Standardization of preservative treated timber species for conductor, insulator and transformer packing of REB
1996 - IRG/WP 96-40071
In order to resolve the post landing failure problem of wooden packing for conductor, insulator, transformer of REB, the names of the suitable timber species from different parts of the world, irrespective of countries of origin have been standardized along with their strength and treatability grades. The CCA treatability of some Pakistani timber species have been presented for example which was t...
A K Lahiry


Growth of sapstain fungi in scots pine and the effect of timber ageing
1998 - IRG/WP 98-10269
A trial was initiated to study the growth of known isolates of sapstain fungi in scots pine (Pinus sylvestris) which had been naturally aged or sterilised by autoclaving or irradiation. Sawlogs cut from commercial thinnings were reduced to billet size and the exposed ends were painted with a bituminous sealant to reduce moisture loss. Some billets were inoculated after autoclaving or gamma-irradia...
N J Strong, J F Webber, R A Eaton


Persistance of active ingredients in treated wood
1993 - IRG/WP 93-50001-20
Disposing of chemically protected waste wood implies the distinction between surface and pressure treatment. Considering that barked round-wood merely contains, after 7 months open storage, less than 30 g per ton of bark or 25 mg per ton of sapwood, depending on the type of insecticide, the bark or sapwood shavings may be incinerated normally, according to less severe legal prescriptions than for ...
E Graf, P Manser, S Rezzonico, B Zgraggen


Movement of borates in a range of timber species at various moisture contents
1998 - IRG/WP 98-30181
Borate-based wood preservatives are used in industrial pre-treatment as well as remedial treatment of timbers in situ. In both of these areas, understanding the mobile nature of these compounds is important in optimizing the main benefits of borates. Considerable work has been conducted on movement of borates in dip-diffusion treatment of freshly felled wood, as well as focusing on subsequent diff...
M W Schoeman, J D Lloyd, M J Manning


Timber preservatives and corrosion
1983 - IRG/WP 3228
A survey of preservative treated timber commodities has illustrated problems that may be caused by corrosion. After treatment, timber should be compatible with commonly used fasteners. Whilst many corrosion methods have been used in the past, no standardized method is used by workers in timber preservation. The Queensland Department of Forestry is developing laboratory test methods for assessing c...
R I Davis


Resistance of six timber species, treated with CCA and CCB, against marine borer attack in Goa waters (India)
1991 - IRG/WP 4166
Panels of Lagerstroemia speciosa, Toona ciliata, Olea dioica, Pinus insignis, Acrocarpus fraxinifolius and Borassus flabellifer, pressure-treated with a 6.6% solution of Copper-Chrome-Arsenic (CCA) and 6% solution of Copper-Chrome-Boric (CCB), were exposed along with untreated controls, in triplicate, in Goa waters to, assess their resistance to damage by marine borers. The control panels were all...
L N Santhakumaran, R V Krishnan


Sampling and analysis of NeXgen-treated timber
1998 - IRG/WP 98-20134
Green sawn timber surfaces of the softwood Caribbean pine and the hardwood white cheesewood were treated by dipping, spraying, and precise spiking with the antisapstain product NeXgen. After storing for either two hours or two weeks, the treated surfaces were sampled by one of four alternative protocols, which included two involving a square wad sampling punch (one hit or six hits), one involving ...
M J Kennedy, D E Ferlazzo, T L Woods, M H Freeman


Field tests with Antiblue and Biocide TT for the prevention of sapstain and mould fungi on Pinus elliottii timber
1992 - IRG/WP 92-3682
Freshly cut and sawn Pinus elliottii timber was dipped in four concentrations of Antiblue (active ingredient sodium pentachlorophenate) and Biucide TT (local substitute), at four immersion times and stacked in the open at Chisengu sawmill. Five weeks later, the timber was assessed for the incidence and intensity of stain and mould. The results showed that Antiblue was the better chemical providing...
A J Masuka


Detoxification of methylene bisthiocyanate by bacteria isolated from freshly felled, anti-sapstain treated timber
1993 - IRG/WP 93-10017
The microbial defacement of freshly-felled timber treated with organic biocides continues to be a major problem in stored lumber. As part of a study to investigate the depletion in chemical activity of methylene-bis-thiocyanate (MBT) in green timber, bacteria were isolated from freshly-felled boards of Corsican pine (Pinus nigra var. maritima Arnold) previously treated with different biocides. The...
R J Wallace, R A Eaton, G R Williams


Detection of methanogenic bacteria in mining timber
1988 - IRG/WP 1352
Methane explosions in gold mines have been attributed to spontaneous ignition of methane/air mixtures. Biogenesis of methane in the heartwood of diseased trees has been shown, but never in timber in service. Studies were therefore undertaken to establish whether methanogens were present in wooden pit props. Core samples were removed by Pressler increment borer from props in disused areas 2,600 m d...
L D Abraham, K Westlake, R I Mackie, J F Putterill, A A W Baecker.


An attempt to grow dry rot fungus Serpula lacrymans on mortar substrate in non-sterile conditions
1989 - IRG/WP 1385
According to many experts, Serpula lacrymans is probably the most dangerous wood destroying fungus in houses. Investigations of KOCH, A.P. (2) showed that incidence of this fungus in percent was around 20% when the frequency of some other standard fungi was far below (Coriolus versicolor: 0.2% for example). The work presented here is a part of a program carried out at CTFT for assessing the resist...
L N Trong


Leaching of active components from preservative-treated timber. Stages 2 & 3: Laboratory testing and comparison with semi-field testing
2004 - IRG/WP 04-20303
This part of the project is focussed on leaching from preservative-treated wood obtained by the laboratory test method CEN/OECD draft guideline, February 2003 ”OECD guideline for the testing of chemicals proposal for new guideline XXX. Estimation of Emissions from Preservative-treated Wood to the Environment: Laboratory Method for wood held in the storage yard after treatment and for wooden comm...
N Morsing, B Lindegaard


Sawn timber of fir (Abies alba Mill.) - Treatability and usability for the Hazard Classes 3 and 4
1999 - IRG/WP 99-40147
Within a national research project, tests on the treatability on sawn timber of fir (Abies alba Mill.) in oscillation pressure, vacuum pressure and double-vacuum processes have been worked out with 95 trunks taken from 3 different altitude levels (up to a height of 590 metres, 600 to 990 metres and over 1000 metres) and from 4 different regions of Switzerland. As the treatability of round wood can...
E Graf, T Bör


A field test with anti-stain chemicals on sawn pine timber in Brazil
1989 - IRG/WP 3513
Field tests were carried out in São Paulo State - Brazil, to evaluate pre-treatment formulations of O-Phenyl-Phenol (OPP) based products. The Sodium Pentachlorophenate solution was used as a reference formulation. The treated test blocks were stacked in a covered shed, and in an uncovered place for air drying. The evaluation was done by measuring the percentage of stained surface on each test blo...
M B B Monteiro, S Brazolin


Breakdown of cellulose derivatives by cellulolytic enzymes. I. Action of fungal ß-glucosidases toward substituted PNP ß-D-glucopyranosides
1998 - IRG/WP 98-10281
The action of fungal ß-glucosidases on the methyl derivatives of p-nitrophenyl (PNP) ß-D-glucopyranoside, which were regioselectively substituted at 0-2, 0-3, 0-4 and 0-6 positions was studied. Several ß-glucosidases from brown-rot, white-rot, and soft-rot fungi and almond were used for the study. These ß-glucosidases did not act on the 2, 3, and 4-0-methyl derivatives, while the 6-0-methyl on...
T Nishimura, I Momohara, M Ishihara


Evaluation of the insecticidal efficacy of deltamethrin and the fungicidal efficacy of its association with TCMTB + MBT in the field of wood preservation
1986 - IRG/WP 1289 E
Deltamethrin possesses many advantages for the insecticidal protection of wood: relatively low toxicity, very reduced evaporation, very prolonged retention in the wood, very slight leaching after having penetrated the wood, and absence of odour. Its association with other active agents or solvents is being studied with regard to chemical compatibility. Compatibility studies have proved positive fo...
J S Duguet


Characteristics and quantity of impregnated wood waste in Germany
1995 - IRG/WP 95-50041
The disposal of wood waste in Germany is one of the main problems not only for the wood preservation industry but also for all concerned with wood waste. Data on characteristics and quantity of wood waste are still needed. Based on criterions given in a previous paper (IRG/WP 93-50006), several assortments have been characterized with regard to their hazardous potential and their logistical aspect...
A Voss, H Willeitner


Which substrate to use in a laboratory test with soft rot micro-fungi: vermiculite or unsterile soil?
1991 - IRG/WP 2372
A draft European Standard is being proposed by CEN TC 38 in which a vermiculite-burial and a soil-burial test to be carried out in succession are required. Various experiments with both procedures were set up with CCA, CC and propiconazole-formulations. The results show that vermiculite and unsterile soil yield comparable threshold values against soft rot. This poses the question of whether a two-...
A R Valcke


Dutch national environmental policy strategy (NMP): Implications throughout the life cycle of treated timber and for the Dutch preservation industry
1993 - IRG/WP 93-50001-31
All overview of relevant environmental legislation and instruments for control is given for each stage of the life cycle of treated timber. Recent policy in the Netherlands has been focused around the "National Environmental Policy Strategy", in which a general policy with regard to reduction of pollution to the air, soil and water is described. The principle is one of an "Integrated Chain of Cont...
P Esser, D A Lewis, A J Pendlebury


Effect of moisture and cellulosic substrate on decay of hardwoods by soft-rot fungi
1982 - IRG/WP 2173
The development by Forintek Canada Corp. of standard test procedures for laboratory preservative evaluations using soft-rot fungi was requested by the American Wood Preservers' Association. In Europe, through cooperative studies in the International Research Group on Wood Preservation, several attempts have been made to produce a standard procedure, but variability in results obtained bet...
A Byrne, R S Smith


Utilization of coconut timber from north Sulawesi, Indonesia. Part 2: Treatability
1994 - IRG/WP 94-40025
Under tropical conditions coconut wood is quickly degraded by mold and blue stain fungi. Low density wood in ground contact is commonly decomposed by wood destroying fungi within a period of only a few months, higher density wood from the outer stem regions within 24 to 30 months (MOSTEIRO, CASIN, SERIBAN 1976; McQUIRE 1975). Moreover, according to McQUIRE (1975) green wood of lower density is hig...
R-D Peek


Leaching of arsenic, copper and chrome from preservative-treated timber in playground equipment
1984 - IRG/WP 3149
Samples were taken from CCA-treated timber in sand play boxes and other play ground equipment. Sand was also sampled. Sand and wood samples were analysed for copper, chrome and arsenic by AAS. About 20-25% of the arsenic had leached from the timber after 2-4 year's exposure in the playgrounds. Very little of the copper and chrome had been leached. Sand collected in the close vicinity of t...
B Henningsson, B Carlsson


Natural durability of larch heartwood against decay
1997 - IRG/WP 97-10201
Larch heartwood has been promoted in Sweden and in other European countries as an alternative to preservative treated timber. It has even beeen stated that larch heartwood is more durable than preservative treated timber. This paper presents a compilation of facts from scientific reports on the durability of larch heartwood. Some recent data from this department are also reported. All data suggest...
T Nilsson


In-house accelerated method for testing decay resistance of treated wood
2004 - IRG/WP 04-20286
Fungicidal compounds often change their effectiveness when they are incorporated into candidate formulations. For this reason fungistatic effectiveness needs to be re-evaluated as many times as the formula has been modified for better performance. To avoid multiple expenses, in-house fungistatic tests are essential. Our goal was to develop in-house usable, simple but reliable and reproductive proc...
N Vidovic


Evaluation of the effectiveness of defence anti-stain in the control of sapstain in laboratory and field tests
1990 - IRG/WP 3593
The anti-sapstain product Defence Anti-stain (DAS) has been evaluated internationally in laboratory and field tests during the years 1988 and 1989. Results of tests carried out by institutes and by own companies in countries like Indonesia, Ivory Coast, Japan, Portugal, Belgium, The Netherlands and Spain will be presented. In the several tests Defence Anti-stain showed a high fungicidal activity t...
G Rustenburg, C J Klaver


Previous Page | Next Page