stone wool - one reason for the increased growth and decay capacity of Serpula lacrymans
1992 - IRG/WP 92-1537
The chemical compositions of stone wool and glass wool were analysed. There was more iron in the stone wool than in the glass wool. It was found that iron present in stone wool was easily dissolved by oxalic acid that Serpula lacrymans is able to produce. The stone wool promoted the decay of pine wood by Serpula lacrymans. The glass wool had no effect on the decay capacity of Serpula Iacrymans. Th...
L Paajanen, A-C Ritschkoff


Dynamics of pressure changes in wood during impregnation
1990 - IRG/WP 3615
Conventional methods of impregnation have to be improved for achieving better penetration of refractory wood species. Basic requirements for an adjustment of treatment schedules are, amoung others, a profound knowledge of the course of pressure changes in the wood during treatment. A new method of pressure measurement was developed which supplies exact and reproducible data. The results show that ...
R D Peek, S Goetsch


An investigation into the influence of soil cation exchange capacity on preservative component depletion
1994 - IRG/WP 94-20050
The mobility of preservative components from treated wood into the soil environment is regarded as an important determinant of preservative performance. Standard procedures for the investigation of this phenomenon have not been developed to any great extent. Soil bed studies conducted in this laboratory using natural soil and modified soil media have provided interesting comparative data on the in...
K J Archer, L Jin


Chapter 1 - Introduction to bamboo
2007 - IRG/WP 07-10635-01
In this introductory chapter the botanical position, distribution, utilization, outlooks, production, research, importance, propagation, natural durability, preservative treatment, importance of preservative treatment, treating principles, research on preservative treatment of bamboos and the objectives of this book have been described briefly under individual caption....
A K Lahiry


Soil-bed studies. Part 2: The efficacy of wood preservative
1983 - IRG/WP 2205
Various methods of decay assessment were investigated. Three stages or phases of decay were identified which could be used to describe the efficacy of a preservative system or virulence of a soil-bed testing medium. These included the lag, decay, and senescent phase. Premature senescence could arise if wood samples became waterlogged. It was concluded that time to failure was unsuitable as a metho...
P Vinden, J F Levy, D J Dickinson


Preliminary studies to assess the effects of aeration and lowered humidity on the decay capacity, growth and survival of the dry rot fungus Serpula lacrymans (Wulf ex. Fr.)
1997 - IRG/WP 97-10208
Novel microcosms were used to test separately the effects of aeration and humidity on the decay capacity, linear spread and survival of Serpula lacrymans. The application of a pumped air supply resulted in an effective cessation of fungal activity when all but the lowest of the air flow rates was used. Furthermore, the lowest air flow rate caused marked growth tropisms away from the stress. In sep...
G A Low, J W Palfreyman, N A White, H J Staines, A Bruce


Effect of treating process on efficacy of CCA in a laboratory decay test
1990 - IRG/WP 3628
Test samples of Pinus radiata sapwood measuring 40x40x500 mm³ were treated with a range of concentrations of the copper-chrome-arsenate (CCA) formulation "Tanalith C" using Rueping (empty cell), Lowry (empty cell) and Bethell (full cell) treatment processes. Samples were then reduced to 40x40x7 mm³ test blocks and exposed to the decay fungus Coniophora puteana using an agar/block technique. Repl...
M E Hedley, K Nasheri, J G Van der Waals


A study of the colonization of wood blocks in a laboratory unsterile soil test
1988 - IRG/WP 2318
CCA treated and untreated beech blocks were exposed to a defined horticultural loam using the method proposed for the collaborative soft rot test in the soft rot sub-group of Working Group Two. At intervals during the incubation wood samples were removed and fungal isolations were made using selective media. Fungi were identified and tested for their cellulolytic ability and their decay capacity i...
M T De Troya, S M Gray, D J Dickinson


Intraspecific variability in feeding capacity of Coptotermes acinaciformis (Froggatt) (Isoptera: Rhinotermitidae)
1983 - IRG/WP 1175
This paper describes laboratory studies to evaluate the comparative feeding capacity within and between five mound colonies of Coptotermes acinaciformis (Froggatt). Matched specimens of mountain ash, pine and coachwood were exposed to five replicate 10 g groups of termites from each colony source. After an initial 8-week exposure period, all groups were assessed for vitality and continued feeding ...
C D Howick, J W Creffield


Effect of soil type and moisture content on soft rot testin
1986 - IRG/WP 2270
Several soils of different types were tested at a range of moisture contents for their suitability for use in a soil burial soft rot test. Their effectiveness was assessed by weight loss in CCA treated and untreated beech and birch outerwood. A horticultural loam (John Innes No. 2) was the most appropriare soil in terms of amount of weight loss caused, tolerance to changes in soil moisture content...
S M Gray


Disproportionate absorption of different constituents of CCA salts
1988 - IRG/WP 3484
Results of preliminary experiments carried out to study selective absorption of different constituents of CCA salts and sludge formation in commercial treatment, using Terminalia myriocarpa and Pinus kesia timbers, are reported in this paper. The objective of these experiments is to evolve simple and practical methods to prevent/minimise sludge formation and differential absorption of the constitu...
V R Sonti, S Sonti, B Chatterjee


An optimum schedule for treating radiata pine
1998 - IRG/WP 98-40105
New Zealand grown radiata pine was treated with copper chrome arsenate preservative using Bethell process. Four different treatment schedules were tried. Keeping the duration of pressure stage constant (either 15 minutes or 45 minutes) and increasing the duration of vacuum (from 15 minutes to 30 minutes) or keeping the duration of vacuum stage constant (either 15 minutes or 30 minutes) and increas...
R Gnanaharan, D R Page


Introducing bamboos for their importance and conservation
2005 - IRG/WP 05-10546
Bamboo is a socio-economically, industrially and environmentally important forest and rural crop in Asia. It is an essential task for the people in this region to conserve the bamboos and preserve the bamboo products for their sustainable continuity. An earnest need for this task is to introduce a variety of important information on bamboos. In this research paper the botanical position, distribut...
A K Lahiry


Soft-rot in Tabebuia sp. wood used in water cooling tower: identification and degradation capacity of the fungi
1998 - IRG/WP 98-10253
Tabebuia sp. (ipe), a native Brazilian wood, is considered of high natural resistance to decaying fungi, and has been used in harsh environments, as cooling towers. Fifty-one fungi, belonging to mitosporic fungi group (Fungi Imperfecti), were isolated from deteriorated Tabebuia sp. wood samples, collected from the mist eliminator and packing of a cooling tower in operation for about 23 years. The ...
S Brazolin, M Tomazello, I H Schoenlein-Crusius


Next Page