Relative performance of copper/chrome/boron (CCB) and copper/chrome/arsenate (CCA) in ground contact
1992 - IRG/WP 92-3694
The performance of four retentions each of an oxide CCA formulation and a salt formulation of CCB in radiata pine and European beech was compared after 18 years' field exposure. In radiata pine CCA oxide was more effective (4 failures out of 40) than CCB (9 failures out of 40). However, in European beech CCB was substantially more effective (22 failures) than CCA oxide (all failed). Analy...
M E Hedley


Comparison of three methods for assessing the in-ground termite resistance of treated timber, durable timber and plastics at sites in Australia, USA and Thailand - First results
1998 - IRG/WP 98-20132
The in-ground resistance of materials to attack by subterranean termites is most commonly assessed with one form or another of the conventional graveyard method, despite the significant shortcomings of this method. In Australia, an alternative method, in which all samples of test materials are placed below-ground, has been in use for more than 10 years. The method provides reliable exposure of sam...
M Lenz, A F Preston, J W Creffield, K J Archer, B M Kard, C Vongkaluang, Y Sornnuwat


A light and electron microscopic study of decayed CCA-treated radiata pine (Pinus radiata) wood from a cooling tower
1994 - IRG/WP 94-10056
An inspection of an industrial cooling tower in New Zealand showed surface decay of 12 year old Pinus radiata wood panels treated with CCA preservative to a retention of around 15 kg/m³ of salt. Wood decay micromorphology typical of that caused by soft rot fungi, white rot fungi, 'stripy' and 'v-shaped' erosion bacteria and cavitation bacteria were all commonly...
A P Singh, R N Wakeling, D R Page


Strength properties of preservative treated pine and spruce wood after super-heated steaming
1984 - IRG/WP 3313
Possible changes of strength properties of CCF pressure impregnated pine and spruce with subsequent steaming at 110°C respective 120°C for 30 min were examined. For spruce analysis of variance indicated that none of the processes had a significant effect on bending strength, compression strength and the corresponding modulus of elasticity as well as on impact bending strength and shear strength ...
R-D Peek


Microscopic characteristics of microbial attacks of CCA-treated radiata pine wood
1993 - IRG/WP 93-10011
Light and electron microscopic observations were made of CCA-treated radiata timbers, which had been placed in service in a vineyard soil as supporting poles and as part of a house pile, to determine the cause of their deterioration. The house pile had failed in service after between 9 and 13 years and was of particular interest because decay was more severe in deeper regions than at the surface a...
A P Singh, R N Wakeling


An appraisal of methods for environmental testing of leachates from salt-treated wood; part 1
1998 - IRG/WP 98-50115
The magnitude and diversity of leaching tests with salt-treated wood, performed by institutes as well as industry, strongly appeal for harmonisation towards one single method. That procedure should be well-defined, cost- and time-effective and moreover be extended with a clear detection and interpretation scheme. The paper(s) presented here tend to evaluate 2 existing leaching methods, the ENV 12...
G M F Van Eetvelde, M Stevens, F Mahieu, H-W Wegen, A Platen


Use of wood-decay fungi for disposal of PCP-treated wood
1995 - IRG/WP 95-50040-33
Although PCP has been classified as a priority pollutant, PCP-treated wood products are currently allowed to be disposed of as ordinary solid (non-hazardous) wastes in the US. Non-regulated disposal of these materials is allowed because PCP concentrations in extracts from PCP-treated products such as utility poles and crossarms, determined by the Toxicity Characteristic Leaching Procedure (TCLP) h...
R T Lamar


Risk of pulmonary damage as a result of an evaporation of ca. 50 ppb = 42 mg HF, evaporated from wood treated by difluorides
1987 - IRG/WP 3401
In this review of the literature the effects of fluorides and fluorine on man are described, especially the low level effects of inhaled HF on human beings. The term "fluoride" is used as a general term everywhere, where exact differentiation between ionic and moluecular forms or between gaseous and particulate forms is uncertain or unnecessary. The term covers all combined forms of the element, r...
H F M Nijman


Effects of alkali treatment on some mechanical and chemical properties of creosote treated oaks
1991 - IRG/WP 2366
To date, there is a lack of information on the effects of chemical treatment on the performance of creosote preservative treated oak sleepers. This factorial experiment was designed to analyze three main effects: species (Quercus alba and Quercus rubra) creosote treatment (treated and untreated), and alkali (NaOH) soaking (0, 1, and 10 percent). The modulus of elasticity (MOE) and fiber stress at ...
P Chow, A J Reinschmidt, E J Barenberg, L C Chang


On-site test for indicative determination of leaching of components of preservatives from treated timber
1993 - IRG/WP 93-50001-12
In the late eighties the environmental concern about treated timber increased and it is still a hot issue in the Netherlands. From the environmental point of view three phases in the timbers life cycle can be distinguished: - the production phase - the service life - the waste phase. In the Netherlands at this moment much emphasis is laid on the production phase. In 1992 this has led to a new legi...
W J Homan, H Militz


Decay and termite durabilities of heat-treated wood
2004 - IRG/WP 04-40272
Decay and termite resistances of Plato-treated timbers were evaluated using a modified JIS decay test method, feeding test in a laboratory scale and a field exposure against Reticulitermes speratus (Kolbe) or Coptotermes formosanus Shiraki. The results showed that no significant decay durability of the treated timbers although mass loss from decay slightly decreased in case of treated timbers. ...
S Doi, K Hanataa, E Kamonji, Yuuji Miyazaki


Preservation of robinia wood (Robinia pseudoacacia L.) stakes by vintners
1982 - IRG/WP 3194
This work discusses decay resistance of robinia wood to fungi Trametes versicolor (L.ex Fr.) Pil. and Coniophora puteana (Schum. ex Fr.) Karst., and also the possibility of influencing its resistance by means of chemical protection. The results showed that natural resistance of robinia wood to these two different agents of wood decay is not the same. It is much less resistant to the fungus Conioph...
R Benko


Protection of wood blocks treated with Trichoderma isolates selected on the basis of preliminary agar screening studies
1996 - IRG/WP 96-10154
Previously reported results of agar interaction screening studies for biocontrol agents of wood decay basidiomycetes showed two Trichoderma viride isolates, killed 16 of 19 target fungi (Tucker and Bruce, 1995). Testing of these isolates in wood was required to assess their performance at preventing decay of wood blocks. Standard testing of chemical wood preservatives is used to determine the toxi...
E J B Tucker, A Bruce, H J Staines


Risk assessment of energetic valorization of treated wood - wooden recycling
1996 - IRG/WP 96-50072
The most useful method for the valorization of wood wastes and wooden wastes is energetic valorization. In France the percentage of wood treated by antisaptain products is around 30%. Currently with the growing regulation, there is a need for cleaner methods and technology to allow sustainable valorization. The preservatives concerned are common organochlorine compounds (NaPCP) less used nowadays ...
G Deroubaix, P Marchal, G Labat


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 1: Laboratory screening tests using a filter paper technique
1977 - IRG/WP 290
Thirty-one miscellaneous formulations have been screened using a filter paper assay technique, for their efficacy in controlling the growth of Chaetomium globosum, Cephalosporium acremonium, and a mixed inoculum of finely ground soft-rotted wood obtained from preservative treated transmission poles. The formulations consisted of various organic compounds and inorganic preparations made from differ...
H Greaves


Termite Field Tests of Various Timber Species Treated with permethrin using supercritical carbon dioxide
2005 - IRG/WP 05-10560
Termite field tests were conducted on permethrin-treated Eucalyptus obliqua heartwood, Pinus radiata sapwood and P. radiata LVL. The permethrin was impregnated using either supercritical carbon dioxide (scCO2) or light organic solvent preservative (LOSP) systems. Comparative permethrin retentions were most accurately achieved in P. radiata sapwood, where no difference between impregnation systems ...
A Qader, L J Cookson, J W Creffield, D Scown


Analysis of water repellents in wood treated with water borne formulations using FTIR
2000 - IRG/WP 00-40176
The use of aqueous water repellent emulsion formulations has increased significantly in the wood treatment industry. These products are primarily used to enhance the weathering characteristics of wood products treated with water borne preservatives systems used in exterior above ground applications. They are also used in pole treatments to improve climbing characteristics and in low VOC millwork t...
P J Walcheski, L Jin


Fungal remediation of CCA-treated wood
2004 - IRG/WP 04-50210
This study evaluates oxalic acid accumulation and bioremediation chromated copper arsenate (CCA) treated wood by three brown-rot fungi, Fomitopsis palustris, Coniophora puteana, and Laetiporus sulphureus and ten mold and staining fungi, Aspergillus niger, Aureobasidium pullulans, Gliocladium virens, Penicillium funiculosum, Rhizopus javanicus, Ceratocystis pilifera, C. peceae, Alternaria alternata...
S N Kartal, Y Imamura


Recycling of treated timber by copper smelter
1994 - IRG/WP 94-50030
A preliminary trial was carried out to see whether copper smelting process is able to recycle CCA treated timber. As a result of the first trial almost a full recovery of both copper and arsenic was achieved. Recovered metals were utilized in manufacturing CCA preservatives. The energy bound in wood is utilized in the flash smelting process and the burning gases are fed to the sulphuric acid plant...
A J Nurmi, L Lindroos


Copper naphthenate-treated Southern Pine pole stubs in field exposure: - Part 1: Gradient & biodeterioration analysis 12 years after treatment
2000 - IRG/WP 00-30242
Naphthenates have been used for the preservation of timber and cellulose since their original identification in Russia in the early 1880's as part of a series of petroleum characterizations. Later work in the development of copper naphthenate as a heavy-duty preservative for poles led to the development of various treating cycles similar to other oil-borne systems. Recent work concerning ...
H M Barnes, M H Freeman


The mechanism of leaching of copper-chrome-arsenic preservatives from treated timber in saline waters
1976 - IRG/WP 374
A mechanism for the leaching of copper-chrome-arsenic preservatives is proposed on the basis of theoretical calculations and experimental studies using timber subjected to a range of water types of different ionic compositions. Complex formation by copper (II) and chromium (III) with chloride and hydroxide ions is shown to affect the leaching rate. Of even greater importance is the salt effect on ...
J Irvine, S-E Dahlgren


Isolation of soil borne bacteria and fungi from treated timber
2001 - IRG/WP 01-50174
Most research in the last few decades has focused on the development of new strategies to control biological attack and the means to quantify this. Comparatively little work has been done to examine the effect that treated timber might have on its surrounding environment. This presentation will describe a methodology that attempts to detect any changes which might occur in the soil microflora foll...
I Stephan, A Stegemann, G Heidrich


Microbial decomposition of salt treated wood
1993 - IRG/WP 93-50001-22
Specialized microorganisms which are able to convert fixed inorganic preservatives from treated wood into water soluble components are investigated. A number of brown rot fungi like Antrodia vaillantii have been isolated from cases of damage and examined under unsterile conditions with CCA-, CCB-, CCF- and CC-treated wood at retention levels of at least 50% higher than recommended for wood in grou...
R-D Peek, I Stephan, H Leithoff


Detection of Termite Attack to Wood Stakes in a Monitoring Station Using Ceramic Gas Sensors and Acoustic Emission (AE) Sensor
2003 - IRG/WP 03-20271
To evaluate the termite activity in monitoring stations non-destructively, metabolic gas from termites and acoustic emission generated by feeding of termites were measured. Ten cylindrical stations with small wood stakes of Japanese red pine (Pinus densiflora) were buried around a house attacked by Coptotermes formosanus SHIRAKI. A sample air in the station was collected by sucking through a drill...
Y Yanase, Y Fujii, S Okumura, T Yoshimura, Y Imamura, T Maekawa, K Suzuki


Raising of the grain and deformation of Scots pine (Pinus sylvestris) treated with water-borne preservatives
1987 - IRG/WP 3456
In Sweden partial impregnation to 10 mm depth of the pine sapwood (class B in the Nordic preservation standard) of joineries was introduced during the seventies. To avoid product quality problems, organic solvent-based systems have been used. However, the Swedish industry today has problems with organic solvents, mainly for environmental reasons. We have studied raising of the grain and deformatio...
G Hägglund, T Sebring