IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 442 documents. Displaying 25 entries per page.


Premature failure of treated timber in wharfs in Papua New Guinea, attributed to defects in design
1991 - IRG/WP 4158
The performance of timber in wharfs in Papua New Guinea has been monitored for a number of years. Premature failure of wharf structures was found in many cases to be due to defects in design rather than ineffective preservative treatment. Above-water timbers were found to be prone to severe checking followed by decay. Protection for the end grain of pile tops and the limiting of radial checking in...
S M Cragg


Interim report on world survey of sap displacement impregnation of timber
1974 - IRG/WP 329
At the 4th Annual Meeting of the IRG held in West Berlin in October 1972 it was suggested that a survey of sap displacement impregnation of timber would be of interest. Accordingly through the courtesy and co-operation of the New Zealand Department of Trade and Industry a questionnaire was circulated to the Trade Commissioners for transmission to the relevant organisations in various parts of the ...
F B Shorland, C G W Mason


Leaching of active components from preservative-treated timber - Ongoing research: Status after approx. 4 months’ out-door exposure
2003 - IRG/WP 03-20276
The Danish Technological Institute is together with manufacturers of active ingredients and formulators of wood preservatives running a project aiming at finding realistic leaching rates from preservative treated wood in hazard class 3 (above ground). The project is focussed on developing a field trial method for investigating leaching. According to BPD hazard assessment has to be carried out f...
N Morsing


Bacterial brown stain on sawn timber cut from water-stored logs
1992 - IRG/WP 92-1532
Brown stains which appear on the surface of sawn radiata pine cut from water-stored logs were identified as tannin-like compounds. They are derived from bacterial breakdown of flavanoid-glucosides. When timber is sawn from infected logs, the free flavanoids migrate to the wood surface as the timber dries. There, they condense and oxidise to form permanent brown discolourations. Stains occurred on ...
M E Hedley, R Meder


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 6: Report of third inspection (24 months) in Australia
1980 - IRG/WP 456
This report presents the results of the third inspection of the IRG/COIPM International Marine Test specimens installed at the Goat Island Marine Biological Station of the Maritime Services Board of New South Wales, in Sydney Harbour. The inspection was completed on 5th December, 1979, after 24 months exposure. As on previous occasions, this inspection was carried out in conformity with the provis...
J Beesley


The natural durability assessments of secondary timber species - field trials
1998 - IRG/WP 98-10297
Secondary or 'alternative' hardwood timber species can replace traditional hardwoods and contribute significantly to satisfying the overall demand for hardwoods in the UK timber market. A selection of these 'alternative' hardwoods is currently being tested at BRE-WTC for natural durability both in ground contact (to EN252) at two field sites, and out of ground c...
E D Suttie, R J Orsler


Exotic timber insect species intercepted in the UK since 1945
1978 - IRG/WP 182
Since the formation of an entomology section at the former Forest Products Laboratory, Princes Risborough, the Laboratory has been called upon to identify and comment upon a wide range of insects and insect damage in imported timber. Very often only the damage remains and frequently dead insects are associated with it, but on other occasions living exotic wood-boring insects enter the UK. Followin...
J M Baker, R W Berry


Dip-diffusion of dressed timber - Effect of drying
1990 - IRG/WP 3603
The effect of drying on BFCA dip-diffused, dressed, freshly sawn timber was determined by the depth of penetration of boron achieved on two test timber species, White Cheesewood (Alstonia scholaris) and Light Hopea (Hopea papuana). The results obtained showed that the light density White cheesewood was completely penetrated even after 3 days drying while Light Hopea, treated immediately achieved 5...
H C Konabe


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 14: Report of fifth inspection (48 months) in Australia
1982 - IRG/WP 484
This report presents the results of the fifth inspection of the IRG/ COIPM Internatlonal Marine Test specimens installed in Sydney Harbour in December, 1977. This inspection took place on 9th December, 1981, just 48 months after the specimens were installed. Earlier reports have contained full details of the treatment and installation of the specimens as well as results of all previous inspections...
J Beesley


The colonisation pattern of anaerobic fungi in wood
1989 - IRG/WP 1403
Timber foundations may be degraded in service in anaerobic conditions. The present work was conducted to investigate whether anaerobic fungi could colonise wood, using rumen fungi as test microorganisms. Strictly anaerobic fungi were isolated and purified from cow dung and goat and sheep rumen fluids respectively. Colonisation of Eucalyptus grandis and Pinus patula by these fungi and Neocallimasti...
A H Wiederhold, M Morrison, A A W Baecker


Structural defects in CCA treated timber fence posts: A case study.
1997 - IRG/WP 97-40084
Since 1983 an environmental improvement programme has been in progress in the city of Dundee. This programme included the erection of rail and pale timber fencing throughout the city. The timbers had been pressure treated with CCA prior to painting with 2 coats of an exterior wood stain finish. However, the larger dimension timber fence posts (100 x 125 x 1500 mm3) regularly developed severe check...
S Muhsin, D C R Sinclair, A Bruce, H J Staines


Ecotoxicological behaviour of leachates from superficially treated timber as an approach for a test strategy of environmental risk assessment in wood preservation
1998 - IRG/WP 98-50101-09
At present for wood preservatives, which in Germany are subject to the quality mark of the RAL-GĂĽtegemeinschaft Holzschutzmittel, health and safety as well as environmental aspects are evaluated by official authorities, as BgVV (Federal Institute for Consumer Health Protection and Veterinary Medicine) and the UBA (Federal Environmental Agency). From the environmental point of view to day there a...
H W Wegen, U J Lucks


Durability of Anogeissus acuminata timber used for plank-built catamarans
2005 - IRG/WP 05-10551
Catamaran, the most versatile traditional fishing craft used along the Indian coast is made hitherto of solid timber of a few selected species of broad-leaved soft woods. Due to scarcity coupled with high cost of these timbers, the craft, of late, are fabricated from the wooden planks of an indigenous hardwood species, namely, Anogeissus acuminata (Yon) belonging to the family Combretaceae. Infor...
M V Rao, M Balaji, V Kuppusamy, K S Rao


Natural durability of fifty species of Indian timber in Goa waters against marine wood-borers
1989 - IRG/WP 4150
Results of the investigations on the natural durabilitv of fifty species of Indian timber, based on data collected bv exposing test panels at Betim near Panaji (Goa) continuously for a period of 11 months are presented. The study revealed that none of the timber species tested has any natural resistance at this locality and all the panels were completely destroyed within 11 months. Details on the ...
L N Santhakumaran, S Udaya Bhaskar, J C Jain


Performance of preservative-treated timber against biodeterioration in Indian waters
1984 - IRG/WP 4106
Results on the investigation on the durability of panels of 32 timber species, pressure-treated with various preservatives and exposed along the Indian coast for varying periods upto a maximum of 15 years, are summarised. Panels of even non-durable timber gave excellent results against biodeterioration after treatment. Their life was comparable to that of treated durable timber. The preservative t...
L N Santhakumaran, J C Jain, M C Tewari


Losses of CCA components and creosote from treated timber to soil
1997 - IRG/WP 97-50098
Components of creosote and CCA preservatives can migrate within the wood and move into surrounding soil. However, at present, the ecological significance of such losses is uncertain. This paper examines the distribution of four target polyaromatic hydrocarbons (PAHs ) and of copper, chromium and arsenic in treated stakes and surrounding soil after long term exposure in field trials. Concentrations...
N J Hudson, R J Murphy


Timber deterioration and its prevention in marine environment
2005 - IRG/WP 05-10559
Wood-borer activity is an established fact in Mumbai harbour that leads to severe deterioration of timber. In order to prevent the deterioration caused by wood borers three resin preservatives containing Zinc borate, Organo-copper polymer (4 wt% Cu) and Organo-Tin polymer Copoly(TBTM-MMA) were used for timber treatment. Test panels were treated using standard method and the...
B S Swami, M Udhayakumar, P Kumar, A B Samui


On the laboratory use of X-rays in timber decay evaluations
1981 - IRG/WP 2144
The paper reports the results of laboratory experiments on the X-raying of some Pinus radiata sapwood blocks infected with Serpula lacrymans to determine the effect of density and moisture content on the absorption of X-rays by wood. It is concluded that with increasing moisture content there is a very marked increase in time required to pass a constant quantity of X-rays through a test block and ...
J D Thornton, J W Creffield, O Collett


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 18. Report of seventh inspection (72 months) in Australia
1984 - IRG/WP 4108
This report includes the results for the 72 month inspection of the IRG/COIPM International Marine Test installed in Sydney Harbour. Although, overall, attack by teredinid and limnorid borers have been most commonly encountered in test specimens at this site, slight attack, mainly by sphaeromatids, has recently been initiated on some hitherto unattacked treated Alstonia scholaris and Pinus sylvest...
L J Cookson, J E Barnacle


Preservative treatment of green timber by diffusion
1984 - IRG/WP 3291
The preservative treatment of green timber by diffusion is reviewed together with criteria which influence the economics of the process. New process options are described which should overcome some of the technical and economic disadvantages of double diffusion. These include the use of coagulating agents which increase the viscosity of the preservative solution and facilitate treatment by momenta...
P Vinden


Chemical treatment of ten Amazonian timber species of low natural durability
1991 - IRG/WP 3640
The objective of this work was to evaluate the performance of 10 amazonian wood species of low natural durability, to treatment with CCA preservative (2% concentration): it was concluded that all species studied are easily treated with this preservative. The sapwood showed high absorption and total penetration. The heartwood is relatively easy to preserve, exception to Parkia nitidae (Fava), Quale...
C S Neta, B F Vianez


Laboratory tests on the natural durability of timber methods and problems
1984 - IRG/WP 2217
In literature a large variety of test methods is mentioned to examine the natural resistance of timber against fungal attack. This concerns the kind of sampling as well as the test procedure, the test fungi, the duration of test, and the classification of the resistance according to the test results. These variations, however, are of great influence on the test result. Long term exposure will lead...
H Willeitner


Differential susceptibility of living and dead timber to colonisation by sapstain and mould fungi
1998 - IRG/WP 98-10288
Field studies have revealed that when timber is irradiated (i.e. killed) it is more susceptible to colonisation by mould fungi than sapstain fungi. By comparison, freshly sawn timber shows very little mould colonisation, tending to be colonised by sapstain fungi. It appears, therefore that the physiological state of the wood may influence the pattern of colonisation. A laboratory trial was underta...
J R Williams, D J Dickinson, J F Webber


The effect of pretreatments on the impregnation of air-dried sawn Belgian spruce
1988 - IRG/WP 3490
In general the impregnation of airdried spruce results in a variable treatment and limited penetration. This is the result of pit aspiration that occurs during drying of the spruce sapwood and heartwood. Spruce timber is becoming of greater importance in Belgium and hence research for better treatment of this vulnerable wood species is needed. Squared airdried timber of different dimensions were e...
J Van Acker, M Stevens


Blue stain in timber in service. Results of further IRG collaborative tests to compare different artificial weathering systems
1981 - IRG/WP 2146
The previous work described in Document No IRG/WP/286 examined 3 preservatives (1% phenyl mercury succinate - PMS, 5% pentachlorophenol - PCP and 1.5% Preventol A4 - PA4) subjected to 5 different artificial weathering systems (BAM Xenotest, Cuprinol Marr, EMPA Xenotest, Gori Atlas and PRL Marr) and after natural weathering at 5 sites (BAM, Cuprinol, EMPA, Gori and PRL). Results showed good correla...
A F Bravery, D J Dickinson


Previous Page | Next Page