A standardised procedure for the treatment of timber with test chemicals
1986 - IRG/WP 2257
A procedure is described which allows the standardisation of sample handling and data manipulation during trials invastigating the treatability of timber with test chemicals. The use of computer software allows the data to be handled efficiently....
J Norton, A Zosars, L E Leightley


Utility, deterioration and preservation of marine timbers in India
2005 - IRG/WP 05-40314
Timber is extensively used in India in the marine environment for various purposes due to its several advantages over modern materials. Infact, its use is increasing in recent years, finding wider and wider applications and this scenario is not going to change in the near future. Though, the bio-deterioration problem is found very severe in tropical waters, still indigenous methods are widely empl...
B Tarakanadha, M V Rao, M Balaji, P K Aggarwal, K S Rao


Observations on the failure of anti-sapstain treated timber under non-drying conditions
1990 - IRG/WP 1437
A range of bacteria and yeasts were isolated from antisapstain treated timber and fresh sawdust. Solution samples containing 100 ppm of TCMTB in a nutrient medium were inoculated with these organisms and incubated at 25°C for 5 days. The levels of TCMTB remaining in solution were determined by HPLC analysis after this time. Results indicated high losses of active ingredient for a range of organis...
G R Williams


Leaching of Active Components from Preservative Treated Timber. Stage 1: Semi-Field Testing
2004 - IRG/WP 04-20302
The project is aiming at finding realistic leaching rates from preservative-treated wood in use class 3 (above ground). The project focuses on developing a field trial method for investigating leaching. Panels are subjected to outdoor exposure under natural weather conditions at a test field at the Danish Technological Institute. The leachate is collected and monitored by chemical analysis of the...
N Morsing, B Lindegaard


Ecotoxicological risks of anti-sapstain preservatives washed off from treated timber
2000 - IRG/WP 00-50144
A field method for ecotoxicity assessment of rain water wash-off from anti-sapstain treated timber was developed. In the course of this study freshly sawn timber treated with 1.5% Busan 30 L (reference preservative) and a control stack with untreated pine were exposed to weathering. The run-off water was ecotoxicologically tested with organisms from three trophic levels (Vibrio fischeri, Kirchneri...
G Aschacher, R Gründlinger


An insight into brown rot decay of timber as revealed by 13C CP/MAS NMR
1985 - IRG/WP 1259
L E Leightley


Biological agents of timber degradation in Portugal. Marine borers
1991 - IRG/WP 4171
A brief report of the studies carried out in Portugal on marine borers is presented. The marine borers found in the portuguese coast are refered as well as the wood species where those organisms were identified. Emphasis is given to a study carried out from 1960 to 1975 at the Tagus estuary in Lisbon with the purpose, among others, of establishing the natural durability of different timbers....
J S Machado, L Nunes


Wood preservation in East European countries
1989 - IRG/WP 3527
The paper discusses the main problems of wood preservation in Bulgaria, Czechoslovakia, German DR, Hungary, Poland, Rumania and the USSR. The main types of wood preservatives produced have been presented, as well as the state of standarization to test their properties. There have been considered methods of wood treatment in use and application range of treated wood....
J Wazny


The collaborative developement of soil acceptance criteria for timber treatment chemicals in New Zealand
1995 - IRG/WP 95-50040-34
In New Zealand, the issue of potential contamination on timber treatment sites arose in the late 80's due to the long history of use of PCP by the industry. One of the recommendations from the task group set up to investigate the issue was the development of a set of acceptance criteria to define trigger levels for remediation. A technical group from the government, industry and regional ...
H C Boyd


Ultrastructure of the attack of a naturally durable timber by tunnelling bacteria
1990 - IRG/WP 1462
The attack of the wood of Eusideroxylon zwageri, a naturally durable species, by tunnelling bacteria (TB) was examined by light microscopy and transmission electron microscopy. Observations were made primarily on fibres. Parenchyma were included in some cases. Both fibres and parenchyma are rich in extractives. In fibres, extractives are primarily present in the lumen. The amber colouration of fib...
A P Singh, T Nilsson, G F Daniel


Migration of active ingredients from treated timber into fresh water
1991 - IRG/WP 3669
Spruce roundwoods and segments were treated with three different wood preservatives. Two of them containing copper and chromium the other one free of chromium. After fixation (3 weeks, 20°C) the specimens were leached by using artifical rain or by shaking the segments for one hour in contact with demineralized water. The water was analysed for the relevant elements of the preservative tested. Lea...
H Klipp, H Willeitner, K Brandt, A Müller-Grimm


An interim report on studies of the tolerance by Sphaeroma (Crustacea: Isopoda) of CCA-treated timber
1982 - IRG/WP 491
In Papua New Guinea any untreated timber exposed to seawater close to mangrove stands is liable to be attacked in the intertidal zone by the crustaceans Sphaeroma terebrans or Sphaeroma triste. Even CCA-treated timber is sometimes vulnerable. The mouth-parts of these animals are adapted for boring, but whether wood particles are ingested remains to be resolved. Some limbs of Sphaeroma terebrans ap...
S M Cragg, J D Icely


An investigation to assess the feasibility of developing an accelerated laboratory test to determine the abrasion resistance of lesser-used timber species for use in marine constructio
2005 - IRG/WP 05-20317
The paper describes the evaluation of a laboratory-accelerated test to compare the shingle abrasion resistance of current and potential timbers for use in marine construction. Useful results were achieved in 47.5 hours, but identified a number of issues to be resolved for the test to be refined and the subsequent results to be interpreted correctly....
G S Sawyer, J R Williams


Observations on the penetration of preservatives into green timber
1985 - IRG/WP 3335
Differences in the rate and extent of diffusion of MBT and NaPCP-based preservatives following a short dip treatment were observed. The importance of preservative distribution as well as toxicity to the target organisms in governing the ultimate performance of any anti-sapstain compound is discussed....
G R Williams, R A Eaton, D A Lewis


Effects of timber surface properties and dipping conditions on uptake of antisapstain actives from two aqueous suspensions, and ultimate effects on efficacy against mould and staining organisms
1995 - IRG/WP 95-30073
Green-off-saw rough sawn Pinus elliottii (slash pine) boards were dipped in aqueous suspensions of two antisapstain formulations, and the resultant surface retentions of active ingredients MTC (methylene bisthiocyanate), CTL (chlorothalonil) or TCMTB (2(thiocyanomethylthio)benzothiazole) were monitored by chemical analysis. Surface retentions increased with suspension concentration and surface rou...
M J Kennedy, T L Woods


The use of C CP/MAS NMR in the chemical identification of decayed and undecayed, tropical timber species
1984 - IRG/WP 1224
13C CP/MAS NMR was found to be an extremely powerful tool for elucidating the chemical composition of Eucalyptus maculata, Pinus elliottii and Alstonia scholaris. The differences in lignin composition were different for each timber and discussed in relation to decay caused by soft-rot and white rot fungi. In particular the presence of syringyl and guaiacyl lignin types are discussed.
L E Leightley


The biological natural durability of timber in ground contact
1994 - IRG/WP 94-20051
The BRE ground contact field trials for the determination of the biological natural durability of different timber species have recently been reviewed. The data obtained from these trials have been used to appraise the different ways in which natural durability may be expressed. It is concluded that the use of the mean as a method of assigning the timber to one of five durability classes may be ac...
G A Smith, R J Orsler


Inventaire des "déchets" ou produits connexes de la filière bois
1993 - IRG/WP 93-50001-33
G Marcotte


Some biological observations on the management of preservativion experiments with submerged timber in the marine environment
1976 - IRG/WP 421 E
P Deschamps


The benefits to New Zealand of boron salt treatment of Pinus radiata
1992 - IRG/WP 92-3692
The historical reasons for New Zealand adopting boric salt diffusion of Pinus radiata are summarised, and present day processes and their associated costs are given. The biological hazards of using Pinus radiata untreated are then argued, using endemic fungal and insect species as examples, as well as a discussion of the risks from species that may yet be accidentally introduced into the country....
D J Cross


Weather testing of timber - discoloration
2001 - IRG/WP 01-20221
The brightness and color saturation of the timber were reduced over time. The perception of an increasingly dark color in the timber over time is due to the gradual reduction in brightness. The period from May to September was characterized by the greatest discoloration of all three periods of the year. Because this period has the largest number of sunlight hours, and the timber is subjected to a ...
T Toyoda, M Azuma, Y Hikita


Estimation of service life of durable timber species by accelerated decay test and fungal cellar test
2002 - IRG/WP 02-20249
Many kinds of durable wood species for outdoor uses has been imported from all over the world to Japan. However information on the natural durability of these species is not sufficient to estimate the service life of them in the climate of Japan. Highly durable species such as Jarrh, Teak, Ipe, Ekki, Selangan batu, Red wood, Western red cedar showed no significant percent mass losses by accelerate...
K Yamamoto, I Momohara


Regulatory and Consumer Challenges Facing Timber Preservation and Durability Interests in New Zealand and Australia
2003 - IRG/WP 03-20282
Timber preservation and durability interests in Australia and New Zealand are facing many challenges and threats arising from regulation and standards changes, to direct competition from competitive materials producers. Industry can address these challenges by pro-active initiation of sound, holistic, research, that addresses the performance needs of the regulators and specifiers and the expectati...
C MacKenzie


Thirty-four year test of on-site preservative treatments to control decay in wood above ground
1993 - IRG/WP 93-30015
This research was initiated in 1958 to investigate efficacy of various preservatives and treating methods for new lumber going into exterior structures of buildings. Post-rail units (2x4 inches) constructed of Southern Pine sapwood, Douglas-fir heartwood, and mill run western hemlock were dip- or brush-treated before or after assembly. Units were trested with pentachlorophenol in various petroleum...
T L Highley, T C Scheffer


Physical and mechanical properties of a suitable constructional timber of Bangladesh
1997 - IRG/WP 97-40102
The study of physical and mechanical properties of lohasirish timber (Derris robusta Roxb.) grown in Bangladesh revealed that the sapwood is whitish to yellowish white, heartwood is dark grey to blackish in colour; the texture is moderately fine, the grain in mostly straight and coarse with whitish rings of parenchyma; shrinkage is moderate; the EMC ranges from 12% to 16%; fuelwood colorific value...