The resistance of thermo-oil modified wood against decay and mould fungi
2009 - IRG/WP 09-40448
Thermally modified wood in comparison to natural wood demonstrates some advantageous functional properties like decreased hygroscopicity, higher dimensional stability. It also has increased durability and improved resistance to fungal decay. However thermal modification of wood may lead to reduced strength properties what may limit the use of wood in mechanically beared constructions. The changes ...
A Fojutowski, A Kropacz, A Noskowiak


Termite resistance of some modified wood species
2009 - IRG/WP 09-40449
During the last few decades, researchers worldwide have investigated and developed new treatment techniques to improve intrinsic wood properties. Some of these techniques were introduced to the market recently and are gaining in importance.. Various wood properties of these new materials have been studied intensively. These include physical-mechanical properties (dimensional stability, moisture ...
H Militz, B C Peters, C J Fitzgerald


Wettability and bonding strength of wood thermally-treated with different combinations of soy oil and chemical additives
2009 - IRG/WP 09-40454
Thermal treatment is a method which has gained wider acceptability as an alternative to the chemical treatment in wood preservation. In order to maximize the benefits of this technique several options have been adopted including the use of soy oil in transferring the heat to the wood. Available information on thermal treatment in general and the oil method in particular show that there are still n...
L Awoyemi, P A Cooper, T Ung


Barefoot-heat-impact of oil-heat-treated wood: An important thermal property of decking boards
2009 - IRG/WP 09-40458
In this study the phenomenon of sensual heat impression was examined, when walking with bare feet on sun exposed wood based decking boards. A suitable method for measuring the heat flux from decking boards into an artificial foot was developed. The method and measuring device is described as well as results from measuring three different decking board materials: Oil-heat-treated spruce (OHT), untr...
A O Rapp, C R Welzbacher, C Brischke


The effect of chemical changes on the wood-moisture relationships in thermally-modified wood
2009 - IRG/WP 09-40473
Small specimens of three wood species were thermally modified following twenty schedules in the 190-245°C temperature range for treatment times between 0.3 and 16 h. Five wood-moisture relations were subsequently determined, namely: anti-swelling efficiency (ASE), movement, hygroscopicity (adsorption and desorption), transversal swelling (radial and tangential directions), and equilibrium moistur...
M M González-Peña, M D C Hale


Onset of mould growth – the effect of climate variability and different geographic locations
2010 - IRG/WP 10-20446
This paper presents a study on how climate conditions at numerous locations in Sweden affect the risk of onset of mould on wood sheltered outdoors. The results indicate that the risk is clearly higher in the south compared to the north of Sweden. These differences are mainly explained by colder and dryer winter periods in the north which is unfavorable for development of mould. The results also sh...
M Häglund, T Isaksson, S Thelandersson


The use of thermal desorption and pyrolysis combined with a semiconductor VOC detector for the on-site detection of preservative-treated wood
2010 - IRG/WP 10-20456
The purpose of this study was twofold; to identify possible marker molecules released from preservative-treated wood upon heat treatment and then develop a prototype detector for this marker. Two methods for heating the samples were used: Pyrolysis combined with Gas-Chromatography with IR-detection and Thermal Desorption combined with Gas-Chromatography with mass detection. A first prototype detec...
I Svensson, A Gonzalez, L Irusta, Mª J Fernandez-Berridi, O Munné


The biological durability approach for wood product performance and service life prediction
2010 - IRG/WP 10-20457
The performance of wood-based products under conditions that enable biodegradation are of concern to all who envisage sustainable use of forest based products. This concern is also the basis of classification of wood species on the basis of their biological durability. Engineers are looking for options to transfer such classification into practical service life values for constructions and related...
J Van Acker, J Van den Bulcke, L De Boever


Improved analysis of field test data related to service life prediction of tropical wood species
2010 - IRG/WP 10-20458
Long field trials of wood in ground contact give valuable data on the natural durability of the material. The European Standard EN 350 gives guidance on how to perform these durability classification, but is limited to the use of averages of in-service life of a set of specimens compared to a reference set. Starting from a database of visual assessment of field stake testing, it is possible to obt...
J Van den Bulcke, A Wong, Ling Wang Choon, Yoon Soo Kim, J Van Acker


Biological performance of wood treated with tar-oil recovered during slow pyrolysis of macadamia nut shells
2010 - IRG/WP 10-30523
This study evaluated decay and termite resistance of wood treated with tar oil obtained from a commercial pyrolysis process of macadamia nut shells. Vacuum-treated pine wood specimens were subjected to various brown and white rot fungi based on the soil-block test method specified by the American Wood Protection Association (AWPA) after leaching process. Treated specimens were also subjected to th...
S Nami Kartal, E Terzi, C Kose, J Hofmeyr, Y Imamura


Treatment of Scots pine wood with oil in water and water in oil emulsion systems: Effects on boron leaching and water absorption
2010 - IRG/WP 10-30535
The aim of this study was to investigate the water absorption and water repellent efficiency of oils and oil water emulsions [oil-in-water (O/W) and water-in-oil (W/O)] and possibilities of reducing the amount of boron leaching from treated wood. Scots pine wood samples treated with waste or sunflower oil and water formulations contained 3%BA. The level of water absorption and water repellent effi...
E D Tomak, Ü C Yildiz, A Can


Natural compounds: A review of their use for wood protection
2010 - IRG/WP 10-30545
A lot of research in the field of wood protection has focused on natural compounds but very few of these have been implemented by industry. This review is an attempt to bring together information from selected area of work: - A brief review of the work done on natural products as organic biocides for wood protection. - Table containing information on natural products, their use as organic biocid...
T Singh, A P Singh


Using plant oils as hydrophobic substances for wood protection
2010 - IRG/WP 10-30550
The increased interest to use oils as hydrophobic agents and the current debate about the further use of creosote emphasises the urgent need of better understanding of plant and other oils as wood protectors. The present study sheds light on the hydrophobic properties and distribution of various plant oils in the anatomical structure of Scots pine sapwood. Oil retentions from approximately 70 to 5...
D Panov, N Terziev, G Daniel


An investigation on some physical properties of oil heat treated poplar wood
2010 - IRG/WP 10-40509
In this study some physical properties of small samples (20×20×20 cm) of poplar wood (Populus nigra var.pyramidalis) after oil heat treatment with linseed oil was investigated. Two time levels (4.5 & 6 hours) and three temperature stages (180,200 & 220°C) were selected. The results of this study showed significant differences in effects of treatment temperature on physical properties of wood....
B Bazyar, D Parsapajouh, H Khademiesalam


Performance of selected types of coated and uncoated modified wood in artificial and natural weathering
2010 - IRG/WP 10-40510
The objective of the present work was to investigate the influence of commercial wood modification methods on weathering behaviour and coating performance. It was aimed to compare modification methods and to set up maps of weathering behaviour for these methods with and without a semi-transparent wood stain. Artificial and natural weathering trials were carried out with a selection of different ty...
G Grüll, L Podgorski, M Truskaller, I Spitaler, V Georges, S Bollmus, A Steitz


Impact of wood species on the performance of exterior wood coatings
2010 - IRG/WP 10-40519
To prolong the service life of a wooden construction the protective function of a coating is of utmost importance. The chemical composition as well as the wood-coating interface affects the performance of this protective layer and obviously wood species have an impact too. This paper discusses the influence of wood species on the overall coating performance. Therefore, a range of opaque waterborne...
I De Windt, J Van den Bulcke, J Van Acker


Effect of Nano-Silver Treatment on Densified Wood Properties. Part One: Swelling, Recovery Set, Bending Strength
2010 - IRG/WP 10-40533
In this research the effect of Nano-Silver treatment on compressed wood properties, was studied. Wood specimens were cut from Popolus alba (poplar) and impregnated with Nano-Silver and water. Then the saturated samples were compressed through radial direction in a hot press under pressure of 6 MPa, for 1 and 4 hours. The temperatures of press were 150°C and 175°C. Swelling (24h), recovery set ...
G Rassam, H Reza Taghiyari, B Jamnani, M Ali Khaje


Combined Effect of Boric Acid and Waste Oil Treatment on Boron Leaching
2010 - IRG/WP 10-50268
In this study it was aimed to investigate the boron leaching amounts in Scots pine wood samples treated with boric acid (BA) and waste oil (WO) alone or by dual treatment. The level of water absorption and water repellent efficiency were determined with cyclical wetting tests, total of 336 hours. Wood samples that have both covered and uncovered transversal section were impregnated with 3% boric a...
Ü C Yildiz, E Dizman


Effect of heating on aldehydes emissions from solid wood
2011 - IRG/WP 10-50277
We have found that acetaldehyde, a probable human carcinogen, is produced from wood through reaction with ethanol. Alcohols are increasingly being used in houses and buildings for cleaning purposes. Acetaldehyde emission from solid wood has been attributed to ethanol acidification by enzymes such as ethanol dehydrogenase. Heating could inactivate these enzymes. In this study, the effects of heatin...
A Ishikawa, K Miyamoto, S Tohmura, A Inoue


Influence of wood swelling agents on penetration and copper leaching of copper-ethanolamine based wood preservatives
2011 - IRG/WP 11-30556
Copper ethanolamine based preservatives are currently the most important solutions for impregnation of wood in ground contact in Europe. One of the issues related to those and similar water based solutions is insufficient penetration to refractory wood species like Norway spruce. In order to elucidate this issue, commercial copper ethanolamine based solution was supplemented with five different wo...
M Humar, N Thaler, B Lesar


Effect of P/F ratio, PF concentration and treating method on boron leaching from wood treated with PF modified boron compounds
2011 - IRG/WP 11-30559
In order to immobilize boron in wood, three kinds of resol-type phenol-formaldehyde (PF) resin with different P/F ratios were synthesized in laboratory and incorporated with three types of boron compounds to treat wood. The used boron compounds included boric acid (BA), borax (BX) and disodium octaborate tetrahydrate (DOT). The leaching test of boron from wood blocks was performed according to the...
Liping Yu, Jinzhen Cao


The potential of propolis and other naturally occurring products for preventing biological decay
2011 - IRG/WP 11-30575
The potential of using a range of naturally occurring plant extracts and propolis from bee hives for enhancing the durability of timber in service as well as helping with the conservation of archaeological timbers is considered in this paper. Results reported demonstrate that there is some degree of protective effect noted, suggesting a viable treatment option might be developed based on a deeper ...
D Jones, N Howard, E Suttie


A Critical Review and Survey of the US Wooden Pallet Industry: Focusing on Market Segmentation & N. American Trends
2011 - IRG/WP 11-40545
This paper reviews the history and current and predicted future use values in N. America. Included in this work is historical data on rationality and wood species used to manufacture wooden pallets in the USA and an ongoing current market survey sent to the 1000 largest manufacturers and re-manufacturers in the USA based on SIC Code 2448(Standard Industrial Code Classification). Although CHEP, the...
M H Freeman


Utilization of thermodesorption coupled to GC-MS to study kinetics of thermodegradation of different wood species
2011 - IRG/WP 11-40559
Thermdesorption coupled to Gas Chromatography coupled to Mass Spectroscopy (TD-GC-MS) has been investigated to identify volatile degradation products generated during wood heat treatment by mild pyrolysis. For this purpose, wood samples of different softwood and hardwood species have been heat treated under nitrogen for different temperatures comprised between 180 and 230°C during 15 min. in the ...
K Candelier, M Chaouch, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Evaluation effect of kiln schedule on Warp, Twist, Bow and surface checks in Poplar Wood
2011 - IRG/WP 11-40565
In this research, to establish a kiln-drying schedule for poplar (Populus nigra) lumber with 75 mm thickness that cut down from North Khorasan province in Iran, with three schedules T5-D2 (Forest Product Laboratory), T5-D3 and T8-D5 were adapted for drying the lumbers down to the final moisture content of 8±2%. primary dry bulb temperature each three schedules was adjusted at 49,49 and 54°C and ...
M. Akhtari, M.Arefkhani