Decontamination of sludges, liquids and soils polluted by “class 1, 2 & 3a” and “temporary” wood treatment products from dipping tanks
2016 - IRG/WP 16-50315
Wood is one of the most widely used building materials as it is easy to find and process. As an organic material, time leads to a degradation of its substance, and even more so when it is exposed to pathogens such as fungi, bacteria and insects. In order to try and inhibit this phenomenon, several preservation treatments have been developed and applied thanks to the production of chemical biocides...
A Zaremski, E Wozniak, S Maman, C Zaremski, S Morel


Assessing the natural durability for different tropical timber species using the mini-block test
2017 - IRG/WP 17-10886
The Xylarium in the Royal Museum for Central Africa (RMCA, Tervuren, Belgium) contains over 60,000 wood-samples, comprising over 12,000 species. These samples are of great historical and scientific value yet have a random format, which complicates standard testing. The wood-durability against Coniophora puteana and Trametes versicolor was tested for 36 species. Due to the random sample sizes the s...
V Deklerck, I De Windt, N Defoirdt, J Van den Bulcke, H Beeckman, E Espinoza, J Van Acker


Genetic characterisation of the deathwatch beetle – Call for support
2017 - IRG/WP 17-10890
The deathwatch beetle (Xestobium rufovillosum) is one of the most important pests of historical wood constructions. Further analysis of the exact nature of the feeding habits regarding diet and wood characteristics might deliver answers for controlling this pest. Also there is little known about genetic variability and population structure within the species. For analysis of infested wood and also...
M Höpken, E Melcher, J Trautner


Underground timber constructions from the First World War are well preserved after 100 years
2017 - IRG/WP 17-10897
During the Great War or World War I many underground constructions have been built for protection from shelling. They were an important part of the trench warfare as they were used as an area to rest and carry out other activities such as eating. They would usually range in size from smaller constructions that could hold several men to larger entities that could hold thousands of soldiers. In the ...
J Van Acker, I De Windt, K Haneca, H Beeckman, F Claeys, S Vandenbussche, J Vandewalle, N Robeyst, A Willems


Case study: “Riesenbühlturm”
2017 - IRG/WP 17-20599
In this case study four 7 m long Douglas fir crossbeams were investigated regarding the remaining metal and moisture content. The crossbeams were replaced from a timber tower after 10 years of service in the Black Forest region (South Germany) due to fungal decay. From each of the crossbeams five stem discs were taken and relevant parameters (density, moisture and remaining metal content) were de...
E Melcher, J Müller


Design and performance prediction of timber structures based on a factorization approach
2017 - IRG/WP 17-20603
Service life of timber structures in outdoor conditions is predominantly affected by the climatic conditions in terms of moisture and temperature over time. On the one hand, the two parameters moisture content and temperature determine the exposure-induced dosage that can lead to fungal infestation and subsequent decay. On the other hand, the material resistance of wood stands in opposition to exp...
L Meyer-Veltrup, C Brischke


Laboratory test to determine the effect on durability of combining biobased building materials with timber in construction
2017 - IRG/WP 17-20604
The use of Structural Insulated panels is a construction approach that is seeing more abundant use and is becoming a widely available method. Preformed units are usually a composite structure which often include a range of bio-based materials such as timber, wool or straw. Traditional laboratory based wood decay tests do not take into account this combination of biobased materials and it may be po...
S F Curling, G A Ormondroyd


Modelling of moisture content in timber bridge details
2017 - IRG/WP 17-20613
The design of details is an important aspect in durability design of timber bridges. Details are often considered the weakest points in bridges due to their tendency to trap and accumulate moisture and thus facilitate decay. When designing maintenance plans and inspection intervals, it is important to know how design choices will come to influence the service life. Moreover, service life and wood ...
J Niklewski, C Brischke, E Frühwald Hansson, L Meyer-Veltrup


Moisture content as a quality control parameter in thermally modified timber production
2017 - IRG/WP 17-20622
Quality assurance (QA) or factory production control (FPC) is necessary to ensure a proper production process. The requirements of QA/FPC can result from EN and national standards, quality assurance systems, or producer-specific rules. TMT producers must ensure that the process was correct, and to ensure traceability of products. In addition to the electronic records, the material should be che...
W Scheiding, H Turkulin, S Stein


An experimental study of mould growth and wood decay in timber frame walls
2017 - IRG/WP 17-20623
This paper deals with parameters related to the occurrence of mould growth and wood decay in timber frame walls. In a first part, the hygrothermal conditions inside a timber frame wall finished with brick veneer cladding are analysed to get an idea of possible moisture related problems. It is shown that, based on the VTT mould prediction model, there is a mould risk on the interface between the in...
M Vanpachtenbeke, J Van den Bulcke, I De Windt, J Langmans, S Roels, J Van Acker


Efficacy of Erythropleum suaveolens (potrodom) and Distemonanthus benthamianus (bonsamdua) water extractives on the durability of five Ghanaian less used timber species of varying perviousness and retentiveness
2017 - IRG/WP 17-30705
Conventional wood preservatives are not only toxic to target bio-deterioration organisms but also to humans, other organisms and the environment. In an effort to find preservatives that are less toxic or non-toxic to man, other organisms and the environment, efficacy of branch bark and heartwood water extracts (0.65 g/ml) of Erythropleum suaveolens (potrodom) and Distemonanthus benthamianus (bonsa...
A Asamoah, K Frimpong-Mensah, C Antwi-Boasiako


Copolymers of tannin extracts as wood protection agents
2017 - IRG/WP 17-30709
Wouldn´t be a dream to preserve wood with the substances which the nature already synthesizes for protecting itself? The idea we would like to pursue is simple: Increase the concentration of these substances, the tannins, trying to fix them properly in wood. It appears easy but it is not. Sensibility against leaching, fungal decay and weathering were observed. In this paper new flavonoid co-polym...
G Tondi, L Sommerauer, A Oberle, A Petutschnigg, M-F Thevenon


Performance of Norway spruce bridge in North-West Spain after 12 years exposure
2017 - IRG/WP 17-40796
Across Europe is very common to find bridges build in sawn and glue-laminated wood. Most of these bridges used softwood wood species such as: fir, spruce, larch and pine. In Spain wooden bridges, became more and more popular since nineties, when sawn and glue-laminated wood were utilized for building exterior wooden structures in overall Spain. This material, sawn and glue-laminated wood, are ma...
D Lorenzo, J Fernández-Golfín, M Touza, M Guaita, A Lozano, J Benito


Durability of energy efficient wooden buildings: a building physical point of view
2017 - IRG/WP 17-40812
The drive for more energy efficient and sustainable buildings resulted in an increased popularity of wooden buildings, even in countries with a masonry tradition. Often guidelines and prescriptions then are copied from other countries. Different climatic boundary conditions and tradition of finishing, though, do require different moisture tolerance criteria. This is clearly the case for water vapo...
S Roels, J Langmans


Corrosion verification experiment of the screw driven into CLT
2017 - IRG/WP 17-40816
Japan has abundant forest resources, but we depend on import for 70 percent of the consumed timber. Japan has the vision which promotes the timber self-sufficiency rate 30% to 50% by 2020. Therefore CLT attracts attention as a new timber material. Japan has a climate with high temperature and humidity, and wooden buildings are often treated with chemicals as a measure against biological deteriorat...
N Wada, H Ishiyama, S Yamamoto


Influence of sea water on timber and metal joints
2017 - IRG/WP 17-40818
In the Great East Japan Earthquake that occurred in March 2011, many buildings suffered from seawater immersion caused by the tsunami. Saito's study revealed that corrosion progresses on metal plate that experienced seawater immersion 1). However, the detailed mechanism of corrosion progresses has not yet been clarified. Therefore, in this study, salinity which is one of causes of corrosion w...
T Nishimura, H Ishiyama, F Hirose, N Wada


Testing the durability of timber products above ground using the block-test method – A critical review
2018 - IRG/WP 18-20637
The block-test method for testing the durability of wood and wood products above ground is reviewed critically with respect to practical aspects, moisture loads, corresponding decay development, and the possibilities of assessing test specimens by determining the dynamic modulus of elasticity (MOEdyn) of wood. In total, 36 blocks representing different modifications of the original set-up and a wi...
C Brischke, A Gellerich, H Militz


Self-Extinguishment Phenomena of Mass Timber in Medium-Scale Compartment Fires
2018 - IRG/WP 18-30729
This paper presents a review of the fire safety risks that mass timber construction may introduce in buildings, with special consideration to medium- and high-rise buildings. These main risks are represented by an effect to the classical fire safety strategy for buildings: (1) Compartmentalisation, to ensure that the fire will not spread farther than the compartment of origin, (2) Preventing verti...
C Gorska, J P Hidalgo


Thermally modified timber treated with methacrylate
2018 - IRG/WP 18-40849
Thermally modified timber (TMT) from Scots pine sapwood similar to Thermo-D quality was impregnated with methacrylate resin by the hot-and-cold method and subsequently cured at elevated temperatures. The results showed that methacrylate resin could be used to reduce colouring of painted TMT wood during accelerated weathering probably by hindering the migration of extractives. The resin itself did ...
O Karlsson, O Myronycheva, DJones, D Elustondo, D Sandberg


Determining the natural durability on xylarium samples: mini-block test, wood powder and chemical profiling
2019 - IRG/WP 19-10944
Xylaria, or wood collections, can be considered sleeping beauties in terms of wood technological and biological output. In this study we focus on determining the natural durability of xylarium specimens from the Federal Xylarium in the Royal Museum for Central Africa. The Federal Xylarium contains over 80,000 specimens, covering more than 13,000 species, mainly from Central Africa. These specimens...
V Deklerck, L De Ligne, J Van den Bulcke, E Espinoza, H Beeckman, J Van Acker


Validation by micro-computed tomography of an assessment method to measure the residual strength of anobiids infested timber
2019 - IRG/WP 19-20650
In this article a quantitative correlation study of pine timber structural elements, which have been subject to attack by anobiids, is presented. The main objective of the study was to establish a valid empirical correlation between the lost material percentage (consumed by beetles) and original/residual apparent density. Since the beetles’ attack produces a diffuse damage with a set of tunnels ...
J L Parracha, M F Pereira, A Maurício, P Faria, L Nunes


Visual assessment of longitudinal wheel timbers and assessing the feasibility of extending wheel timber service life in the UK railway network
2019 - IRG/WP 19-20651
Timber has been a versatile building material for centuries and during the start of the Railway Age in the nineteenth century it was in considerable demand for use in the railway network, particularly bridge building. Timber is still in service and widely used throughout the UK railway network. The resilience and favourable strength to weight ratio and its relative ease of fabrication make it an...
J R Williams


Development of accelerated decay test for CLT using a fungus grown on agar medium
2019 - IRG/WP 19-20664
CLT is a large-scale wooden board which consists of several layers of sawn lumber stacked in altering directions. Therefore, a lot of large cross sections appear on all narrow faces of CLT. As water penetrates easily into timber from cross section, wooden material whose cross section is exposed to water in in a usage environment is susceptible to deterioration by organisms. Wood deterioration orga...
T Miyauchi, K Kambara, W Ohmura, T Mori, H Matsunaga, N Hattori


Preservative Treatment of CLT: An Example at Shimojishima Airport
2019 - IRG/WP 19-30748
Cross laminated timber (CLT) is a relatively new construction method that allows multi-storey construction using solid wood instead of concrete or steel. It is a method favoured by progressive architects and recognized for its much lower environmental footprint. Wood is an excellent construction material and is a long-term carbon sink that also performs well in the event of earthquakes and fire....
J Lloyd, N Yamashita, A Taylor


Treatability of native and exotic alternative timber species
2019 - IRG/WP 19-40864
The service life of moderately durable species can be extended significantly if the challenge of effective treatment of refractory wood species can be overcome. Along with preservative effectiveness, the performance of preservative in treated wood depends on factors such as retention and penetration in treated wood, the wood anatomy, the uniformity of penetration and micro-distribution within the ...
D Page, T Singh


Previous Page | Next Page