Applicability of wood durability testing methods to bio-based building materials
2015 - IRG/WP 15-20561
It is well known that organic materials may be susceptible to attack from a range of fungal organisms and any bio-based material used in locations where there is the possibility of microbiological activity must be expected to be able to withstand or prevent such attack. There are a wide range of test methods and standards in place to test susceptibility although most of these test individual compo...
S F Curling, B K Stefanowski, E Mansour, G A Ormondroyd


Performance of bio-based building materials – viewpoints from the first year of COST Action FP1303
2015 - IRG/WP 15-20572
Maintaining and expanding the market potential for bio-based building products in indoor and outdoor construction uses remains a key activity for industries in the forestry and biotechnological sector, particularly in Europe. Whilst there are ongoing activities within IRG for collecting and populating a database on performance on wood, the performance data for many other (i.e. non-wood) "environme...
D Jones


Wood protectors to control Bursaphelenchus xylophilus
2015 - IRG/WP 15-30661
Bursaphelenchus xylophilus, the pine wilt nematode (PWN), is a quarantine organism with a high potential to damage Conifer forests in Europe. The European Union is concerned in the protection of forest stands from the propagation and dispersion of this pathogen. In this line, the current control measures have been unsuccessful in preventing the dispersion of this organism, as it continues to be de...
M T Troya, C S Arcos, A Navas, L Robertson, M Conde, F Llinares


Building solid foundations to support market growth of preserved wood in the UK – treatment quality, product approval and the largest national field trial of preservative treated wood in 50 years
2015 - IRG/WP 15-30662
The Wood Protection Association (WPA) has just commissioned Britain’s largest ever durability trial of home grown timber, having contracted Building Research Establishment (BRE) to conduct a long term controlled field trial of sawn and pressure treated British Softwood posts at two sites with differing soil conditions. This large scale Field Trial is the last of an innovative and substantial thr...
E Suttie, G Ewbank


Performance of kiln-dried and air-dried anti-sapstain treated pallet timber under use scenarios against wood discolouring fungi
2015 - IRG/WP 30669
During their lifespan there is a high probability that wooden pallets and packaging material will be exposed to rainfall or rewetting conditions, increasing the risk of growth of discolouring fungi. Kiln-drying of wooden pallets and packaging material without anti-sapstain treatment does not give efficient protection against wood discolouring fungi during rewetting periods. However additional temp...
A Steitz, E Stoyanova, N Pfabigan, R Gründlinger


Remedial treatment of difficult to access timber in buildings
2015 - IRG/WP 15-40691
The quest to understand remedial treatment for timber framing begun following the ‘leaky building crisis’ in New Zealand which came to prominence in 2000. Several in-situ remedial treatment products are used in New Zealand. However, effectiveness of these treatments is still unclear particularly in situations where not all faces of the timber can be assessed. This research was conducted to det...
T Singh, I Simpson, D Page


Effect of exposure site on metal migration from copper azole, alkaline copper quat or chromated copper arsenate treated southern pine decking
2015 - IRG/WP 15-50313
Metal migration from chromated copper arsenate, copper azole or alkaline copper quaternary compound treated southern pine lumber was assessed at sites in Mississippi and Oregon. Metal levels tended to be consistently higher in decks exposed in Mississippi. Rainfall characteristics did differ slightly at the two sites, but the levels did not appear to be of a magnitude that might affect metal mobi...
J J Morrell, H M Barnes


Shells of Coconut and their Durability against Termite Attack
2015 - IRG 15-10853
All tropical and subtropical areas of the Earth are inhabited by termites. In climates with moderate temperatures, they occur less frequently. Especially wood and non-wood materials that grows in tropical areas and used there in timber constructions and woodworking, wood durability and protection against termites should be researched. This paper reports findings from an experimental “AW011” la...
M Dass, A H H Wong, W Unger


Termite Management and the U.S. Experience: A Case for Wood Treatment & Integrated Control
2015 - IRG/WP 15-30678
A brief overview of termite control is given using specific experiences from the U.S.A. Five major types of termite treatment now prevail: soil applied chemical barriers, in-structure chemical barriers (in-situ applied wood and foundation treatments), physical barriers, treated wood and termite baits. In general, ‘stand-alone’ pretreatments or ‘primary’ treatments are often discussed and ...
J D Lloyd, K van den Meiracker


Termiticide Residues in Building Foundation Aggregate Fills After Trench and Surface Applications
2015 - IRG/WP 15-30679
Termiticide concentrations (ppm) in aggregate fill were determined by measuring active ingredient (a.i.) residues of two pyrethroid termiticides, Up-Cyde Pro® 2EC-cypermethrin, and BaseLine® EC-bifenthrin, at 24.0 hours, and then at 6.0- and 12.0-months after ‘horizontal’ surface applications, perimeter ‘trenching and rodding’ applications, or ‘rodding only’ trench applications at lo...
B M Kard, C E Koneman, K T Shelton, C C Luper, R A Grantham


Fungal decay of archaeological waterlogged oak timber: role of the mineral content
2016 - IRG/WP 16-10873
In service, wood foundation poles are subjected to water level fluctuation in soil. While wood is saturated by water only bacterial decay occurs. When oxygen content increases and moisture content decreases, severe fungal attack may occur. To evaluate the long term fungal durability of wood foundation pole in the context of service, 300 years waterlogged archaeological wood poles were used. The oa...
A Besserer, M Letellier, E Fredon, Q Kleindienst, M-L Antoine, C Perrin, J Lallemand, C Rose, M-C Trouy


Modelling the performance of bio-based building materials
2016 - IRG/WP 16-20582
The ‘bio-based economy’ represents a growing area of development globally and covers a wide range of building materials including wood and wood-based products. A ‘bio-based’ material is intentionally made from substances derived from living (or once-living) organisms. In this context it means that the materials and products are made from renewable resources, with the criteria that a renewa...
C Brischke


Screening of fastener resistance in contact with untreated wood using different test designs
2016 - IRG/WP 16-30686
The performance of fasteners in wooden constructions is an important aspect especially regarding corrosion resistance. In an early stage corrosion of fasteners in untreated timber becomes often visible as a discoloration on the surface of the timber resulting in bad appearance of the product followed by complaints. In order to develop an accelerated test for the assessment of fastener performance ...
E Melcher, S Wolf, U Cera


Hygrothermal performance of ventilated wooden cladding
2016 - IRG/WP 16-40733
The risk for an attack of wooden claddings by decay and discolouring fungi strongly depends on the moisture and temperature conditions in the building envelope. The design of the cladding has a major influence on its hygrothermal performance. In the present study, different wooden ventilated cladding designs were investigated at a test house in Mid-Norway for four years. The objective was to incre...
K Nore, U Hundhausen


Creosote leaching from timber bridges in Norway – a practical classification approach
2016 - IRG/WP 16-40744
Creosote is widely used as a wood preservative for highway timber bridges in Norway. However, excessive creosote leaching at various highway timber bridge sites leads to a bad reputation for the use of creosote treated timber constructions and the use of wood in general. Macro- and micro anatomical factors such as amount of heartwood, annual ring width, annual ring orientation, ray- height and com...
A Treu, K Zimmer


Decontamination of sludges, liquids and soils polluted by “class 1, 2 & 3a” and “temporary” wood treatment products from dipping tanks
2016 - IRG/WP 16-50315
Wood is one of the most widely used building materials as it is easy to find and process. As an organic material, time leads to a degradation of its substance, and even more so when it is exposed to pathogens such as fungi, bacteria and insects. In order to try and inhibit this phenomenon, several preservation treatments have been developed and applied thanks to the production of chemical biocides...
A Zaremski, E Wozniak, S Maman, C Zaremski, S Morel


Assessing the natural durability for different tropical timber species using the mini-block test
2017 - IRG/WP 17-10886
The Xylarium in the Royal Museum for Central Africa (RMCA, Tervuren, Belgium) contains over 60,000 wood-samples, comprising over 12,000 species. These samples are of great historical and scientific value yet have a random format, which complicates standard testing. The wood-durability against Coniophora puteana and Trametes versicolor was tested for 36 species. Due to the random sample sizes the s...
V Deklerck, I De Windt, N Defoirdt, J Van den Bulcke, H Beeckman, E Espinoza, J Van Acker


Genetic characterisation of the deathwatch beetle – Call for support
2017 - IRG/WP 17-10890
The deathwatch beetle (Xestobium rufovillosum) is one of the most important pests of historical wood constructions. Further analysis of the exact nature of the feeding habits regarding diet and wood characteristics might deliver answers for controlling this pest. Also there is little known about genetic variability and population structure within the species. For analysis of infested wood and also...
M Höpken, E Melcher, J Trautner


Underground timber constructions from the First World War are well preserved after 100 years
2017 - IRG/WP 17-10897
During the Great War or World War I many underground constructions have been built for protection from shelling. They were an important part of the trench warfare as they were used as an area to rest and carry out other activities such as eating. They would usually range in size from smaller constructions that could hold several men to larger entities that could hold thousands of soldiers. In the ...
J Van Acker, I De Windt, K Haneca, H Beeckman, F Claeys, S Vandenbussche, J Vandewalle, N Robeyst, A Willems


Case study: “Riesenbühlturm”
2017 - IRG/WP 17-20599
In this case study four 7 m long Douglas fir crossbeams were investigated regarding the remaining metal and moisture content. The crossbeams were replaced from a timber tower after 10 years of service in the Black Forest region (South Germany) due to fungal decay. From each of the crossbeams five stem discs were taken and relevant parameters (density, moisture and remaining metal content) were de...
E Melcher, J Müller


Design and performance prediction of timber structures based on a factorization approach
2017 - IRG/WP 17-20603
Service life of timber structures in outdoor conditions is predominantly affected by the climatic conditions in terms of moisture and temperature over time. On the one hand, the two parameters moisture content and temperature determine the exposure-induced dosage that can lead to fungal infestation and subsequent decay. On the other hand, the material resistance of wood stands in opposition to exp...
L Meyer-Veltrup, C Brischke


Modelling of moisture content in timber bridge details
2017 - IRG/WP 17-20613
The design of details is an important aspect in durability design of timber bridges. Details are often considered the weakest points in bridges due to their tendency to trap and accumulate moisture and thus facilitate decay. When designing maintenance plans and inspection intervals, it is important to know how design choices will come to influence the service life. Moreover, service life and wood ...
J Niklewski, C Brischke, E Frühwald Hansson, L Meyer-Veltrup


Comparative Durability of Timber Bridges in the USA
2017 - IRG/WP 17-20615
As engineers begin to utilize life-cycle-cost design approaches for timber bridges, there is a necessity for more reliable data about their durability and expected service life. This paper summarizes a comprehensive effort to assess the current condition of more than one hundred timber highway bridge superstructures throughout the United States. This national study was jointly administered by the ...
J P Wacker, B K Brashaw


Moisture performance of wood determined in laboratory and field trials
2017 - IRG/WP 17-20621
It is widely accepted that wood moisture content (MC) is the key factor when it comes to durability of wooden structures exposed to weathering. The moisture performance of wood and wood-based products has been recognized as key element in wood durability and wood protection. Actually, it should be considered as major component of the material-intrinsic resistance of wood, but never found its way i...
D Kržišnik, N Thaler, B Lesar, M Humar


Moisture content as a quality control parameter in thermally modified timber production
2017 - IRG/WP 17-20622
Quality assurance (QA) or factory production control (FPC) is necessary to ensure a proper production process. The requirements of QA/FPC can result from EN and national standards, quality assurance systems, or producer-specific rules. TMT producers must ensure that the process was correct, and to ensure traceability of products. In addition to the electronic records, the material should be che...
W Scheiding, H Turkulin, S Stein