Experimental test site to prevent maritime pine logs from bluestaining: water-spraying and water-immersion methods
2003 - IRG/WP 03-10497
Following a storm which led to windfall wood, a research project was launched to develop preservation methods with a low environmental impact for maritime pine logs. These preservation methods are intended to be suitable for large-scale storage areas of maritime pine. In addition the aim was to maintain wood quality during long term storage. An experimental field test with 1 900 m3 of maritime pin...
I Le Bayon, H Callot, D Reuling, C Brunet, P Castéra


CEN Draft Standard (38 N 460F): Méthode d'essai pour determiner l'efficacité d'un produit de préservation du bois en milieu marin
1986 - IRG/WP 4132 F
G Castan


Proposed test procedure to determine the effect of timber substrate on the effectiveness of a copper/chrome/arsenic preservative in seawater
1975 - IRG/WP 411
R A Eaton


The Fifth Annual Report of the International Research Group on Wood Preservation 1973-1974
1974 - IRG/WP 531
IRG Secretariat


Rapport sur l'activité du Comité CEN/TC 38 "Méthodes d'essais des produits de préservation des bois" du Comité Européen de Normalisation (CEN)
1986 - IRG/WP 2266
G Castan


Editorial corrections to Document No: IRG/WP/304
1972 - IRG/WP 305
Anonymous


The rate of redistribution and loss of leachable preservatives under service conditions
1993 - IRG/WP 93-30026
This paper describes experiments carried out to determine patterns of preservative redistribution and any associated losses which occur when wood containing unfixed water-soluble wood preservatives is exposed to service conditions where leaching is possible. Scots pine sapwood treated with disodium octaborate was used as a model system. Results are recorded and discussed for trials representing pa...
R J Orsler, G E Holland


Framework document for an international code of good practices for wood preservation and wood protection (anti-sapstain) facilities
1992 - IRG/WP 92-3683
At the Kyoto meeting, the Health & Safety committee agreed to form a task force to prepare a global plan for writing a code of good practices (Code) for wood protection and preservation facilities (Doc. No. IRG/WP/3681). The Canadian document had been presented to the IRG group earlier (Doc. No. IRG/WP/3447) and similar documents were solicited from other countries for preparing a framework do...
V N P Mathur, G Das


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water: Final report
1987 - IRG/WP 4133
Three timbers chosen as reference species were treated with 3, 6 and 10% solutions of CCA and CCB preservatives and exposed for up to 93 months at 8 tropical and temperate marine sites. Eleven local species treated in the same way were exposed at 4 of the 8 sites. There was no apparent difference in performance between CCA and CCB treated specimens. The severest test site was Panama Canal but mari...
R A Eaton


The Second Annual Report of the International Research Group on Wood Preservation 1970-1971
1971 - IRG/WP 502
IRG Secretariat


The Fifteenth Annual Report of the International Research Group on Wood Preservation 1985-1986
1986 - IRG/WP 5243
R Cockcroft


The International Research Group on Wood Preservation
1979 - IRG/WP 582
J M Baker


An insight into brown rot decay of timber as revealed by 13C CP/MAS NMR
1985 - IRG/WP 1259
L E Leightley


New developments in wood preservation
1974 - IRG/WP 335
Most of the developments in wood preservation in recent years have been stimulated by changing circumstances, particularly the increasing interest in reducing hazards and environmental, pollution but also the serious difficulties that are now being encountered in obtaining economic supplies of established preservatives. There is perhaps a danger that new controls to reduce pollution dangers may be...
B A Richardson


The biological natural durability of timber in ground contact
1994 - IRG/WP 94-20051
The BRE ground contact field trials for the determination of the biological natural durability of different timber species have recently been reviewed. The data obtained from these trials have been used to appraise the different ways in which natural durability may be expressed. It is concluded that the use of the mean as a method of assigning the timber to one of five durability classes may be ac...
G A Smith, R J Orsler


Estimation of service life of durable timber species by accelerated decay test and fungal cellar test
2002 - IRG/WP 02-20249
Many kinds of durable wood species for outdoor uses has been imported from all over the world to Japan. However information on the natural durability of these species is not sufficient to estimate the service life of them in the climate of Japan. Highly durable species such as Jarrh, Teak, Ipe, Ekki, Selangan batu, Red wood, Western red cedar showed no significant percent mass losses by accelerate...
K Yamamoto, I Momohara


Wood preservation and the environment: A Canadian perspective
1990 - IRG/WP 3577
The non-pressure (surface) and pressure treatment of wood impacts on the environment in four ways. These are: through the production of treated wood at sawmills and pressure treating facilities; during the storage of treated wood prior to use; when the pressure treated wood is placed in service; and finally, when the treated product reaches the end of its useful life and must be disposed. By refer...
J N R Ruddick


Biological agents of timber degradation in Portugal. Marine borers
1991 - IRG/WP 4171
A brief report of the studies carried out in Portugal on marine borers is presented. The marine borers found in the portuguese coast are refered as well as the wood species where those organisms were identified. Emphasis is given to a study carried out from 1960 to 1975 at the Tagus estuary in Lisbon with the purpose, among others, of establishing the natural durability of different timbers....
J S Machado, L Nunes


Rapport sur l'activité du CNE/TC 38 'Méthodes d'essais des produits de préservation du bois'
1977 - IRG/WP 288
G Castan


An investigation to assess the feasibility of developing an accelerated laboratory test to determine the abrasion resistance of lesser-used timber species for use in marine constructio
2005 - IRG/WP 05-20317
The paper describes the evaluation of a laboratory-accelerated test to compare the shingle abrasion resistance of current and potential timbers for use in marine construction. Useful results were achieved in 47.5 hours, but identified a number of issues to be resolved for the test to be refined and the subsequent results to be interpreted correctly....
G S Sawyer, J R Williams


Studies on the preservation of structrual plywood - Part 1: Decay resistance of structural plywood
1974 - IRG/WP 238
The weight loss and the decreases in the compression strength and in the modulus of elasticity were measured to determine the decay resistance of structural plywood (lauan). Test pieces (50x25xA mm³) were exposed to the wood destroying fungi (Coriolus versicolor and Coriolellus palustris) for 2-3 or 2-4 months. After exposure, the measurement of the compression strength was carried out on the pie...
K Minami, Y Kenjo, S Sugiyama


Tests on preservation of wood against marine borers
1976 - IRG/WP 417
The Instituto del Legno has carried out for some years a series of trials about the biodeterioration of wood in the sea. The investigations included the settlement and activity of marine borers, the natural durability of indigenous and tropical woods and the preservation of wood for marine use. This paper reports the trials on the effectiveness of some preservatives in protecting wood against mari...
A Gambetta, E Orlandi


Thirty-four year test of on-site preservative treatments to control decay in wood above ground
1993 - IRG/WP 93-30015
This research was initiated in 1958 to investigate efficacy of various preservatives and treating methods for new lumber going into exterior structures of buildings. Post-rail units (2x4 inches) constructed of Southern Pine sapwood, Douglas-fir heartwood, and mill run western hemlock were dip- or brush-treated before or after assembly. Units were trested with pentachlorophenol in various petroleum...
T L Highley, T C Scheffer


Observations on the penetration of preservatives into green timber
1985 - IRG/WP 3335
Differences in the rate and extent of diffusion of MBT and NaPCP-based preservatives following a short dip treatment were observed. The importance of preservative distribution as well as toxicity to the target organisms in governing the ultimate performance of any anti-sapstain compound is discussed....
G R Williams, R A Eaton, D A Lewis


Questionnaire on university instruction in the subject of wood preservation
1977 - IRG/WP 79
J Wazny