The effect of extent and location of decay on strength loss in constructional timber
1994 - IRG/WP 94-30039
Radiata pine heartwood billets, 50 x 100 x 1000 mm³ were end-sealed and treated with copper-chrome-arsenate preservative (NZ Type I) to a range of retentions and penetration patterns. Cross-sections, 10 mm thick, were cut from the centre of each billet and used for determination of preservative distribution, for preservative analysis and for decay tests. The decay test consisted of laying samples...
M E Hedley, H Bier


On-site test for indicative determination of leaching of components of preservatives from treated timber
1993 - IRG/WP 93-50001-12
In the late eighties the environmental concern about treated timber increased and it is still a hot issue in the Netherlands. From the environmental point of view three phases in the timbers life cycle can be distinguished: - the production phase - the service life - the waste phase. In the Netherlands at this moment much emphasis is laid on the production phase. In 1992 this has led to a new legi...
W J Homan, H Militz


Penetration of surface applied deltamethrin micro-emulsion formulations in four European timber species
1994 - IRG/WP 94-20030
The Netherland's Government, in line with many other European Governments initiated a programme (KWS2000) aimed at significantly reducing the emission of volatile organic compounds by the year 2000. As part of this programme a research project is currently underway to evaluate the potential for replacing organic solvent based remedial treatments with micro-emulsion formulations of the sam...
P Esser, W L D Suitela, A J Pendlebury


Occupant re-entry times following insecticidal remedial treatments of timber in dwellings
1995 - IRG/WP 95-50055
This work was carried out principally to obtain quantitative data on the aerial concentrations of permethrin and white spirit likely to arise following the remedial treatment of timber in buildings, using insecticidal formulations. Such data are needed to allow assessments to be made of the length of time buildings should remain unoccupied following such treatments prior to re-occupation, and the ...
R J Orsler, G E Holland, G M F Van Eetvelde


Quality of timber impregnated with preservatives of class AB after three years in service
2002 - IRG/WP 02-20241
Quality of impregnated timber is most often expressed by penetration and retention of the preservative used. Relatively less information is available about the performance of the final product, e.g. decks, panels etc. regarding product’s surface checks, deformations and overall appearance. Together with the timber durability, the above mention features are of esthetical importance in the above g...
N Terziev


Termite Field Tests of Various Timber Species Treated with permethrin using supercritical carbon dioxide
2005 - IRG/WP 05-10560
Termite field tests were conducted on permethrin-treated Eucalyptus obliqua heartwood, Pinus radiata sapwood and P. radiata LVL. The permethrin was impregnated using either supercritical carbon dioxide (scCO2) or light organic solvent preservative (LOSP) systems. Comparative permethrin retentions were most accurately achieved in P. radiata sapwood, where no difference between impregnation systems ...
A Qader, L J Cookson, J W Creffield, D Scown


Alternatives to CCA for ground contact protection of timber: a perspective from UK on performance and service life expectations
2002 - IRG/WP 02-30289
The proposed amendment to the European Union's Marketing and Use Directive (1976/769/EEC) in respect of arsenic in CCA wood preservatives seeks to restrict the use of CCA across the European Union. CCA is an extremely important wood preservative in the UK from the manufacturing of the product to the extent of use of CCA-treated timber. Based on our experience and judgement on the use of ...
E D Suttie, A F Bravery, T B Dearling


SEM investigation of the production of extracellular mucilaginous material (ECM) by some wood inhabiting and wood decay fungi when grown on inert surfaces
1997 - IRG/WP 97-10194
A range of wood inhabiting and wood decay fungi have been studied for their production of extracellular mucilage when grown on inert surfaces, for comparison with their growth on wood. The species tested were: Coniophora puteana, Coriolus versicolor, Chaetomium globosum, Trichoderma harzianum, Ceratocystis coerulescens, Ophiostoma piceae, Mucor sp. and Penicillium sp. They were grown on plastic me...
A R Abu, R J Murphy, D J Dickinson


Recycling of treated timber by copper smelter
1994 - IRG/WP 94-50030
A preliminary trial was carried out to see whether copper smelting process is able to recycle CCA treated timber. As a result of the first trial almost a full recovery of both copper and arsenic was achieved. Recovered metals were utilized in manufacturing CCA preservatives. The energy bound in wood is utilized in the flash smelting process and the burning gases are fed to the sulphuric acid plant...
A J Nurmi, L Lindroos


The mechanism of leaching of copper-chrome-arsenic preservatives from treated timber in saline waters
1976 - IRG/WP 374
A mechanism for the leaching of copper-chrome-arsenic preservatives is proposed on the basis of theoretical calculations and experimental studies using timber subjected to a range of water types of different ionic compositions. Complex formation by copper (II) and chromium (III) with chloride and hydroxide ions is shown to affect the leaching rate. Of even greater importance is the salt effect on ...
J Irvine, S-E Dahlgren


Isolation of soil borne bacteria and fungi from treated timber
2001 - IRG/WP 01-50174
Most research in the last few decades has focused on the development of new strategies to control biological attack and the means to quantify this. Comparatively little work has been done to examine the effect that treated timber might have on its surrounding environment. This presentation will describe a methodology that attempts to detect any changes which might occur in the soil microflora foll...
I Stephan, A Stegemann, G Heidrich


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 21: Report of eighth inspection (7 years) in Australia
1985 - IRG/WP 4119
This report tabulates the seven year (86 month) inspection results, obtained on 28 Fabruary l985, of the IRG/COIPM International Marine Test at Goat Island, Australia. This test was installed in December 1977. The results are given in Tables 1-6. Table 7 lists the number of marine borers identified from blocks (2 cm and 6 cm long respectively) cut from the ends of specimens removed at the previous...
L J Cookson, J E Barnacle


Production of exraxellular hydrogen peroxide and oxalic acid by brown-rot fungus Poria placenta
1995 - IRG/WP 95-10112
Hydrogen peroxide and oxalic acid have been suggested to be essential in the degradation of wood carbohydrates by brown-rot fungi. Hydrogen peroxide has been suggested to be one of the diffusible low molecular weight agents produced by brown-rot fungi for the degradation of wood carbohydrates by generating highly active radicals. The production of hydrogen peroxide and oxalic acid by Poria placent...
A-C Ritschkoff, M Rättö, J Buchert, L Viikari


Volatile organic compounds (VOC) measured during drying of impregnated timber
2004 - IRG/WP 04-50216
Discussion about drying of impregnated timber has taken place in the Nordic countries under eighties and nineties and goes on nowadays. The drying increase the value of production and the customer gets fewer problems when handles the timber. This introduces a positive attitude to the impregnation as a process and its products. Beside the important information about the advantages of impregnated ti...
N Terziev, V Djokic


A field test with anti-sapstain chemicals on sawn pine timber stored and seasoned under different conditions
1984 - IRG/WP 3245
Newly sawn timber of European redwood (Pinus sylvestris L.) was dip treated in four different anti-sapstain chemicals. The protectife effect against sapstain, mould and decay was examined after 10 weeks' and 10 months' storage in open and closed stacks. The results showed that the performance of individual chemicals was different in open and close stacks, although the wood as wel...
D J Dickinson, B Henningsson


Premature failure of treated timber in wharfs in Papua New Guinea, attributed to defects in design
1991 - IRG/WP 4158
The performance of timber in wharfs in Papua New Guinea has been monitored for a number of years. Premature failure of wharf structures was found in many cases to be due to defects in design rather than ineffective preservative treatment. Above-water timbers were found to be prone to severe checking followed by decay. Protection for the end grain of pile tops and the limiting of radial checking in...
S M Cragg


Interim report on world survey of sap displacement impregnation of timber
1974 - IRG/WP 329
At the 4th Annual Meeting of the IRG held in West Berlin in October 1972 it was suggested that a survey of sap displacement impregnation of timber would be of interest. Accordingly through the courtesy and co-operation of the New Zealand Department of Trade and Industry a questionnaire was circulated to the Trade Commissioners for transmission to the relevant organisations in various parts of the ...
F B Shorland, C G W Mason


Wood preservation in Australia
1984 - IRG/WP 3316
Wood preservation in Australia is presented as an integral part of the forest products industry. The history of its development, as well as its current status and activities are described. Preservation operations in Australia are broadly based, and the industry diversified to combat a wide range of hazards, and to utilise many wood species, for differing end-uses. The Timber Preservers’ Associat...
H Greaves


Leaching of active components from preservative-treated timber - Ongoing research: Status after approx. 4 months’ out-door exposure
2003 - IRG/WP 03-20276
The Danish Technological Institute is together with manufacturers of active ingredients and formulators of wood preservatives running a project aiming at finding realistic leaching rates from preservative treated wood in hazard class 3 (above ground). The project is focussed on developing a field trial method for investigating leaching. According to BPD hazard assessment has to be carried out f...
N Morsing


Studies on the resistance of DMDHEU treated wood against white-rot and brown-rot fungi
2005 - IRG/WP 05-10566
Beech wood (Fagus sylvatica) modified with the textile finishing agent 1,3 dimethylol-4,5-dihydroxyethylen urea (DMDHEU) has shown to improve durability against the white-rot fungus Trametes versicolor. In a mini-block test, the weight loss over eight weeks of incubation decreased with increasing weight percent gain (WPG) of DMDHEU. At 25% WPG, no significant weight loss was observed, while untrea...
P Verma, C Mai, A Krause, H Militz


Bacterial brown stain on sawn timber cut from water-stored logs
1992 - IRG/WP 92-1532
Brown stains which appear on the surface of sawn radiata pine cut from water-stored logs were identified as tannin-like compounds. They are derived from bacterial breakdown of flavanoid-glucosides. When timber is sawn from infected logs, the free flavanoids migrate to the wood surface as the timber dries. There, they condense and oxidise to form permanent brown discolourations. Stains occurred on ...
M E Hedley, R Meder


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 6: Report of third inspection (24 months) in Australia
1980 - IRG/WP 456
This report presents the results of the third inspection of the IRG/COIPM International Marine Test specimens installed at the Goat Island Marine Biological Station of the Maritime Services Board of New South Wales, in Sydney Harbour. The inspection was completed on 5th December, 1979, after 24 months exposure. As on previous occasions, this inspection was carried out in conformity with the provis...
J Beesley


The natural durability assessments of secondary timber species - field trials
1998 - IRG/WP 98-10297
Secondary or 'alternative' hardwood timber species can replace traditional hardwoods and contribute significantly to satisfying the overall demand for hardwoods in the UK timber market. A selection of these 'alternative' hardwoods is currently being tested at BRE-WTC for natural durability both in ground contact (to EN252) at two field sites, and out of ground c...
E D Suttie, R J Orsler


Exotic timber insect species intercepted in the UK since 1945
1978 - IRG/WP 182
Since the formation of an entomology section at the former Forest Products Laboratory, Princes Risborough, the Laboratory has been called upon to identify and comment upon a wide range of insects and insect damage in imported timber. Very often only the damage remains and frequently dead insects are associated with it, but on other occasions living exotic wood-boring insects enter the UK. Followin...
J M Baker, R W Berry


Dip-diffusion of dressed timber - Effect of drying
1990 - IRG/WP 3603
The effect of drying on BFCA dip-diffused, dressed, freshly sawn timber was determined by the depth of penetration of boron achieved on two test timber species, White Cheesewood (Alstonia scholaris) and Light Hopea (Hopea papuana). The results obtained showed that the light density White cheesewood was completely penetrated even after 3 days drying while Light Hopea, treated immediately achieved 5...