Study of the degradation caused by micro-organisms in Pinus sp. waterlogged wood
1989 - IRG/WP 1411
So far, the different Centers are trying the restoration and the conservation of wood structures, coming from subaquatic archeological deposits, with interest from the historic - artistic point of view. The main objective of this paper has been the determination of the decay level of Pinus sp. wood coming from a roman ship (approximately 2000 years old), where we have analyzed their physical prope...
M T De Troya, M C Escorial, J Garcia, A Cabanas


The improvement of wood durability by retification process
1993 - IRG/WP 93-40015
A material with new properties is obtained by retification process. It consists of a light pyrolysis of wood which becomes more stable and especially more resistant to fungal attack with few decrease of mechanical properties. Tests were carried out on three susceptible wood species (Poplar, Spruce, Fir) that are used in construction and are difficult to treat with wood preservatives. Retified wood...
D Dirol, R Guyonnet


Alkaline building materials and controlled moisture conditions as causes for dry rot Serpula lacrymans growing only in houses
1985 - IRG/WP 1272
Dry rot Serpula lacrymans ( Fr.) S.F. Gray is commonly found in houses, though never with certainly in nature, like other wood destroying fungi which grow both indoors and outdoors. In investigating series of dry rot instances it was shown that this fungus is always found in covered places, close to a moisture source, the distance being from 0 a maximum of 600 cm. Owing to the dry rot has been abl...
J Bech-Andersen


Comparison of the FRIM and forest research laboratory methods for screening of anti-sapstain formulations
1999 - IRG/WP 99-20170
Two laboratory methods for screening of anti-sapstain formulations were compared. The method adopted by the Forest Research Institute Malaysia (FRIM) involved 3 weeks assessment of rubberwood (Hevea brasiliensis) blocks, dipped in the candidate formulation and inoculated with mycelial/spore suspension of sapstain (Botryodiplodia theobromae) or decay (Schizophyllum commune) fungi, and incubated on ...
A H H Wong, D R Eden, C M Chittenden, M E Hedley, R N Wakeling


Resistance of acetylated wood to biological degradation. Evaluation of field test
1997 - IRG/WP 97-30139
Acetylated wood samples were tested in ground contact (stake test) at two test fields, one in Simlångsdalen, Sweden, and one in Viikki, Finland, according to European standard EN 252. The test samples were inspected annually and their condition was compared with that of untreated controls and of samples treated with two reference CCA preservatives. The use of untreated controls and preservative t...
P Larsson Brelid, R Simonson, Ö Bergman


Multicomponent biocide systems protect wood from decay fungi, mold fungi, and termites for interior applications
2004 - IRG/WP 04-30333
Concerns about indoor air quality due to mold growth have increased dramatically in the United States. In the absence of proper moisture management, fungicides need to be developed for indoor use to control mold establishment. An ideal fungicide for prevention of indoor mold growth on wood-based materials needs to specifically prevent spore germination and provide long-term protection under condit...
C A Clausen,V W Yang


Some studies on fungal deterioration of rubber wood (Hevea brasiliensis)
1980 - IRG/WP 2140
For the sreening of anti-stain chemicals trials with selected agricultural fungicides and new chemicals were carried out. Botryodiplodia theobromae, Aspergillus sp. and Penicillium sp. were used at test organisms. For testing the durability of rubber wood (Hevea brasiliensis) suitable local rotting fungi (Basidiomycetes), based on high degrading power, which may later be employed in standard tests...
A Sujan, A G Tan, M Stevens


Cytoplasmic and extracellular localization of manganese II dependent peroxidase(s) in white rot fungi during degradation of woody materials
1989 - IRG/WP 1416
The manner by which lignin is degraded in-situ in natural substrates by white rot fungi still remains a controversial issue particularly the distribution and role(s) played by lignin degrading enzymes (i.e. manganese II peroxidase and lignin peroxidase). In the present study, use was made of anti-manganese II peroxidase and immunolabelling techniques in conjunction with transmission electron micro...
G F Daniel, B Pettersson, T Nilsson, J Volc


Tunnelling bacteria
1983 - IRG/WP 1186
The micromorphology of decay in wood caused by a certain group of single-cell bacteria, called tunnelling bacteria (TB), is described. TB are characterised by their tunnelling ability within the secondary cell walls of wood fibres. Pure cultures of TB have not yet been obtained although the typical decay patterns can be reproduced using mixed bacterial cultures. Some indications of lignin degradin...
T Nilsson, G F Daniel


Chitosan for wood protection - state of the art
2005 - IRG/WP 05-30378
The aim of this paper was to give a state of the art description of chitosan as a wood protecting agent. Chitosan is a metal free natural compound derived from crustacean shells and is under evaluation as an environmentally benign wood protecting agent. Information from journals states that chitosan may act both fungistatically and at higher concentrations, as fungitoxic, but the mode of action is...
M Eikenes, G Alfredsen, E Larnøy, H Militz, B Kreber, C Chittenden


Fungal siderophores and their rôle in wood biodegradation
1990 - IRG/WP 1442
Iron and other metals such as manganese, play an important role in the metabolic functions of fungi that cause wood deterioration. These transition metals are also found in, or associated with, the extracellular fungal enzymes shown to be directly involved in the decay process. Recently our research group was able to show that siderophores (low molecular weight biological chelators) are produced b...
J Jellison, B Goodell, F Fekete, V Chandhoke


The need for realism in wood preservation research. A key address
1983 - IRG/WP 3254
The approval of a chemical for use as a timber preservative and the design of in service retention requirements represents an act linking fundamental research and commercial timber preservation. How difficult is it to translate figures generated through controlled experimentation into working specifications and how confident can we be in the methods used to provide such figures? The chairman of Wo...
L E Leightley


Evaluation of teak sawdayst Tectona grandis L Fil as a potential source to obtain a natural wood preservative in Colombia
2004 - IRG/WP 04-30356
Plantation Teak (Tectona grandis L. Fil) has been tested as a possible source of natural wood preservatives due to the known excellent durability of old-growth teak wood. Field tests (ground proximity termite and above ground simulated decking exposures) were established in Colombia in April 2003 at two different test sites with different climates (Tropical Dry and Rain forest). Teak heartwood ex...
A Castillo, Y Cabrera, A F Preston, R Morris


Adequate preservative treatment of kiln dried Eucalyptus camaldulensis and Acacia mangium for tropical and subtropical wood poles
1996 - IRG/WP 96-40075
The Eucalyptus camaldulensis and Acacia mangium round timbers kiln-dried at EMC and full cell pressure treated with CCA-C ensured requisite penetration and adequate dry retention (30 kg/m³ or 4% w/w). The sufficient inherent strength, seasoning property, treatability of sapwood and heartwood equivalent to 44% of radius, natural durability of heartwood, and field investigation on service performan...
A K Lahiry


Micromorphology of decay in Keruing heartwood by the basidiomycetes Phellinus contiguus and Dacrymyces stillatus
2002 - IRG/WP 02-10454
This study aimed to characterise the micromorphology of fungal decay in a wooden handrailing in an above ground exposure at the Thames embankment in London. Keruing heartwood (Dipterocarpus spp.) was determined as the construction timber and the two basidiomycetes Phellinus contiguus and Dacrymyces stillatus identified as main decay organisms. Their decay patterns within Keruing heartwood were...
G Kleist, M Ray, R J Murphy


Microbial decay in an extremely durable Malaysian hardwood Belian (Eusideroxylon zwageri) - an overview
1997 - IRG/WP 97-10216
The heartwood of Belian (Eusideroxylon zwageri) is highly regarded among the naturally durable Malaysian hardwoods, and is therefore a choice timber for soilcontact use in the humid tropics such as untreated telecommunication poles, fence posts and railway sleepers. The high microbial resistance of the wood is evidenced by the mere superficial degradation observed in some pole samples after 20 yea...
A H H Wong, A P Singh


The high decay resistance in the sapwood of the naturally durable Malaysian hardwood Belian (Eusideroxylon zwageri)
2001 - IRG/WP 01-10410
It has long been assumed that the observed natural durability of the heartwood in certain timbers is perhaps associated with a relatively lower decay susceptibility also of the sapwood of these species. While the heartwood of Belian is reputedly highly decay resistant among the tropical hardwoods of Southeast Asia, laboratory decay tests reported in this paper have also confirmed the high decay re...
A A H Wong, A P Singh


A rearing procedure for the house longhorn beetle Hylotrupes bajulus L
1973 - IRG/WP 228
The technique practised at the Princes Risborough Laboratory for culturing Hylotrupes bajulus is described. It is modified from methods previously suggested by German workers. A protein and vitamin enriched wood diet to accelerate larval growth is employed and larvae are subsequently given a period of cool storage to induce pupation. Adults are confined in groups with prepared surfaces for egg lay...
R W Berry


Efficacy of fumigants in the eradication of decay fungi implanted in southern pine timbers
1986 - IRG/WP 3365
Southern pine timbers (15.2 cm x 15.2 cm x 4.26 m) were fumigated at midlength to evaluate the effectiveness of the fumigants chloropicrin, Vapam, Diazomet, Busan 40, Vanicide 51, Vanicide TH, sodium bisulfite, and ethanolamine in eradication of decay fungi. The fumigants were introduced into 2.54 cm holes which were closed immediately with rubber stoppers. Movement and persistence of lethal conce...
T L Highley, W E Eslyn


Microscopic analysis of southern pine utility pole core segments
1992 - IRG/WP 92-1542
Fifteen macroscopic core descriptive categories were evaluated by microscopic analysis for accuracy in detecting decay and judging decay severity. Five categories were good indicators of decay as decay was detected in 28 of 48 samples. Five categories were possible indicators of early decay as decay was detected in 6 of 40 core segments and an additional 18 contained hyphae. The remaining five cat...
S E Anagnost, C J K Wang, M Wright


Performance of Tuff Brite C™ and other formulations against blue-stain, mold and brown-stain in freshly-sawn rubberwood (Hevea brasiliensis) in the humid tropics of Peninsular Malaysia
1997 - IRG/WP 97-30163
The relative anti-sapstain and anti-mold efficacies, including brown-stain development in freshly-sawn rubberwood (Hevea brasiliensis) in the Malaysian tropics, between selected water-based product concentrations of formulations Tuff Brite CTM without/with added Borax (at 1.5/0, 1/1.5, 1.5/1.5 and 2%/1.5%), PQ8TM without/with added Borax (at 2.5/0, 1.5/1.5, 2/1.5 and 2.5%/1.5%) and NeXgenTM/NeX-Br...
A H H Wong, T L Woods


Depth of foraging of subterranean termites in tropical Australia
1996 - IRG/WP 96-10141
Stakes of radiata pine (Pinus radiata D.Don) of varying lengths to 800 mm were inserted vertically in the soil with all but their lower 100 mm sheathed in a capped UPVC tube representing a physical barrier to termites. In one series of trials, termites were encouraged to aggregate at the upper ends of the tubes, in order to determine whether they would descend to the lower end of the barrier. In a...
L R Miller, M Hoschke, M Neal


Window test. Direct testing of wood resistance to decay: A study of its fitness, its reliability and its accelerating factor
1984 - IRG/WP 2219
This is the results of an experiment using the window-test specimens, exposing the specimens to three different types of testing procedure: 1. Natural infestation in the open air; 2. Artificial infestation and exposure in the open air; 3. Artificial infestation in a green-house. The results show good similiraties of the three parallel tests in term of decay, and assess the reliability of the windo...
G R Y Déon, L N Trong


Nasutitermes exitiosus and wood-rotting fungi in Eucalyptus regnans, E. acmenioides, E. wandoo, and E. marginata: force-feeding, laboratory study
1985 - IRG/WP 1231
Under a force-feeding regime, the termitid Nasutitermes exitiosus was fed on four eucalypt timbers infested with several fungal species to investigate the influence of such fungus-infested timbers on mass of wood lost, termite biomass, fat content and water content. The results showed that wood mass losses were markedly affected by species of fungi and timber. The interaction of fungi and timbers ...
D B A Ruyooka


Properties of cellulose degraded by the brown rot fungus, Postia placenta
1988 - IRG/WP 1350
To gain further understanding of the nature of the cellulose depolymerizing agent or agents of brown-rot fungi, brown-rotted cellulose was chemically and physically characterized. Various culture conditions, such as low nitrogen and elevated oxygen levels, did not induce degradation of cellulose by Postia placenta in liquid cultures. Therefore, brown-rotted cellulose for analysis was prepared by a...
T L Highley, R E Ibach, T K Kirk


Previous Page | Next Page